메뉴 건너뛰기




Volumn 89, Issue 11, 2006, Pages 3481-3490

Monazite coatings on SiC fibers II: Oxidation protection

Author keywords

[No Author keywords available]

Indexed keywords

OXIDE-SCALE GROWTH RATE; PARABOLIC KINETICS; SILICA OXIDATION; UNCOATED FIBERS;

EID: 33750282009     PISSN: 00027820     EISSN: 15512916     Source Type: Journal    
DOI: 10.1111/j.1551-2916.2006.01241.x     Document Type: Article
Times cited : (37)

References (91)
  • 1
    • 0026097278 scopus 로고
    • Some new perspective on oxidation of silicon carbide and silicon nitride
    • K. L. Luthra, "Some New Perspective on Oxidation of Silicon Carbide and Silicon Nitride," J. Am. Ceram. Soc., 74, 1095-103 (1990).
    • (1990) J. Am. Ceram. Soc. , vol.74 , pp. 1095-1103
    • Luthra, K.L.1
  • 2
    • 0025414938 scopus 로고
    • Oxidation of silicon carbide-reinforced oxide-matrix composites at 1375 to 1575°C
    • K. L. Luthra and H. D. Park, "Oxidation of Silicon Carbide-Reinforced Oxide-Matrix Composites at 1375 to 1575°C," J. Am. Ceram. Soc., 73, 1014-23 (1990).
    • (1990) J. Am. Ceram. Soc. , vol.73 , pp. 1014-1023
    • Luthra, K.L.1    Park, H.D.2
  • 4
    • 0032655394 scopus 로고    scopus 로고
    • Variation of oxidation rate of silicon carbide with water-vapor pressure
    • E. J. Opila, "Variation of Oxidation Rate of Silicon Carbide with Water-Vapor Pressure," J. Am. Ceram. Soc., 82, 625-36 (1999).
    • (1999) J. Am. Ceram. Soc. , vol.82 , pp. 625-636
    • Opila, E.J.1
  • 5
    • 0032119878 scopus 로고    scopus 로고
    • Combined effects of exposure to salt (NaCl) water and oxidation on the strength of uncoated and BN-coated nicalon™ fibers
    • T. A. Parthasarathy, C. A. Folsom, and L. P. Zawada, "Combined Effects of Exposure to Salt (NaCl) Water and Oxidation on the Strength of Uncoated and BN-Coated Nicalon™ Fibers," J. Am. Ceram. Soc., 81, 1812-8 (1998).
    • (1998) J. Am. Ceram. Soc. , vol.81 , pp. 1812-1818
    • Parthasarathy, T.A.1    Folsom, C.A.2    Zawada, L.P.3
  • 6
    • 0037302361 scopus 로고    scopus 로고
    • Effectiveness of monazite coatings in oxide/oxide composites in extending life after long-term exposure at high-temperature
    • K. A. Keller, T. Mah. T. A. Parthasarathy, E. E. Boakye, P. Mogilevsky, and M. K. Cinibulk, "Effectiveness of Monazite Coatings in Oxide/Oxide Composites in Extending Life after Long-Term Exposure at High-Temperature," J. Am. Ceram. Soc., 86, 325-32 (2003).
    • (2003) J. Am. Ceram. Soc. , vol.86 , pp. 325-332
    • Keller, K.A.1    Mah, T.2    Parthasarathy, T.A.3    Boakye, E.E.4    Mogilevsky, P.5    Cinibulk, M.K.6
  • 8
    • 0035789796 scopus 로고    scopus 로고
    • Development of Si-M-C-(O) tyranno fiber containing a small amount of sol-gel-derived oxide
    • K. Kumagawa, H. Yamaoka, M. Shibuya, and T. Yamamura, "Development of Si-M-C-(O) Tyranno Fiber Containing a Small Amount of Sol-Gel-Derived Oxide," Ceram. Eng. Sci. Proc., 22, 399-406 (2001).
    • (2001) Ceram. Eng. Sci. Proc. , vol.22 , pp. 399-406
    • Kumagawa, K.1    Yamaoka, H.2    Shibuya, M.3    Yamamura, T.4
  • 9
    • 0035789693 scopus 로고    scopus 로고
    • A thermally conductive SiC-polycrystalline fiber and its fiber-bonded ceramic
    • T. Ishikawa, M. Sato, S. Kajii, Y. Tanaka, and M. Suzuki, "A Thermally Conductive SiC-Polycrystalline Fiber and its Fiber-Bonded Ceramic," Ceram. Ens. Sci. Proc., 22, 471-80 (2001).
