메뉴 건너뛰기




Volumn 35, Issue 6, 2010, Pages 689-696

Adhesive quality of self-adhesive and conventional adhesive resin cement to Y-TZP ceramic before and after aging conditions

Author keywords

[No Author keywords available]

Indexed keywords

2 PROPANOL; MAXCEM; PANAVIA FLUORO; PANAVIA-FLUORO; RELY X; RELY-X; RESIN CEMENT; SILANE DERIVATIVE; SILICON DIOXIDE; SOLVENT; VARIOLINK; WATER; Y TZP CERAMIC; Y-TZP CERAMIC; YTTRIUM; ZIRCONIUM;

EID: 78649974956     PISSN: 03617734     EISSN: None     Source Type: Journal    
DOI: 10.2341/10-157-L     Document Type: Article
Times cited : (60)

References (46)
  • 1
    • 5344226305 scopus 로고    scopus 로고
    • Influence of different adhesive resin cements on the fracture strength of aluminum oxide ceramic posterior crowns
    • Komine F, Tomic M, Gerds T & Strub JR (2004) Influence of different adhesive resin cements on the fracture strength of aluminum oxide ceramic posterior crowns The Journal of Prosthetic Dentistry 92(4) 359-364.
    • (2004) The Journal of Prosthetic Dentistry , vol.92 , Issue.4 , pp. 359-364
    • Komine, F.1    Tomic, M.2    Gerds, T.3    Strub, J.R.4
  • 2
    • 0032917811 scopus 로고    scopus 로고
    • Zirconia as a ceramic biomaterial
    • Piconi C & Maccauro G (1999) Zirconia as a ceramic biomaterial Biomaterials 20(1) 1-25.
    • (1999) Biomaterials , vol.20 , Issue.1 , pp. 1-25
    • Piconi, C.1    Maccauro, G.2
  • 3
    • 48549103602 scopus 로고    scopus 로고
    • All-ceramic inlay-retained fixed partial dentures: Preliminary results from a clinical study
    • Ohlmann B, Rammelsberg P, Schmitter M, Schwarz S & Gabbert O (2008) All-ceramic inlay-retained fixed partial dentures: Preliminary results from a clinical study Journal of Dentistry 36(9) 692-696.
    • (2008) Journal of Dentistry , vol.36 , Issue.9 , pp. 692-696
    • Ohlmann, B.1    Rammelsberg, P.2    Schmitter, M.3    Schwarz, S.4    Gabbert, O.5
  • 4
    • 32044438490 scopus 로고    scopus 로고
    • Microtensile bond strength of a resin cement to glass infiltrated zirconia-reinforced ceramic: The effect of surface conditioning
    • DOI 10.1016/j.dental.2005.04.021, PII S0109564105001739
    • Amaral R, Özcan M, Bottino MA & Valandro LF (2006) Microtensile bond strength of a resin cement to glass infiltrated zirconia-reinforced ceramic: The effect of surface conditioning Dental Materials 22(3) 283-290. (Pubitemid 43199618)
    • (2006) Dental Materials , vol.22 , Issue.3 , pp. 283-290
    • Amaral, R.1    Ozcan, M.2    Bottino, M.A.3    Valandro, L.F.4
  • 5
    • 41449099480 scopus 로고    scopus 로고
    • Effect of conditioning methods on the microtensile bond strength of phosphate monomer-based cement on zirconia ceramic in dry and aged conditions
    • DOI 10.1002/jbm.b.30908
    • Amaral R, Valandro LF, Balducci I, Özcan M & Bottino MA (2008) Effect of conditioning methods on the microtensile bond strength of phosphate monomer-based cement on zirconia ceramic in dry and aged conditions Journal of Biomedical Materials Research Part B: Applied Biomaterials 85(1) 1-9. (Pubitemid 351458220)
    • (2008) Journal of Biomedical Materials Research - Part B Applied Biomaterials , vol.85 , Issue.1 , pp. 1-9
    • Amaral, R.1    Ozcan, M.2    Valandro, L.F.3    Balducci, I.4    Bottino, M.A.5
  • 6
    • 33744789998 scopus 로고    scopus 로고
    • Effect of zirconium-oxide ceramic surface treatments on the bond strength to adhesive resin
    • Atsu SS, Kilicarslan MA, Kucukesmen HC & Aka PS (2006) Effect of zirconium-oxide ceramic surface treatments on the bond strength to adhesive resin Journal of Prosthetic Dentistry 95(6) 430-436.
