Volumn 2, Issue 6, 2008, Pages 439-456

Nanoscratch behaviour, structure and nanoindentation of multilayer TiN/CrN coatings

Author keywords

Delamination; Nanoindentation; Nanoscratch; Residual stress; TiN CrN nanolaminates; X ray Diffraction; XTEM

Indexed keywords

DELAMINATION; ELASTIC DEFORMATION; ELASTOPLASTICITY; MONOLAYERS; MULTILAYERS; NANOINDENTATION; NANOTECHNOLOGY; RESIDUAL STRESSES; TITANIUM NITRIDE; UNLOADING; X RAY DIFFRACTION;

EID: 58149394320     PISSN: 1749785X     EISSN: 17497868     Source Type: Journal    
DOI: 10.1504/IJSURFSE.2008.022284     Document Type: Article
Times cited : (4)

References (24)
  • 1
    • 36148958283 scopus 로고    scopus 로고
    • Stress, interfacial effects and mechanical properties of nanoscale multilayered coatings
    • Abadias, G., Michel, A., Tromas, C., Jaouen, C. and Dub, S.N. (2007) 'Stress, interfacial effects and mechanical properties of nanoscale multilayered coatings', Surface and Coatings Technology, Vol. 202, pp.844-853.
    • (2007) Surface and Coatings Technology , vol.202 , pp. 844-853
    • Abadias, G.1    Michel, A.2    Tromas, C.3    Jaouen, C.4    Dub, S.N.5
  • 2
    • 0037331265 scopus 로고    scopus 로고
    • Deposition of TiN/CrN hard superlatiices by reactive d.c. magnetron sputtering
    • Barshilia, H.C. and Rajam, K.S. (2003) 'Deposition of TiN/CrN hard superlatiices by reactive d.c. magnetron sputtering', Bull. Mater. Sci., Vol. 26, No. 2, pp.233-237.
    • (2003) Bull. Mater. Sci , vol.26 , Issue.2 , pp. 233-237
    • Barshilia, H.C.1    Rajam, K.S.2
  • 3
    • 0142217260 scopus 로고    scopus 로고
    • Structure, hardness and thermal stability of nanolayered TiN/CrN multilayer coatings
    • Barshilia, H.C., Jain, A., and Rajam, K.S. (2004) 'Structure, hardness and thermal stability of nanolayered TiN/CrN multilayer coatings', Vacuum, Vol. 72, pp.241-248.
    • (2004) Vacuum , vol.72 , pp. 241-248
    • Barshilia, H.C.1    Jain, A.2    Rajam, K.S.3
  • 4
    • 10844239699 scopus 로고    scopus 로고
    • Structure, hardness and thermal stability of TiAIN and nanolayered TiAlN/CrN multilayer coatings
    • Barshilia, H.C., Surya Prakash, M., Jain, A. and Rajam, K.S. (2005) 'Structure, hardness and thermal stability of TiAIN and nanolayered TiAlN/CrN multilayer coatings', Vacuum, Vol. 77, pp. 169-179.
    • (2005) Vacuum , vol.77 , pp. 169-179
    • Barshilia, H.C.1    Surya Prakash, M.2    Jain, A.3    Rajam, K.S.4
  • 5
    • 21344474540 scopus 로고    scopus 로고
    • Nanotribological and nanomechanical properties of 5-80 nm tetrahedral amorphous carbon films on silicon
    • Beake, B.D. and Lau, S.P. (2005) 'Nanotribological and nanomechanical properties of 5-80 nm tetrahedral amorphous carbon films on silicon', Diamond and Related Materials, Vol. 14, pp.1535-1542.
    • (2005) Diamond and Related Materials , vol.14 , pp. 1535-1542
    • Beake, B.D.1    Lau, S.P.2
  • 6
    • 0031191696 scopus 로고    scopus 로고
    • Failure mode maps in thin film scratch adhesion tests
    • Bull, S.J. (1997) 'Failure mode maps in thin film scratch adhesion tests', Tribology International, Vol. 30, No. 7, pp.491-498.
    • (1997) Tribology International , vol.30 , Issue.7 , pp. 491-498
    • Bull, S.J.1
  • 7
    • 17644378376 scopus 로고    scopus 로고
    • Nanomechanical and nanotribological properties of carbon based films
    • Charitidis, C. and Logothetidis, S. (2005) 'Nanomechanical and nanotribological properties of carbon based films', Thin Solid Films Vol. 482, pp.120-125.
    • (2005) Thin Solid Films , vol.482 , pp. 120-125
    • Charitidis, C.1    Logothetidis, S.2
  • 8
    • 0033894298 scopus 로고    scopus 로고
    • A comparative study of the nanoscratching behavior of amorphous carbon films grown under various deposition conditions
    • Charitidis, C., Logothetidis, S. and Gioti, M. (2000) 'A comparative study of the nanoscratching behavior of amorphous carbon films grown under various deposition conditions', Surface and Coatings Technology Vol. 125, p.201.