    • (2001) Ceram. Ens. Sci. Proc. , vol.22 , pp. 471-480
    • Ishikawa, T.1    Sato, M.2    Kajii, S.3    Tanaka, Y.4    Suzuki, M.5
  • 10
    • 0034539781 scopus 로고    scopus 로고
    • SYLRAMIC™ SiC fibers for CMC reinforcement
    • R. E. Jones, D. Petrak, J. Rabe, and A. Szweda, "SYLRAMIC™ SiC Fibers for CMC Reinforcement," J. Nuclear Mater., 283-287, 556-9 (2000).
    • (2000) J. Nuclear Mater. , vol.283-287 , pp. 556-559
    • Jones, R.E.1    Petrak, D.2    Rabe, J.3    Szweda, A.4
  • 13
    • 0041639510 scopus 로고    scopus 로고
    • Monazite coatings on fibers: II: Coating without strength degradation
    • E. E. Boakye, R. S. Hay, P. Mogilevsky, and L. M. Douglas, "Monazite Coatings on Fibers: II: Coating Without Strength Degradation," J. Am. Ceram. Soc., 84, 2793-801 (2001).
    • (2001) J. Am. Ceram. Soc. , vol.84 , pp. 2793-2801
    • Boakye, E.E.1    Hay, R.S.2    Mogilevsky, P.3    Douglas, L.M.4
  • 14
    • 0033667099 scopus 로고    scopus 로고
    • Monazite coalings on nextel 720™, 610™, and tyranno-sa fiber tows; effects of precursors on fiber strength
    • E. E. Boakye, M. D. Petry, R. S. Hay, and L. M. Douglas, "Monazite Coalings on Nextel 720™, 610™, and Tyranno-SA Fiber Tows; Effects of Precursors on Fiber Strength," Ceram. Eng. Sci. Proc., 21, 229-36 (2000).
    • (2000) Ceram. Eng. Sci. Proc. , vol.21 , pp. 229-236
    • Boakye, E.E.1    Petry, M.D.2    Hay, R.S.3    Douglas, L.M.4
  • 15
    • 84859696616 scopus 로고
    • "Method for Coating Continuous Tows"; U.S. Patent #5,217,533
    • R. S. Hay, "Method for Coating Continuous Tows"; U.S. Patent #5,217,533, 1993.
    • (1993)
    • Hay, R.S.1
  • 16
    • 0033189440 scopus 로고    scopus 로고
    • Continuous coating of oxide fiber tows using liquid precursors: Monazite coatings on nextel 720
    • E. Boakye, R. S. Hay, and M. D. Petry, "Continuous Coating of Oxide Fiber Tows Using Liquid Precursors: Monazite Coatings on Nextel 720," J. Am. Ceram. Soc., 82, 2321-31 (1999).
    • (1999) J. Am. Ceram. Soc. , vol.82 , pp. 2321-2331
    • Boakye, E.1    Hay, R.S.2    Petry, M.D.3
  • 17
    • 0029291341 scopus 로고
    • Influence of alumina reaction tube impurities on the oxidation of chemically-vapor-deposiled silicon carbide
    • E. Opila, "Influence of Alumina Reaction Tube Impurities on the Oxidation of Chemically-Vapor-Deposiled Silicon Carbide," J. Am Ceram. Soc., 78, 1107-10 (1995).
    • (1995) J. Am Ceram. Soc. , vol.78 , pp. 1107-1110
    • Opila, E.1
  • 18
  • 19
    • 84987344259 scopus 로고
    • Oxidation kinetics of silicon carbide crystals and ceramics: I. In dry oxygen
    • J. A. Costello and R. A. Tressler, "Oxidation Kinetics of Silicon Carbide Crystals and Ceramics: I. In Dry Oxygen," J. Am. Ceram. Soc., 69, 674-81 (1986).
    • (1986) J. Am. Ceram. Soc. , vol.69 , pp. 674-681
    • Costello, J.A.1    Tressler, R.A.2
  • 21
    • 0030244427 scopus 로고    scopus 로고
    • Method for preparation of TEM specimens of coated fibers
    • M. K. Cinibulk, J. R. Welch, and R. S. Hay, "Method for Preparation of TEM Specimens of Coated Fibers," J. Am. Ceram. Soc., 79, 2481-4 (1996).