    • (2006) Journal of Prosthetic Dentistry , vol.95 , Issue.6 , pp. 430-436
    • Atsu, S.S.1    Kilicarslan, M.A.2    Kucukesmen, H.C.3    Aka, P.S.4
  • 8
    • 1842855215 scopus 로고    scopus 로고
    • Durability of the resin bond strength to the alumina ceramic Procera
    • Hummel M & Kern M (2004) Durability of the resin bond strength to the alumina ceramic Procera Dental Materials 20(5) 498-508.
    • (2004) Dental Materials , vol.20 , Issue.5 , pp. 498-508
    • Hummel, M.1    Kern, M.2
  • 9
    • 0031598657 scopus 로고    scopus 로고
    • Bonding to zirconia ceramic: Adhesion methods and their durability
    • Kern M & Wegner SM (1998) Bonding to zirconia ceramic: Adhesion methods and their durability Dental Materials 14(1) 64-71.
    • (1998) Dental Materials , vol.14 , Issue.1 , pp. 64-71
    • Kern, M.1    Wegner, S.M.2
  • 10
    • 1942456928 scopus 로고    scopus 로고
    • In vitro evaluation of shear bond strengths of resin to densely-sintered high-purity zirconium-oxide ceramic after long-term storage and thermal cycling
    • Blatz MB, Sadan A, Martin J & Lang B (2004) In vitro evaluation of shear bond strengths of resin to densely-sintered high-purity zirconium-oxide ceramic after long-term storage and thermal cycling Journal of Prosthetic Dentistry 91(4) 356-362.
    • (2004) Journal of Prosthetic Dentistry , vol.91 , Issue.4 , pp. 356-362
    • Blatz, M.B.1    Sadan, A.2    Martin, J.3    Lang, B.4
  • 11
    • 0141727597 scopus 로고    scopus 로고
    • Effect of surface conditioning methods on the bond strength of luting cement to ceramics
    • Özcan M & Vallittu PK (2003) Effect of surface conditioning methods on the bond strength of luting cement to ceramics Dental Materials 19(8) 725-731.
    • (2003) Dental Materials , vol.19 , Issue.8 , pp. 725-731
    • Özcan, M.1    Vallittu, P.K.2
  • 12
    • 0034242898 scopus 로고    scopus 로고
    • Characterisation of tribochemically assisted bonding of composite resin to porcelain and metal
    • Sun R, Suansuwan N, Kilpatrick N & Swain M (2000) Characterisation of tribochemically assisted bonding of composite resin to porcelain and metal Journal of Dentistry 28(6) 441-445.
    • (2000) Journal of Dentistry , vol.28 , Issue.6 , pp. 441-445
    • Sun, R.1    Suansuwan, N.2    Kilpatrick, N.3    Swain, M.4
  • 14
    • 19744367539 scopus 로고    scopus 로고
    • The shear bond strength between luting cements and zirconia ceramics after two pre-treatments
    • Piwowarczyk A, Lauer HC & Sorensen JA (2005) The shear bond strength between luting cements and zirconia ceramics after two pre-treatments Operative Dentistry 30(3) 382388.
    • (2005) Operative Dentistry , vol.30 , Issue.3 , pp. 382388
    • Piwowarczyk, A.1    Lauer, H.C.2    Sorensen, J.A.3
  • 15
    • 33646153045 scopus 로고    scopus 로고
    • Bonding of resin composite luting cements to zirconium oxide by two air-particle abrasion methods
    • Kumbuloglu O, Lassila LVJ, User A & Vallitu PK (2006) Bonding of resin composite luting cements to zirconium oxide by two air-particle abrasion methods Operative Dentistry 31(2) 248-255. (Pubitemid 43633135)
    • (2006) Operative Dentistry , vol.31 , Issue.2 , pp. 248-255
    • Kumbuloglu, O.1    Lassila, L.V.J.2    User, A.3    Vallittu, P.K.4
  • 16
    • 33845290307 scopus 로고    scopus 로고
    • Durability of the resin bond strength to zirconia ceramic after using different surface conditioning methods
    • Wolfart M, Lehmann F, Wolfart S & Kern M (2007) Durability of the resin bond strength to zirconia ceramic after using different surface conditioning methods Dental Materials 23(1) 45-50.
