Surface characterisation and bonding of Y-TZP following non-thermal plasma treatment

Author keywords

Adhesion; Contact angle; Microtensile; Non thermal plasma; Surface energy; Y TZP

Indexed keywords

ALUMINUM OXIDE; ARGON; BIOMATERIAL; CARBON; DENTAL MATERIAL; INORGANIC COMPOUND; METHACRYLIC ACID DERIVATIVE; METHACRYLOYLOXYDECYL DIHYDROGEN PHOSPHATE; OXYGEN; RELY X UNICEM; RESIN; RESIN CEMENT; SILICON CARBIDE; SILICON DERIVATIVE; SILICON DIOXIDE; YTTRIA STABILIZED TETRAGONAL ZIRCONIA; YTTRIUM; Z100 COMPOSITE RESIN; ZIRCONIUM;

EID: 84873731111     PISSN: 03005712     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.jdent.2012.10.002     Document Type: Article
Times cited : (119)

References (46)
  • 5
    • 71349083001 scopus 로고    scopus 로고
    • Influence of air-abrasion on zirconia ceramic bonding using an adhesive composite resin
    • B. Yang, A. Barloi, and M. Kern Influence of air-abrasion on zirconia ceramic bonding using an adhesive composite resin Dental Materials 26 2010 44 50
    • (2010) Dental Materials , vol.26 , pp. 44-50
    • Yang, B.1    Barloi, A.2    Kern, M.3
  • 7
    • 43049151150 scopus 로고    scopus 로고
    • Influence of different surface treatments on the short-term bond strength and durability between a zirconia post and a composite resin core material
    • G. Akgungor, D. Sen, and M. Aydin Influence of different surface treatments on the short-term bond strength and durability between a zirconia post and a composite resin core material Journal of Prosthetic Dentistry 99 2008 388 399
    • (2008) Journal of Prosthetic Dentistry , vol.99 , pp. 388-399
    • Akgungor, G.1    Sen, D.2    Aydin, M.3
  • 9
    • 2442423176 scopus 로고    scopus 로고
    • Effect of post-silanization drying on the bond strength of composite to ceramic
    • C. Shen, W.S. Oh, and J.R. Williams Effect of post-silanization drying on the bond strength of composite to ceramic Journal of Prosthetic Dentistry 91 2004 453 458
    • (2004) Journal of Prosthetic Dentistry , vol.91 , pp. 453-458
    • Shen, C.1    Oh, W.S.2    Williams, J.R.3
  • 11
    • 33845290307 scopus 로고    scopus 로고
    • Durability of the resin bond strength to zirconia ceramic after using different surface conditioning methods
    • M. Wolfart, F. Lehmann, S. Wolfart, and M. Kern Durability of the resin bond strength to zirconia ceramic after using different surface conditioning methods Dental Materials 23 2007 45 50
    • (2007) Dental Materials , vol.23 , pp. 45-50
    • Wolfart, M.1    Lehmann, F.2    Wolfart, S.3    Kern, M.4
  • 12
    • 30344433724 scopus 로고    scopus 로고
    • Effect of thermocycling on bond strength of luting cements to zirconia ceramic
    • H. Luthy, O. Loeffel, and C.H. Hammerle Effect of thermocycling on bond strength of luting cements to zirconia ceramic Dental Materials 22 2006 195 200
    • (2006) Dental Materials , vol.22 , pp. 195-200
    • Luthy, H.1    Loeffel, O.2    Hammerle, C.H.3
  • 13
    • 0034208413 scopus 로고    scopus 로고
    • Long-term resin bond strength to zirconia ceramic
    • S.M. Wegner, and M. Kern Long-term resin bond strength to zirconia ceramic Journal of Adhesive Dentistry 2 2000 139 147
    • (2000) Journal of Adhesive Dentistry , vol.2 , pp. 139-147
    • Wegner, S.M.1    Kern, M.2
  • 16
    • 42449099988 scopus 로고    scopus 로고
    • Effect of various surface conditioning methods on the adhesion of dual-cure resin cement with MDP functional monomer to zirconia after thermal aging
