메뉴 건너뛰기




Volumn 68, Issue 6, 2010, Pages 354-359

The effect of laser treatment on bonding between zirconia ceramic surface and resin cement

Author keywords

Airborne particle abrasion; Laser etching; Surface treatment; Zirconium oxide

Indexed keywords

RESIN; RESIN CEMENT; ZIRCONIUM; ZIRCONIUM OXIDE;

EID: 77958033483     PISSN: 00016357     EISSN: 15023850     Source Type: Journal    
DOI: 10.3109/00016357.2010.514720     Document Type: Article
Times cited : (87)

References (31)
  • 1
    • 0141720639 scopus 로고    scopus 로고
    • Bond strengths of porcelain laminate veneers to tooth surfaces prepared with acid and Er, Cr:YSGG laser etching
    • Usumez A, Aykent F. Bond strengths of porcelain laminate veneers to tooth surfaces prepared with acid and Er, Cr:YSGG laser etching. J Prosthet Dent 2003;90:24-30.
    • (2003) J. Prosthet Dent. , vol.90 , pp. 24-30
    • Usumez, A.1    Aykent, F.2
  • 2
    • 0034132457 scopus 로고    scopus 로고
    • Shear bond strength of resin luting cement to glass-infiltrated porous aluminum oxide cores
    • Sen D, Poyrazoglu E, Tuncelli B, Goller G. Shear bond strength of resin luting cement to glass-infiltrated porous aluminum oxide cores. J Prosthet Dent 2000;83:210-15.
    • (2000) J. Prosthet Dent. , vol.83 , pp. 210-215
    • Sen, D.1    Poyrazoglu, E.2    Tuncelli, B.3    Goller, G.4
  • 3
    • 33744789998 scopus 로고    scopus 로고
    • Effect of zirconium-oxide ceramic surface treatments on the bond strength to adhesive resin
    • Atsu SS, Kilicarslan MA, Kucukesmen HC, Aka PS. Effect of zirconium-oxide ceramic surface treatments on the bond strength to adhesive resin. J Prosthet Dent 2006;95:430-6.
    • (2006) J. Prosthet Dent. , vol.95 , pp. 430-436
    • Atsu, S.S.1    Kilicarslan, M.A.2    Kucukesmen, H.C.3    Aka, P.S.4
  • 4
    • 58149229394 scopus 로고    scopus 로고
    • Influence of surface treatments and resin cement selection on bonding to densely-sintered zirconium-oxide ceramic
    • de Oyague RC, Monticelli F, Toledano M, Osorio E, Ferrari M, Osorio R. Influence of surface treatments and resin cement selection on bonding to densely-sintered zirconium-oxide ceramic. Dent Mater 2009;25:172-9.
    • (2009) Dent. Mater. , vol.25 , pp. 172-179
    • De Oyague, R.C.1    Monticelli, F.2    Toledano, M.3    Osorio, E.4    Ferrari, M.5    Osorio, R.6
  • 5
    • 33846944025 scopus 로고    scopus 로고
    • Pilot evaluation of resin composite cement adhesion to zirconia using a novel silane system
    • Matinlinna JP, Lassila LV, Vallittu PK. Pilot evaluation of resin composite cement adhesion to zirconia using a novel silane system. Acta Odontol Scand 2007;65:44-51.
    • (2007) Acta Odontol. Scand. , vol.65 , pp. 44-51
    • Matinlinna, J.P.1    Lassila, L.V.2    Vallittu, P.K.3
  • 6
    • 42449099988 scopus 로고    scopus 로고
    • Effect of various surface conditioning methods on the adhesion of dual-cure resin cement with MDP functional monomer to zirconia after thermal aging
    • Ozcan M, Nijhuis H, Valandro LF. Effect of various surface conditioning methods on the adhesion of dual-cure resin cement with MDP functional monomer to zirconia after thermal aging. Dent Mater J 2008;27:99-104.
    • (2008) Dent. Mater. J. , vol.27 , pp. 99-104
