Volumn 24, Issue 12, 2008, Pages 1676-1685

Y-TZP ceramic processing from coprecipitated powders: A comparative study with three commercial dental ceramics

Author keywords

Alumina; Dental ceramics; Fracture toughness; Zirconia

Indexed keywords

ALUMINA; ALUMINUM; ANALYSIS OF VARIANCE (ANOVA); BUILDING MATERIALS; CERIUM; COPRECIPITATION; CRYSTALS; DENTAL MATERIALS; FRACTURE; FRACTURE TOUGHNESS; HARDNESS; HARDNESS TESTING; LANTHANUM; LIGHT METALS; MATERIALS PROPERTIES; MECHANICAL PROPERTIES; ORE TREATMENT; POWDERS; POWER AMPLIFIERS; PRECIPITATION (CHEMICAL); QUALITY CONTROL; REGRESSION ANALYSIS; SILICON; SINTERING; VICKERS HARDNESS; VICKERS HARDNESS TESTING; YTTRIA STABILIZED ZIRCONIA; YTTRIUM ALLOYS; ZIRCONIA; ZIRCONIUM;

EID: 54049117580     PISSN: 01095641     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.dental.2008.04.002     Document Type: Article
Times cited : (67)

References (32)
  • 1
    • 0034264517 scopus 로고    scopus 로고
    • Structural reliability of alumina-, feldspar-, leucite-, mica-, and zirconia-based ceramics
    • Tinschert J., Zwez D., Marx R., and Anusavice K.J. Structural reliability of alumina-, feldspar-, leucite-, mica-, and zirconia-based ceramics. J Dent 28 (2000) 529-535
    • (2000) J Dent , vol.28 , pp. 529-535
    • Tinschert, J.1    Zwez, D.2    Marx, R.3    Anusavice, K.J.4
  • 2
    • 1842732685 scopus 로고    scopus 로고
    • Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part I. Pressable and alumina glass-infiltrated ceramics
    • Guazzato M., Albakry M., Ringer S.P., and Swain M.V. Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part I. Pressable and alumina glass-infiltrated ceramics. Dent Mater 20 (2004) 441-448
    • (2004) Dent Mater , vol.20 , pp. 441-448
    • Guazzato, M.1    Albakry, M.2    Ringer, S.P.3    Swain, M.V.4
  • 3
    • 1842783267 scopus 로고    scopus 로고
    • Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part II. Zirconia-based dental ceramics
    • Guazzato M., Albakry M., Ringer S.P., and Swain M.V. Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part II. Zirconia-based dental ceramics. Dent Mater 20 (2004) 449-456
    • (2004) Dent Mater , vol.20 , pp. 449-456
    • Guazzato, M.1    Albakry, M.2    Ringer, S.P.3    Swain, M.V.4
  • 4
    • 0032917811 scopus 로고    scopus 로고
    • Zirconia as ceramic biomaterial
    • Piconi C., and Maccauro G. Zirconia as ceramic biomaterial. Biomaterials 20 (1999) 1-25
    • (1999) Biomaterials , vol.20 , pp. 1-25
    • Piconi, C.1    Maccauro, G.2
  • 6
    • 9444293406 scopus 로고    scopus 로고
    • Fracture resistance behavior of alumina-zirconia composites
    • Szutkowska M. Fracture resistance behavior of alumina-zirconia composites. J Mater Process Technol 153-154 (2004) 868-874
    • (2004) J Mater Process Technol , vol.153-154 , pp. 868-874
    • Szutkowska, M.1
  • 9
    • 0030244480 scopus 로고    scopus 로고
    • Effect of heat-treatment on grain size phase assemblage, and mechanical properties of 3 mol% Y-TZP
    • Ruiz L., and Readley M.J. Effect of heat-treatment on grain size phase assemblage, and mechanical properties of 3 mol% Y-TZP. J Am Ceram Soc 79 (1996) 2331-2340
    • (1996) J Am Ceram Soc , vol.79 , pp. 2331-2340
    • Ruiz, L.1    Readley, M.J.2
  • 14
    • 0034135262 scopus 로고    scopus 로고
    • Synthesis of nanocrystalline zirconia powders for TZP ceramics by a nitrate-citrate combustion route
    • Juarez R.E., Lamas D.G., Lascalea G.E., and Walsöe de Reca N.E. Synthesis of nanocrystalline zirconia powders for TZP ceramics by a nitrate-citrate combustion route. J Eur Ceram Soc 20 (2000) 133-138
    • (2000) J Eur Ceram Soc , vol.20 , pp. 133-138
    • Juarez, R.E.1    Lamas, D.G.2    Lascalea, G.E.3    Walsöe de Reca, N.E.4
  • 16
    • 0000587728 scopus 로고    scopus 로고
    • Low temperature sintering and microstructural development of nanocrystalline Y-TZP powders
    • Duran P., Villegas M., Capel F., Recio P., and Moure C. Low temperature sintering and microstructural development of nanocrystalline Y-TZP powders. J Eur Ceram Soc 16 (1996) 945-952
    • (1996) J Eur Ceram Soc , vol.16 , pp. 945-952
    • Duran, P.1    Villegas, M.2    Capel, F.3    Recio, P.4    Moure, C.5
  • 17
    • 0031621128 scopus 로고    scopus 로고
    • Soft chemistry routes to zirconia ceramics
    • Segal D. Soft chemistry routes to zirconia ceramics. Key Eng Mater 153-154 (1998) 241-250
    • (1998) Key Eng Mater , vol.153-154 , pp. 241-250
    • Segal, D.1
  • 19
    • 0030189364 scopus 로고    scopus 로고
    • Indentation size effect: reality or artifact?
