Volumn 93, Issue 2, 2010, Pages 318-323

Bond strength to high-crystalline content zirconia after different surface treatments

Author keywords

Adhesion; Ceramic; Surface modification; Zirconia

Indexed keywords

BOND STRENGTH; CERAMIC; CERAMIC SURFACE; CHEMICAL SURFACES; CHEMICAL TREATMENTS; COMPOSITE DISC; CONTROL GROUPS; IN-VITRO; INITIAL VALUES; MECHANICAL TREATMENTS; MICROTENSILE TESTING; RESIN CEMENT; SURFACE CHEMICALS; SURFACE MODIFICATION; THERMOCYCLING; ZIRCONIUM OXIDE;

EID: 77951180327     PISSN: 15524973     EISSN: 15524981     Source Type: Journal    
DOI: 10.1002/jbm.b.31549     Document Type: Article
Times cited : (39)

References (31)
  • 1
    • 0022140086 scopus 로고
    • Development of dental ceramics
    • Jones DW. Development of dental ceramics. Dent Clin North Am 1985;29:621-644.
    • (1985) Dent Clin North Am , vol.29 , pp. 621-644
    • Jones, D.W.1
  • 2
    • 0000653434 scopus 로고
    • The reinforcement of dental porcelain with ceramic oxides
    • McLean JW. The reinforcement of dental porcelain with ceramic oxides. Brit Dent J 1965;119:251-267.
    • (1965) Brit Dent J , vol.119 , pp. 251-267
    • McLean, J.W.1
  • 4
    • 0027546239 scopus 로고
    • A new all-ceramic crown. A dense-sintered, high-purity alumina coping with porcelain
    • Andersson M, Oden A. A new all-ceramic crown. A dense-sintered, high-purity alumina coping with porcelain. Acta Odontol Scand 1993;51:59-64.
    • (1993) Acta Odontol Scand , vol.51 , pp. 59-64
    • Andersson, M.1    Oden, A.2
  • 5
    • 0032917811 scopus 로고    scopus 로고
    • Zirconia as a ceramic biomaterial
    • Piconi C, Maccauro G. Zirconia as a ceramic biomaterial. Biomaterials 1999;20:1-25.
    • (1999) Biomaterials , vol.20 , pp. 1-25
    • Piconi, C.1    Maccauro, G.2
  • 6
    • 33846030118 scopus 로고    scopus 로고
    • Engineering long term clinical success of advanced ceramic prostheses
    • DOI 10.1007/s10856-006-0661-1, Special Section: Selected Papers from the ASME Winter Annual Meeting: Materials and Interfaces with Medicine and Dentistry
    • Rekow D, Thompson VP. Engineering long term clinical success of advanced ceramic prostheses. J Mater Sci Mater Med 2007;18:47-56. (Pubitemid 46046716)
    • (2007) Journal of Materials Science: Materials in Medicine , vol.18 , Issue.1 , pp. 47-56
    • Rekow, D.1    Thompson, V.P.2
  • 7
    • 38349162274 scopus 로고    scopus 로고
    • Stabilized zirconia as a structural ceramic: An overview
    • Kelly JR, Denry I. Stabilized zirconia as a structural ceramic: An overview. Dent Mater 2008;24:289-298.
    • (2008) Dent Mater , vol.24 , pp. 289-298
    • Kelly, J.R.1    Denry, I.2
  • 10
    • 0035351260 scopus 로고    scopus 로고
    • Fracture Resistance of Lithium Disilicate-, Alumina-, and Zirconia-Based Three-Unit Fixed Partial Dentures: A Laboratory Study
    • Tinschert J, Natt G, Mautsch W, Augthun M, Spiekermann H. Fracture resistance of lithium disilicate-, alumina-, and zirconia-based three-unit fixed partial dentures: A laboratory study. Int J Prosthodont 2001;14:231-238. (Pubitemid 33672458)
    • (2001) International Journal of Prosthodontics , vol.14 , Issue.3 , pp. 231-238
    • Tinschert, J.1    Natt, G.2    Mautsch, W.3    Augthun, M.4    Spiekermann, H.5
  • 11
    • 0034264517 scopus 로고    scopus 로고
    • Structural reliability of alumina-, feldspar-, leucite-, mica- and zirconia-based ceramics
    • Tinschert J, Zwez D, Marx R, Anusavice KJ. Structural reliability of alumina-, feldspar-, leucite-, mica- and zirconia-based ceramics. J Dent 2000;28:529-535.
    • (2000) J Dent , vol.28 , pp. 529-535
    • Tinschert, J.1    Zwez, D.2    Marx, R.3    Anusavice, K.J.4
  • 12
    • 34147132866 scopus 로고    scopus 로고
    • Effect of surface treatments on the bond strength of a zirconia-reinforced ceramic to composite resin
    • Della Bona A, Borba M, Benetti P, Cecchetti D. Effect of surface treatments on the bond strength of a zirconia-reinforced ceramic to composite resin. Braz Oral Res 2007;21: 10-15.
