Volumn 88, Issue 9, 2009, Pages 817-822

Surface conditioning influences zirconia ceramic bonding

Author keywords

Air abrasion; Ceramic primer; Durability; Resin bonding; Zirconia ceramic

Indexed keywords

ALLOY PRIMER; ALUMINUM OXIDE; METAL PRIMER; METHACRYLIC ACID DERIVATIVE; METHACRYLOYLOXYDECYL DIHYDROGEN PHOSPHATE; MULTILINK ADHESIVE SYSTEM; RESIN; RESIN CEMENT; THIOKETONE; WATER; ZIRCONIUM; ZIRCONIUM OXIDE;

EID: 70349481496     PISSN: 00220345     EISSN: None     Source Type: Journal    
DOI: 10.1177/0022034509340881     Document Type: Article
Times cited : (255)

References (32)
  • 1
    • 33744789998 scopus 로고    scopus 로고
    • Effect of zirconium-oxide ceramic surface treatments on the bond strength to adhesive resin
    • Atsu SS, Kilicarslan MA, Kucukesmen HC, Aka PS (2006). Effect of zirconium-oxide ceramic surface treatments on the bond strength to adhesive resin. J Prosthet Dent 95: 430-436.
    • (2006) J Prosthet Dent , vol.95 , pp. 430-436
    • Atsu, S.S.1    Kilicarslan, M.A.2    Kucukesmen, H.C.3    Aka, P.S.4
  • 2
    • 33846268014 scopus 로고    scopus 로고
    • Effect of sandblasting and heat treatment on biaxial flexure strength of the zirconia/alumina nanocomposite
    • Ban S., Sato H., Suehiro Y., Nakanishi H., Nawa M. (2007). Effect of sandblasting and heat treatment on biaxial flexure strength of the zirconia/alumina nanocomposite. Key Engineer Mater 330 (Pt 1). 353-356.
    • (2007) Key Engineer Mater , vol.330 , Issue.1 , pp. 353-356
    • Ban, S.1    Sato, H.2    Suehiro, Y.3    Nakanishi, H.4    Nawa, M.5
  • 3
    • 0038644503 scopus 로고    scopus 로고
    • Resin-ceramic bonding: A review of the literature
    • Blatz MB, Sadan A., Kern M. (2003). Resin-ceramic bonding: a review of the literature. J Prosthet Dent 89: 268-274.
    • (2003) J Prosthet Dent , vol.89 , pp. 268-274
    • Blatz, M.B.1    Sadan, A.2    Kern, M.3
  • 4
    • 1942456928 scopus 로고    scopus 로고
    • In vitro evaluation of shear bond strengths of resin to densely-sintered high-purity zirconium-oxide ceramic after long-term storage and thermal cycling
    • Blatz MB, Sadan A., Martin J., Lang B. (2004). In vitro evaluation of shear bond strengths of resin to densely-sintered high-purity zirconium-oxide ceramic after long-term storage and thermal cycling. J Prosthet Dent 91: 356-362.
    • (2004) J Prosthet Dent , vol.91 , pp. 356-362
    • Blatz, M.B.1    Sadan, A.2    Martin, J.3    Lang, B.4
  • 5
    • 34548648100 scopus 로고    scopus 로고
    • Influence of surface treatment and simulated aging on bond strengths of luting agents to zirconia
    • Blatz MB, Chiche G., Holst S., Sadan A. (2007). Influence of surface treatment and simulated aging on bond strengths of luting agents to zirconia. Quintessence Int 38: 745-753.
    • (2007) Quintessence Int , vol.38 , pp. 745-753
    • Blatz, M.B.1    Chiche, G.2    Holst, S.3    Sadan, A.4
  • 6
    • 32044466739 scopus 로고    scopus 로고
    • The influence of surface modification techniques on the performance of a Y-TZP dental ceramic
    • Curtis AR, Wright AJ, Fleming GJ (2006). The influence of surface modification techniques on the performance of a Y-TZP dental ceramic. J Dent 34: 195-206.
    • (2006) J Dent , vol.34 , pp. 195-206
    • Curtis, A.R.1    Wright, A.J.2    Fleming, G.J.3
  • 7
    • 0345868765 scopus 로고    scopus 로고
    • Influence of grinding, sandblasting, polishing and heat treatment on the flexural strength of a glass-infiltrated alumina-reinforced dental ceramic
    • Guazzato M., Albakry M., Quach L., Swain MV (2004). Influence of grinding, sandblasting, polishing and heat treatment on the flexural strength of a glass-infiltrated alumina-reinforced dental ceramic. Biomaterials 25: 2153-2160.
    • (2004) Biomaterials , vol.25 , pp. 2153-2160
    • Guazzato, M.1    Albakry, M.2    Quach, L.3    Swain, M.V.4
  • 8
    • 1842855215 scopus 로고    scopus 로고
    • Durability of the resin bond strength to the alumina ceramic Procera
