메뉴 건너뛰기




Volumn 22, Issue 3, 2006, Pages 283-290

Microtensile bond strength of a resin cement to glass infiltrated zirconia-reinforced ceramic: The effect of surface conditioning

Author keywords

Bond strength; Microtensile test; Silane coupling agent; Silica coating; Surface conditioning methods; Zirconia ceramics

Indexed keywords

ABRASION; CEMENTS; COOLING WATER; DISTILLERIES; GLASS; RESINS; SILANES; ZIRCONIUM;

EID: 32044438490     PISSN: 01095641     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.dental.2005.04.021     Document Type: Article
Times cited : (200)

References (37)
  • 1
    • 0021903030 scopus 로고
    • Etched porcelain veneers: The current state of the art
    • J.R. Calamia Etched porcelain veneers: the current state of the art Quintessence Int 1 1985 5 12
    • (1985) Quintessence Int , vol.1 , pp. 5-12
    • Calamia, J.R.1
  • 2
    • 0023413139 scopus 로고
    • Shear strength of the composite bond to etched porcelain
    • I. Stangel, D. Nathanson, and C.S. Hsu Shear strength of the composite bond to etched porcelain J Dent Res 66 1987 1460 1465
    • (1987) J Dent Res , vol.66 , pp. 1460-1465
    • Stangel, I.1    Nathanson, D.2    Hsu, C.S.3
  • 3
    • 0028523833 scopus 로고
    • Effect of porcelain surface treatments on bond strengths of composite resin bonded to porcelain
    • J.W. Thurmond, W. Barkmeier, and T.M. Wilwerding Effect of porcelain surface treatments on bond strengths of composite resin bonded to porcelain J Prosthet Dent 72 1994 355 359
    • (1994) J Prosthet Dent , vol.72 , pp. 355-359
    • Thurmond, J.W.1    Barkmeier, W.2    Wilwerding, T.M.3
  • 4
    • 0028489343 scopus 로고
    • Comparison of acidulated phosphate fluoride gel and hydrofluoric acid etchants for porcelain-composite repair
    • D.F. Tylka, and G. Stewart Comparison of acidulated phosphate fluoride gel and hydrofluoric acid etchants for porcelain-composite repair J Prosthet Dent 72 1994 121 127
    • (1994) J Prosthet Dent , vol.72 , pp. 121-127
    • Tylka, D.F.1    Stewart, G.2
  • 5
    • 0029299001 scopus 로고
    • Adhesion of composite to porcelain with various surface conditions
    • M. Aida, T. Hayakawa, and K. Mizukawa Adhesion of composite to porcelain with various surface conditions J Prosthet Dent 73 1995 464 470
    • (1995) J Prosthet Dent , vol.73 , pp. 464-470
    • Aida, M.1    Hayakawa, T.2    Mizukawa, K.3
  • 6
    • 0024103132 scopus 로고    scopus 로고
    • Tensile bond to resin cements to porcelain veneers
    • J.I. Nicholls Tensile bond to resin cements to porcelain veneers J Prosthet Dent 60 1998 443 447
    • (1998) J Prosthet Dent , vol.60 , pp. 443-447
    • Nicholls, J.I.1
  • 8
    • 0027605367 scopus 로고
    • Bond strength of composite to etched and sandblasted porcelain
    • D.M. Wolf, J.M. Powers, and K.L. O'Keefe Bond strength of composite to etched and sandblasted porcelain Am J Dent 6 1993 155 158
    • (1993) Am J Dent , vol.6 , pp. 155-158
    • Wolf, D.M.1    Powers, J.M.2    O'Keefe, K.L.3
  • 9
    • 0029266741 scopus 로고
    • Bonding to glass infiltrated alumina ceramic: Adhesive methods and their durability
    • M. Kern, and V.P. Thompson Bonding to glass infiltrated alumina ceramic: adhesive methods and their durability J Prosthet Dent 73 1995 240 249
    • (1995) J Prosthet Dent , vol.73 , pp. 240-249
    • Kern, M.1    Thompson, V.P.2
  • 10
    • 0141727597 scopus 로고    scopus 로고
    • Effect of surface conditioning methods on the bond strength of luting cement to ceramics
    • M. Özcan, and P.K. Vallittu Effect of surface conditioning methods on the bond strength of luting cement to ceramics Dent Mater 19 2003 725 731
    • (2003) Dent Mater , vol.19 , pp. 725-731
    • Özcan, M.1    Vallittu, P.K.2
  • 11
    • 0035461093 scopus 로고    scopus 로고
    • Effects of surface treatments on bond strength of glass-infiltrated ceramic
    • Y.C. Lu, H. Tseng, Y.H. Shih, and S.Y. Lee Effects of surface treatments on bond strength of glass-infiltrated ceramic J Oral Rehabil 28 2001 805 813
    • (2001) J Oral Rehabil , vol.28 , pp. 805-813
    • Lu, Y.C.1    Tseng, H.2    Shih, Y.H.3    Lee, S.Y.4
  • 12
