Volumn 89, Issue 6, 2010, Pages 592-596

Damage and reliability of Y-TZP after cementation surface treatment

Author keywords

Cone fracture; Fatigue reliability; Radial fracture; Surface treatment; Zirconia framework

Indexed keywords

ALUMINUM OXIDE; BIOMEDICAL AND DENTAL MATERIALS; DIAMOND; METAL PRIMER; METHACRYLIC ACID DERIVATIVE; RESIN; RESIN CEMENT; TUNGSTEN CARBIDE; TUNGSTEN DERIVATIVE; WATER; Y TZP CERAMIC; Y-TZP CERAMIC; YTTRIUM; ZIRCONIUM;

EID: 77953247575     PISSN: 00220345     EISSN: 15440591     Source Type: Journal    
DOI: 10.1177/0022034510363253     Document Type: Article
Times cited : (97)

References (26)
  • 1
    • 59149092803 scopus 로고    scopus 로고
    • Bridging the gap between clinical failure and laboratory fracture strength tests using a fractographic approach
    • Aboushelib MN, Feilzer AJ, Kleverlaan CJ (2008). Bridging the gap between clinical failure and laboratory fracture strength tests using a fractographic approach. Dent Mater 25: 383-391.
    • (2008) Dent Mater , vol.25 , pp. 383-391
    • Aboushelib, M.N.1    Feilzer, A.J.2    Kleverlaan, C.J.3
  • 2
    • 0024546336 scopus 로고
    • Mechanical properties and short-term in-vivo evaluation of yttrium-oxide-partially-stabilized zirconia
    • Christel P., Meunier A., Heller M., Torre JP, Peille CN (1989). Mechanical properties and short-term in-vivo evaluation of yttrium-oxide- partially-stabilized zirconia. J Biomed Mater Res 23: 45-61.
    • (1989) J Biomed Mater Res , vol.23 , pp. 45-61
    • Christel, P.1    Meunier, A.2    Heller, M.3    Torre, J.P.4    Peille, C.N.5
  • 4
    • 32044466739 scopus 로고    scopus 로고
    • The influence of surface modification techniques on the performance of a Y-TZP dental ceramic
    • Curtis AR, Wright AJ, Fleming GJ (2006). The influence of surface modification techniques on the performance of a Y-TZP dental ceramic. J Dent 34: 195-206.
    • (2006) J Dent , vol.34 , pp. 195-206
    • Curtis, A.R.1    Wright, A.J.2    Fleming, G.J.3
  • 5
    • 0026142466 scopus 로고
    • An artificial oral environment for testing dental materials
    • DeLong R., Douglas WH (1991). An artificial oral environment for testing dental materials. IEEE Trans Biomed Eng 38: 339-345.
    • (1991) IEEE Trans Biomed Eng , vol.38 , pp. 339-345
    • Delong, R.1    Douglas, W.H.2
  • 6
    • 0035319974 scopus 로고    scopus 로고
    • Reliability and strength of all-ceramic dental restorations fabricated by direct ceramic machining (DCM)
    • Filser F., Kocher P., Weibel F., Luthy H., Scharer P., Gauckler LJ (2001). Reliability and strength of all-ceramic dental restorations fabricated by direct ceramic machining (DCM). Int J Comput Dent 4: 89-106.
    • (2001) Int J Comput Dent , vol.4 , pp. 89-106
    • Filser, F.1    Kocher, P.2    Weibel, F.3    Luthy, H.4    Scharer, P.5    Gauckler, L.J.6
  • 7
    • 84979455274 scopus 로고
    • Phase analysis in zirconia systems
    • Garvie RC, Nicholson PS (1972). Phase analysis in zirconia systems. J Am Ceram Soc 55: 303-305.
    • (1972) J Am Ceram Soc , vol.55 , pp. 303-305
    • Garvie, R.C.1    Nicholson, P.S.2
  • 8
    • 11844264547 scopus 로고    scopus 로고
    • Influence of surface and heat treatments on the flexural strength of Y-TZP dental ceramic
    • Guazzato M., Quach L., Albakry M., Swain MV (2005). Influence of surface and heat treatments on the flexural strength of Y-TZP dental ceramic. J Dent 33: 9-18.
    • (2005) J Dent , vol.33 , pp. 9-18
    • Guazzato, M.1    Quach, L.2    Albakry, M.3    Swain, M.V.4
  • 9
    • 33847067200 scopus 로고    scopus 로고
    • Fracture of porcelain-veneered structures in fatigue
    • Kim B., Zhang Y., Pines M., Thompson VP (2007). Fracture of porcelain-veneered structures in fatigue. J Dent Res 86: 142-146.
    • (2007) J Dent Res , vol.86 , pp. 142-146
