Volumn 25, Issue 9, 2009, Pages 1116-1121

Surface modification for enhanced silanation of zirconia ceramics

Author keywords

Adhesion; Chemical functionalization; Microtensile; Silanation; Zirconia

Indexed keywords

ADHESIVE BONDING; ADHESIVE FAILURE; ANALYSIS OF FAILURE MODES; BONDING TECHNIQUES; CHEMICAL BONDINGS; CHEMICAL FUNCTIONALIZATION; COHESIVE FAILURES; COMPOSITE BLOCKS; COMPOSITE FAILURE; CROSSHEAD SPEED; DATA SUPPORT; DENTAL CERAMIC; FRACTURE SURFACES; GASPHASE; HIGH STRENGTH; MICROTENSILE; MICROTENSILE TESTING; PEAK STRESS; PRACTICAL METHOD; RESIN CEMENT; SEED LAYER; SILANATION; SILANE PRETREATMENT; STRENGTH VALUES; SURFACE MODIFICATION; TENSILE FORCES; ULTRA-THIN; ZIRCONIA CERAMIC;

EID: 67651119977     PISSN: 01095641     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.dental.2009.03.008     Document Type: Article
Times cited : (140)

References (30)
  • 1
    • 0038644503 scopus 로고    scopus 로고
    • Resin-ceramic bonding: a review of the literature
    • Blatz M.B., Sadan A., and Kern M. Resin-ceramic bonding: a review of the literature. J Prosthet Dent 89 2 (2003) 268-274
    • (2003) J Prosthet Dent , vol.89 , Issue.2 , pp. 268-274
    • Blatz, M.B.1    Sadan, A.2    Kern, M.3
  • 2
    • 0023413139 scopus 로고
    • Shear strength of the composite bond to etched porcelain
    • Stangel I., Nathanson D., and Hsu C.S. Shear strength of the composite bond to etched porcelain. J Dent Res 66 9 (1987) 1460-1465
    • (1987) J Dent Res , vol.66 , Issue.9 , pp. 1460-1465
    • Stangel, I.1    Nathanson, D.2    Hsu, C.S.3
  • 3
    • 0024616164 scopus 로고
    • Porcelain-to-composite bond strengths using four organosilane materials
    • Bailey J.H. Porcelain-to-composite bond strengths using four organosilane materials. J Prosthet Dent 61 1 (1989) 174-177
    • (1989) J Prosthet Dent , vol.61 , Issue.1 , pp. 174-177
    • Bailey, J.H.1
  • 4
    • 0027336936 scopus 로고
    • Molecular orientation of silane at the surface of colloidal silica
    • Soderholm K.J.M., and Shang S.W. Molecular orientation of silane at the surface of colloidal silica. J Dent Res 72 6 (1993) 1050-1054
    • (1993) J Dent Res , vol.72 , Issue.6 , pp. 1050-1054
    • Soderholm, K.J.M.1    Shang, S.W.2
  • 5
    • 0028523833 scopus 로고
    • Effect of porcelain surface treatments on bond strengths of composite resin bonded to porcelain
    • Thurmond J.W., Barkmeier W.W., and Wilwerding T.M. Effect of porcelain surface treatments on bond strengths of composite resin bonded to porcelain. J Prosthet Dent 72 3 (1994) 355-359
    • (1994) J Prosthet Dent , vol.72 , Issue.3 , pp. 355-359
    • Thurmond, J.W.1    Barkmeier, W.W.2    Wilwerding, T.M.3
  • 6
    • 0029299001 scopus 로고
    • Adhesion of composite to porcelain with various surface conditions
    • Aida M., Hayakawa T., and Mizukawa K. Adhesion of composite to porcelain with various surface conditions. J Prosthet Dent 73 4 (1995) 464-470
    • (1995) J Prosthet Dent , vol.73 , Issue.4 , pp. 464-470
    • Aida, M.1    Hayakawa, T.2    Mizukawa, K.3
  • 7
    • 0036497561 scopus 로고    scopus 로고
    • Bond durability of the resin-bonded and silane treated ceramic surface
    • Hooshmand T., Van Noort R., and Keshvad A. Bond durability of the resin-bonded and silane treated ceramic surface. Dent Mater 18 (2002) 179-188
    • (2002) Dent Mater , vol.18 , pp. 179-188
    • Hooshmand, T.1    Van Noort, R.2    Keshvad, A.3
  • 8
    • 0042994079 scopus 로고    scopus 로고
    • Silane treatment effects on glass/resin interfacial shear strengths
    • Debnath S., Wunder S.L., McCool J.I., and Baran G.R. Silane treatment effects on glass/resin interfacial shear strengths. Dent Mater 19 (2003) 441-448
    • (2003) Dent Mater , vol.19 , pp. 441-448
    • Debnath, S.1    Wunder, S.L.2    McCool, J.I.3    Baran, G.R.4
  • 9
    • 2442423176 scopus 로고    scopus 로고
    • Effect of post-silanization drying on the bond strength of composite to ceramic
    • Shen C., Oh W.-S., and Williams J.R. Effect of post-silanization drying on the bond strength of composite to ceramic. J Prosthet Dent 91 4 (2004) 453-458