    • (2007) Braz Oral Res , vol.21 , pp. 10-15
    • Della Bona, A.1    Borba, M.2    Benetti, P.3    Cecchetti, D.4
  • 13
    • 0034157359 scopus 로고    scopus 로고
    • Bond strength of luting cements to zirconium oxide ceramics
    • Derand P, Derand T. Bond strength of luting cements to zirconium oxide ceramics. Int J Prosthodont 2000;13:131-135.
    • (2000) Int J Prosthodont , vol.13 , pp. 131-135
    • Derand, P.1    Derand, T.2
  • 14
    • 25844498493 scopus 로고    scopus 로고
    • The influence of ceramic surface treatments on the tensile bond strength of composite resin to all-ceramic coping materials
    • DOI 10.1016/j.prosdent.2005.08.012, PII S0022391305004385
    • Kim BK, Bae HE, Shim J, Lee K. The influence of ceramic surface treatments on the tensile bond strength of composite resin to all-ceramic coping materials. J Prosthet Dent 2005; 94:357-362. (Pubitemid 41392972)
    • (2005) Journal of Prosthetic Dentistry , vol.94 , Issue.4 , pp. 357-362
    • Kim, B.-K.1    Bae, H.E.-K.2    Shim, J.-S.3    Lee, K.-W.4
  • 15
    • 0141727597 scopus 로고    scopus 로고
    • Effect of surface conditioning methods on the bond strength of luting cement to ceramics
    • Ozcan M, Vallittu PK. Effect of surface conditioning methods on the bond strength of luting cement to ceramics. Dent Mater 2003;19:725-731.
    • (2003) Dent Mater , vol.19 , pp. 725-731
    • Ozcan, M.1    Vallittu, P.K.2
  • 16
    • 0041919708 scopus 로고    scopus 로고
    • Effect of etching and airborne particle abrasion on the microstructure of different dental ceramics
    • Borges GA, Sophr AM, Goes MF, Sobrinho LC, Chan DCN. Effect of etching and airborne particle abrasion on the microstructure of different dental ceramics. J Prosthet Dent 2003; 89:479-488.
    • (2003) J Prosthet Dent , vol.89 , pp. 479-488
    • Borges, G.A.1    Sophr, A.M.2    Goes, M.F.3    Sobrinho, L.C.4    Chan, D.C.N.5
  • 17
    • 36049040304 scopus 로고    scopus 로고
    • Selective infiltration-etching technique for a strong and durable bond of resin cements to zirconia-based materials
    • Aboushelib MN, Kleverlaan CJ, Feilzer AJ. Selective infiltration-etching technique for a strong and durable bond of resin cements to zirconia-based materials. J Prosthet Dent 2007;98: 379-388.
    • (2007) J Prosthet Dent , vol.98 , pp. 379-388
    • Aboushelib, M.N.1    Kleverlaan, C.J.2    Feilzer, A.J.3
  • 19
    • 33947507846 scopus 로고    scopus 로고
    • Effect of alumina-blasting and adhesive primers on bonding between resin luting agent and zirconia ceramics
    • Tsuo Y, Yoshida K, Atsuta M. Effect of alumina-blasting and adhesive primers on bonding between resin luting agent and zirconia ceramics. Dent Mater J 2006;25:669-674.
    • (2006) Dent Mater J , vol.25 , pp. 669-674
    • Tsuo, Y.1    Yoshida, K.2    Atsuta, M.3
  • 20
    • 33845290307 scopus 로고    scopus 로고
    • Durability of the resin bond strength to zirconia ceramic after using different surface conditioning methods
    • DOI 10.1016/j.dental.2005.11.040, PII S0109564105003568
    • Wolfart M, Lehmann F, Wolfart S, Kern M. Durability of the resin bond strength to irconia ceramic after using different surface conditioning methods. Dent Mater 2007;23:45-50. (Pubitemid 44880064)
    • (2007) Dental Materials , vol.23 , Issue.1 , pp. 45-50
    • Wolfart, M.1    Lehmann, F.2    Wolfart, S.3    Kern, M.4
  • 21
    • 0038644503 scopus 로고    scopus 로고
    • Resin-ceramic bonding: A review of the literature
    • Blatz MB, Sadan A, Kern M. Resin-ceramic bonding: a review of the literature. J Prosthet Dent 2003;89:268-274.
    • (2003) J Prosthet Dent , vol.89 , pp. 268-274
    • Blatz, M.B.1    Sadan, A.2    Kern, M.3
  • 22
    • 0035222454 scopus 로고    scopus 로고
    • Effect of three adhesive primers for a noble metal on the shear bond strengths of three resin cements
