메뉴 건너뛰기




Volumn 1, Issue 3, 2014, Pages

Nanoporous alumina as templates for multifunctional applications

Author keywords

[No Author keywords available]

Indexed keywords

ALUMINA; NANOSTRUCTURED MATERIALS; NANOWIRES;

EID: 84925287402     PISSN: None     EISSN: 19319401     Source Type: Journal    
DOI: 10.1063/1.4893546     Document Type: Review
Times cited : (241)

References (318)
  • 12
    • 4444289857 scopus 로고
    • 10.1126/science.268.5216.1466
    • H. Masuda and K. Fukuda, Science 268, 1466 (1995). 10.1126/science.268. 5216.1466
    • (1995) Science , vol.268 , pp. 1466
    • Masuda, H.1    Fukuda, K.2
  • 13
    • 33748262432 scopus 로고    scopus 로고
    • Fast fabrication of long-range ordered porous alumina membranes by hard anodization
    • DOI 10.1038/nmat1717, PII NMAT1717
    • W. Lee, R. Ji, U. Gosele, and K. Nielsch, Nat. Mater. 5, 741 (2006). 10.1038/nmat1717 (Pubitemid 44320327)
    • (2006) Nature Materials , vol.5 , Issue.9 , pp. 741-747
    • Lee, W.1    Ji, R.2    Gosele, U.3    Nielsch, K.4
  • 14
    • 66249084159 scopus 로고    scopus 로고
    • 10.1021/la804281v
    • D. Losic and D. Losic, Langmuir 25, 5426 (2009). 10.1021/la804281v
    • (2009) Langmuir , vol.25 , pp. 5426
    • Losic, D.1    Losic, D.2
  • 16
    • 34547790831 scopus 로고    scopus 로고
    • Inorganic hollow nanoparticles and nanotubes in nanomedicine. Part 1. Drug/gene delivery applications
    • DOI 10.1016/j.drudis.2007.06.002, PII S1359644607002486
    • S. J. Son, X. Bai, and S. B. Lee, Drug Discovery Today 12, 650 (2007). 10.1016/j.drudis.2007.06.002 (Pubitemid 47238640)
    • (2007) Drug Discovery Today , vol.12 , Issue.15-16 , pp. 650-656
    • Son, S.J.1    Bai, X.2    Lee, S.B.3
  • 18
    • 0034712032 scopus 로고    scopus 로고
    • Room temperature magnetic quantum cellular automata
    • DOI 10.1126/science.287.5457.1466
    • R. P. Cowburn and M. E. Welland, Science 287, 1466 (2000). 10.1126/science.287.5457.1466 (Pubitemid 30127135)
    • (2000) Science , vol.287 , Issue.5457 , pp. 1466-1468
    • Cowburn, R.P.1    Welland, M.E.2
  • 24
    • 34547728680 scopus 로고    scopus 로고
    • Nano-porous anodic aluminium oxide membranes with 6-19 nm pore diameters formed by a low-potential anodizing process
    • DOI 10.1088/0957-4484/18/34/345302, PII S0957448407493254
    • F. Zhang, X. H. Liu, C. F. Pan, and J. Zhu, Nanotechnology 18, 345302 (2007). 10.1088/0957-4484/18/34/345302 (Pubitemid 47228439)
    • (2007) Nanotechnology , vol.18 , Issue.34 , pp. 345302
    • Zhang, F.1    Liu, X.2    Pan, C.3    Zhu, J.4
  • 25
    • 0034825623 scopus 로고    scopus 로고
    • Square and triangular nanohole array architectures in anodic alumina
    • DOI 10.1002/1521 -4095 (200102)1 3:3<189::AID- ADMA189>3.0.CO;2-Z
    • H. Masuda, H. Asoh, M. Watanabe, K. Nishio, M. Nakao, and T. Tamamura, Adv. Mater. 13, 189 (2001). 10.1002/1521-4095(200102)13:3<189::AID- ADMA189>3.0.CO;2-Z (Pubitemid 32873911)
    • (2001) Advanced Materials , vol.13 , Issue.3 , pp. 189-192
    • Masuda, H.1    Asoh, H.2    Watanabe, M.3    Nishio, K.4    Nakao, M.5    Tamamura, T.6
  • 29
    • 0344894538 scopus 로고    scopus 로고
    • 10.1002/ (SICI)1521- 4095(199904) 11:6<483::AID- ADMA483> 3.0.CO;2-I
    • A. P. Li, F. Muller, A. Birner, K. Nielsch, and U. Gosele, Adv. Mater. 11, 483 (1999). 10.1002/(SICI)1521-4095(199904)11:6<483::AID-ADMA483>3.0. CO;2-I
    • (1999) Adv. Mater. , vol.11 , pp. 483
    • Li, A.P.1    Muller, F.2    Birner, A.3    Nielsch, K.4    Gosele, U.5