    • Ozcan, M.1    Nijhuis, H.2    Valandro, L.F.3
  • 8
    • 34047214549 scopus 로고    scopus 로고
    • A short-term clinical evaluation of IPS Empress 2 crowns
    • Toksavul S, Toman M. A short-term clinical evaluation of IPS Empress 2 crowns. Int J Prosthodont 2007;20:168-72.
    • (2007) Int. J. Prosthodont , vol.20 , pp. 168-172
    • Toksavul, S.1    Toman, M.2
  • 9
    • 0036652611 scopus 로고    scopus 로고
    • An 11-year clinical evaluation of leucite-reinforced glass-ceramic crowns: A retrospective study
    • Fradeani M, Redemagni M. An 11-year clinical evaluation of leucite-reinforced glass-ceramic crowns: a retrospective study. Quintessence Int 2002;33:503-10.
    • (2002) Quintessence Int. , vol.33 , pp. 503-510
    • Fradeani, M.1    Redemagni, M.2
  • 11
    • 34250185998 scopus 로고    scopus 로고
    • Effect of loading method on the fracture mechanics of two layered all-ceramic restorative systems
    • Aboushelib MN, de Jager N, Kleverlaan CJ, Feilzer AJ. Effect of loading method on the fracture mechanics of two layered all-ceramic restorative systems. Dent Mater 2007;23:952-9.
    • (2007) Dent. Mater. , vol.23 , pp. 952-959
    • Aboushelib, M.N.1    De Jager, N.2    Kleverlaan, C.J.3    Feilzer, A.J.4
  • 12
    • 57749176443 scopus 로고    scopus 로고
    • An in vitro evaluation of the long-term resin bond to a new densely sintered high-purity zirconium-oxide ceramic surface
    • Phark JH, Duarte S, Jr., Blatz M, Sadan A. An in vitro evaluation of the long-term resin bond to a new densely sintered high-purity zirconium-oxide ceramic surface. J Prosthet Dent 2009;101:29-38.
    • (2009) J. Prosthet Dent. , vol.101 , pp. 29-38
    • Phark, J.H.1    Duarte Jr., S.2    Blatz, M.3    Sadan, A.4
  • 13
    • 71349085258 scopus 로고    scopus 로고
    • The effect of different surface treatments on bond strength between leucite reinforced feldspathic ceramic and composite resin
    • Fabianelli A, Pollington S, Papacchini F, Goracci C, Cantoro A, Ferrari M, et al. The effect of different surface treatments on bond strength between leucite reinforced feldspathic ceramic and composite resin. J Dent 2010;38:39-43.
    • (2010) J. Dent. , vol.38 , pp. 39-43
    • Fabianelli, A.1    Pollington, S.2    Papacchini, F.3    Goracci, C.4    Cantoro, A.5    Ferrari, M.6
  • 14
    • 0036490134 scopus 로고    scopus 로고
    • Are adhesive technologies needed to support ceramics? An assessment of the current evidence
    • Burke FJ, Fleming GJ, Nathanson D, Marquis PM. Are adhesive technologies needed to support ceramics? An assessment of the current evidence. J Adhes Dent 2002;4:7-22.
    • (2002) J. Adhes Dent. , vol.4 , pp. 7-22
    • Burke, F.J.1    Fleming, G.J.2    Nathanson, D.3    Marquis, P.M.4
  • 15
    • 0032160199 scopus 로고    scopus 로고
    • Dental luting agents: A review of the current literature
    • Rosenstiel SF, Land MF, Crispin BJ. Dental luting agents: A review of the current literature. J Prosthet Dent 1998;80:280-301.
    • (1998) J. Prosthet Dent. , vol.80 , pp. 280-301
    • Rosenstiel, S.F.1    Land, M.F.2    Crispin, B.J.3
  • 16
    • 0036559426 scopus 로고    scopus 로고
    • The use of chairside silica coating for different dental applications: A clinical report