    • (2007) Dental Materials , vol.23 , Issue.1 , pp. 45-50
    • Wolfart, M.1    Lehmann, F.2    Wolfart, S.3    Kern, M.4
  • 17
    • 33745743170 scopus 로고    scopus 로고
    • Bond strength of a resin cement to high-alumina and zirconia-reinforced ceramics: The effect of surface conditioning
    • Valandro LF, Özcan M, Bottino MC, Bottino MA, Scotti R & Bona AD (2006) Bond strength of resin cement to highalumina and zirconia-reinforced ceramics: The effect of surface conditioning Journal of Adhesive Dentistry 8(3) 175-181. (Pubitemid 44014526)
    • (2006) Journal of Adhesive Dentistry , vol.8 , Issue.3 , pp. 175-181
    • Valandro, L.F.1    Ozcan, M.2    Bottino, M.C.3    Bottino, M.A.4    Scotti, R.5    Della, B.A.6
  • 18
    • 0034157359 scopus 로고    scopus 로고
    • Bond strength of luting cements to zirconium oxide ceramics
    • Derand P & Derand T (2000) Bond strength of luting cements to zirconium oxide ceramics International Journal of Prosthodontics 13(2) 131-135.
    • (2000) International Journal of Prosthodontics , vol.13 , Issue.2 , pp. 131-135
    • Derand, P.1    Derand, T.2
  • 19
    • 30344433724 scopus 로고    scopus 로고
    • Effect of thermocycling on bond strength of luting cements to zirconia ceramic
    • DOI 10.1016/j.dental.2005.04.016, PII S0109564105001569
    • Lüthy H, Loeffel O & Hammerle CH (2006) Effect of thermocycling on bond strength of luting cements to zirconia ceramic Dental Materials 22(2) 195-200. (Pubitemid 43061319)
    • (2006) Dental Materials , vol.22 , Issue.2 , pp. 195-200
    • Luthy, H.1    Loeffel, O.2    Hammerle, C.H.F.3
  • 21
    • 33750387981 scopus 로고    scopus 로고
    • Microtensile bond strength and interfacial properties of self-etching and self-adhesive resin cements used to lute composite onlays under different seating forces
    • Goracci C, Cury AH, Cantoro A, Papacchini F, Tay FR & Ferrari M (2006) Microtensile bond strength and interfacial properties of self-etching and self-adhesive resin cements used to lute composite onlays under different seating forces Journal of Adhesive Dentistry 8(5) 327-335.
    • (2006) Journal of Adhesive Dentistry , vol.8 , Issue.5 , pp. 327-335
    • Goracci, C.1    Cury, A.H.2    Cantoro, A.3    Papacchini, F.4    Tay, F.R.5    Ferrari, M.6
  • 23
    • 20444408006 scopus 로고    scopus 로고
    • In vitro retentive strength of zirconium oxide ceramic crowns using different luting agents
    • DOI 10.1016/j.prosdent.2005.04.011, PII S0022391305002362
    • Ernst CP, Cohnen U, Stender E & Willershausen B (2005) In vitro retentive strength of zirconium oxide ceramic crowns using different luting agents Journal of Prosthetic Dentistry 93(6) 551-558. (Pubitemid 40798345)
    • (2005) Journal of Prosthetic Dentistry , vol.93 , Issue.6 , pp. 551-558
    • Ernst, C.-P.1    Cohnen, U.2    Stender, E.3    Willershausen, B.4
  • 26
    • 48549085496 scopus 로고    scopus 로고
    • Comparison of resin cement adhesion to Y-TZP ceramic following manufacturers' instructions of the cements only
    • Özcan M, Kerkdijk KS & Valandro LF (2008) Comparison of resin cement adhesion to Y-TZP ceramic following manufacturers' instructions of the cements only Clinical Oral Investigations 12(3) 279-282.
    • (2008) Clinical Oral Investigations , vol.12 , Issue.3 , pp. 279-282
    • Özcan, M.1    Kerkdijk, K.S.2    Valandro, L.F.3
  • 27
    • 42449099988 scopus 로고    scopus 로고
    • Effect of various surface conditioning methods on the adhesion of dual-cure resin cement with MDP functional monomer to Zirconia after thermal aging
    • Özcan M, Nijhuis H & Valandro LF (2008) Effect of various surface conditioning methods on the adhesion of dual-cure resin cement with MDP functional monomer to Zirconia after thermal aging Dental Materials Journal 27(1) 99-104.
