메뉴 건너뛰기




Volumn 26, Issue 1, 2010, Pages 44-50

Influence of air-abrasion on zirconia ceramic bonding using an adhesive composite resin

Author keywords

Air abrasion; Bonding; Self adhesive luting resin composite; Zirconia ceramic

Indexed keywords

ABRASION PRESSURES; BOND STRENGTH; COMPOSITE RESINS; CROSSHEAD SPEED; LOW PRESSURES; LUTING COMPOSITES; LUTING RESINS; MECHANICAL STRENGTH; PARTICLE ABRASION; PLEXIGLAS TUBE; REDUCED PRESSURE; RESIN-BOND; SELF-ADHESIVE; SURFACE CONDITIONING; SURFACE CONDITIONS; TENSILE BOND STRENGTH; THERMOCYCLING; UNIVERSAL TESTING MACHINES; ZIRCONIA CERAMIC;

EID: 71349083001     PISSN: 01095641     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.dental.2009.08.008     Document Type: Article
Times cited : (209)

References (34)
  • 1
    • 0038644503 scopus 로고    scopus 로고
    • Resin-ceramic bonding: a review of the literature
    • Blatz M.B., Sadan A., and Kern M. Resin-ceramic bonding: a review of the literature. J Prosthet Dent 89 (2003) 268-274
    • (2003) J Prosthet Dent , vol.89 , pp. 268-274
    • Blatz, M.B.1    Sadan, A.2    Kern, M.3
  • 2
    • 69549124443 scopus 로고    scopus 로고
    • Resin bonding to oxide ceramics for dental restorations
    • Kern M. Resin bonding to oxide ceramics for dental restorations. J Adhes Sci Technol 23 (2009) 1097-1111
    • (2009) J Adhes Sci Technol , vol.23 , pp. 1097-1111
    • Kern, M.1
  • 3
    • 34548648100 scopus 로고    scopus 로고
    • Influence of surface treatment and simulated aging on bond strengths of luting agents to zirconia
    • Blatz M.B., Chiche G., Holst S., and Sadan A. Influence of surface treatment and simulated aging on bond strengths of luting agents to zirconia. Quintessence Int 38 (2007) 745-753
    • (2007) Quintessence Int , vol.38 , pp. 745-753
    • Blatz, M.B.1    Chiche, G.2    Holst, S.3    Sadan, A.4
  • 4
    • 30344433724 scopus 로고    scopus 로고
    • Effect of thermocycling on bond strength of luting cements to zirconia ceramic
    • Lüthy H., Loeffel O., and Hämmerle C.H. Effect of thermocycling on bond strength of luting cements to zirconia ceramic. Dent Mater 22 (2006) 195-200
    • (2006) Dent Mater , vol.22 , pp. 195-200
    • Lüthy, H.1    Loeffel, O.2    Hämmerle, C.H.3
  • 5
    • 19744367539 scopus 로고    scopus 로고
    • The shear bond strength between luting cements and zirconia ceramics after two pre-treatments
    • Piwowarczyk A., Lauer H.C., and Sorensen J.A. The shear bond strength between luting cements and zirconia ceramics after two pre-treatments. Oper Dent 30 (2005) 382-388
    • (2005) Oper Dent , vol.30 , pp. 382-388
    • Piwowarczyk, A.1    Lauer, H.C.2    Sorensen, J.A.3
  • 7
    • 0031598657 scopus 로고    scopus 로고
    • Bonding to zirconia ceramic: adhesion methods and their durability
    • Kern M., and Wegner S.M. Bonding to zirconia ceramic: adhesion methods and their durability. Dent Mater 14 (1998) 64-71
    • (1998) Dent Mater , vol.14 , pp. 64-71
    • Kern, M.1    Wegner, S.M.2
  • 9
    • 0141727597 scopus 로고    scopus 로고
    • Effect of surface conditioning methods on the bond strength of luting cement to ceramics
    • Özcan M., and Vallittu P.K. Effect of surface conditioning methods on the bond strength of luting cement to ceramics. Dent Mater 19 (2003) 725-731
    • (2003) Dent Mater , vol.19 , pp. 725-731
    • Özcan, M.1    Vallittu, P.K.2
  • 12
    • 2342589454 scopus 로고    scopus 로고
    • Cementation of zirconium-oxide ceramic restorations
    • Blatz M.B. Cementation of zirconium-oxide ceramic restorations. Pract Proced Aesthet Dent 16 (2004) 14