  • 30
    • 0034274309 scopus 로고    scopus 로고
    • 10.1002/ 1521-4095 (200009)12: 17<1252:: AID-ADMA1252 >3.0.CO;2-0
    • D. Almawlawi, K. A. Bosnick, A. Osika, and M. Moskovits, Adv. Mater. 12, 1252 (2000). 10.1002/1521-4095(200009)12:17<1252::AID-ADMA1252>3.0.CO;2-0
    • (2000) Adv. Mater. , vol.12 , pp. 1252
    • Almawlawi, D.1    Bosnick, K.A.2    Osika, A.3    Moskovits, M.4
  • 31
    • 0034224641 scopus 로고    scopus 로고
    • 10.1002/ 1521-4095 (200007)12: 14<1031:: AID-ADMA1031> 3.0.CO;2-R
    • H. Masuda, K. Yasui, and K. Nishio, Adv. Mater. 12, 1031 (2000). 10.1002/1521-4095(200007)12:14<1031::AID-ADMA1031>3.0.CO;2-R
    • (2000) Adv. Mater. , vol.12 , pp. 1031
    • Masuda, H.1    Yasui, K.2    Nishio, K.3
  • 32
    • 33745042865 scopus 로고    scopus 로고
    • Observation of isolated nanopores formed by patterned anodic oxidation of aluminum thin films
    • DOI 10.1063/1.2212535
    • Q. Y. Huang, W. K. Lye, and M. L. Reed, Appl. Phys. Lett. 88, 233112 (2006). 10.1063/1.2212535 (Pubitemid 43877764)
    • (2006) Applied Physics Letters , vol.88 , Issue.23 , pp. 233112
    • Huang, Q.1    Lye, W.-K.2    Reed, M.L.3
  • 33
    • 33748279629 scopus 로고    scopus 로고
    • Large-scale ordering of porous Si using anodic aluminum oxide grown by directed self-assembly
    • DOI 10.1063/1.2337560
    • J. Zou, X. Y. Qi, L. W. Tan, and B. J. H. Stadler, Appl. Phys. Lett. 89, 093106 (2006). 10.1063/1.2337560 (Pubitemid 44319979)
    • (2006) Applied Physics Letters , vol.89 , Issue.9 , pp. 093106
    • Zou, J.1    Qi, X.2    Tan, L.3    Stadier, B.J.H.4
  • 34
    • 33750012098 scopus 로고    scopus 로고
    • Fabrication of large-scale patterned gold-nanopillar arrays on a silicon substrate using imprinted porous alumina templates
    • DOI 10.1002/smll.200600311
    • B. Wolfrum, Y. Mourzina, D. Mayer, D. Schwaab, and A. Offenhausser, Small 2, 1256 (2006). 10.1002/smll.200600311 (Pubitemid 44569165)
    • (2006) Small , vol.2 , Issue.11 , pp. 1256-1260
    • Wolfrum, B.1    Mourzina, Y.2    Mayer, D.3    Schwaab, D.4    Offenhausser, A.5
  • 35
    • 16344366047 scopus 로고    scopus 로고
    • Mechanism of guided self-organization producing quasi-monodomain porous alumina
    • DOI 10.1016/j.electacta.2004.11.004, PII S0013468604011181
    • J. Choi, R. B. Wehrspohn, and U. Gosele, Electrochim. Acta 50, 2591 (2005). 10.1016/j.electacta.2004.11.004 (Pubitemid 40467120)
    • (2005) Electrochimica Acta , vol.50 , Issue.13 , pp. 2591-2595
    • Choi, J.1    Wehrspohn, R.B.2    Gosele, U.3
  • 36
    • 33747171412 scopus 로고    scopus 로고
    • Wafer-scale Ni imprint stamps for porous alumina membranes based on interference lithography
    • DOI 10.1002/smll.200600100
    • W. Lee, R. Ji, C. A. Ross, U. Gosele, and K. Nielsch, Small 2, 978 (2006). 10.1002/smll.200600100 (Pubitemid 44230995)
    • (2006) Small , vol.2 , Issue.8-9 , pp. 978-982
    • Lee, W.1    Ji, R.2    Ross, C.A.3    Gosele, U.4    Nielsch, K.5
  • 39
    • 79956053999 scopus 로고    scopus 로고
    • Growth of ordered, single-domain, alumina nanopore arrays with holographically patterned aluminum films
    • DOI 10.1063/1.1517719
    • Z. Sun and H. K. Kim, Appl. Phys. Lett. 81, 3458 (2002). 10.1063/1.1517719 (Pubitemid 35360494)
    • (2002) Applied Physics Letters , vol.81 , Issue.18 , pp. 3458
    • Sun, Z.1    Kim, H.K.2
  • 41
    • 33845236570 scopus 로고    scopus 로고
    • Fabrication and characterization of porous anodic alumina films from impure aluminum foils