    • Hummel M., Kern M. (2004). Durability of the resin bond strength to the alumina ceramic Procera. Dent Mater 20: 498-508.
    • (2004) Dent Mater , vol.20 , pp. 498-508
    • Hummel, M.1    Kern, M.2
  • 9
    • 0034231366 scopus 로고    scopus 로고
    • Bond strength of luting cements to zirconium oxide ceramics (letter to the Editor)
    • Kern M. (2000). Bond strength of luting cements to zirconium oxide ceramics (letter to the Editor). Int J Prosthodont 13: 350.
    • (2000) Int J Prosthodont , vol.13 , pp. 350
    • Kern, M.1
  • 10
    • 70349492788 scopus 로고    scopus 로고
    • Durability of resin bonding to zirconia ceramic using different primers
    • Kern M., Lehmann F. (2009). Durability of resin bonding to zirconia ceramic using different primers. J Adhes Dent 11 (in press).
    • (2009) J Adhes Dent , vol.11
    • Kern, M.1    Lehmann, F.2
  • 11
    • 0032017987 scopus 로고    scopus 로고
    • Bonding to alumina ceramic in restorative dentistry over up to five years
    • Kern M., Strub JR (1998). Bonding to alumina ceramic in restorative dentistry over up to five years. J Dent 26: 245-249.
    • (1998) J Dent , vol.26 , pp. 245-249
    • Kern, M.1    Strub, J.R.2
  • 12
    • 0027596321 scopus 로고
    • Sandblasting and silica-coating of dental alloys: Volume loss, morphology and changes in the surface composition
    • Kern M., Thompson VP (1993). Sandblasting and silica-coating of dental alloys: volume loss, morphology and changes in the surface composition. Dent Mater 9: 155-161.
    • (1993) Dent Mater , vol.9 , pp. 155-161
    • Kern, M.1    Thompson, V.P.2
  • 13
    • 0028435067 scopus 로고
    • Sandblasting and silica coating of a glass-infiltrated alumina ceramic: Volume loss, morphology, and changes in the surface composition
    • Kern M., Thompson VP (1994). Sandblasting and silica coating of a glass-infiltrated alumina ceramic: volume loss, morphology, and changes in the surface composition. J Prosthet Dent 71: 453-461.
    • (1994) J Prosthet Dent , vol.71 , pp. 453-461
    • Kern, M.1    Thompson, V.P.2
  • 14
    • 0031598657 scopus 로고    scopus 로고
    • Bonding to zirconia ceramic: Adhesion methods and their durability
    • Kern M., Wegner SM (1998). Bonding to zirconia ceramic: adhesion methods and their durability. Dent Mater 14: 64-71.
    • (1998) Dent Mater , vol.14 , pp. 64-71
    • Kern, M.1    Wegner, S.M.2
  • 15
    • 0033222358 scopus 로고    scopus 로고
    • The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic
    • Kosmac T., Oblak C., Jevnikar P., Funduk N., Marion L. (1999). The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic. Dent Mater 15: 426-433.
    • (1999) Dent Mater , vol.15 , pp. 426-433
    • Kosmac, T.1    Oblak, C.2    Jevnikar, P.3    Funduk, N.4    Marion, L.5
  • 16
    • 30344433724 scopus 로고    scopus 로고
    • Effect of thermocycling on bond strength of luting cements to zirconia ceramic
    • LÁthy H., Loeffel O., HÁCurrency signmmerle CHF (2006). Effect of thermocycling on bond strength of luting cements to zirconia ceramic. Dent Mater 22: 195-200.
    • (2006) Dent Mater , vol.22 , pp. 195-200
    • Láthy, H.1    Loeffel, O.2    Hácurrency Signmmerle, C.H.F.3
  • 18
    • 0041888380 scopus 로고    scopus 로고
    • Effect of surface topography on the bond strength of a composite to three different types of ceramic
    • Oh WS, Shen C. (2003). Effect of surface topography on the bond strength of a composite to three different types of ceramic. J Prosthet Dent 90: 241-246.
    • (2003) J Prosthet Dent , vol.90 , pp. 241-246
    • Oh, W.S.1    Shen, C.2
  • 19
    • 0141727597 scopus 로고    scopus 로고
    • Effect of surface conditioning methods on the bond strength of luting cement to ceramics
    • Ázcan M., Vallittu PK (2003). Effect of surface conditioning methods on the bond strength of luting cement to ceramics. Dent Mater 19: 725-731.
    • (2003) Dent Mater , vol.19 , pp. 725-731