    • M. Ozcan, H. Nijhuis, and L.F. Valandro Effect of various surface conditioning methods on the adhesion of dual-cure resin cement with MDP functional monomer to zirconia after thermal aging Dental Materials Journal 27 2008 99 104
    • (2008) Dental Materials Journal , vol.27 , pp. 99-104
    • Ozcan, M.1    Nijhuis, H.2    Valandro, L.F.3
  • 19
    • 79953243766 scopus 로고    scopus 로고
    • Development of a novel surface modification for improved bonding to zirconia
    • J.R. Piascik, S.D. Wolter, and B.R. Stoner Development of a novel surface modification for improved bonding to zirconia Dental Materials 27 2011 99 105
    • (2011) Dental Materials , vol.27 , pp. 99-105
    • Piascik, J.R.1    Wolter, S.D.2    Stoner, B.R.3
  • 27
  • 28
    • 78651248334 scopus 로고    scopus 로고
    • Adhesion/cementation to zirconia and other non-silicate ceramics: Where are we now?
    • J.Y. Thompson, B.R. Stoner, J.R. Piascik, and R. Smith Adhesion/cementation to zirconia and other non-silicate ceramics: where are we now? Dental Materials 27 2011 71 82
    • (2011) Dental Materials , vol.27 , pp. 71-82
    • Thompson, J.Y.1    Stoner, B.R.2    Piascik, J.R.3    Smith, R.4
  • 29
    • 58149229394 scopus 로고    scopus 로고
    • Influence of surface treatments and resin cement selection on bonding to densely-sintered zirconium-oxide ceramic
    • R.C. de Oyague, F. Monticelli, M. Toledano, E. Osorio, M. Ferrari, and R. Osorio Influence of surface treatments and resin cement selection on bonding to densely-sintered zirconium-oxide ceramic Dental Materials 25 2009 172 179
    • (2009) Dental Materials , vol.25 , pp. 172-179
    • De Oyague, R.C.1    Monticelli, F.2    Toledano, M.3    Osorio, E.4    Ferrari, M.5    Osorio, R.6
  • 30
    • 59349112720 scopus 로고    scopus 로고
    • Effect of water aging on microtensile bond strength of dual-cured resin cements to pre-treated sintered zirconium-oxide ceramics
    • R.C. Oyague, F. Monticelli, M. Toledano, E. Osorio, M. Ferrari, and R. Osorio Effect of water aging on microtensile bond strength of dual-cured resin cements to pre-treated sintered zirconium-oxide ceramics Dental Materials 25 2009 392 399
    • (2009) Dental Materials , vol.25 , pp. 392-399
    • Oyague, R.C.1    Monticelli, F.2    Toledano, M.3    Osorio, E.4    Ferrari, M.5    Osorio, R.6
  • 31
    • 0032017987 scopus 로고    scopus 로고
    • Bonding to alumina ceramic in restorative dentistry: Clinical results over up to 5 years
    • M. Kern, and J.R. Strub Bonding to alumina ceramic in restorative dentistry: clinical results over up to 5 years Journal of Dentistry 26 1998 245 249
    • (1998) Journal of Dentistry , vol.26 , pp. 245-249
    • Kern, M.1    Strub, J.R.2
  • 33
    • 70349481496 scopus 로고    scopus 로고
    • Surface conditioning influences zirconia ceramic bonding
    • M. Kern, A. Barloi, and B. Yang Surface conditioning influences zirconia ceramic bonding Journal of Dental Research 88 2009 817 822
    • (2009) Journal of Dental Research , vol.88 , pp. 817-822
    • Kern, M.1    Barloi, A.2    Yang, B.3
  • 34
    • 69549124443 scopus 로고    scopus 로고
    • Resin bonding to oxide ceramics for dental restorations
    • M. Kern Resin bonding to oxide ceramics for dental restorations Journal of Adhesion Science and Technology 23 2009 1097 1111