    • (1996) J. Am. Ceram. Soc. , vol.79 , pp. 2481-2484
    • Cinibulk, M.K.1    Welch, J.R.2    Hay, R.S.3
  • 22
    • 0031251201 scopus 로고    scopus 로고
    • TEM specimen preparation and characterization of ceramic coatings on fiber tows
    • R. S. Hay, J. R. Welch, and M. K. Cinibulk, "TEM Specimen Preparation and Characterization of Ceramic Coatings on Fiber Tows," Thin Solid Films, 308-309, 389-92 (1997).
    • (1997) Thin Solid Films , vol.308-309 , pp. 389-392
    • Hay, R.S.1    Welch, J.R.2    Cinibulk, M.K.3
  • 23
    • 33845561817 scopus 로고
    • Statistical significance of linear least-squares parameters
    • M. D. Pattengill and D. E. Sands, "Statistical Significance of Linear Least-Squares Parameters," J. Chain. Educ., 56, 244-7 (1979).
    • (1979) J. Chain. Educ. , vol.56 , pp. 244-247
    • Pattengill, M.D.1    Sands, D.E.2
  • 24
    • 0016428180 scopus 로고
    • Oxidation of 6h-alpha silicon carbide platelets
    • R. C. A. Harris, "Oxidation of 6h-Alpha Silicon Carbide Platelets," J. Am. Ceram. Soc., 58, 7-9 (1975).
    • (1975) J. Am. Ceram. Soc. , vol.58 , pp. 7-9
    • Harris, R.C.A.1
  • 25
    • 84859672293 scopus 로고    scopus 로고
    • National Institute of Standards and Technology (NIST) and the National Institutes of Health (NIH)
    • C. Fiori, C. Swyt-Thomas, and R. Myklebust. National Institute of Standards and Technology (NIST) and the National Institutes of Health (NIH) (available at http://www.cstl.nist.gov/div837/Division/outputs/DTSA/DTSA.htm).
    • Fiori, C.1    Swyt-Thomas, C.2    Myklebust, R.3
  • 26
    • 0036501436 scopus 로고    scopus 로고
    • Characterization of the medium-range structure of Si-Al-C-O, Si-Zr-C-O and Si-Al-C tyranno fibers by small angle x-ray scattering
    • K. Suzuki, K. Kumagawa, T. Kamiyama, and M. Shibuya, " Characterization of the Medium-Range Structure of Si-Al-C-O, Si-Zr-C-O and Si-Al-C Tyranno Fibers by Small Angle X-Ray Scattering," J. Mater. Sci., 37, 949-53 (2002).
    • (2002) J. Mater. Sci. , vol.37 , pp. 949-953
    • Suzuki, K.1    Kumagawa, K.2    Kamiyama, T.3    Shibuya, M.4
  • 27
    • 0141572304 scopus 로고    scopus 로고
    • Long term oxidation of a SiC fiber-bonded composite in air at 1500°C
    • A. Otsuka, Y. Matsumura, K. Hosono, and R. Tanaka, "Long Term Oxidation of a SiC Fiber-Bonded Composite in Air at 1500°C," J. Eur. Ceram. Soc., 23, 3125-34 (2003).
    • (2003) J. Eur. Ceram. Soc. , vol.23 , pp. 3125-3134
    • Otsuka, A.1    Matsumura, Y.2    Hosono, K.3    Tanaka, R.4
  • 28
    • 0028403925 scopus 로고
    • Oxidation kinetics of chemically vapor-deposited silicon carbide in wet oxygen
    • E. J. Opila, "Oxidation Kinetics of Chemically Vapor-Deposited Silicon Carbide in Wet Oxygen," J. Am. Ceram. Soc., 77, 730-6 (1994).
    • (1994) J. Am. Ceram. Soc. , vol.77 , pp. 730-736
    • Opila, E.J.1
  • 29
    • 84975376970 scopus 로고
    • Thermal oxidation and electrolytic etching of silicon carbide
    • W. von Munch and I. Pfaffeneder, "Thermal Oxidation and Electrolytic Etching of Silicon Carbide," J. Electrochem. Soc., 122, 642-3 (1975).