    • (2004) Pract Proced Aesthet Dent , vol.16 , pp. 14
    • Blatz, M.B.1
  • 13
    • 0041888380 scopus 로고    scopus 로고
    • Effect of surface topography on the bond strength of a composite to three different types of ceramic
    • Oh W.S., and Shen C. Effect of surface topography on the bond strength of a composite to three different types of ceramic. J Prosthet Dent 90 (2003) 241-246
    • (2003) J Prosthet Dent , vol.90 , pp. 241-246
    • Oh, W.S.1    Shen, C.2
  • 14
    • 14844296500 scopus 로고    scopus 로고
    • The effect of ceramic surface treatment on bonding to densely sintered alumina ceramic
    • Valandro L.F., Della Bona A., Antonio Bottino M., and Neisser M.P. The effect of ceramic surface treatment on bonding to densely sintered alumina ceramic. J Prosthet Dent 93 (2005) 253-259
    • (2005) J Prosthet Dent , vol.93 , pp. 253-259
    • Valandro, L.F.1    Della Bona, A.2    Antonio Bottino, M.3    Neisser, M.P.4
  • 15
    • 34548694768 scopus 로고    scopus 로고
    • Adhesive cementation of high-strength ceramics
    • Blatz M.B. Adhesive cementation of high-strength ceramics. J Esthet Restor Dent 19 (2007) 238-239
    • (2007) J Esthet Restor Dent , vol.19 , pp. 238-239
    • Blatz, M.B.1
  • 16
    • 0034208413 scopus 로고    scopus 로고
    • Long-term resin bond strength to zirconia ceramic
    • Wegner S.M., and Kern M. Long-term resin bond strength to zirconia ceramic. J Adhes Dent 2 (2000) 139-147
    • (2000) J Adhes Dent , vol.2 , pp. 139-147
    • Wegner, S.M.1    Kern, M.2
  • 17
    • 33845290307 scopus 로고    scopus 로고
    • Durability of the resin bond strength to zirconia ceramic after using different surface conditioning methods
    • Wolfart M., Lehmann F., Wolfart S., and Kern M. Durability of the resin bond strength to zirconia ceramic after using different surface conditioning methods. Dent Mater 23 (2007) 45-50
    • (2007) Dent Mater , vol.23 , pp. 45-50
    • Wolfart, M.1    Lehmann, F.2    Wolfart, S.3    Kern, M.4
  • 21
    • 0036490134 scopus 로고    scopus 로고
    • Are adhesive technologies needed to support ceramics? An assessment of the current evidence
    • Burke F.J., Fleming G.J., Nathanson D., and Marquis P.M. Are adhesive technologies needed to support ceramics? An assessment of the current evidence. J Adhes Dent 4 (2002) 7-22
    • (2002) J Adhes Dent , vol.4 , pp. 7-22
    • Burke, F.J.1    Fleming, G.J.2    Nathanson, D.3    Marquis, P.M.4
  • 22
    • 33847107611 scopus 로고    scopus 로고
    • Panavia F 2.0 bonding to contaminated zirconia ceramic after different cleaning procedures
    • Quaas A.C., Yang B., and Kern M. Panavia F 2.0 bonding to contaminated zirconia ceramic after different cleaning procedures. Dent Mater 23 (2007) 506-512
    • (2007) Dent Mater , vol.23 , pp. 506-512
    • Quaas, A.C.1    Yang, B.2    Kern, M.3
  • 23
    • 16344363996 scopus 로고    scopus 로고
    • Influence of surface and heat treatments on the flexural strength of a glass-infiltrated alumina/zirconia-reinforced dental ceramic
    • Guazzato M., Albakry M., Quach L., and Swain M.V. Influence of surface and heat treatments on the flexural strength of a glass-infiltrated alumina/zirconia-reinforced dental ceramic. Dent Mater 21 (2005) 454-463
    • (2005) Dent Mater , vol.21 , pp. 454-463
    • Guazzato, M.1    Albakry, M.2    Quach, L.3    Swain, M.V.4
  • 24
    • 33845465853 scopus 로고    scopus 로고
    • Effect of surface condition of dental zirconia ceramic (Denzir) on bonding
