Influence of surface treatments on surface roughness, phase transformation, and biaxial flexural strength of Y-TZP ceramics

Author keywords

Biaxial flexural strength; Surface roughness; Surface treatment; X ray diffraction; Y TZP

Indexed keywords

AFTER-TREATMENT; BI-AXIAL FLEXURAL STRENGTH; CONTROL GROUPS; CRYSTALLINE PHASE; DC CONTROL; DISK SPECIMENS; MONOCLINIC ZIRCONIA; PHASE TRANSFORMATION; ROUGHNESS SURFACES; SURFACE GRINDING; TETRAGONAL ZIRCONIA; TWO-WAY ANOVA; WEIBULL MODULUS; WEIBULL STATISTICS;

EID: 71649097261     PISSN: 15524973     EISSN: 15524981     Source Type: Journal    
DOI: 10.1002/jbm.b.31477     Document Type: Article
Times cited : (172)

References (40)
  • 1
    • 38949168448 scopus 로고    scopus 로고
    • The firing procedure influences properties of a zirconia core ceramic
    • DOI 10.1016/j.dental.2007.04.008, PII S010956410700142X
    • Oilo M, Gjerdet NR, Tvinnereim HM. The firing procedure influences properties of a zirconia core ceramic. Dent Mater 2008;24:471-475. (Pubitemid 351215516)
    • (2008) Dental Materials , vol.24 , Issue.4 , pp. 471-475
    • Oilo, M.1    Gjerdet, N.R.2    Tvinnereim, H.M.3
  • 2
    • 0027613970 scopus 로고
    • Interface histology of unloaded and early loaded partially stabilized zirconia endosseous implant in initial bone healing
    • Akagawa Y, Ichikawa Y, Nikai H, Tsuru H. Interface histology of unloaded and early loaded partially stabilized zirconia endosseous implant in initial bone healing. J Prosthet Dent 1993;69:599-604.
    • (1993) J Prosthet Dent , vol.69 , pp. 599-604
    • Akagawa, Y.1    Ichikawa, Y.2    Nikai, H.3    Tsuru, H.4
  • 3
    • 5444257231 scopus 로고    scopus 로고
    • Clinical success of zirconium oxide posts with resin composite or glass-ceramic cores in endodontically treated teeth: A 4-year retrospective study
    • Paul SJ, Werder P. Clinical success of zirconium oxide posts with resin composite or glass-ceramic cores in endodontically treated teeth: A 4-year retrospective study. Int J Prosthodont 2004;17:524-528. (Pubitemid 39360695)
    • (2004) International Journal of Prosthodontics , vol.17 , Issue.5 , pp. 524-528
    • Paul, S.J.1    Werder, P.2
  • 4
    • 0033301391 scopus 로고    scopus 로고
    • Zirconia TZP and alumina advanced technologies for the manufacturing of single crowns
    • Luthardt RG, Sandkuhl O, Reitz B. Zirconia TZP and alumina advanced technologies for the manufacturing of single crowns. Eur J Prosthodont Rest Dent 1999;7:113-119.
    • (1999) Eur J Prosthodont Rest Dent , vol.7 , pp. 113-119
    • Luthardt, R.G.1    Sandkuhl, O.2    Reitz, B.3
  • 5
    • 35148891671 scopus 로고    scopus 로고
    • An overview of zirconia ceramics: Basic properties and clinical applications
    • Manicone PF, Rossi Iommetti P, Raffaelli L. An overview of zirconia ceramics: Basic properties and clinical applications. J Dent 2007;35:819-826.
    • (2007) J Dent , vol.35 , pp. 819-826
    • Manicone, P.F.1    Rossi Iommetti, P.2    Raffaelli, L.3
  • 6
    • 33748596081 scopus 로고    scopus 로고
    • In vitro evaluation of low-temperature aging effects and finishing procedures on the flexural strength and structural stability of Y-TZP dental ceramics
    • Papanagiotou HP, Morgano SM, Giordano RA, Pober R. In vitro evaluation of low-temperature aging effects and finishing procedures on the flexural strength and structural stability of Y-TZP dental ceramics. J Prosthet Dent 2006;96:154-164.
    • (2006) J Prosthet Dent , vol.96 , pp. 154-164
    • Papanagiotou, H.P.1    Morgano, S.M.2    Giordano, R.A.3    Pober, R.4
  • 7
    • 0032917811 scopus 로고    scopus 로고
    • Zirconia as a ceramic biomaterial
    • Piconi C, Maccauro G. Zirconia as a ceramic biomaterial. Biomaterials 1999;20:1-25.