    • (1975) J. Electrochem. Soc. , vol.122 , pp. 642-643
    • Von Munch, W.1    Pfaffeneder, I.2
  • 30
    • 0034333550 scopus 로고    scopus 로고
    • Oxidation behaviour of ceramic fibres from the Si-C-N-O system and related sub-systems
    • G. Chollon, "Oxidation Behaviour of Ceramic Fibres from the Si-C-N-O System and Related Sub-Systems," J. Eur. Ceram. Soc., 20, 1959-74 (2000).
    • (2000) J. Eur. Ceram. Soc. , vol.20 , pp. 1959-1974
    • Chollon, G.1
  • 31
    • 0030652313 scopus 로고    scopus 로고
    • Structure and properties of SYLRAMIC™ silicon carbide fiber - A polycrystalline, stoichiometric β-SiC composition
    • J. Lipowitz, J. A. Rabe, A. Zangvil, and Y. Xu, "Structure and Properties of SYLRAMIC™ Silicon Carbide Fiber - A Polycrystalline, Stoichiometric β-SiC Composition," Ceram. Eng. Sci. Proc. A, 18, 147-57 (1997).
    • (1997) Ceram. Eng. Sci. Proc. A , vol.18 , pp. 147-157
    • Lipowitz, J.1    Rabe, J.A.2    Zangvil, A.3    Xu, Y.4
  • 32
    • 0032297844 scopus 로고    scopus 로고
    • The role of substitutional boron in carbon oxidation
    • L. R. Radovic, M. Karra, K. Skokova, and P. A. Thrower, "The Role of Substitutional Boron in Carbon Oxidation," Carbon, 36, 1841-54 (1998).
    • (1998) Carbon , vol.36 , pp. 1841-1854
    • Radovic, L.R.1    Karra, M.2    Skokova, K.3    Thrower, P.A.4
  • 33
    • 0015382412 scopus 로고
    • Effect of absorbed phosphorus oxychloride on the oxidation behavior of graphite
    • D. W. McKee, "Effect of Absorbed Phosphorus Oxychloride on the Oxidation Behavior of Graphite," Carbon, 10, 491 (1972).
    • (1972) Carbon , vol.10 , pp. 491
    • McKee, D.W.1
  • 34
    • 23144464677 scopus 로고    scopus 로고
    • The influence of aluminum phosphates on graphite oxidation
    • C. R. Maier and L. E. Jones, "The Influence of Aluminum Phosphates on Graphite Oxidation," Carbon, 43, 2272-6 (2005).
    • (2005) Carbon , vol.43 , pp. 2272-2276
    • Maier, C.R.1    Jones, L.E.2
  • 35
    • 17744409239 scopus 로고    scopus 로고
    • Improvement of the oxidation resistance of TiAl Alloys by using the chlorine effect
    • M. Schütze and M. Hald, "Improvement of the Oxidation Resistance of TiAl Alloys by Using the Chlorine Effect," Mater. Sci. Eng. A, 239-240, 847-58 (1997).
    • (1997) Mater. Sci. Eng. A , vol.239-240 , pp. 847-858
    • Schütze, M.1    Hald, M.2
  • 39
    • 0012765188 scopus 로고    scopus 로고
    • Investigations of the microalloying effect of chlorine in the oxidation of TiAl alloys
    • G. Schumacher, F. Dettenwanger, and M. Schutze, "Investigations of the Microalloying Effect of Chlorine in the Oxidation of TiAl Alloys," Mater. High Temperatures, 17, 53-8 (2000).
    • (2000) Mater. High Temperatures , vol.17 , pp. 53-58
    • Schumacher, G.1    Dettenwanger, F.2    Schutze, M.3
  • 42
    • 0032083695 scopus 로고    scopus 로고
    • A phosphoric acid surface treatment for improved oxidation resistance of gamma titanium aluminides
    • W. B. Retallick, M. P. Brady, and D. L. Humphrey, "A Phosphoric Acid Surface Treatment for Improved Oxidation Resistance of Gamma Titanium Aluminides," Intermetallics, 6, 335-7 (1998).
    • (1998) Intermetallics , vol.6 , pp. 335-337
    • Retallick, W.B.1    Brady, M.P.2    Humphrey, D.L.3
  • 43
    • 0034299925 scopus 로고    scopus 로고
    • XRD investigations of the phosphorus effect on the oxidation of TiAl alloys by high-resolution methods
    • G. Schumacher, F. Dettenwanger, M. Schutze, A. Iberl, and D. D. Reil, "XRD Investigations of the Phosphorus Effect on the Oxidation of TiAl Alloys by High-Resolution Methods," Oxidation Metals, 54, 317-37 (2000).