    • Uo M., Sjogren G., Sundh A., Goto M., Watari F., and Bergman M. Effect of surface condition of dental zirconia ceramic (Denzir) on bonding. Dent Mater J 25 (2006) 626-631
    • (2006) Dent Mater J , vol.25 , pp. 626-631
    • Uo, M.1    Sjogren, G.2    Sundh, A.3    Goto, M.4    Watari, F.5    Bergman, M.6
  • 26
    • 0033222358 scopus 로고    scopus 로고
    • The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic
    • Kosmac T., Oblak C., Jevnikar P., Funduk N., and Marion L. The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic. Dent Mater 15 (1999) 426-433
    • (1999) Dent Mater , vol.15 , pp. 426-433
    • Kosmac, T.1    Oblak, C.2    Jevnikar, P.3    Funduk, N.4    Marion, L.5
  • 27
    • 0029266741 scopus 로고
    • Bonding to glass infiltrated alumina ceramic: adhesive methods and their durability
    • Kern M., and Thompson V.P. Bonding to glass infiltrated alumina ceramic: adhesive methods and their durability. J Prosthet Dent 73 (1995) 240-249
    • (1995) J Prosthet Dent , vol.73 , pp. 240-249
    • Kern, M.1    Thompson, V.P.2
  • 28
    • 0042994076 scopus 로고    scopus 로고
    • Effect of different luting materials on the marginal adaptation of Class I ceramic inlay restorations in vitro
    • Bott B., and Hannig M. Effect of different luting materials on the marginal adaptation of Class I ceramic inlay restorations in vitro. Dent Mater 19 (2003) 264-269
    • (2003) Dent Mater , vol.19 , pp. 264-269
    • Bott, B.1    Hannig, M.2
  • 29
    • 42449099988 scopus 로고    scopus 로고
    • Effect of various surface conditioning methods on the adhesion of dual-cure resin cement with MDP functional monomer to zirconia after thermal aging
    • Özcan M., Nijhuis H., and Valandro L.F. Effect of various surface conditioning methods on the adhesion of dual-cure resin cement with MDP functional monomer to zirconia after thermal aging. Dent Mater J 27 (2008) 99-104
    • (2008) Dent Mater J , vol.27 , pp. 99-104
    • Özcan, M.1    Nijhuis, H.2    Valandro, L.F.3
  • 30
    • 0029202388 scopus 로고
    • Effects of treatment and storage conditions on ceramic/composite bond strength
    • Roulet J.F., Söderholm K.J., and Longmate J. Effects of treatment and storage conditions on ceramic/composite bond strength. J Dent Res 74 (1995) 381-387
    • (1995) J Dent Res , vol.74 , pp. 381-387
    • Roulet, J.F.1    Söderholm, K.J.2    Longmate, J.3
  • 32
    • 0034231366 scopus 로고    scopus 로고
    • Bond strength of luting cements to zirconium oxide ceramics
    • Kern M. Bond strength of luting cements to zirconium oxide ceramics. Int J Prosthodont 13 (2000) 350
    • (2000) Int J Prosthodont , vol.13 , pp. 350
    • Kern, M.1
  • 33
    • 33744789998 scopus 로고    scopus 로고
    • Effect of zirconium-oxide ceramic surface treatments on the bond strength to adhesive resin
    • Atsu S.S., Kilicarslan M.A., Kucukesmen H.C., and Aka P.S. Effect of zirconium-oxide ceramic surface treatments on the bond strength to adhesive resin. J Prosthet Dent 95 (2006) 430-436
    • (2006) J Prosthet Dent , vol.95 , pp. 430-436
    • Atsu, S.S.1    Kilicarslan, M.A.2    Kucukesmen, H.C.3    Aka, P.S.4
  • 34
    • 0032017987 scopus 로고    scopus 로고
    • Bonding to alumina ceramic in restorative dentistry: clinical results over up to 5 years
    • Kern M., and Strub J.R. Bonding to alumina ceramic in restorative dentistry: clinical results over up to 5 years. J Dent 26 (1998) 245-249
    • (1998) J Dent , vol.26 , pp. 245-249
    • Kern, M.1    Strub, J.R.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.