    • (2004) J Prosthet Dent , vol.91 , Issue.4 , pp. 453-458
    • Shen, C.1    Oh, W.-S.2    Williams, J.R.3
  • 11
    • 32044438490 scopus 로고    scopus 로고
    • Microtensile bond strength of a resin cement to glass infiltrated zirconia-reinforced ceramic: the effect of surface conditioning
    • Amaral R., Ozcan M., Bottino M.A., and Valandro L.F. Microtensile bond strength of a resin cement to glass infiltrated zirconia-reinforced ceramic: the effect of surface conditioning. Dent Mater 22 (2006) 283-290
    • (2006) Dent Mater , vol.22 , pp. 283-290
    • Amaral, R.1    Ozcan, M.2    Bottino, M.A.3    Valandro, L.F.4
  • 12
    • 27744579062 scopus 로고    scopus 로고
    • Bond strength of composite luting cement to zirconia ceramic surfaces
    • Derand T., Molin M., and Kvam K. Bond strength of composite luting cement to zirconia ceramic surfaces. Dent Mater 21 (2005) 1158-1162
    • (2005) Dent Mater , vol.21 , pp. 1158-1162
    • Derand, T.1    Molin, M.2    Kvam, K.3
  • 13
    • 0031598657 scopus 로고    scopus 로고
    • Bonding to zirconia ceramic: adhesion methods and their durability
    • Kern M., and Wegner S.M. Bonding to zirconia ceramic: adhesion methods and their durability. Dent Mater 14 (1998) 64-71
    • (1998) Dent Mater , vol.14 , pp. 64-71
    • Kern, M.1    Wegner, S.M.2
  • 14
    • 33746275632 scopus 로고    scopus 로고
    • The effect of a novel saline blend system on resin bond strength to silica-coated Ti substrate
    • Matilinna J.P., Lassila L.V.J., and Vallittu P.K. The effect of a novel saline blend system on resin bond strength to silica-coated Ti substrate. J Dent 34 (2006) 436-443
    • (2006) J Dent , vol.34 , pp. 436-443
    • Matilinna, J.P.1    Lassila, L.V.J.2    Vallittu, P.K.3
  • 15
    • 33847415776 scopus 로고    scopus 로고
    • Effects of ceramic treatments on the bond strength of an adhesive luting agent to CAD-CAM ceramic
    • Peumans M., Hikita K., Munck J.De., Van Landuyt K., Poitevin A., Lambrechts P., et al. Effects of ceramic treatments on the bond strength of an adhesive luting agent to CAD-CAM ceramic. J Dent 35 (2007) 282-288
    • (2007) J Dent , vol.35 , pp. 282-288
    • Peumans, M.1    Hikita, K.2    Munck, J.De.3    Van Landuyt, K.4    Poitevin, A.5    Lambrechts, P.6
  • 16
    • 0041419469 scopus 로고    scopus 로고
    • Effect of ceramic surface treatment on the shear bond strengths of two resin luting agents to all-ceramic materials
    • Saygili G., and Sahmali S. Effect of ceramic surface treatment on the shear bond strengths of two resin luting agents to all-ceramic materials. J Oral Rehab 30 (2003) 758-764
    • (2003) J Oral Rehab , vol.30 , pp. 758-764
    • Saygili, G.1    Sahmali, S.2
  • 17
    • 33744789998 scopus 로고    scopus 로고
    • Effect of zirconium-oxide ceramic surface treatments on the bond strength to adhesive resin
    • Stsu S.S., Kilicarslan M.A., Kucuk H.C., and Aka P.S. Effect of zirconium-oxide ceramic surface treatments on the bond strength to adhesive resin. J Prosthet Dent 95 4 (2006) 430-436
    • (2006) J Prosthet Dent , vol.95 , Issue.4 , pp. 430-436
    • Stsu, S.S.1    Kilicarslan, M.A.2    Kucuk, H.C.3    Aka, P.S.4
  • 18
    • 1942456928 scopus 로고    scopus 로고
    • In vitro evaluation of shear bond strengths of resin to densely-sintered high-purity zirconium-oxide ceramic after long-term storage and thermal cycling
    • Blatz M.B., Sadan A., Martin J., and Lang B. In vitro evaluation of shear bond strengths of resin to densely-sintered high-purity zirconium-oxide ceramic after long-term storage and thermal cycling. J Prosthet Dent 91 (2004) 356-362
    • (2004) J Prosthet Dent , vol.91 , pp. 356-362
    • Blatz, M.B.1    Sadan, A.2    Martin, J.3    Lang, B.4
  • 19
    • 13444310582 scopus 로고    scopus 로고
    • Effect of surface treatments on the resin bond to zirconium-based ceramic
    • Bottino M.A., Valandro L.F., Scotti R., and Buso L. Effect of surface treatments on the resin bond to zirconium-based ceramic. Int J Prosthodont 18 (2005) 60-65
    • (2005) Int J Prosthodont , vol.18 , pp. 60-65