    • (2000) Oxidation Metals , vol.54 , pp. 317-337
    • Schumacher, G.1    Dettenwanger, F.2    Schutze, M.3    Iberl, A.4    Reil, D.D.5
  • 44
    • 0030114875 scopus 로고    scopus 로고
    • 3 II. Oxygen diffusion in undoped single crystals
    • 3 II. Oxygen Diffusion in Undoped Single Crystals," Philos. Mag. A, 73, 899-917 (1996).
    • (1996) Philos. Mag. A , vol.73 , pp. 899-917
    • Prot, D.1    Monty, C.2
  • 45
    • 0030115080 scopus 로고    scopus 로고
    • 3 IV. Oxygen grain-boundary self-diffusion in undoped and yttria-doped alumina polycryslals
    • 3 IV. Oxygen Grain-Boundary Self-Diffusion in Undoped and Yttria-Doped Alumina Polycryslals," Philos. Mag. A, 73, 935-49 (1996).
    • (1996) Philos. Mag. A , vol.73 , pp. 935-949
    • Prot, D.1    Le Gall, M.2    Lesage, B.3    Huntz, A.M.4    Monty, C.5
  • 47
    • 0001652254 scopus 로고
    • Permeation of gaseous oxygen through vitreous silica
    • F. J. Norton, "Permeation of Gaseous Oxygen Through Vitreous Silica," Nature, 191, 701 (1961).
    • (1961) Nature , vol.191 , pp. 701
    • Norton, F.J.1
  • 48
    • 84977251912 scopus 로고
    • Diffusion of oxygen in fused silica
    • E. L. Williams, "Diffusion of Oxygen in Fused Silica," j. Am. Ceram. Soc., 48, 190-4 (1965).
    • (1965) J. Am. Ceram. Soc. , vol.48 , pp. 190-194
    • Williams, E.L.1
  • 49
    • 0037387536 scopus 로고    scopus 로고
    • Impurity effects on alumina scale growth
    • P. Y. Hou, "Impurity Effects on Alumina Scale Growth," J. Am. Ceram. Soc., 86, 660-8 (2003).
    • (2003) J. Am. Ceram. Soc. , vol.86 , pp. 660-668
    • Hou, P.Y.1
  • 52
    • 0022101566 scopus 로고
    • Oxidation of ion-implanted titanium in the 750-950&C temperature range
    • M. Pons, M. Caillet, and A. Galerie, "Oxidation of Ion-Implanted Titanium in the 750-950&C Temperature Range," J. Less-Comm. Metals, 109, 45-56 (1985).
    • (1985) J. Less-comm. Metals , vol.109 , pp. 45-56
    • Pons, M.1    Caillet, M.2    Galerie, A.3
  • 54
    • 1642621158 scopus 로고
    • General relationship for the thermal oxidation of silicon
    • B. E. Deal and A. S. Grove, "General Relationship for the Thermal Oxidation of Silicon," J. Appl. Phys., 36, 3770-8 (1965).
    • (1965) J. Appl. Phys. , vol.36 , pp. 3770-3778
    • Deal, B.E.1    Grove, A.S.2
  • 55
    • 9644258602 scopus 로고    scopus 로고
    • Transport of oxygen in silicate glasses
    • R. H. Doremus, "Transport of Oxygen in Silicate Glasses," J. Non-Cryst. Solids, 349, 242-7 (2004).
    • (2004) J. Non-cryst. Solids , vol.349 , pp. 242-247
    • Doremus, R.H.1
  • 56
    • 23044432054 scopus 로고    scopus 로고
    • 3. III. Measurements of dissolution kinetics, diffusion coefficient, and solubility by infrared photoluminescence
    • 3. III. Measurements of Dissolution Kinetics, Diffusion Coefficient, and Solubility by Infrared Photoluminescence," J. Appl. Phys., 98, 013529-1-013529-7 (2005).
    • (2005) J. Appl. Phys. , vol.98 , pp. 135291-135297
    • Kajihara, K.1    Kamioka, H.2    Hirano, M.3    Miura, T.4    Skuja, L.5    Hosono, H.6
  • 57
    • 0032658449 scopus 로고    scopus 로고
    • Gas solubility in glass principles and structural implications
    • J. F. Shackelford, "Gas Solubility in Glass Principles and Structural Implications," J. Non-Cryst. Solids, 253, 231-41 (1999).