    • (2000) Surface and Coatings Technology , vol.125 , pp. 201
    • Charitidis, C.1    Logothetidis, S.2    Gioti, M.3
  • 9
    • 1842815872 scopus 로고    scopus 로고
    • Historical developments and new trends in tribological and solid lubricant coatings
    • Vols
    • Donnet, C. and Erdemir, A. (2004) 'Historical developments and new trends in tribological and solid lubricant coatings', Surface and Coatings Technology, Vols. 180-181, pp. 76-84.
    • (2004) Surface and Coatings Technology , vol.180-181 , pp. 76-84
    • Donnet, C.1    Erdemir, A.2
  • 10
    • 3843073046 scopus 로고    scopus 로고
    • The nano-scratch behaviour of different diamond-like carbon film-substrate systems
    • Huang, L-Y., Lu, J. and Xu, K-W. (2004) 'The nano-scratch behaviour of different diamond-like carbon film-substrate systems', Journal of Physics D: Applied Physics, Vol. 37, pp.2135-2139.
    • (2004) Journal of Physics D: Applied Physics , vol.37 , pp. 2135-2139
    • Huang, L.-Y.1    Lu, J.2    Xu, K.-W.3
  • 11
    • 0035423792 scopus 로고    scopus 로고
    • Nano-scratch and fretting wear study of DLC coatings for biomedical application
    • Huang, L-Y., Xu, K-W., Lub, J., Guelorget, B. and Chena, H. (2002) 'Nano-scratch and fretting wear study of DLC coatings for biomedical application', Diamond and Related Materials, Vol. 10, pp. 1448-1456.
    • (2002) Diamond and Related Materials , vol.10 , pp. 1448-1456
    • Huang, L.-Y.1    Xu, K.-W.2    Lub, J.3    Guelorget, B.4    Chena, H.5
  • 12
    • 1342268810 scopus 로고    scopus 로고
    • Design criteria for wear-resistant nanostructured and glassy-metal coatings
    • Vols
    • Leyland, A. and Matthews, A. (2004) 'Design criteria for wear-resistant nanostructured and glassy-metal coatings', Surface and Coatings Technology, Vols. 177-178, pp.317-324.
    • (2004) Surface and Coatings Technology , vol.177-178 , pp. 317-324
    • Leyland, A.1    Matthews, A.2
  • 13
    • 0036564749 scopus 로고    scopus 로고
    • Initial growth and texture formation during reactive magnetron sputtering of TiN on Si(111)
    • Li, T.Q., Noda, S., Tsuji, Y., Ohsawa, T. and Komiyarna, H. (2002) 'Initial growth and texture formation during reactive magnetron sputtering of TiN on Si(111)', J. Vac. Sci. Technol. A, Vol. 20, No. 3, pp.583-588.
    • (2002) J. Vac. Sci. Technol. A , vol.20 , Issue.3 , pp. 583-588
    • Li, T.Q.1    Noda, S.2    Tsuji, Y.3    Ohsawa, T.4    Komiyarna, H.5
  • 14
    • 27144553745 scopus 로고    scopus 로고
    • Residual stresses of diamond and diamondlike carbon films
    • 073515/5
    • Liu, E., Li, L., Blanpain, B. and Celis, J.P. (2005) 'Residual stresses of diamond and diamondlike carbon films', Journal of Applied Physics Vol. 98, pp.073515/1-073515/5.
    • (2005) Journal of Applied Physics , vol.98 , pp. 073515-73521
    • Liu, E.1    Li, L.2    Blanpain, B.3    Celis, J.P.4
  • 15
    • 0033506669 scopus 로고    scopus 로고
    • TEM observations of wear mechanisms of TiAlCrN and TiAlN/CrN coatings grown by combined steered-arc/unbalanced magnetron deposition
    • Vols
    • Luo, Q., Rainforth, W.M. and Munz, W-D. (1999) 'TEM observations of wear mechanisms of TiAlCrN and TiAlN/CrN coatings grown by combined steered-arc/unbalanced magnetron deposition', Wear, Vols. 225-229, pp.74-82.
    • (1999) Wear , vol.225-229 , pp. 74-82
    • Luo, Q.1    Rainforth, W.M.2    Munz, W.-D.3
  • 16
    • 24644520755 scopus 로고    scopus 로고
    • Formation of a semiconductive surface film on nanomultilayered TiN/CrN coatings and its correlation with corrosion protection of steel
    • Mendibide, C., Steyer, P. and Millet, J-P. (2005) 'Formation of a semiconductive surface film on nanomultilayered TiN/CrN coatings and its correlation with corrosion protection of steel', Surface and Coatings Technology, Vol. 200, pp.109-112.
    • (2005) Surface and Coatings Technology , vol.200 , pp. 109-112