    • DOI 10.1149/1.2387104
    • D. Lo and R. A. Budiman, J. Electrochem. Soc. 154, C60 (2007). 10.1149/1.2387104 (Pubitemid 44866319)
    • (2007) Journal of the Electrochemical Society , vol.154 , Issue.1
    • Lo, D.1    Budiman, R.A.2
  • 43
    • 0034076895 scopus 로고    scopus 로고
    • Oxidation kinetics of nickel particles: Comparison between free particles and particles in an oxide matrix
    • DOI 10.1016/S0038-092X(00)00025-6, PII S0038092X00000256, Materials for Windows and Thermal Collectors Part A
    • R. Karmhag, T. Tesfamichael, E. Wackelgard, A. Niklasson, and M. Nygren, Sol. Energy 68, 329 (2000). 10.1016/S0038-092X(00)00025-6 (Pubitemid 30327740)
    • (2000) Solar Energy , vol.68 , Issue.4 , pp. 329-333
    • Karmhag, R.1    Tesfamichael, T.2    Wackelgard, E.3    Niklasson, G.A.4    Nygren, M.5
  • 46
    • 13444257850 scopus 로고    scopus 로고
    • Shape and size control of regularly arrayed nanodots fabricated using ultrathin alumina masks
    • DOI 10.1021/cm048609c
    • Y. Lei and W. K. Chim, Chem. Mater. 17, 580 (2005). 10.1021/cm048609c (Pubitemid 40204173)
    • (2005) Chemistry of Materials , vol.17 , Issue.3 , pp. 580-585
    • Lei, Y.1    Chim, W.-K.2
  • 48
    • 33751228420 scopus 로고    scopus 로고
    • Anodic formation of low-aspect-ratio porous alumina films for metal-oxide sensor application
    • DOI 10.1016/j.electacta.2006.01.081, PII S001346860600421X
    • G. Gorokh, A. Mozalev, D. Solovei, V. Khatko, E. Llobet, and X. Correig, Electrochim. Acta 52, 1771 (2006). 10.1016/j.electacta.2006.01.081 (Pubitemid 44791292)
    • (2006) Electrochimica Acta , vol.52 , Issue.4 , pp. 1771-1780
    • Gorokh, G.1    Mozalev, A.2    Solovei, D.3    Khatko, V.4    Llobet, E.5    Correig, X.6
  • 49
    • 33947113273 scopus 로고    scopus 로고
    • Controlled drug release using nanoporous anodic aluminum oxide on stent
    • DOI 10.1016/j.tsf.2006.10.029, PII S0040609006011710
    • H. J. Kang, D. J. Kim, S. J. Park, J. B. Yoo, and Y. S. Ryu, Thin Solid Films 515, 5184 (2007). 10.1016/j.tsf.2006.10.029 (Pubitemid 46399814)
    • (2007) Thin Solid Films , vol.515 , Issue.12 , pp. 5184-5187
    • Kang, H.-J.1    Kim, D.J.2    Park, S.-J.3    Yoo, J.-B.4    Ryu, Y.S.5
  • 52
    • 84925288614 scopus 로고    scopus 로고
    • Ph.D. thesis, Martin-Luther University.
    • J. Choi, Ph.D. thesis, Martin-Luther University, 2004.
    • (2004)
    • Choi, J.1
  • 53
    • 0021835109 scopus 로고
    • Fundamental studies elucidating anodic barrier-type film growth on aluminium
    • DOI 10.1016/0040-6090(85)90014-8
    • P. Skeldon, K. Shimizu, G. E. Thompson, and G. C. Wood, Thin Solid Films 123, 127 (1985). 10.1016/0040-6090(85)90014-8 (Pubitemid 15493522)
    • (1985) Thin Solid Films , vol.123 , Issue.2 , pp. 127-133
    • Skeldon, P.1    Shimizu, K.2    Thompson, G.E.3    Wood, G.C.4
  • 57
    • 0023145454 scopus 로고
    • Anion incorporation and migration during barrier film formation on aluminium
    • DOI 10.1016/0010-938X(87)90121-1
    • Y. Xu, G. E. Thompson, G. C. Wood, and B. Bethune, Corros. Sci. 27, 83 (1987). 10.1016/0010-938X(87)90121-1 (Pubitemid 17530993)
    • (1987) Corrosion Science , vol.27 , Issue.1 , pp. 83-102
    • Xu, Y.1    Thompson, G.E.2    Wood, G.C.3    Bethune, B.4
  • 58
    • 33846786588 scopus 로고    scopus 로고
    • Anion impurities in porous alumina membranes: Existence and functionality
    • DOI 10.1016/j.micromeso.2006.10.025, PII S1387181106004513
