Volumn 186, Issue , 2012, Pages 210-218

Long-term mechanical reliability of ceramic thick-film circuits and mechanical sensors under static load

Author keywords

Ceramic substrates and circuits; Piezoresistive sensors; SCG; Static fatigue; Thick film technology

Indexed keywords

CERAMIC SUBSTRATES; PIEZORESISTIVE SENSORS; SCG; STATIC FATIGUE; THICK-FILM TECHNOLOGY;

EID: 84867328533     PISSN: 09244247     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.sna.2012.05.031     Document Type: Conference Paper
Times cited : (11)

References (38)
  • 2
    • 0003369788 scopus 로고
    • Ceramics in microelectronic packaging
    • R.R. Tummala Ceramics in microelectronic packaging Advances in Ceramics 26 1989 3 16
    • (1989) Advances in Ceramics , vol.26 , pp. 3-16
    • Tummala, R.R.1
  • 3
    • 84867333795 scopus 로고    scopus 로고
    • Entwicklungspotentiale keramischer Substratwerkstoffe
    • Development potential of ceramic substrate materials
    • A. Roosen Entwicklungspotentiale keramischer Substratwerkstoffe Development potential of ceramic substrate materials IMAPS Deutschland Konferenz 1999
    • (1999) IMAPS Deutschland Konferenz
    • Roosen, A.1
  • 4
    • 77952958876 scopus 로고    scopus 로고
    • Overview on fabrication of three-dimensional structures in multi-layer ceramic substrate
    • L.E. Khoong, Y.M. Tan, and Y.C. Lam Overview on fabrication of three-dimensional structures in multi-layer ceramic substrate Journal of the European Ceramic Society 30 2010 1973 1987
    • (2010) Journal of the European Ceramic Society , vol.30 , pp. 1973-1987
    • Khoong, L.E.1    Tan, Y.M.2    Lam, Y.C.3
  • 9
    • 0942289070 scopus 로고    scopus 로고
    • High-strain response of piezoresistive thick-film resistors on titanium alloy substrates
    • C. Jacq, T. Maeder, and P. Ryser High-strain response of piezoresistive thick-film resistors on titanium alloy substrates Journal of the European Ceramic Society 24 2004 1897 1900
    • (2004) Journal of the European Ceramic Society , vol.24 , pp. 1897-1900
    • Jacq, C.1    Maeder, T.2    Ryser, P.3
  • 10
    • 82755161782 scopus 로고    scopus 로고
    • Low-firing thick-film piezoresistive sensors for medical instruments
    • T. Maeder, C. Jacq, P. Ryser, Low-firing thick-film piezoresistive sensors for medical instruments, Sensors and Actuators, in press.
    • Sensors and Actuators
    • Maeder, T.1    Jacq, C.2    Ryser, P.3
  • 12
    • 58149496411 scopus 로고    scopus 로고
    • Design and characterisation of low-cost thick-film piezoresistive force sensors for the 100 mN to 100 N range
    • Koszalin
    • T. Maeder, V. Fahrny, S. Stauss, G. Corradini, and P. Ryser Design and characterisation of low-cost thick-film piezoresistive force sensors for the 100 mN to 100 N range Proc., XXIX Int. Conf. of IMAPS Poland Koszalin 2005 429 434
    • (2005) Proc., XXIX Int. Conf. of IMAPS Poland , pp. 429-434
    • Maeder, T.1    Fahrny, V.2    Stauss, S.3    Corradini, G.4    Ryser, P.5
  • 13
    • 33847351187 scopus 로고    scopus 로고
    • Fabrication of a millinewton force sensor using low temperature co-fired ceramic (LTCC) technology
    • H. Birol, T. Maeder, I. Nadzeyka, M. Boers, and P. Ryser Fabrication of a millinewton force sensor using low temperature co-fired ceramic (LTCC) technology Sensors and Actuators A 134 2007 334 338
    • (2007) Sensors and Actuators A , vol.134 , pp. 334-338
    • Birol, H.1    Maeder, T.2    Nadzeyka, I.3    Boers, M.4    Ryser, P.5
  • 16
    • 78650264650 scopus 로고    scopus 로고
    • Integrated LTCC pressure/flow/temperature multisensor for compressed air diagnostics
    • Y. Fournier, T. Maeder, G. Boutinard-Rouelle, A. Barras, N. Craquelin, and P. Ryser Integrated LTCC pressure/flow/temperature multisensor for compressed air diagnostics Sensors 10 2010 11156 11173
    • (2010) Sensors , vol.10 , pp. 11156-11173
    • Fournier, Y.1    Maeder, T.2    Boutinard-Rouelle, G.3    Barras, A.4    Craquelin, N.5    Ryser, P.6
  • 17
    • 79958172295 scopus 로고    scopus 로고
    • Integrated SMD pressure/flow/temperature multisensor for compressed air in LTCC technology: Thermal flow and temperature sensing
    • T. Maeder, Y. Fournier, J.-B. Coma, N. Craquelin, and P. Ryser Integrated SMD pressure/flow/temperature multisensor for compressed air in LTCC technology: thermal flow and temperature sensing Microelectronics Reliability 51 2011 1245 1249
    • (2011) Microelectronics Reliability , vol.51 , pp. 1245-1249
    • Maeder, T.1    Fournier, Y.2    Coma, J.-B.3    Craquelin, N.4    Ryser, P.5
  • 20
    • 4243359525 scopus 로고    scopus 로고
    • Slow crack growth behavior and life/reliability analysis of 96 wt % alumina at ambient temperature with various specimen/loading configurations