    • (2009) Journal of Adhesion Science and Technology , vol.23 , pp. 1097-1111
    • Kern, M.1
  • 35
    • 34548648100 scopus 로고    scopus 로고
    • Influence of surface treatment and simulated aging on bond strengths of luting agents to zirconia
    • M.B. Blatz, G. Chiche, S. Holst, and A. Sadan Influence of surface treatment and simulated aging on bond strengths of luting agents to zirconia Quintessence International 38 2007 745 753
    • (2007) Quintessence International , vol.38 , pp. 745-753
    • Blatz, M.B.1    Chiche, G.2    Holst, S.3    Sadan, A.4
  • 40
    • 33847107611 scopus 로고    scopus 로고
    • 2.0 bonding to contaminated zirconia ceramic after different cleaning procedures
    • A.C. Quaas, B. Yang, M. Kern, and F. Panavia 2.0 bonding to contaminated zirconia ceramic after different cleaning procedures Dental Materials 23 2007 506 512
    • (2007) Dental Materials , vol.23 , pp. 506-512
    • Quaas, A.C.1    Yang, B.2    Kern, M.3    Panavia, F.4
  • 41
    • 34247381199 scopus 로고    scopus 로고
    • Characterization and surface treatment effects on topography of a glass-infiltrated alumina/zirconia-reinforced ceramic
    • A. Della Bona, T.A. Donassollo, F.F. Demarco, A.A. Barrett, and J.J. Mecholsky Jr. Characterization and surface treatment effects on topography of a glass-infiltrated alumina/zirconia-reinforced ceramic Dental Materials 23 2007 769 775
    • (2007) Dental Materials , vol.23 , pp. 769-775
    • Della Bona, A.1    Donassollo, T.A.2    Demarco, F.F.3    Barrett, A.A.4    Mecholsky, Jr.J.J.5
  • 42
    • 77956929149 scopus 로고    scopus 로고
    • Effect of sandblasting and various metal primers on the shear bond strength of resin cement to Y-TZP ceramic
    • J.-Y. Yun, S.-R. Ha, J.-B. Lee, and S.-H. Kim Effect of sandblasting and various metal primers on the shear bond strength of resin cement to Y-TZP ceramic Dental Materials 26 2010 650 658
    • (2010) Dental Materials , vol.26 , pp. 650-658
    • Yun, J.-Y.1    Ha, S.-R.2    Lee, J.-B.3    Kim, S.-H.4
  • 43
    • 32044438490 scopus 로고    scopus 로고
    • Microtensile bond strength of a resin cement to glass infiltrated zirconia-reinforced ceramic: The effect of surface conditioning
    • R. Amaral, M. Ozcan, M.A. Bottino, and L.F. Valandro Microtensile bond strength of a resin cement to glass infiltrated zirconia-reinforced ceramic: the effect of surface conditioning Dental Materials 22 2006 283 290
    • (2006) Dental Materials , vol.22 , pp. 283-290
    • Amaral, R.1    Ozcan, M.2    Bottino, M.A.3    Valandro, L.F.4
  • 44
    • 33750813035 scopus 로고    scopus 로고
    • Static solvent contact angle measurements, surface free energy and wettability determination of various self-assembled monolayers on silicon dioxide
    • D. Janssen, R. De Palma, S. Verlaak, P. Heremans, and W. Dehaen Static solvent contact angle measurements, surface free energy and wettability determination of various self-assembled monolayers on silicon dioxide Thin Solid Films 515 2006 1433 1438
    • (2006) Thin Solid Films , vol.515 , pp. 1433-1438
    • Janssen, D.1    De Palma, R.2    Verlaak, S.3    Heremans, P.4    Dehaen, W.5
  • 45
    • 84929752052 scopus 로고    scopus 로고
    • Cambridge University Press New York
    • A. Fridman Plasma Chemistry 2008 Cambridge University Press New York
    • (2008) Plasma Chemistry
    • Fridman, A.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.