    • (2008) Dental Materials Journal , vol.27 , Issue.1 , pp. 99-104
    • Özcan, M.1    Nijhuis, H.2    Valandro, L.F.3
  • 28
    • 34248359144 scopus 로고    scopus 로고
    • Durability of resin-dentin bonds: Effects of direct/indirect exposure and storage media
    • DOI 10.1016/j.dental.2006.06.030, PII S0109564106001989
    • Toledano M, Osório R, Osório E, Aguilera FS, Yamauti M, Pashley DH & Tay F (2007) Durability of resin-dentin bonds: Effects of direct/indirect exposure and storage media Dental Materials 23(7) 885-892. (Pubitemid 46734317)
    • (2007) Dental Materials , vol.23 , Issue.7 , pp. 885-892
    • Toledano, M.1    Osorio, R.2    Osorio, E.3    Aguilera, F.S.4    Yamauti, M.5    Pashley, D.H.6    Tay, F.7
  • 30
    • 0034208413 scopus 로고    scopus 로고
    • Long-term resin bond strength to zirconia ceramic
    • Wegner SM & Kern M (2000) Long-term resin bond strength to zirconia ceramic Journal of Adhesive Dentistry 2(2) 139-147.
    • (2000) Journal of Adhesive Dentistry , vol.2 , Issue.2 , pp. 139-147
    • Wegner, S.M.1    Kern, M.2
  • 31
    • 0036636774 scopus 로고    scopus 로고
    • Resin bond strength to densely sintered alumina ceramic
    • Friederich R & Kern M (2002) Resin bond strength to densely sintered alumina ceramic International Journal of Prosthodontics 15(4) 333-338.
    • (2002) International Journal of Prosthodontics , vol.15 , Issue.4 , pp. 333-338
    • Friederich, R.1    Kern, M.2
  • 32
    • 25844498493 scopus 로고    scopus 로고
    • The influence of ceramic surface treatments on the tensile bond strength of composite resin to all-ceramic coping materials
    • Kim BK, Bae HE, Shim JS & Lee KW (2005) The influence of ceramic surface treatments on the tensile bond strength of composite resin to all-ceramic coping materials Journal of Prosthetic Dentistry 94(4) 357-362.
    • (2005) Journal of Prosthetic Dentistry , vol.94 , Issue.4 , pp. 357-362
    • Kim, B.K.1    Bae, H.E.2    Shim, J.S.3    Lee, K.W.4
  • 33
    • 0033222358 scopus 로고    scopus 로고
    • The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic
    • Kosmac T, Oblak C, Jevnikar P, Funduk N & Marion L (1999) The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic Dental Materials 15(6) 426-433.
    • (1999) Dental Materials , vol.15 , Issue.6 , pp. 426-433
    • Kosmac, T.1    Oblak, C.2    Jevnikar, P.3    Funduk, N.4    Marion, L.5
  • 34
    • 54049117580 scopus 로고    scopus 로고
    • Y-TZP ceramic processing from coprecipitated powders: A comparative study with three commercial dental ceramics
    • Lazar DR, Bottino MC, Özcan M, Valandro LF, Amaral R, Ussui V & Bressiani AH (2008) Y-TZP ceramic processing from coprecipitated powders: A comparative study with three commercial dental ceramics Dental Materials 24(12) 1676-1678.
    • (2008) Dental Materials , vol.24 , Issue.12 , pp. 1676-1678
    • Lazar, D.R.1    Bottino, M.C.2    Özcan, M.3    Valandro, L.F.4    Amaral, R.5    Ussui, V.6    Bressiani, A.H.7
  • 35
    • 0005522027 scopus 로고
    • The role of water transport in composite materials
    • Comyn J (eds) Elsevier Applied Science
    • Marom G (1985) The role of water transport in composite materials In: Comyn J (eds) Polymer Permeability Great Britain, Elsevier Applied Science 341-374.
    • (1985) Polymer Permeability Great Britain , pp. 341-374
    • Marom, G.1
  • 36
    • 34548648100 scopus 로고    scopus 로고
    • Influence of surface treatment and simulated aging on bond strengths of luting agents to zirconia
    • Blatz MB, Chiche G, Holst S & Sadan A (2007) Influence of surface treatment and simulated aging on bond strengths of luting agents to zirconia Quintessence International 38(9) 745-753.
    • (2007) Quintessence International , vol.38 , Issue.9 , pp. 745-753
    • Blatz, M.B.1    Chiche, G.2    Holst, S.3    Sadan, A.4
  • 37
    • 59349112720 scopus 로고    scopus 로고
    • Effect of water aging on microtensile bond strength of dual-cured resin cements to pre-treated sintered zirconium-oxide ceramics
    • Oyagüe RC, Monticelli F, Toledano M, Osório E, Ferrari M & Osório R (2009) Effect of water aging on microtensile bond strength of dual-cured resin cements to pre-treated sintered zirconium-oxide ceramics Dental Materials 25(3) 392-399.