    • Yoshida K, Kamada K, Sawase T, Atsuta M. Effect of three adhesive primers for a noble metal on the shear bond strengths of three resin cements. J Oral Rehabil 2001;28:14-19. (Pubitemid 33754604)
    • (2001) Journal of Oral Rehabilitation , vol.28 , Issue.1 , pp. 14-19
    • Yoshida, K.1    Kamada, K.2    Sawase, T.3    Atsuta, M.4
  • 23
    • 0033135430 scopus 로고    scopus 로고
    • A study on the adsorption structure of an adhesive monomer for precious metals by surface-enhanced Raman scattering spectroscopy
    • DOI 10.1016/S0142-9612(98)00238-5, PII S0142961298002385
    • Suzuki M, Fujishima A, Miyazaki T, Hisamitsu H, Kojima K, Kadoma Y. A study on the adsorption structure of an adhesive monomer for precious metals by surface-enhanced Raman scattering spectroscopy. Biomaterials 1999;20:839-845. (Pubitemid 29184765)
    • (1999) Biomaterials , vol.20 , Issue.9 , pp. 839-845
    • Suzuki, M.1    Fujishima, A.2    Miyazaki, T.3    Hisamitsu, H.4    Kojima, K.5    Kadoma, Y.6
  • 24
    • 0031598657 scopus 로고    scopus 로고
    • Bonding to zirconia ceramic: Adhesion methods and their durability
    • PII S01095641980000116
    • Kern M, Wegner SM. Bonding to zirconia ceramic: Adhesion methods and their durability. Dent Mater 1998;14:64-71. (Pubitemid 128419490)
    • (1998) Dental Materials , vol.14 , Issue.1 , pp. 64-71
    • Kern, M.1    Wegner, S.M.2
  • 25
    • 0029266741 scopus 로고
    • Bonding to a glass infiltrated alumina ceramic: Adhesion methods and their durability
    • Kern M, Thompson VP. Bonding to a glass infiltrated alumina ceramic: Adhesion methods and their durability. J Prosthet Dent 1995;73:240-249.
    • (1995) J Prosthet Dent , vol.73 , pp. 240-249
    • Kern, M.1    Thompson, V.P.2
  • 26
    • 1842855215 scopus 로고    scopus 로고
    • Durability of the resin bond strength to the alumina ceramic Procera
    • Hummel M, Kern M. Durability of the resin bond strength to the alumina ceramic Procera. Dent Mater 2004;20:498-508.
    • (2004) Dent Mater , vol.20 , pp. 498-508
    • Hummel, M.1    Kern, M.2
  • 27
    • 30344433724 scopus 로고    scopus 로고
    • Effect of thermocycling on bond strength of luting cements to zirconia ceramic
    • DOI 10.1016/j.dental.2005.04.016, PII S0109564105001569
    • Lüthy H, Loeffel O, Hammerle CH. Effect of thermocycling on bond strength of luting cements to zirconia ceramic. Dent Mater 2006;22:195-200. (Pubitemid 43061319)
    • (2006) Dental Materials , vol.22 , Issue.2 , pp. 195-200
    • Luthy, H.1    Loeffel, O.2    Hammerle, C.H.F.3
  • 28
    • 0034208413 scopus 로고    scopus 로고
    • Long-term resin bond strength to zirconia ceramic
    • Wegner SM, Kern M. Long-term resin bond strength to zirconia ceramic. J Adhes Dent 2000;2:139-147.
    • (2000) J Adhes Dent , vol.2 , pp. 139-147
    • Wegner, S.M.1    Kern, M.2
  • 30
    • 38049076540 scopus 로고    scopus 로고
    • Microtensile bond strength of different components of core veneered all-ceramic restorations. Part 3: Double veneer technique
    • Aboushelib MN, Kleverlaan CJ, Feilzer AJ. Microtensile bond strength of different components of core veneered all-ceramic restorations. Part 3: Double veneer technique. J Prosthodont 2008;17:9-13.
    • (2008) J Prosthodont , vol.17 , pp. 9-13
    • Aboushelib, M.N.1    Kleverlaan, C.J.2    Feilzer, A.J.3
  • 31
    • 12444251147 scopus 로고    scopus 로고
    • Bonding of an auto-adhesive luting material to enamel and dentin
    • DOI 10.1016/j.dental.2004.03.002, PII S0109564104000338
    • De Munck J, Vargas M, Van Landuyt K, Hikita K, Lambrechts P, Van Meerbeek B. Bonding of an auto-adhesive luting material to enamel and dentin. Dent Mater 2004;20: 963-971. (Pubitemid 40146126)
    • (2004) Dental Materials , vol.20 , Issue.10 , pp. 963-971
    • De Munck, J.1    Vargas, M.2    Van Landuyt, K.3    Hikita, K.4    Lambrechts, P.5    Van Meerbeek, B.6


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.