    • D. H. Fan, G. Q. Ding, W. Z. Shen, and M. J. Zheng, Microporous Mesoporous Mater. 100, 154 (2007). 10.1016/j.micromeso.2006.10.025 (Pubitemid 46205379)
    • (2007) Microporous and Mesoporous Materials , vol.100 , Issue.1-3 , pp. 154-159
    • Fan, D.H.1    Ding, G.Q.2    Shen, W.Z.3    Zheng, M.J.4
  • 62
    • 33748698336 scopus 로고
    • 10.1038/290230a0
    • G. E. Thompson and G. C. Wood, Nature 290, 230 (1981). 10.1038/290230a0
    • (1981) Nature , vol.290 , pp. 230
    • Thompson, G.E.1    Wood, G.C.2
  • 63
    • 27644436031 scopus 로고    scopus 로고
    • Self-ordering of anodic porous alumina formed in organic acid electrolytes
    • DOI 10.1016/j.electacta.2005.05.058, PII S0013468605006961
    • S. Ono, M. Saito, and H. Asoh, Electrochim. Acta 51, 827 (2005). 10.1016/j.electacta.2005.05.058 (Pubitemid 41554096)
    • (2005) Electrochimica Acta , vol.51 , Issue.5 , pp. 827-833
    • Ono, S.1    Saito, M.2    Asoh, H.3
  • 67
    • 0036489690 scopus 로고    scopus 로고
    • 10.1063/1.1436499
    • S. K. Thamida and H. C. Chang, Chaos 12, 240 (2002). 10.1063/1.1436499
    • (2002) Chaos , vol.12 , pp. 240
    • Thamida, S.K.1    Chang, H.C.2
  • 69
    • 0017537038 scopus 로고
    • Luminescence, breakdown and colouring of anodic oxide films on aluminium
    • DOI 10.1016/0013-4686(77)85011-1
    • S. Tajima, Electrochim. Acta 22, 995 (1977). 10.1016/0013-4686(77)85011-1 (Pubitemid 8548918)
    • (1977) Electrochimica Acta , vol.22 , Issue.9 , pp. 995-1011
    • Tajima, S.1
  • 70
    • 0005656995 scopus 로고    scopus 로고
    • Self-organized formation of hexagonal pore arrays in anodic alumina
    • DOI 10.1063/1.121004, PII S0003695198035104
    • O. Jessensky, F. Muller, and U. Gosele, Appl. Phys. Lett. 72, 1173 (1998). 10.1063/1.121004 (Pubitemid 128677832)
    • (1998) Applied Physics Letters , vol.72 , Issue.10 , pp. 1173-1175
    • Jessensky, O.1    Muller, F.2    Gosele, U.3
  • 75
    • 54949096158 scopus 로고    scopus 로고
    • 10.1002/adma.200800845
    • Z. X. Su and W. Z. Zhou, Adv. Mater. 20, 3663 (2008). 10.1002/adma.200800845
    • (2008) Adv. Mater. , vol.20 , pp. 3663
    • Su, Z.X.1    Zhou, W.Z.2
  • 77
    • 33845664964 scopus 로고    scopus 로고
    • Temperature influence on well-ordered nanopore structures grown by anodization of aluminium in sulphuric acid
    • DOI 10.1016/j.electacta.2006.07.053, PII S0013468606008127
    • G. D. Sulka and K. G. Parkola, Electrochim. Acta 52, 1880 (2007). 10.1016/j.electacta.2006.07.053 (Pubitemid 44958412)
    • (2007) Electrochimica Acta , vol.52 , Issue.5 , pp. 1880-1888
    • Sulka, G.D.1    Parkola, K.G.2
  • 78
    • 31944439816 scopus 로고    scopus 로고
    • Aluminium anodising in low acidity sulphate baths: Growth mechanism and nanostructure of porous anodic films
    • DOI 10.1007/s10008-005-0665-7
    • G. Patermarakis, J. Solid State Electrochem. 10, 211 (2006). 10.1007/s10008-005-0665-7 (Pubitemid 43190433)
    • (2006) Journal of Solid State Electrochemistry , vol.10 , Issue.4 , pp. 211-222
    • Patermarakis, G.1
  • 83
    • 24644504140 scopus 로고    scopus 로고
    • Fabrication of ideally ordered nanoporous alumina films and integrated alumina nanotubule arrays by high-field anodization
    • DOI 10.1002/adma.200500401
    • S. Z. Chu, K. Wada, S. Inoue, M. Isogai, and A. Yasumori, Adv. Mater. 17, 2115 (2005). 10.1002/adma.200500401 (Pubitemid 41284802)
    • (2005) Advanced Materials , vol.17 , Issue.17 , pp. 2115-2119
    • Chu, S.-Z.1    Wada, K.2    Inoue, S.3    Isogai, M.4    Yasumori, A.5