    • (2009) Dental Materials , vol.25 , Issue.3 , pp. 392-399
    • Oyagüe, R.C.1    Monticelli, F.2    Toledano, M.3    Osório, E.4    Ferrari, M.5    Osório, R.6
  • 38
    • 33846944025 scopus 로고    scopus 로고
    • Pilot evaluation of resin composite cement adhesion to zirconia using a novel silane system
    • DOI 10.1080/00016350600973060, PII 770193585
    • Matinlinna JP, Lassila LV & Vallittu PK (2007) Pilot evaluation of resin composite cement adhesion to zirconia using a novel silane system Acta Odontologica Scandinavica 65(1) 44-51. (Pubitemid 46254438)
    • (2007) Acta Odontologica Scandinavica , vol.65 , Issue.1 , pp. 44-51
    • Matinlinna, J.P.1    Lassila, L.V.J.2    Vallittu, P.K.3
  • 39
    • 0037052920 scopus 로고    scopus 로고
    • Probing the molecular interactions in the diffusion of water through epoxy and epoxy-bismaleimide networks
    • Musto P, Ragosta G, Scarinzi G & Mascia L (2002) Probing the molecular interactions in the diffusion of water through epoxy and epoxy-bismaleimide networks Journal of Polymer Science Part B: Polymer Physics 40(10) 922-938.
    • (2002) Journal of Polymer Science Part B: Polymer Physics , vol.40 , Issue.10 , pp. 922-938
    • Musto, P.1    Ragosta, G.2    Scarinzi, G.3    Mascia, L.4
  • 40
    • 4444297012 scopus 로고    scopus 로고
    • In vitro shear bond strength of cementing agents to fixed prosthodontic restorative materials
    • Piwowarczyk A, Lauer HC & Sorensen JA (2004) In vitro shear bond strength of cementing agents to fixed prosthodontic restorative materials Journal of Prosthetic Dentistry 92(3) 265-273.
    • (2004) Journal of Prosthetic Dentistry , vol.92 , Issue.3 , pp. 265-273
    • Piwowarczyk, A.1    Lauer, H.C.2    Sorensen, J.A.3
  • 43
    • 77950202373 scopus 로고    scopus 로고
    • The effect of zirconia surface treatment on flexural strength and shear bond strength to a resin cement
    • Qeblawi DM, Muñoz CA, Brewer JD & Monaco EA Jr (2010) The effect of zirconia surface treatment on flexural strength and shear bond strength to a resin cement Journal of Prosthetic Dentistry 103(4) 210-220.
    • (2010) Journal of Prosthetic Dentistry , vol.103 , Issue.4 , pp. 210-220
    • Qeblawi, D.M.1    Muñoz, C.A.2    Brewer, J.D.3    Monaco Jr., E.A.4
  • 44
    • 35148865193 scopus 로고    scopus 로고
    • Influence of thermal expansion mismatch and fatigue loading on phase changes in porcelain veneered Y-TZP zirconia discs
    • De Kler M, de Jager N, Meegdes M & van der Zel JM (2007) Influence of thermal expansion mismatch and fatigue loading on phase changes in porcelain veneered Y-TZP zirconia discs Journal of Oral Rehabilitation 34(11) 841-847.
    • (2007) Journal of Oral Rehabilitation , vol.34 , Issue.11 , pp. 841-847
    • De Kler, M.1    De Jager, N.2    Meegdes, M.3    Van Der Zel, J.M.4
  • 45
    • 11844264547 scopus 로고    scopus 로고
    • Influence of surface and heat treatments on the flexural strength of Y-TZP dental ceramic
    • DOI 10.1016/j.jdent.2004.07.001, PII S0300571204001125
    • Guazzato M, Quach L, Albakry M & Swain MV (2005) Influence of surface and heat treatments on the flexural strength of Y-TZP dental ceramic Journal of Dentistry 33(1) 9-18. (Pubitemid 40093557)
    • (2005) Journal of Dentistry , vol.33 , Issue.1 , pp. 9-18
    • Guazzato, M.1    Quach, L.2    Albakry, M.3    Swain, M.V.4
  • 46
    • 71649097261 scopus 로고    scopus 로고
    • Influence of surface treatments on surface roughness, phase transformation, and biaxial flexural strength of Y-TZP ceramics
    • Karakoca S & Yilmaz H (2009) Influence of surface treatments on surface roughness, phase transformation, and biaxial flexural strength of Y-TZP ceramics Journal of Biomedical Materials Research Part B: Applied Biomaterials 91(2) 930-937
    • (2009) Journal of Biomedical Materials Research Part B: Applied Biomaterials , vol.91 , Issue.2 , pp. 930-937
    • Karakoca, S.1    Yilmaz, H.2