    • Mendibide, C.1    Steyer, P.2    Millet, J.-P.3
  • 17
    • 33751275786 scopus 로고    scopus 로고
    • Improvement of the tribological behaviour of PVD nanostratified TiN/CrN coatings - an explanation
    • Mendibide, C., Steyer, P., Fontaine, J. and Goudeau, P. (2006) 'Improvement of the tribological behaviour of PVD nanostratified TiN/CrN coatings - an explanation,' Surface and Coatings Technology, Vol. 201, pp.4119-4124.
    • (2006) Surface and Coatings Technology , vol.201 , pp. 4119-4124
    • Mendibide, C.1    Steyer, P.2    Fontaine, J.3    Goudeau, P.4
  • 18
    • 41949121582 scopus 로고    scopus 로고
    • Increase of hardness and oxidation resistance of VN coating by nanoscale multilayered structurization with AIN
    • Park, J-K. and Baik, Y-J. (2008) 'Increase of hardness and oxidation resistance of VN coating by nanoscale multilayered structurization with AIN', Materials Letters, Vol. 62, pp.2528-2530.
    • (2008) Materials Letters , vol.62 , pp. 2528-2530
    • Park, J.-K.1    Baik, Y.-J.2
  • 19
    • 0036470387 scopus 로고    scopus 로고
    • Preferred orientation and hardness enhancement of TiN/CrN superlattice coatings deposited by reactive magnetron sputtering
    • Yang, Q., He, C., Zhao, L.R. and Immarigeon, J-P. (2002) 'Preferred orientation and hardness enhancement of TiN/CrN superlattice coatings deposited by reactive magnetron sputtering', Scripta Materialia, Vol. 46, pp.293-297.
    • (2002) Scripta Materialia , vol.46 , pp. 293-297
    • Yang, Q.1    He, C.2    Zhao, L.R.3    Immarigeon, J.-P.4
  • 20
    • 0036720572 scopus 로고    scopus 로고
    • Effect of film thickness on the stress and adhesion of diamond-like carbon coatings
    • Sheeja, D., Tay, B.K., Leong, K.W. and Lee, C.H. (2002) 'Effect of film thickness on the stress and adhesion of diamond-like carbon coatings', Diamond and Related Materials, Vol. 11, pp.1643-1647.
    • (2002) Diamond and Related Materials , vol.11 , pp. 1643-1647
    • Sheeja, D.1    Tay, B.K.2    Leong, K.W.3    Lee, C.H.4
  • 21
    • 0031235205 scopus 로고    scopus 로고
    • Mechanical properties of ceramic multilayers: TiN/CrN, TiN/ZrN andTiN/TaN
    • Soe, W-H. and Yamamoto, R. (1997) 'Mechanical properties of ceramic multilayers: TiN/CrN, TiN/ZrN andTiN/TaN', Materials Chemisny and Physics, Vol. 50, pp.176-181.
    • (1997) Materials Chemisny and Physics , vol.50 , pp. 176-181
    • Soe, W.-H.1    Yamamoto, R.2
  • 22
    • 38149091839 scopus 로고    scopus 로고
    • Mechanical and tribological properties of multilayered TiSiN/CrN coatings synthesized by a cathodic arc deposition process
    • Yang, S-M., Chang,Y-Y., Lin, D-Y., Wang, D-Y. and Wu, W. (2008) 'Mechanical and tribological properties of multilayered TiSiN/CrN coatings synthesized by a cathodic arc deposition process', Surface and Coatings Technology, Vol. 202, pp.2176-2181.
    • (2008) Surface and Coatings Technology , vol.202 , pp. 2176-2181
    • Yang, S.-M.1    Chang, Y.-Y.2    Lin, D.-Y.3    Wang, D.-Y.4    Wu, W.5
  • 23
    • 0032394142 scopus 로고    scopus 로고
    • Structure and mechanical properties of polycrystalline CrN/TiN superlattices
    • Yashar, P., Barnett, S.A., Rechner, J. and Sproul, W.D. (1998) 'Structure and mechanical properties of polycrystalline CrN/TiN superlattices', J. Vac. Sci. Technol., Vol. A16, No. 50, pp.2913-2918.
    • (1998) J. Vac. Sci. Technol , vol.A16 , Issue.50 , pp. 2913-2918
    • Yashar, P.1    Barnett, S.A.2    Rechner, J.3    Sproul, W.D.4
  • 24
    • 18744379452 scopus 로고    scopus 로고
    • Nanoindentation and nanoscratch behaviors of DLC coatings on different steel substrates
    • Zhang, T.H. and Huan, Y. (2005) 'Nanoindentation and nanoscratch behaviors of DLC coatings on different steel substrates', Composites Science and Technology, Vol. 65, pp.1409-1413.
    • (2005) Composites Science and Technology , vol.65 , pp. 1409-1413
    • Zhang, T.H.1    Huan, Y.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.