  • 84
    • 35348949043 scopus 로고    scopus 로고
    • Novel structure of AAO film fabricated by constant current anodization
    • DOI 10.1002/adma.200701284
    • S. Y. Zhao, K. Chan, A. Yelon, and T. Veres, Adv. Mater. 19, 3004 (2007). 10.1002/adma.200701284 (Pubitemid 47597904)
    • (2007) Advanced Materials , vol.19 , Issue.19 , pp. 3004-3007
    • Zhao, S.1    Chan, K.2    Yelon, A.3    Veres, T.4
  • 87
    • 33749526886 scopus 로고    scopus 로고
    • Fabrication of highly ordered nanoporous alumina films by stable high-field anodization
    • DOI 10.1088/0957-4484/17/20/010, PII S0957448406298490, 010
    • Y. B. Li, M. J. Zheng, L. Ma, and W. Z. Shen, Nanotechnology 17, 5101 (2006). 10.1088/0957-4484/17/20/010 (Pubitemid 44523718)
    • (2006) Nanotechnology , vol.17 , Issue.20 , pp. 5101-5105
    • Li, Y.1    Zheng, M.2    Ma, L.3    Shen, W.4
  • 88
    • 36448997050 scopus 로고    scopus 로고
    • Optimum self-ordered nanopore arrays with 130-270 nm interpore distances formed by hard anodization in sulfuric/oxalic acid mixtures
    • DOI 10.1088/0022-3727/40/22/025, PII S0022372707570002
    • M. A. Kashi, A. Ramazani, M. Noormohammadi, M. Zarei, and P. Marashi, J. Phys. D: Appl. Phys. 40, 7032 (2007). 10.1088/0022-3727/40/22/025 (Pubitemid 350163947)
    • (2007) Journal of Physics D: Applied Physics , vol.40 , Issue.22 , pp. 7032-7040
    • Kashi, M.A.1    Ramazani, A.2    Noormohammadi, M.3    Zarei, M.4    Marashi, P.5
  • 90
    • 41849133161 scopus 로고    scopus 로고
    • Structural engineering of nanoporous anodic aluminium oxide by pulse anodization of aluminium
    • DOI 10.1038/nnano.2008.54, PII NNANO200854
    • W. Lee, K. Schwirn, M. Steinhart, E. Pippel, R. Scholz, and U. Gosele, Nat. Nanotechnol. 3, 234 (2008). 10.1038/nnano.2008.54 (Pubitemid 351499397)
    • (2008) Nature Nanotechnology , vol.3 , Issue.4 , pp. 234-239
    • Lee, W.1    Schwirn, K.2    Steinhart, M.3    Pippel, E.4    Scholz, R.5    Gosele, U.6
  • 92
    • 78650100140 scopus 로고    scopus 로고
    • 10.1088/0957-4484/21/48/485304
    • W. Lee and J. C. Kim, Nanotechnology 21, 485304 (2010). 10.1088/0957-4484/21/48/485304
    • (2010) Nanotechnology , vol.21 , pp. 485304
    • Lee, W.1    Kim, J.C.2
  • 93
    • 67650312570 scopus 로고    scopus 로고
    • 10.1002/smll.200801645
    • D. Losic, M. Lillo, and D. Losic, Small 5, 1392 (2009). 10.1002/smll.200801645
    • (2009) Small , vol.5 , pp. 1392
    • Losic, D.1    Lillo, M.2    Losic, D.3
  • 98
    • 84856141207 scopus 로고    scopus 로고
    • 10.1088/0957-4484/23/7/075303
    • G. D. Sulka and K. Hnida, Nanotechnology 23, 075303 (2012). 10.1088/0957-4484/23/7/075303
    • (2012) Nanotechnology , vol.23 , pp. 075303
    • Sulka, G.D.1    Hnida, K.2
  • 99
  • 105
    • 16244401148 scopus 로고    scopus 로고
    • A facile approach to preparation of nanostripes on the electropolished aluminum surface
    • DOI 10.1016/j.matlet.2005.01.036, PII S0167577X0500073X
    • L. B. Kong, Y. Huang, Y. Guo, and H. L. Li, Mater. Lett. 59, 1656 (2005). 10.1016/j.matlet.2005.01.036 (Pubitemid 40454371)
    • (2005) Materials Letters , vol.59 , Issue.13 , pp. 1656-1659
    • Kong, L.-B.1    Huang, Y.2    Guo, Y.3    Li, H.-L.4
  • 111
    • 18244378771 scopus 로고    scopus 로고
    • Differences in the magnetic properties of Co, Fe, and Ni 250-300 nm wide nanowires electrodeposited in amorphous anodized alumina templates
    • DOI 10.1021/cm047870q