    • 0035404137 scopus 로고    scopus 로고
    • The effect of surface treatment on the shear bond strength of luting cement to a glass-infiltrated alumina ceramic
    • M. Özcan, H.N. Alkumru, and D. Gemalmaz The effect of surface treatment on the shear bond strength of luting cement to a glass-infiltrated alumina ceramic Int J Prosthodont 14 2001 335 339
    • (2001) Int J Prosthodont , vol.14 , pp. 335-339
    • Özcan, M.1    Alkumru, H.N.2    Gemalmaz, D.3
  • 13
    • 0031598657 scopus 로고    scopus 로고
    • Bonding to zirconia ceramic: Adhesion methods and their durability
    • M. Kern, and S.M. Wegner Bonding to zirconia ceramic: adhesion methods and their durability Dent Mater 14 1998 64 71
    • (1998) Dent Mater , vol.14 , pp. 64-71
    • Kern, M.1    Wegner, S.M.2
  • 14
    • 0034157359 scopus 로고    scopus 로고
    • Bond strength of luting cements to zirconium oxide ceramics
    • P. Derand, and T. Derand Bond strength of luting cements to zirconium oxide ceramics Int J Prosthodont 13 2000 131 135
    • (2000) Int J Prosthodont , vol.13 , pp. 131-135
    • Derand, P.1    Derand, T.2
  • 15
    • 0028441251 scopus 로고
    • Bonding of resin cements to an aluminous ceramic: A new surface treatment
    • M. Sadoun, and E. Asmussen Bonding of resin cements to an aluminous ceramic: a new surface treatment Dent Mater 10 1994 185 189
    • (1994) Dent Mater , vol.10 , pp. 185-189
    • Sadoun, M.1    Asmussen, E.2
  • 16
    • 0032195704 scopus 로고    scopus 로고
    • A brief history and current status of metal/ceramic surface conditioning concepts for resin bonding in dentistry
    • M. Özcan, P. Pfeiffer, and İ. Nergiz A brief history and current status of metal/ceramic surface conditioning concepts for resin bonding in dentistry Quintessence Int 29 1998 713 724
    • (1998) Quintessence Int , vol.29 , pp. 713-724
    • Özcan, M.1    Pfeiffer, P.2    Nergiz, I.3
  • 17
    • 0023967360 scopus 로고
    • Causes of failure following oral rehabilitation: Biological versus technical factors
    • J.R. Strub, S. Stiffler, and P. Scharer Causes of failure following oral rehabilitation: biological versus technical factors Quintessence Int 19 1988 215 222
    • (1988) Quintessence Int , vol.19 , pp. 215-222
    • Strub, J.R.1    Stiffler, S.2    Scharer, P.3
  • 20
    • 84989509463 scopus 로고
    • Silicoating. Evaluation of a new method of bonding composite resin to metal
    • A. Peutzfeldt, and E. Asmussen Silicoating. Evaluation of a new method of bonding composite resin to metal Scand J Dent Res 96 1988 171 176
    • (1988) Scand J Dent Res , vol.96 , pp. 171-176
    • Peutzfeldt, A.1    Asmussen, E.2
  • 21
    • 0036559426 scopus 로고    scopus 로고
    • The use of chairside silica coating for different dental applications
    • M. Özcan The use of chairside silica coating for different dental applications J Prosthet Dent 87 2002 469 472
    • (2002) J Prosthet Dent , vol.87 , pp. 469-472
    • Özcan, M.1
  • 22
    • 0038644503 scopus 로고    scopus 로고
    • Resin-ceramic bonding: A review of the literature
    • M.B. Blatz, A. Sadan, and M. Kern Resin-ceramic bonding: a review of the literature J Prosthet Dent 89 2003 268 274
    • (2003) J Prosthet Dent , vol.89 , pp. 268-274
    • Blatz, M.B.1    Sadan, A.2    Kern, M.3
  • 23
    • 0037315569 scopus 로고    scopus 로고
    • Evaluation of alternative intraoral repair techniques for fractured ceramic-fused-to-metal restorations
    • M. Özcan Evaluation of alternative intraoral repair techniques for fractured ceramic-fused-to-metal restorations J Oral Rehabil 30 2003 194 203
    • (2003) J Oral Rehabil , vol.30 , pp. 194-203
    • Özcan, M.1
  • 24
    • 0027546239 scopus 로고
    • A new all-ceramic crown-A dense-sintered, high purity alumina coping with porcelain
    • M. Andersson, and A. Oden A new all-ceramic crown-A dense-sintered, high purity alumina coping with porcelain Acta Odontol Scand 51 1993 59 64
    • (1993) Acta Odontol Scand , vol.51 , pp. 59-64
    • Andersson, M.1    Oden, A.2
  • 25
    • 0032917811 scopus 로고    scopus 로고
    • Zirconia as a ceramic biomaterial
    • C. Piconi, and G. Maccauro Zirconia as a ceramic biomaterial Biomaterials 20 1999 1 25