    • (1999) Biomaterials , vol.20 , pp. 1-25
    • Piconi, C.1    Maccauro, G.2
  • 8
    • 34250164925 scopus 로고    scopus 로고
    • The biaxial flexural strength and fatigue property of Lava Y-TZP dental ceramic
    • DOI 10.1016/j.dental.2006.09.003, PII S0109564106002454
    • Pittayachawan P, McDonald A, Petrie A, Knowles JC. The biaxial flexural strength and fatigue property of Lava Y-TZP dental ceramic. Dent Mater 2007;23:1018-1029. (Pubitemid 46907965)
    • (2007) Dental Materials , vol.23 , Issue.8 , pp. 1018-1029
    • Pittayachawan, P.1    McDonald, A.2    Petrie, A.3    Knowles, J.C.4
  • 9
    • 21244506130 scopus 로고    scopus 로고
    • A clinical report and overview of scientific studies and clinical procedures conducted on the 3M ESPE Lava all-ceramic system
    • DOI 10.1111/j.1532-849X.2005.00003.x
    • Piwowarczyk A, Ottl P, Lauer HC, Kuretzky T. A clinical report and overview of scientific studies and clinical procedures conducted on the 3M ESPE Lava all-ceramic system. J Prosthodont 2005;14:39-45. (Pubitemid 41679756)
    • (2005) Journal of Prosthodontics , vol.14 , Issue.1 , pp. 39-45
    • Piwowarczyk, A.1    Ottl, P.2    Lauer, H.-C.3    Kuretzky, T.4
  • 10
    • 0035319974 scopus 로고    scopus 로고
    • Reliability and strength of all-ceramic dental restorations fabricated by direct ceramic machining (DCM)
    • Filser F, Kocher P, Weibel F, Lüthy H, Schärer P, Gauckler LJ. Reliability and strength of all-ceramic dental restorations fabricated by direct ceramic machining (DCM). J Comput Dent 2001;4:89-106.
    • (2001) J Comput Dent , vol.4 , pp. 89-106
    • Filser, F.1    Kocher, P.2    Weibel, F.3    Lüthy, H.4    Schärer, P.5    Gauckler, L.J.6
  • 12
    • 0035495965 scopus 로고    scopus 로고
    • Computer-assisted generation of all-ceramic crowns and fixed partial dentures
    • Besimo CE, Spielmann HP, Rohner HP. Computer-assisted generation of all-ceramic crowns and fixed partial dentures. Int J Comput Dent 2001;4:243-262.
    • (2001) Int J Comput Dent , vol.4 , pp. 243-262
    • Besimo, C.E.1    Spielmann, H.P.2    Rohner, H.P.3
  • 13
    • 34247491685 scopus 로고    scopus 로고
    • Load-bearing capacity of all-ceramic posterior four-unit fixed partial dentures with different zirconia frameworks
    • Kohorst P, Herzog TJ, Borchers L, Stiesch-Scholz M. Load-bearing capacity of all-ceramic posterior four-unit fixed partial dentures with different zirconia frameworks. Eur J Oral Sci 2007;115:161-166.
    • (2007) Eur J Oral Sci , vol.115 , pp. 161-166
    • Kohorst, P.1    Herzog, T.J.2    Borchers, L.3    Stiesch-Scholz, M.4
  • 17
    • 0033222358 scopus 로고    scopus 로고
    • The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic
    • Kosmac T, Oblak C, Jevnikar P, Funduk N, Marion L. The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic. Dent Mater 1999;15426-15433
    • (1999) Dent Mater , pp. 15426-15433
    • Kosmac, T.1    Oblak, C.2    Jevnikar, P.3    Funduk, N.4    Marion, L.5
  • 19
    • 0037828938 scopus 로고    scopus 로고
    • Biaxial flexural strength, elastic moduli, and x-ray diffraction characterization of three pressable all-ceramic materials
    • DOI 10.1067/mpr.2003.42
    • Albakry M, Guazzato M, Swain MV. Biaxial flexural strength, elastic moduli, and X-ray diffraction characterization of three pressable all-ceramic materials. J Prosthet Dent 2003;89:374-380. (Pubitemid 37323893)
    • (2003) Journal of Prosthetic Dentistry , vol.89 , Issue.4 , pp. 374-380
    • Albakry, M.1    Guazzato, M.2    Swain, M.V.3
  • 20
    • 0042128629 scopus 로고    scopus 로고
    • Weibull analysis and flexural strength of hot-pressed core and veneered ceramic structures
    • Bona AD, Anusavice KJ, DeHoff PH. Weibull analysis and flexural strength of hot-pressed core and veneered ceramic structures. Dent Mater 2003;19:662-669.