    • J. Qin, J. Nogues, M. Mikhaylova, A. Roig, J. S. Munoz, and M. Muhammed, Chem. Mater. 17, 1829 (2005). 10.1021/cm047870q (Pubitemid 40625804)
    • (2005) Chemistry of Materials , vol.17 , Issue.7 , pp. 1829-1834
    • Qin, J.1    Nogues, J.2    Mikhaylova, M.3    Roig, A.4    Munoz, J.S.5    Muhammed, M.6
  • 133
    • 25844494922 scopus 로고    scopus 로고
    • Effect of ac electrodeposition conditions on the growth of high aspect ratio copper nanowires in porous aluminum oxide templates
    • DOI 10.1021/jp051320d
    • N. J. Gerein and J. A. Haber, J. Phys. Chem. B 109, 17372 (2005). 10.1021/jp051320d (Pubitemid 41396182)
    • (2005) Journal of Physical Chemistry B , vol.109 , Issue.37 , pp. 17372-17385
    • Gerein, N.J.1    Haber, J.A.2
  • 134
    • 0037581942 scopus 로고    scopus 로고
    • Uniform nickel deposition into ordered alumina pores by pulsed electrodeposition
    • DOI 10.1002/ (SICI)1521- 4095 (200004)12:8 <582::AID- ADMA582 >3.0.CO;2-3
    • K. Nielsch, F. Muller, A. P. Li, and U. Gosele, Adv. Mater. 12, 582 (2000). 10.1002/(SICI)1521-4095(200004)12:8<582::AID-ADMA582>3.0.CO;2-3 (Pubitemid 30593886)
    • (2000) Advanced Materials , vol.12 , Issue.8 , pp. 582-586
    • Nielsch, K.1    Muller, F.2    Li, A.-P.3    Gosele, U.4
  • 137
    • 39849111658 scopus 로고    scopus 로고
    • Fe nanowires in nanoporous alumina: Geometric effect versus influence of pore walls
    • DOI 10.1021/jp711621v
    • J. M. Baik, M. Schierhorn, and M. Moskovits, J. Phys. Chem. C 112, 2252 (2008). 10.1021/jp711621v (Pubitemid 351316400)
    • (2008) Journal of Physical Chemistry C , vol.112 , Issue.7 , pp. 2252-2255
    • Baik, J.M.1    Schierhorn, M.2    Moskovits, M.3
  • 138
    • 0036802783 scopus 로고    scopus 로고
    • 2 and Si substrates
    • DOI 10.1088/0957-4484/13/5/317, PII S0957448402373379
    • A. Cai, H. Zhang, H. Hua, and Z. Zhang, Nanotechnology 13, 627 (2002). 10.1088/0957-4484/13/5/317 (Pubitemid 35263792)
    • (2002) Nanotechnology , vol.13 , Issue.5 , pp. 627-630
    • Cai, A.1    Zhang, H.2    Hua, H.3    Zhang, Z.4
  • 141
    • 31944447221 scopus 로고    scopus 로고
    • Arrays of electroplated multilayered Co/Cu nanowires with controlled magnetic anisotropy
    • DOI 10.1002/adem.200500162
    • K. R. Pirota and M. Vazquez, Adv. Eng. Mater. 7, 1111 (2005). 10.1002/adem.200500162 (Pubitemid 43188184)
    • (2005) Advanced Engineering Materials , vol.7 , Issue.12 , pp. 1111-1113
    • Pirota, K.R.1    Vazquez, M.2
  • 147
    • 42049103709 scopus 로고    scopus 로고
    • Magnetic domain-wall racetrack memory
    • DOI 10.1126/science.1145799
    • S. S. P. Parkin, M. Hayashi, and L. Thomas, Science 320, 190 (2008). 10.1126/science.1145799 (Pubitemid 351521407)
    • (2008) Science , vol.320 , Issue.5873 , pp. 190-194
    • Parkin, S.S.P.1    Hayashi, M.2    Thomas, L.3
  • 156
    • 36049009457 scopus 로고    scopus 로고
    • Angular dependence of coercivity in magnetic nanotubes
    • DOI 10.1088/0957-4484/18/44/445706, PII S0957448407536512
    • J. Escrig, M. Daub, P. Landeros, K. Nielsch, and D. Altbir, Nanotechnology 18, 445706 (2007). 10.1088/0957-4484/18/44/445706 (Pubitemid 350093307)
    • (2007) Nanotechnology , vol.18 , Issue.44 , pp. 445706
    • Escrig, J.1    Daub, M.2    Landeros, P.3    Nielsch, K.4    Altbir, D.5
  • 167
    • 0035576089 scopus 로고    scopus 로고
    • 10.1063/1.1412275
    • R. Hertel, J. Appl. Phys. 90, 5752 (2001). 10.1063/1.1412275
    • (2001) J. Appl. Phys. , vol.90 , pp. 5752
    • Hertel, R.1
  • 176
  • 178
    • 42149174345 scopus 로고    scopus 로고