    • (1999) J. Non-cryst. Solids , vol.253 , pp. 231-241
    • Shackelford, J.F.1
  • 59
    • 84944648082 scopus 로고
    • Revised effective ion radii and systematic studies of interatomic distances in halides and chalogenides
    • R. D. Shannon, "Revised Effective Ion Radii and Systematic Studies of Interatomic Distances in Halides and Chalogenides," Acta Crystallogr., A32, 751-67 (1976).
    • (1976) Acta Crystallogr. , vol.A32 , pp. 751-767
    • Shannon, R.D.1
  • 60
    • 9644272409 scopus 로고    scopus 로고
    • Inert gas solubility in binary germania-silioa glasses
    • C. C. Tournour and J. E. Shelby, "Inert Gas Solubility in Binary Germania-Silioa Glasses," J. Non-Cryst. Solids, 349, 209-14 (2004).
    • (2004) J. Non-cryst. Solids , vol.349 , pp. 209-214
    • Tournour, C.C.1    Shelby, J.E.2
  • 61
    • 0026961976 scopus 로고
    • Oxygen mobility in silicon dioxide and silicate glasses: A review
    • M. A. Lamkin and F. L. Riley, "Oxygen Mobility in Silicon Dioxide and Silicate Glasses: A Review," J. Eur. Ceram. Soc., 10, 347-67 (1992).
    • (1992) J. Eur. Ceram. Soc. , vol.10 , pp. 347-367
    • Lamkin, M.A.1    Riley, F.L.2
  • 62
    • 0015561541 scopus 로고
    • Effect of alkali oxides on the diffusion of helium in a simple borosilicate glass
    • V. O. Altemose, "Effect of Alkali Oxides on the Diffusion of Helium in a Simple Borosilicate Glass," J. Am. Ceram. Soc., 56, 1-4 (1973).
    • (1973) J. Am. Ceram. Soc. , vol.56 , pp. 1-4
    • Altemose, V.O.1
  • 63
    • 0015627914 scopus 로고
    • Effect of phase separation on helium migration in sodium silicate glasses
    • J. E. Shelby, "Effect of Phase Separation on Helium Migration in Sodium Silicate Glasses," J. Am. Ceram. Soc., 56, 263-6 (1973).
    • (1973) J. Am. Ceram. Soc. , vol.56 , pp. 263-266
    • Shelby, J.E.1
  • 66
    • 0345714589 scopus 로고    scopus 로고
    • Fiber lasers: Materials, structures and technologies
    • J. Kirchhof, S. Unger, and A. Schwuchow, "Fiber Lasers: Materials, Structures and Technologies," Proc. SPIE, 4957, 1 (2003).
    • (2003) Proc. SPIE , vol.4957 , pp. 1
    • Kirchhof, J.1    Unger, S.2    Schwuchow, A.3
  • 69
    • 0024607323 scopus 로고
    • Dopant redistribution during thermal oxidation of monocrystalline beta-SiC thin films
    • J. W. Palmour, R. F. Davis, H. S. Kong, S. F. Corcoran, and D. P. Griffis, "Dopant Redistribution During Thermal Oxidation of Monocrystalline Beta-SiC Thin Films," J. Electrochem. Soc., 136, 502-7 (1989).
    • (1989) J. Electrochem. Soc. , vol.136 , pp. 502-507
    • Palmour, J.W.1    Davis, R.F.2    Kong, H.S.3    Corcoran, S.F.4    Griffis, D.P.5
  • 70
    • 0017958446 scopus 로고
    • Thermal oxidation of heavily phosphorus-doped silicon
    • C. P. Ho, J. D. Plummer, B. E. Deal, and Meindl, "Thermal Oxidation of Heavily Phosphorus-Doped Silicon," J. Electrochem. Soc., 125, 665-71 (1978).
    • (1978) J. Electrochem. Soc. , vol.125 , pp. 665-671
    • Ho, C.P.1    Plummer, J.D.2    Deal, B.E.3    Meindl4
  • 71
    • 0017981216 scopus 로고
    • Thermal oxidation of phosphorus-doped polycrystalline silicon in wet oxygen
    • H. Sunami, "Thermal Oxidation of Phosphorus-Doped Polycrystalline Silicon in Wet Oxygen," J. Electrochem. Soc., 125, 892-7 (1978).