    • Kim, B.1    Zhang, Y.2    Pines, M.3    Thompson, V.P.4
  • 10
    • 58149391384 scopus 로고    scopus 로고
    • Damage maps of veneered zirconia under simulated mastication
    • Kim JW, Kim JH, Janal MN, Zhang Y. (2008). Damage maps of veneered zirconia under simulated mastication. J Dent Res 87: 1127-1132.
    • (2008) J Dent Res , vol.87 , pp. 1127-1132
    • Kim, J.W.1    Kim, J.H.2    Janal, M.N.3    Zhang, Y.4
  • 11
    • 33644642412 scopus 로고    scopus 로고
    • A single-retainer zirconium dioxide ceramic resin-bonded fixed partial denture for single tooth replacement: A clinical report
    • Komine F., Tomic M. (2005). A single-retainer zirconium dioxide ceramic resin-bonded fixed partial denture for single tooth replacement: a clinical report. J Oral Sci 47: 139-142.
    • (2005) J Oral Sci , vol.47 , pp. 139-142
    • Komine, F.1    Tomic, M.2
  • 12
    • 0033222358 scopus 로고    scopus 로고
    • The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic
    • Kosmac T., Oblak C., Jevnikar P., Funduk N., Marion L. (1999). The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic. Dent Mater 15: 426-433.
    • (1999) Dent Mater , vol.15 , pp. 426-433
    • Kosmac, T.1    Oblak, C.2    Jevnikar, P.3    Funduk, N.4    Marion, L.5
  • 14
    • 0035512807 scopus 로고    scopus 로고
    • Use of contact testing in the characterization and design of all-ceramic crownlike layer structures: A review
    • Lawn BR, Deng Y., Thompson VP (2001). Use of contact testing in the characterization and design of all-ceramic crownlike layer structures: a review. J Prosthet Dent 86: 495-510.
    • (2001) J Prosthet Dent , vol.86 , pp. 495-510
    • Lawn, B.R.1    Deng, Y.2    Thompson, V.P.3
  • 18
    • 46249121351 scopus 로고    scopus 로고
    • Mechanical properties of dental zirconia ceramics changed with sandblasting and heat treatment
    • Sato H., Yamada K., Pezzotti G., Nawa M., Ban S. (2008). Mechanical properties of dental zirconia ceramics changed with sandblasting and heat treatment. Dent Mater J 27: 408-414.
    • (2008) Dent Mater J , vol.27 , pp. 408-414
    • Sato, H.1    Yamada, K.2    Pezzotti, G.3    Nawa, M.4    Ban, S.5
  • 19
  • 21
    • 0034264517 scopus 로고    scopus 로고
    • Structural reliability of alumina-, feldspar-, leucite-, mica- and zirconia-based ceramics
    • Tinschert J., Zwez D., Marx R., Anusavice KJ (2000). Structural reliability of alumina-, feldspar-, leucite-, mica- and zirconia-based ceramics. J Dent 28: 529-535.
    • (2000) J Dent , vol.28 , pp. 529-535
    • Tinschert, J.1    Zwez, D.2    Marx, R.3    Anusavice, K.J.4
  • 22
    • 40749115551 scopus 로고    scopus 로고
    • Strength influencing variables on CAD/CAM zirconia frameworks
    • Wang H., Aboushelib MN, Feilzer AJ (2008). Strength influencing variables on CAD/CAM zirconia frameworks. Dent Mater 24: 633-638.
    • (2008) Dent Mater , vol.24 , pp. 633-638
    • Wang, H.1    Aboushelib, M.N.2    Feilzer, A.J.3
  • 23
    • 29244474632 scopus 로고    scopus 로고
    • A new design for all-ceramic inlay-retained fixed partial dentures: A report of 2 cases
    • Wolfart S., Kern M. (2006). A new design for all-ceramic inlay-retained fixed partial dentures: a report of 2 cases. Quintessence Int 37: 27-33.
    • (2006) Quintessence Int , vol.37 , pp. 27-33
    • Wolfart, S.1    Kern, M.2
  • 24
    • 33845290307 scopus 로고    scopus 로고
    • Durability of the resin bond strength to zirconia ceramic after using different surface conditioning methods
    • Wolfart S., Lehmann F., Wolfart M., Kern M. (2007). Durability of the resin bond strength to zirconia ceramic after using different surface conditioning methods. Dent Mater 23: 45-50.
    • (2007) Dent Mater , vol.23 , pp. 45-50
    • Wolfart, S.1    Lehmann, F.2    Wolfart, M.3    Kern, M.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.