    • First-order reversal curve diagrams of magnetic entities with mean interaction field: A physical analysis perspective
    • DOI 10.1063/1.2830955
    • F. Beron, D. Menard, and A. Yelon, J. Appl. Phys. 103, 07D908 (2008). 10.1063/1.2830955 (Pubitemid 351538432)
    • (2008) Journal of Applied Physics , vol.103 , Issue.7
    • Bron, F.1    Mnard, D.2    Yelon, A.3
  • 183
    • 33846809295 scopus 로고    scopus 로고
    • Magnetotransport studies of a single nickel nanowire
    • DOI 10.1088/0957-4484/18/1/015202, PII S095744840731369X
    • Y. Rheem, B. Y. Yoo, W. P. Beyermann, and N. V. Myung, Nanotechnology 18, 015202 (2007). 10.1088/0957-4484/18/1/015202 (Pubitemid 46212161)
    • (2007) Nanotechnology , vol.18 , Issue.1 , pp. 015202
    • Rheem, Y.1    Yoo, B.-Y.2    Beyermann, W.P.3    Myung, N.V.4
  • 203
    • 0035947887 scopus 로고    scopus 로고
    • Magnetism of FE, CO and NI nanowires in self-assembled arrays
    • DOI 10.1088/0953-8984/13/25/201, PII S0953898401201581
    • D. J. Sellmyer, M. Zheng, and R. Skomski, J. Phys.: Condens. Matter 13, R433 (2001). 10.1088/0953-8984/13/25/201 (Pubitemid 32621439)
    • (2001) Journal of Physics Condensed Matter , vol.13 , Issue.25
    • Sellmyer, D.J.1    Zheng, M.2    Skomski, R.3
  • 207
    • 7244243987 scopus 로고
    • 10.1103/PhysRevLett.71.3557
    • H. B. Braun, Phys. Rev. Lett. 71, 3557 (1993). 10.1103/PhysRevLett.71. 3557
    • (1993) Phys. Rev. Lett. , vol.71 , pp. 3557
    • Braun, H.B.1
  • 209
    • 0000050688 scopus 로고
    • 10.1063/1.336671
    • P. Gaunt, J. Appl. Phys. 59, 4129 (1986). 10.1063/1.336671
    • (1986) J. Appl. Phys. , vol.59 , pp. 4129
    • Gaunt, P.1
  • 210
    • 0000389106 scopus 로고
    • 10.1103/PhysRevLett.63.457
    • R. H. Victora, Phys. Rev. Lett. 63, 457 (1989). 10.1103/PhysRevLett.63. 457
    • (1989) Phys. Rev. Lett. , vol.63 , pp. 457
    • Victora, R.H.1
  • 216
    • 0037095160 scopus 로고    scopus 로고
    • Exact nucleation modes in arrays of magnetic particles
    • DOI 10.1063/1.1452251
    • R. Skomski, J. Appl. Phys. 91, 7053 (2002). 10.1063/1.1452251 (Pubitemid 34636724)
    • (2002) Journal of Applied Physics , vol.91 , Issue.10 , pp. 7053
    • Skomski, R.1
  • 229
    • 34248526271 scopus 로고    scopus 로고
    • Ferromagnetic nanotubes by atomic layer deposition in anodic alumina membranes
    • DOI 10.1063/1.2712057
    • M. Daub, M. Knez, U. Goesele, and K. Nielsch, J. Appl. Phys. 101, 09J111 (2007). 10.1063/1.2712057 (Pubitemid 46759476)
    • (2007) Journal of Applied Physics , vol.101 , Issue.9
    • Daub, M.1    Knez, M.2    Goesele, U.3    Nielsch, K.4
  • 236
    • 33748304449 scopus 로고    scopus 로고
    • An easy way to construct an ordered array of nickel nanotubes: The triblock-copolymer-assisted hard-template method
    • DOI 10.1002/adma.200600275
    • F. F. Tao, M. Y. Guan, Y. Jiang, J. M. Zhu, Z. Xu, and Z. L. Xue, Adv. Mater. 18, 2161 (2006). 10.1002/adma.200600275 (Pubitemid 44325311)
    • (2006) Advanced Materials , vol.18 , Issue.16 , pp. 2161-2164
    • Tao, F.1    Guan, M.2    Jiang, Y.3    Zhu, J.4    Xu, Z.5    Xue, Z.6
  • 238
    • 37649026063 scopus 로고    scopus 로고
    • Template synthesis of an array of nickel nanotubules and its magnetic behaviour
    • DOI 10.1002/ 1521-4095 (200111) 13: 21< 1631::AID- ADMA1631> 3.0.CO;2-R
    • J. C. Bao, C. Y. Tie, Z. Xu, Q. F. Zhou, D. Shen, and Q. Ma, Adv. Mater. 13, 1631 (2001). 10.1002/1521-4095(200111)13:21<1631::AID-ADMA1631>3.0. CO;2-R (Pubitemid 33084779)