    • Ázcan, M.1    Vallittu, P.K.2
  • 20
    • 48549085496 scopus 로고    scopus 로고
    • Comparison of resin cement adhesion to Y-TZP ceramic following manufacturersĝ instructions of the cements only
    • Ázcan M., Kerkdijk S., Valandro LF (2007). Comparison of resin cement adhesion to Y-TZP ceramic following manufacturersĝ instructions of the cements only. Clin Oral Investig 12: 279-282.
    • (2007) Clin Oral Investig , vol.12 , pp. 279-282
    • Ázcan, M.1    Kerkdijk, S.2    Valandro, L.F.3
  • 21
    • 42449099988 scopus 로고    scopus 로고
    • Effect of various surface conditioning methods on the adhesion of dual-cure resin cement with MDP functional monomer to zirconia after thermal aging
    • Ázcan M., Nijhuis H., Valandro LF (2008). Effect of various surface conditioning methods on the adhesion of dual-cure resin cement with MDP functional monomer to zirconia after thermal aging. Dent Mater J 27: 99-104.
    • (2008) Dent Mater J , vol.27 , pp. 99-104
    • Ázcan, M.1    Nijhuis, H.2    Valandro, L.F.3
  • 22
    • 19744367539 scopus 로고    scopus 로고
    • The shear bond strength between luting cements and zirconia ceramics after two pre-treatments
    • Piwowarczyk A., Lauer HC, Sorensen JA (2005). The shear bond strength between luting cements and zirconia ceramics after two pre-treatments. Oper Dent 30: 382-388.
    • (2005) Oper Dent , vol.30 , pp. 382-388
    • Piwowarczyk, A.1    Lauer, H.C.2    Sorensen, J.A.3
  • 23
    • 33845465853 scopus 로고    scopus 로고
    • Effect of surface condition of dental zirconia ceramic (Denzir) on bonding
    • Uo M., Sjogren G., Sundh A., Goto M., Watari F., Bergman M. (2006). Effect of surface condition of dental zirconia ceramic (Denzir) on bonding. Dent Mater J 25: 626-631.
    • (2006) Dent Mater J , vol.25 , pp. 626-631
    • Uo, M.1    Sjogren, G.2    Sundh, A.3    Goto, M.4    Watari, F.5    Bergman, M.6
  • 24
    • 14844296500 scopus 로고    scopus 로고
    • The effect of ceramic surface treatment on bonding to densely sintered alumina ceramic
    • Valandro LF, Della Bona A., Bottino MA, Neisser MP (2005). The effect of ceramic surface treatment on bonding to densely sintered alumina ceramic. J Prosthet Dent 93: 253-259.
    • (2005) J Prosthet Dent , vol.93 , pp. 253-259
    • Valandro, L.F.1    Della Bona, A.2    Bottino, M.A.3    Neisser, M.P.4
  • 25
    • 0034208413 scopus 로고    scopus 로고
    • Long-term resin bond strength to zirconia ceramic
    • Wegner S., Kern M. (2000). Long-term resin bond strength to zirconia ceramic. J Adhes Dent 2: 139-147.
    • (2000) J Adhes Dent , vol.2 , pp. 139-147
    • Wegner, S.1    Kern, M.2
  • 26
    • 0036561939 scopus 로고    scopus 로고
    • Effect of different artificial aging conditions on ceramic/composite bond strength
    • Wegner SM, Gerdes W., Kern M. (2002). Effect of different artificial aging conditions on ceramic/composite bond strength. Int J Prosthodont 15: 267-272.
    • (2002) Int J Prosthodont , vol.15 , pp. 267-272
    • Wegner, S.M.1    Gerdes, W.2    Kern, M.3
  • 27
    • 33845290307 scopus 로고    scopus 로고
    • Durability of the resin bond strength to zirconia ceramic after using different surface conditioning methods
    • Wolfart M., Lehmann F., Wolfart S., Kern M. (2007). Durability of the resin bond strength to zirconia ceramic after using different surface conditioning methods. Dent Mater 23: 45-50.
    • (2007) Dent Mater , vol.23 , pp. 45-50
    • Wolfart, M.1    Lehmann, F.2    Wolfart, S.3    Kern, M.4
  • 30
    • 34548289824 scopus 로고    scopus 로고
    • Mechanical properties of dual-cured resin luting agents for ceramic restoration
    • Yoshida K., Tsuo Y., Meng X., Atsuta M. (2007). Mechanical properties of dual-cured resin luting agents for ceramic restoration. J Prosthodont 16: 370-376.
    • (2007) J Prosthodont , vol.16 , pp. 370-376
    • Yoshida, K.1    Tsuo, Y.2    Meng, X.3    Atsuta, M.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.