    • Bottino, M.A.1    Valandro, L.F.2    Scotti, R.3    Buso, L.4
  • 20
    • 1842855215 scopus 로고    scopus 로고
    • Durability of the resin bond strength to the alumina ceramic Procera
    • Hummel M., and Kern M. Durability of the resin bond strength to the alumina ceramic Procera. Dent Mater 20 (2004) 498-508
    • (2004) Dent Mater , vol.20 , pp. 498-508
    • Hummel, M.1    Kern, M.2
  • 21
    • 33646153045 scopus 로고    scopus 로고
    • Bonding of resin composite sureface treatments on the tensile bond strength of composite resin to all-ceramic coping materials
    • Kumbuloglu O., Lassila L.V.J., User A., and Vallittu P.K. Bonding of resin composite sureface treatments on the tensile bond strength of composite resin to all-ceramic coping materials. Oper Dent 31 2 (2006) 248-255
    • (2006) Oper Dent , vol.31 , Issue.2 , pp. 248-255
    • Kumbuloglu, O.1    Lassila, L.V.J.2    User, A.3    Vallittu, P.K.4
  • 22
    • 30344433724 scopus 로고    scopus 로고
    • Effect of thermocycling on bond strength of luting cements to zirconia ceramic
    • Lüthy J., Loeffel O., and Hammerle C.H.F. Effect of thermocycling on bond strength of luting cements to zirconia ceramic. Dent Mater 22 (2006) 195-200
    • (2006) Dent Mater , vol.22 , pp. 195-200
    • Lüthy, J.1    Loeffel, O.2    Hammerle, C.H.F.3
  • 23
    • 33645419309 scopus 로고    scopus 로고
    • Bonding of dual-cured resin cement to zirconia ceramic using phosphate acid ester monomer and zirconate coupler
    • Yoshida K., Tsuo Y., and Atsuta M. Bonding of dual-cured resin cement to zirconia ceramic using phosphate acid ester monomer and zirconate coupler. J Biomed Mater Res B 77 1 (2006) 28-33
    • (2006) J Biomed Mater Res B , vol.77 , Issue.1 , pp. 28-33
    • Yoshida, K.1    Tsuo, Y.2    Atsuta, M.3
  • 24
    • 33745743170 scopus 로고    scopus 로고
    • Bond strength of a resin cement to high-alumina and zirconia-reinforced ceramics: the effect of surface conditioning
    • Valandro L.F., Özcan M., Bottino M.A., Bottina M.C., Scotti R., and Della Bona A. Bond strength of a resin cement to high-alumina and zirconia-reinforced ceramics: the effect of surface conditioning. J Adhes Dent 8 (2006) 175-181
    • (2006) J Adhes Dent , vol.8 , pp. 175-181
    • Valandro, L.F.1    Özcan, M.2    Bottino, M.A.3    Bottina, M.C.4    Scotti, R.5    Della Bona, A.6
  • 25
    • 47249119701 scopus 로고    scopus 로고
    • Innovations in bonding zirconia-based materials: Part I
    • Aboushelib M.N., Matinlinna J.P., Salameh Z., and Ounsi H. Innovations in bonding zirconia-based materials: Part I. Dent Mater 24 (2008) 1268-1272
    • (2008) Dent Mater , vol.24 , pp. 1268-1272
    • Aboushelib, M.N.1    Matinlinna, J.P.2    Salameh, Z.3    Ounsi, H.4
  • 26
    • 0141727597 scopus 로고    scopus 로고
    • Effect of surface conditioning methods on the bond strength of luting cement to ceramics
    • Ozcan M., and Vallittu P.K. Effect of surface conditioning methods on the bond strength of luting cement to ceramics. Dental Mater 19 8 (2003) 725-731
    • (2003) Dental Mater , vol.19 , Issue.8 , pp. 725-731
    • Ozcan, M.1    Vallittu, P.K.2
  • 27
    • 32144435105 scopus 로고    scopus 로고
    • Durable anti stiction coatings by molecular vapor deposition (MVD)
    • Kobrin B., Chinn J., and Ashurst R.W. Durable anti stiction coatings by molecular vapor deposition (MVD). NSTI Nanotech 2 (2005) 247-350
    • (2005) NSTI Nanotech , vol.2 , pp. 247-350
    • Kobrin, B.1    Chinn, J.2    Ashurst, R.W.3
  • 28
    • 67651110718 scopus 로고    scopus 로고
    • US Patent 2006/0251765 A1, Applied MicroStructures, Inc
    • US Patent 2006/0251765 A1, Applied MicroStructures, Inc.
  • 29
    • 0029372422 scopus 로고
    • Shear versus tensile bond strength of resin composite bonded to ceramic
    • Della Bona A., and van Noort R. Shear versus tensile bond strength of resin composite bonded to ceramic. J Dent Res 74 (1995) 1591-1596
    • (1995) J Dent Res , vol.74 , pp. 1591-1596
    • Della Bona, A.1    van Noort, R.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.