    • (2001) Advanced Materials , vol.13 , Issue.21
    • Bao, J.1    Tie, C.2    Xu, Z.3    Zhou, Q.4    Shen, D.5    Ma, Q.6
  • 241
    • 0001560484 scopus 로고    scopus 로고
    • 10.1103/PhysRevB.54.8021
    • T. Nakanishi and T. Ando, Phys. Rev. B 54, 8021 (1996). 10.1103/PhysRevB.54.8021
    • (1996) Phys. Rev. B , vol.54 , pp. 8021
    • Nakanishi, T.1    Ando, T.2
  • 242
    • 0001452778 scopus 로고    scopus 로고
    • 10.1103/PhysRevB.58.10583
    • S. Uryu and T. Ando, Phys. Rev. B 58, 10583 (1998). 10.1103/PhysRevB.58. 10583
    • (1998) Phys. Rev. B , vol.58 , pp. 10583
    • Uryu, S.1    Ando, T.2
  • 243
    • 33745048690 scopus 로고    scopus 로고
    • Enhanced transmission through periodic arrays of subwavelength holes: The role of localized waveguide resonances
    • DOI 10.1103/PhysRevLett.96.233901
    • Z. C. Ruan and M. Qiu, Phys. Rev. Lett. 96, 233901 (2006). 10.1103/PhysRevLett.96.233901 (Pubitemid 43877879)
    • (2006) Physical Review Letters , vol.96 , Issue.23 , pp. 233901
    • Ruan, Z.1    Qiu, M.2
  • 245
    • 68149112636 scopus 로고    scopus 로고
    • 10.1002/adma.200900809
    • S. Neusser and D. Grundler, Adv. Mater. 21, 2927 (2009). 10.1002/adma.200900809
    • (2009) Adv. Mater. , vol.21 , pp. 2927
    • Neusser, S.1    Grundler, D.2
  • 267
  • 273
    • 47249129812 scopus 로고    scopus 로고
    • A large-area mesoporous array of magnetic nanostructure with perpendicular anisotropy integrated on Si wafers
    • DOI 10.1088/0957-4484/19/32/325302, PII S0957448408787956
    • M. T. Rahman, N. N. Shams, and C. H. Lai, Nanotechnology 19, 325302 (2008). 10.1088/0957-4484/19/32/325302 (Pubitemid 351991717)
    • (2008) Nanotechnology , vol.19 , Issue.32 , pp. 325302
    • Rahman, M.T.1    Shams, N.N.2    Lai, C.-H.3
  • 290
    • 20444372316 scopus 로고    scopus 로고
    • Optical imaging in drug discovery and diagnostic applications
    • DOI 10.1016/j.addr.2005.01.021, PII S0169409X05000566, Non-Invasive Spectroscopic and Imagign Techniques in Drug Delivery
    • K. Licha and C. Olbrich, Adv. Drug Delivery Rev. 57, 1087 (2005). 10.1016/j.addr.2005.01.021 (Pubitemid 40797571)
    • (2005) Advanced Drug Delivery Reviews , vol.57 , Issue.8 , pp. 1087-1108
    • Licha, K.1    Olbrich, C.2
  • 291
    • 0034296247 scopus 로고    scopus 로고
    • Negative refraction makes a perfect lens
    • DOI 10.1103/PhysRevLett.85.3966
    • J. B. Pendry, Phys. Rev. Lett. 85, 3966 (2000). 10.1103/PhysRevLett.85. 3966 (Pubitemid 32027228)
    • (2000) Physical Review Letters , vol.85 , Issue.18 , pp. 3966-3969
    • Pendry, J.B.1
  • 295
    • 0037458417 scopus 로고    scopus 로고
    • 10.1103/PhysRevLett.90.077405
    • D. R. Smith and D. Schurig, Phys. Rev. Lett. 90, 077405 (2003). 10.1103/PhysRevLett.90.077405
    • (2003) Phys. Rev. Lett. , vol.90 , pp. 077405
    • Smith, D.R.1    Schurig, D.2
  • 299
    • 44649134569 scopus 로고    scopus 로고
    • 10.1103/PhysRevB.77.233101
    • W. T. Lu and S. Sridhar, Phys. Rev. B 77, 233101 (2008). 10.1103/PhysRevB.77.233101
    • (2008) Phys. Rev. B , vol.77 , pp. 233101
    • Lu, W.T.1    Sridhar, S.2
  • 307
    • 38849174818 scopus 로고    scopus 로고
    • Complex thermoelectric materials
    • DOI 10.1038/nmat2090, PII NMAT2090
    • G. J. Snyder and E. S. Toberer, Nat. Mater. 7, 105 (2008). 10.1038/nmat2090 (Pubitemid 351187650)
    • (2008) Nature Materials , vol.7 , Issue.2 , pp. 105-114
    • Snyder, G.J.1    Toberer, E.S.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.