    • (2003) Dent Mater , vol.19 , pp. 662-669
    • Bona, A.D.1    Anusavice, K.J.2    Dehoff, P.H.3
  • 21
    • 0036518474 scopus 로고    scopus 로고
    • Flexural strength of In-Ceram alumina and In-Ceram zirconia core materials
    • Chong KH, Chai J, Takahashi Y, Wozniak W. Flexural strength of In-Ceram alumina and In-Ceram zirconia core materials. Int J Prosthodont 2002;15:183-188.
    • (2002) Int J Prosthodont , vol.15 , pp. 183-188
    • Chong, K.H.1    Chai, J.2    Takahashi, Y.3    Wozniak, W.4
  • 22
    • 31544457886 scopus 로고    scopus 로고
    • Microstructural and crystallographic surface changes after grinding zirconia-based dental ceramics
    • Denry IL, Holloway JA. Microstructural and crystallographic surface changes after grinding zirconia-based dental ceramics. J Biomed Mater Res B Appl Biomater 2006;76:440-448.
    • (2006) J Biomed Mater Res B Appl Biomater , vol.76 , pp. 440-448
    • Denry, I.L.1    Holloway, J.A.2
  • 23
    • 38349192796 scopus 로고    scopus 로고
    • State of the art of zirconia for dental applications
    • Denry I, Kelly JR. State of the art of zirconia for dental applications. Dent Mater 2008;24:299-307.
    • (2008) Dent Mater , vol.24 , pp. 299-307
    • Denry, I.1    Kelly, J.R.2
  • 24
    • 84979455274 scopus 로고
    • Phase analysis in zirconia systems
    • Garvie RC, Nicholson PS. Phase analysis in zirconia systems. J Am Ceram Soc 1972;55:303-305.
    • (1972) J Am Ceram Soc , vol.55 , pp. 303-305
    • Garvie, R.C.1    Nicholson, P.S.2
  • 25
    • 0006757528 scopus 로고
    • International Organization for Standardization ISO 6872: 1995(E). 2nd ed. Geneva, Switzerland: ISO
    • International Organization for Standardization ISO 6872: 1995(E). Dental Ceramics, 2nd ed. Geneva, Switzerland: ISO; 1995.
    • (1995) Dental Ceramics
  • 27
    • 16344363996 scopus 로고    scopus 로고
    • Influence of surface and heat treatments on the flexural strength of a glass-infiltrated alumina/zirconia-reinforced dental ceramic
    • DOI 10.1016/j.dental.2004.07.010, PII S0109564104001307
    • Guazzato M, Albakry M, Quach L, Swain MV. Influence of surface and heat treatments on the flexural strength of a glass-infiltrated alumina/zirconia- reinforced dental ceramic. Dent Mater 2005;21:454-463. (Pubitemid 40467035)
    • (2005) Dental Materials , vol.21 , Issue.5 , pp. 454-463
    • Guazzato, M.1    Albakry, M.2    Quach, L.3    Swain, M.V.4
  • 28
    • 33645356680 scopus 로고    scopus 로고
    • Surface roughness of five different dental ceramic core materials after grinding and polishing
    • Kou W, Molin M, Sjögren G. Surface roughness of five different dental ceramic core materials after grinding and polishing. J Oral Rehabil 2006;33:117-124.
    • (2006) J Oral Rehabil , vol.33 , pp. 117-124
    • Kou, W.1    Molin, M.2    Sjögren, G.3
  • 29
    • 40749115551 scopus 로고    scopus 로고
    • Strength influencing variables on CAD/CAM zirconia frameworks
    • Wang H, Aboushelib MN, Feilzer AJ. Strength influencing variables on CAD/CAM zirconia frameworks. Dent Mater 2008;24:633-638.