    • (1999) Biomaterials , vol.20 , pp. 1-25
    • Piconi, C.1    MacCauro, G.2
  • 26
    • 0023967360 scopus 로고
    • Causes of failure following oral rehabilitation: Biological versus technical factors
    • J.R. Strub, S. Stiffler, and P. Scharer Causes of failure following oral rehabilitation: biological versus technical factors Quintessence Int 19 1988 215 222
    • (1988) Quintessence Int , vol.19 , pp. 215-222
    • Strub, J.R.1    Stiffler, S.2    Scharer, P.3
  • 27
    • 0036635362 scopus 로고    scopus 로고
    • Micro-shear bond strength of dual-cured resin cement to glass ceramics
    • Y. Shimada, S. Yamaguchi, and J. Tagami Micro-shear bond strength of dual-cured resin cement to glass ceramics Dent Mater 18 2002 380 388
    • (2002) Dent Mater , vol.18 , pp. 380-388
    • Shimada, Y.1    Yamaguchi, S.2    Tagami, J.3
  • 28
    • 0029372422 scopus 로고
    • Shear vs. tensile bond strength of resin composite bonded to ceramic
    • A. Della Bona, and R. van Noort Shear vs. tensile bond strength of resin composite bonded to ceramic J Dent Res 74 1995 1591 1596
    • (1995) J Dent Res , vol.74 , pp. 1591-1596
    • Della Bona, A.1    Van Noort, R.2
  • 29
    • 0038655268 scopus 로고    scopus 로고
    • Adhesion testing with the microtensile method: Effects of dental substrate and adhesive system on bond strength measurements
    • P.E. Cardoso, F.T. Sadek, C. Goracci, and M. Ferrari Adhesion testing with the microtensile method: effects of dental substrate and adhesive system on bond strength measurements J Adhes Dent 4 2002 291 297
    • (2002) J Adhes Dent , vol.4 , pp. 291-297
    • Cardoso, P.E.1    Sadek, F.T.2    Goracci, C.3    Ferrari, M.4
  • 30
    • 0043130574 scopus 로고    scopus 로고
    • Microtensile bond strength testing of luting cements to prefabricated CAD/CAM ceramic and composite blocks.5
    • A.A. El Zohairy, A.J. De Gee, M.M. Mohsen, and A.J. Feilzer Microtensile bond strength testing of luting cements to prefabricated CAD/CAM ceramic and composite blocks.5 Dent Mater 2003 19
    • (2003) Dent Mater , pp. 19
    • El Zohairy, A.A.1    De Gee, A.J.2    Mohsen, M.M.3    Feilzer, A.J.4
  • 32
    • 0034573599 scopus 로고    scopus 로고
    • Microtensile strength of composite bonded to hot-pressed ceramics
    • A. Della Bona, K.J. Anusavice, and C. Shen Microtensile strength of composite bonded to hot-pressed ceramics J Adhesive Dent 2 2000 305 313
    • (2000) J Adhesive Dent , vol.2 , pp. 305-313
    • Della Bona, A.1    Anusavice, K.J.2    Shen, C.3
  • 33
    • 0030307205 scopus 로고    scopus 로고
    • Effect of cubic leucite stabilization on the flexural strength of feldspathic dental porcelain
    • I.L. Denry, J.R. Mackert Jr, J.A. Holloway, and S.F. Rosenstiel Effect of cubic leucite stabilization on the flexural strength of feldspathic dental porcelain J Dent Res 75 1996 1928 1935
    • (1996) J Dent Res , vol.75 , pp. 1928-1935
    • Denry, I.L.1    Jr, R.M.J.2    Holloway, J.A.3    Rosenstiel, S.F.4
  • 34
    • 0030135524 scopus 로고    scopus 로고
    • Leucite crystallization during processing of a heat-pressed dental ceramic
    • J.R. Mackert, and C.M. Russell Leucite crystallization during processing of a heat-pressed dental ceramic Int J Prosthodont 9 1996 261 265
    • (1996) Int J Prosthodont , vol.9 , pp. 261-265
    • MacKert, J.R.1    Russell, C.M.2
  • 35
    • 0034330293 scopus 로고    scopus 로고
    • Water-enhanced crystallization of leucite in dental porcelain
    • J.R. Mackert Jr, A.L. Williams, J.W. Ergle, and C.M. Russell Water-enhanced crystallization of leucite in dental porcelain Dent Mater 16 2000 426 431
    • (2000) Dent Mater , vol.16 , pp. 426-431
    • Jr, R.M.J.1    Williams, A.L.2    Ergle, J.W.3    Russell, C.M.4
  • 36
    • 0026461934 scopus 로고
    • Slip-casting alumina ceramics for crown and bridge restorations
    • L. Probster, and J. Diehl Slip-casting alumina ceramics for crown and bridge restorations Quintessence Int 23 1992 25 31
    • (1992) Quintessence Int , vol.23 , pp. 25-31
    • Probster, L.1    Diehl, J.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.