    • (1978) J. Electrochem. Soc. , vol.125 , pp. 892-897
    • Sunami, H.1
  • 72
    • 0020197410 scopus 로고
    • Thermal oxidation of heavily phosphorus-doped thin films of polycrystalline silicon
    • K. C. Saraswat and H. Singh, "Thermal Oxidation of Heavily Phosphorus-Doped Thin Films of Polycrystalline Silicon," J. Electrochem. Soc., 129, 2321-6 (1982).
    • (1982) J. Electrochem. Soc. , vol.129 , pp. 2321-2326
    • Saraswat, K.C.1    Singh, H.2
  • 73
    • 0012751637 scopus 로고
    • Reverse dopant redistribution during the initial stages of the oxidation of heavily doped silicon in dry oxygen
    • H. Z. Massoud, "Reverse Dopant Redistribution During the Initial Stages of the Oxidation of Heavily Doped Silicon in Dry Oxygen," Appl. Phys. Lett., 53, 497-9 (1988).
    • (1988) Appl. Phys. Lett. , vol.53 , pp. 497-499
    • Massoud, H.Z.1
  • 74
  • 82
    • 0020703747 scopus 로고
    • Oxygen transport through glass layers
    • J. Schlichting, "Oxygen Transport Through Glass Layers," J. Non-Cryst. Solids, 63, 173-81 (1984).
    • (1984) J. Non-cryst. Solids , vol.63 , pp. 173-181
    • Schlichting, J.1
  • 85
    • 17444433018 scopus 로고    scopus 로고
    • Kinetics of ultrathin thermal oxide growth on Si(001) surfaces
    • H. Shimizu and T. Sato, "Kinetics of Ultrathin Thermal Oxide Growth on Si(001) Surfaces," Jpn. J. Appl. Phys., 44, 808-12 (2005).
    • (2005) Jpn. J. Appl. Phys. , vol.44 , pp. 808-812
    • Shimizu, H.1    Sato, T.2
  • 86
    • 0026827156 scopus 로고
    • Effect of aluminum on ac surface photovoltages in thermally oxidized n-type silicon wafer
    • H. Shimizu and C. Munakata, "Effect of Aluminum on AC Surface Photovoltages in Thermally Oxidized n-Type Silicon Wafer," Jpn. J. Appl. Phys., 31, 729-31 (1992).
    • (1992) Jpn. J. Appl. Phys. , vol.31 , pp. 729-731
    • Shimizu, H.1    Munakata, C.2
  • 87
    • 0020168005 scopus 로고
    • The oxidation inhibition in nitrogen-implanted silicon
    • W. J. M. J. Josquin and Y. Tamminga, "The Oxidation Inhibition in Nitrogen-Implanted Silicon." J. Electrochem. Soc., 129, 1803-11 (1982).
    • (1982) J. Electrochem. Soc. , vol.129 , pp. 1803-1811
    • Josquin, W.J.M.J.1    Tamminga, Y.2
  • 88
    • 9544236208 scopus 로고    scopus 로고
    • Diffusion of phosphorus doped silica for active optical fibers
    • J. Kirchhof, S. Unger, and J. Dellith, "Diffusion of Phosphorus Doped Silica for Active Optical Fibers," J. Non-Cryst. Solids, 345 and 346, 234-8 (2004).
    • (2004) J. Non-cryst. Solids , vol.345-346 , pp. 234-238
    • Kirchhof, J.1    Unger, S.2    Dellith, J.3
  • 89
    • 0032594195 scopus 로고    scopus 로고
    • Phosphorus diffusion in silicon oxide and oxynitride gate dielectrics
    • K. A. Ellis and R. A. Buhram, "Phosphorus Diffusion in Silicon Oxide and Oxynitride Gate Dielectrics," Electrochem. Solid-State Lett., 2, 516-8 (1999).
    • (1999) Electrochem. Solid-state Lett. , vol.2 , pp. 516-518
    • Ellis, K.A.1    Buhram, R.A.2
  • 90
    • 0345013091 scopus 로고    scopus 로고
    • Diffusion coefficients of aluminium and rare earths in vitreous silica
    • J. Kirchhof, S. Unger, and B. Knappe, "Diffusion Coefficients of Aluminium and Rare Earths in Vitreous Silica," Phys. Chem. Glass, 43C, 499-502 (2002).
    • (2002) Phys. Chem. Glass , vol.43 C , pp. 499-502
    • Kirchhof, J.1    Unger, S.2    Knappe, B.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.