    • Glenn Research Center (USA)
    • S.R. Choi, M. Powers, N.N. Nemeth, Slow crack growth behavior and life/reliability analysis of 96 wt % alumina at ambient temperature with various specimen/loading configurations, report TM-2000-210206, NASA, Glenn Research Center (USA), 2000.
    • (2000) Report TM-2000-210206, NASA
    • Choi, S.R.1    Powers, M.2    Nemeth, N.N.3
  • 23
    • 34250118123 scopus 로고
    • Evaluation of the life of ceramics from subcritical crack growth parameters
    • G.A. Gogotsi, and V.P. Zavada Evaluation of the life of ceramics from subcritical crack growth parameters Strength of Materials 17 1985 210 214
    • (1985) Strength of Materials , vol.17 , pp. 210-214
    • Gogotsi, G.A.1    Zavada, V.P.2
  • 26
    • 0036132150 scopus 로고    scopus 로고
    • Crack growth resistance of alumina, zirconia and zirconia toughened alumina ceramics for joint prostheses
    • A.H. De Aza, J. Chevalier, G. Fantozzi, M. Schehl, and R. Torrecillas Crack growth resistance of alumina, zirconia and zirconia toughened alumina ceramics for joint prostheses Biomaterials 23 2003 937 945
    • (2003) Biomaterials , vol.23 , pp. 937-945
    • De Aza, A.H.1    Chevalier, J.2    Fantozzi, G.3    Schehl, M.4    Torrecillas, R.5
  • 27
    • 0018167801 scopus 로고
    • Les encres sérigraphiables en microélectronique hybride: Les matériaux et leur comportement
    • Screenable inks in hybrid microelectronics: the materials and their behaviour
    • M. Monneraye Les encres sérigraphiables en microé lectronique hybride: les matériaux et leur comportement Screenable inks in hybrid microelectronics: the materials and their behaviour Acta Electronica 21 1978 263 281
    • (1978) Acta Electronica , vol.21 , pp. 263-281
    • Monneraye, M.1
  • 29
    • 0019180862 scopus 로고
    • Progress in and technology of low-cost silver containing thick-film conductors
    • CHMT-3
    • B.E. Taylor, J.J. Felten, and J.R. Larry Progress in and technology of low-cost silver containing thick-film conductors IEEE Trans. Comp. Hyb. Manuf. Technol. 1980 504 517 CHMT-3
    • (1980) IEEE Trans. Comp. Hyb. Manuf. Technol. , pp. 504-517
    • Taylor, B.E.1    Felten, J.J.2    Larry, J.R.3
  • 30
    • 30244479544 scopus 로고
    • Sintering of Ag-Pd in the presence of a reactive glass
    • S.S. Cole Sintering of Ag-Pd in the presence of a reactive glass Journal of the American Ceramic Society 55 1972 296 299
    • (1972) Journal of the American Ceramic Society , vol.55 , pp. 296-299
    • Cole, S.S.1
  • 31
    • 33645551060 scopus 로고    scopus 로고
    • Influence of processing and conduction materials on properties of co-fired resistors in LTCC structures
    • H. Birol, T. Maeder, and P. Ryser Influence of processing and conduction materials on properties of co-fired resistors in LTCC structures Journal of the European Ceramic Society 26 2006 1937 1941
    • (2006) Journal of the European Ceramic Society , vol.26 , pp. 1937-1941
    • Birol, H.1    Maeder, T.2    Ryser, P.3
  • 32
    • 0034178026 scopus 로고    scopus 로고
    • Thermal expansion and corrosion behavior of lead-borosilicate glasses
    • I.L. Trubnikov Thermal expansion and corrosion behavior of lead-borosilicate glasses Refractories and Industrial Ceramics 41 2000 169 171
    • (2000) Refractories and Industrial Ceramics , vol.41 , pp. 169-171
    • Trubnikov, I.L.1
  • 34
    • 50949092928 scopus 로고    scopus 로고
    • High temperature reliability of aluminium wire-bonds to thin film, thick film and low temperature co-fired ceramic (LTCC) substrate metallization
    • R. Johannessen, F. Oldervoll, and F. Strisland High temperature reliability of aluminium wire-bonds to thin film, thick film and low temperature co-fired ceramic (LTCC) substrate metallization Microelectronics Reliability 48 2008 1711 1719
    • (2008) Microelectronics Reliability , vol.48 , pp. 1711-1719
    • Johannessen, R.1    Oldervoll, F.2    Strisland, F.3
  • 35
    • 0027573859 scopus 로고
    • Strengthening of soda-lime-silica glass by sol-gel- and melt-derived coatings
    • P.F. James, M. Chen, and F.R. Jones Strengthening of soda-lime-silica glass by sol-gel- and melt-derived coatings Journal of Non-Crystalline Solids 155 1993 99 109
    • (1993) Journal of Non-Crystalline Solids , vol.155 , pp. 99-109
    • James, P.F.1    Chen, M.2    Jones, F.R.3
  • 36
    • 0024874875 scopus 로고
    • Methods for improving the mechanical properties of oxide glasses
    • I.W. Donald Methods for improving the mechanical properties of oxide glasses Journal of Materials Science 24 1989 4177 4208
    • (1989) Journal of Materials Science , vol.24 , pp. 4177-4208
    • Donald, I.W.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.