Volumn 23, Issue 16, 2003, Pages 3125-3134

Long term oxidation of a SiC fiber-bonded composite in air at 1500 °C

Author keywords

Coatings; Composites; Cristobalite; CVD coating; Interfaces; Oxidation; SiC SiC

Indexed keywords

AMORPHOUS MATERIALS; CHEMICAL VAPOR DEPOSITION; HEATING; OXIDATION; SILICON CARBIDE; X RAY DIFFRACTION ANALYSIS;

EID: 0141572304     PISSN: 09552219     EISSN: None     Source Type: Journal    
DOI: 10.1016/S0955-2219(03)00116-X     Document Type: Article
Times cited : (9)

References (17)
  • 1
    • 0016974220 scopus 로고
    • Synthesis of continuous SiC fibers with high tensile strength
    • Yajima S. Hayashi J. Omori M. Synthesis of continuous SiC fibers with high tensile strength J. Am. Ceram. Soc. 59 1976 324-327
    • (1976) J. Am. Ceram. Soc. , vol.59 , pp. 324-327
    • Yajima, S.1    Hayashi, J.2    Omori, M.3
  • 3
    • 0029376096 scopus 로고
    • Precursor-derived covalent ceramics
    • Bill J. Aldinger F. Precursor-derived covalent ceramics Adv. Mater. 7 9 1995 775-787
    • (1995) Adv. Mater. , vol.7 , Issue.9 , pp. 775-787
    • Bill, J.1    Aldinger, F.2
  • 4
    • 33751385410 scopus 로고
    • Preceramic polymer routes to silicon carbide
    • Laine B.M. Babonneau F. Preceramic polymer routes to silicon carbide Chem. Mater. 5 1993 260-279
    • (1993) Chem. Mater. , vol.5 , pp. 260-279
    • Laine, B.M.1    Babonneau, F.2
  • 5
    • 0029338689 scopus 로고
    • Reaction mechanisms of silicon carbide fiber synthesis by heat treatment of polycarbosilane fibers cured by radiation
    • Sugimoto T. Shimoo T. Okamura K. Seguchi T. Reaction mechanisms of silicon carbide fiber synthesis by heat treatment of polycarbosilane fibers cured by radiation J. Am. Ceram. Soc. 78 7 1995 1849-1852
    • (1995) J. Am. Ceram. Soc. , vol.78 , Issue.7 , pp. 1849-1852
    • Sugimoto, T.1    Shimoo, T.2    Okamura, K.3    Seguchi, T.4
  • 7
    • 0032546023 scopus 로고    scopus 로고
    • High-strength alkali-resistant sintered SiC fibre stable to 2,200 °C
    • London
    • Ishikawa T. Kohtoku Y. Kumagawa K. Yamamura T. Nagasawa T. High-strength alkali-resistant sintered SiC fibre stable to 2,200 °C Nature (London) 391 1998 773-775
    • (1998) Nature , vol.391 , pp. 773-775
    • Ishikawa, T.1    Kohtoku, Y.2    Kumagawa, K.3    Yamamura, T.4    Nagasawa, T.5
  • 9
    • 0000452770 scopus 로고
    • The effects of an aggressive environment on subcritical crack growth of a continuous-fiber ceramic composites
    • Heneger C.H.Jr. Jones R.H. The effects of an aggressive environment on subcritical crack growth of a continuous-fiber ceramic composites Ceram. Eng. Sci. Proc. 13 7-8 1992 411-419
    • (1992) Ceram. Eng. Sci. Proc. , vol.13 , Issue.7-8 , pp. 411-419
    • Heneger C.H., Jr.1    Jones, R.H.2
  • 10
    • 0028383019 scopus 로고
    • Oxidation mechanisms and kinetics of 1D-SiC/C/SiC composite materials: I, an experimental approach
    • Filipuzzi L. Camus G. Naslain R. Thebault J. Oxidation mechanisms and kinetics of 1D-SiC/C/SiC composite materials: I, an experimental approach J. Am. Ceram. Soc. 77 2 1994 459-466
    • (1994) J. Am. Ceram. Soc. , vol.77 , Issue.2 , pp. 459-466
    • Filipuzzi, L.1    Camus, G.2    Naslain, R.3    Thebault, J.4
  • 11
    • 0031097209 scopus 로고    scopus 로고
    • Oxidation of the carbon interface in nicalon-fiber-reinforced silicon carbide composite
    • Windisch C.F.Jr. Henager C.H.Jr. Springer G.D. Jones R.H. Oxidation of the carbon interface in nicalon-fiber-reinforced silicon carbide composite J. Am. Ceram. Soc. 80 3 1997 569-574
    • (1997) J. Am. Ceram. Soc. , vol.80 , Issue.3 , pp. 569-574
    • Windisch, C.F.1    Henager, C.H.2    Springer, G.D.3    Jones, R.H.4
  • 12
    • 0031379511 scopus 로고    scopus 로고
    • Stress-rupture of nicalon/SiC continuous fiber ceramic composites in air at 950 °C
    • Lara-Curzio E. Stress-rupture of nicalon/SiC continuous fiber ceramic composites in air at 950 °C J. Am. Ceram. Soc. 80 12 1997 3268-3272
    • (1997) J. Am. Ceram. Soc. , vol.80 , Issue.12 , pp. 3268-3272
    • Lara-Curzio, E.1
  • 13
    • 0031197287 scopus 로고    scopus 로고
    • m minicomposites with carbon and boron nitride interfaces at elevated temperatures in air
    • m minicomposites with carbon and boron nitride interfaces at elevated temperatures in air J. Am. Ceram., Soc. 80 8 1997 2029-2042
    • (1997) J. Am. Ceram., Soc. , vol.80 , Issue.8 , pp. 2029-2042
    • Morscher, G.N.1
  • 14
    • 0033355761 scopus 로고    scopus 로고
    • A multi-layer CVD-SiC coating for oxidation protection of carbon/carbon composite
    • Otsuka A. Sakamoto K. Masumoto H. A multi-layer CVD-SiC coating for oxidation protection of carbon/carbon composite Mater. Sci. Res. Int 5 3 1999 163-168
    • (1999) Mater. Sci. Res. Int , vol.5 , Issue.3 , pp. 163-168
    • Otsuka, A.1    Sakamoto, K.2    Masumoto, H.3
  • 15
    • 0009513594 scopus 로고    scopus 로고
    • Improvement in oxidation resistance of a C/C composite by using CVD-SiC coating with SiC fiber-composite layer
    • Otsuka A. Matsumura Y. Masumoto H. Kitagawa K. Arai N. Improvement in oxidation resistance of a C/C composite by using CVD-SiC coating with SiC fiber-composite layer TANSO 2000 194 2000 254-260
    • (2000) TANSO 2000 , vol.194 , pp. 254-260
    • Otsuka, A.1    Matsumura, Y.2    Masumoto, H.3    Kitagawa, K.4    Arai, N.5


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.