    • (2008) Dent Mater , vol.24 , pp. 633-638
    • Wang, H.1    Aboushelib, M.N.2    Feilzer, A.J.3
  • 30
    • 0041919708 scopus 로고    scopus 로고
    • Effect of etching and airborne particle abrasion on the microstructure of different dental ceramics
    • Borges GA, Sophr AM, de Goes MF, Sobrinho LC, Chan DC. Effect of etching and airborne particle abrasion on the microstructure of different dental ceramics. J Prosthet Dent 2003;89:479-488.
    • (2003) J Prosthet Dent , vol.89 , pp. 479-488
    • Borges, G.A.1    Sophr, A.M.2    De Goes, M.F.3    Sobrinho, L.C.4    Chan, D.C.5
  • 31
    • 32044466739 scopus 로고    scopus 로고
    • The influence of surface modification techniques on the performance of a Y-TZP dental ceramic
    • Curtis AR, Wright AJ, Fleming GJ. The influence of surface modification techniques on the performance of a Y-TZP dental ceramic. J Dent 2006;34:195-206.
    • (2006) J Dent , vol.34 , pp. 195-206
    • Curtis, A.R.1    Wright, A.J.2    Fleming, G.J.3
  • 32
    • 35148865193 scopus 로고    scopus 로고
    • Influence of thermal expansion mismatch and fatigue loading on phase changes in porcelain veneered Y-TZP zirconia discs
    • De Kler M, de Jager N, Meegdes M, van der Zel JM. Influence of thermal expansion mismatch and fatigue loading on phase changes in porcelain veneered Y-TZP zirconia discs. J Oral Rehabil 2007;34:841-847.
    • (2007) J Oral Rehabil , vol.34 , pp. 841-847
    • De Kler, M.1    De Jager, N.2    Meegdes, M.3    Van Der Zel, J.M.4
  • 33
  • 34
    • 36849045738 scopus 로고    scopus 로고
    • Chemical solubility and flexural strength of zirconia-based ceramics
    • Chai J, Chu FC, Chow TW, Liang BM. Chemical solubility and flexural strength of zirconia-based ceramics. Int J Prosthodont 2007;20:587-595.
    • (2007) Int J Prosthodont , vol.20 , pp. 587-595
    • Chai, J.1    Chu, F.C.2    Chow, T.W.3    Liang, B.M.4
  • 35
    • 11844264547 scopus 로고    scopus 로고
    • Influence of surface and heat treatments on the flexural strength of Y-TZP dental ceramic
    • DOI 10.1016/j.jdent.2004.07.001, PII S0300571204001125
    • Guazzato M, Quach L, Albakry M, Swain MV. Influence of surface and heat treatments on the flexural strength of Y-TZP dental ceramic. J Dent 2005;33:9-18. (Pubitemid 40093557)
    • (2005) Journal of Dentistry , vol.33 , Issue.1 , pp. 9-18
    • Guazzato, M.1    Quach, L.2    Albakry, M.3    Swain, M.V.4
  • 36
    • 0029258615 scopus 로고
    • Fracture mechanics principles
    • Mecholsky JJ Jr. Fracture mechanics principles. Dent Mater 1995;11:111-112.
    • (1995) Dent Mater , vol.11 , pp. 111-112
    • Mecholsky Jr., J.J.1
  • 37
    • 0029258806 scopus 로고
    • Perspectives on strength
    • Kelly JR. Perspectives on strength. Dent Mater 1995;11:103-110.
    • (1995) Dent Mater , vol.11 , pp. 103-110
    • Kelly, J.R.1
  • 38
    • 34547603573 scopus 로고    scopus 로고
    • Flexural strength and fracture toughness of dental core ceramics
    • Yilmaz H, Aydin C, Gul BE. Flexural strength and fracture toughness of dental core ceramics. J Prosthet Dent 2007;98:120-128.
    • (2007) J Prosthet Dent , vol.98 , pp. 120-128
    • Yilmaz, H.1    Aydin, C.2    Gul, B.E.3
  • 39
    • 0036582509 scopus 로고    scopus 로고
    • The effect of surface roughness on the flexure strength of an alumina reinforced all-ceramic crown material
    • DOI 10.1016/S0300-5712(02)00012-X, PII S030057120200012X
    • Bhamra G, Palin WM, Fleming GJ. The effect of surface roughness on the flexure strength of an alumina reinforced all-ceramic crown material. J Dent 2002;30:153-160. (Pubitemid 40433441)
    • (2002) Journal of Dentistry , vol.30 , Issue.4 , pp. 153-160
    • Bhamra, G.1    Palin, W.M.2    Fleming, G.J.P.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.