    • Iost A., and Bigot R. Indentation size effect: reality or artifact?. J Mater Sci 31 (1996) 3573-3577
    • (1996) J Mater Sci , vol.31 , pp. 3573-3577
    • Iost, A.1    Bigot, R.2
  • 20
    • 0024733853 scopus 로고
    • Vickers indentation fracture toughness test. Part 1-review of literature and formulation of standardized indentation toughness equations
    • Ponton C.B., and Rawlings R.D. Vickers indentation fracture toughness test. Part 1-review of literature and formulation of standardized indentation toughness equations. Mater Sci Technol 5 (1989) 865-872
    • (1989) Mater Sci Technol , vol.5 , pp. 865-872
    • Ponton, C.B.1    Rawlings, R.D.2
  • 21
    • 0001620911 scopus 로고    scopus 로고
    • An algorithm of digital image processing applied to quantification of grains with discontinuous boundaries
    • Pinto L.C.M., Vasconcelos V., Vasconcelos W.L., and Bressiani J.C. An algorithm of digital image processing applied to quantification of grains with discontinuous boundaries. Acta Microscopica 5 (1996) 168-169
    • (1996) Acta Microscopica , vol.5 , pp. 168-169
    • Pinto, L.C.M.1    Vasconcelos, V.2    Vasconcelos, W.L.3    Bressiani, J.C.4
  • 22
    • 0021602378 scopus 로고
    • 3-containing tetragonal polycrystals (Y-TZP)
    • Advances in ceramics. Claussen N., Rühle M., and Heuer A.H. (Eds), The American Ceramic Society, Columbus, Oh
    • 3-containing tetragonal polycrystals (Y-TZP). In: Claussen N., Rühle M., and Heuer A.H. (Eds). Advances in ceramics. Science and Technology of zirconia II vol. 12 (1984), The American Ceramic Society, Columbus, Oh 352-370
    • (1984) Science and Technology of zirconia II , vol.12 , pp. 352-370
    • Rühle, M.1    Claussen, N.2    Heuer, A.H.3
  • 24
    • 0030288785 scopus 로고    scopus 로고
    • Sintering, microstructure and mechanical properties of commercial Y-TZPs
    • Singh R., Gill C., Lawson S., and Dransfield G.P. Sintering, microstructure and mechanical properties of commercial Y-TZPs. J Mater Sci 31 (1996) 6055-6062
    • (1996) J Mater Sci , vol.31 , pp. 6055-6062
    • Singh, R.1    Gill, C.2    Lawson, S.3    Dransfield, G.P.4
  • 26
    • 34547603573 scopus 로고    scopus 로고
    • Flexural strength and fracture toughness of dental core ceramics
    • Yilmaz H., Aydin C., and Gul B.E. Flexural strength and fracture toughness of dental core ceramics. J Prosthet Dent 98 (2007) 120-128
    • (2007) J Prosthet Dent , vol.98 , pp. 120-128
    • Yilmaz, H.1    Aydin, C.2    Gul, B.E.3
  • 27
    • 21244506130 scopus 로고    scopus 로고
    • A clinical report and overview of scientific studies and clinical procedures conducted on 3M ESPE Lava™ all-ceramic system
    • Piwowarczyk A., Ottl P., Lauer H., and Kuretzky T. A clinical report and overview of scientific studies and clinical procedures conducted on 3M ESPE Lava™ all-ceramic system. J Prosthodont 14 (2005) 39-45
    • (2005) J Prosthodont , vol.14 , pp. 39-45
    • Piwowarczyk, A.1    Ottl, P.2    Lauer, H.3    Kuretzky, T.4
  • 29
    • 0031598657 scopus 로고    scopus 로고
    • Bonding to zirconia ceramic: adhesion methods and their durability
    • Kern M., and Wegner S.M. Bonding to zirconia ceramic: adhesion methods and their durability. Dent Mater 14 (1998) 64-71
    • (1998) Dent Mater , vol.14 , pp. 64-71
    • Kern, M.1    Wegner, S.M.2
  • 30
    • 0036561939 scopus 로고    scopus 로고
    • Effect of different artificial aging conditions on ceramic-composite bond strength
    • Wegner S.M., Gerdes W., and Kern M. Effect of different artificial aging conditions on ceramic-composite bond strength. Int J Prosthodont 15 (2002) 267-272
    • (2002) Int J Prosthodont , vol.15 , pp. 267-272
    • Wegner, S.M.1    Gerdes, W.2    Kern, M.3
  • 31
    • 0141727597 scopus 로고    scopus 로고
    • Effect of surface conditioning methods on the bond strength of luting cement to ceramics
    • Özcan M., and Vallittu P.K. Effect of surface conditioning methods on the bond strength of luting cement to ceramics. Dent Mater 19 (2003) 725-731
    • (2003) Dent Mater , vol.19 , pp. 725-731
    • Özcan, M.1    Vallittu, P.K.2
  • 32
    • 34250649888 scopus 로고    scopus 로고
    • To what extend does the longevity of fixed dental prostheses depend on the function of cement?
    • Edelhoff D., and Özcan M. To what extend does the longevity of fixed dental prostheses depend on the function of cement?. Clin Oral Implants Res 18 (2007) 193-204
    • (2007) Clin Oral Implants Res , vol.18 , pp. 193-204
    • Edelhoff, D.1    Özcan, M.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.