    • Ozcan M. The use of chairside silica coating for different dental applications: a clinical report. J Prosthet Dent 2002;87:469-72.
    • (2002) J. Prosthet Dent. , vol.87 , pp. 469-472
    • Ozcan, M.1
  • 17
    • 0141727597 scopus 로고    scopus 로고
    • Effect of surface conditioning methods on the bond strength of luting cement to ceramics
    • Ozcan M, Vallittu PK. Effect of surface conditioning methods on the bond strength of luting cement to ceramics. Dent Mater 2003;19:725-31.
    • (2003) Dent. Mater. , vol.19 , pp. 725-731
    • Ozcan, M.1    Vallittu, P.K.2
  • 18
    • 50349096922 scopus 로고    scopus 로고
    • The effect of hydrofluoric acid surface treatment and bond strength of a zirconia veneering ceramic
    • Chaiyabutr Y, McGowan S, Phillips KM, Kois JC, Giordano RA. The effect of hydrofluoric acid surface treatment and bond strength of a zirconia veneering ceramic. J Prosthet Dent 2008;100:194-202.
    • (2008) J. Prosthet Dent. , vol.100 , pp. 194-202
    • Chaiyabutr, Y.1    McGowan, S.2    Phillips, K.M.3    Kois, J.C.4    Giordano, R.A.5
  • 19
    • 70249108785 scopus 로고    scopus 로고
    • Surface roughness and bond strengths of glass-infiltrated aluminaceramics prepared using various surface treatments
    • Ersu B, Yuzugullu B, Ruya Yazici A, Canay S. Surface roughness and bond strengths of glass-infiltrated aluminaceramics prepared using various surface treatments. J Dent 2009;37:848-56.
    • (2009) J. Dent. , vol.37 , pp. 848-856
    • Ersu, B.1    Yuzugullu, B.2    Yazici, A.R.3    Canay, S.4
  • 20
    • 0035404137 scopus 로고    scopus 로고
    • The effect of surface treatment on the shear bond strength of luting cement to a glass-infiltrated alumina ceramic
    • Ozcan M, Alkumru HN, Gemalmaz D. The effect of surface treatment on the shear bond strength of luting cement to a glass-infiltrated alumina ceramic. Int J Prosthodont 2001;14:335-9.
    • (2001) Int. J. Prosthodont , vol.14 , pp. 335-339
    • Ozcan, M.1    Alkumru, H.N.2    Gemalmaz, D.3
  • 21
    • 0035241455 scopus 로고    scopus 로고
    • A combined carbon dioxide/erbium laser for soft and hard tissue procedures
    • Convissar RA, Goldstein EE. A combined carbon dioxide/erbium laser for soft and hard tissue procedures. Dent Today 2001;20:66-71.
    • (2001) Dent. Today , vol.20 , pp. 66-71
    • Convissar, R.A.1    Goldstein, E.E.2
  • 23
    • 0038644503 scopus 로고    scopus 로고
    • Resin-ceramic bonding: A review of the literature
    • Blatz MB, Sadan A, Kern M. Resin-ceramic bonding:a review of the literature. J Prosthet Dent 2003;89:268-74.
    • (2003) J. Prosthet Dent. , vol.89 , pp. 268-274
    • Blatz, M.B.1    Sadan, A.2    Kern, M.3
  • 24
    • 0031598657 scopus 로고    scopus 로고
    • Bonding to zirconia ceramic: Adhesion methods and their durability
    • Kern M, Wegner SM. Bonding to zirconia ceramic: adhesion methods and their durability. Dent Mater 1998;14:64-71.
    • (1998) Dent. Mater. , vol.14 , pp. 64-71
    • Kern, M.1    Wegner, S.M.2
  • 25
    • 1842855215 scopus 로고    scopus 로고
    • Durability of the resin bond strength to the alumina ceramic Procera
    • Hummel M, Kern M. Durability of the resin bond strength to the alumina ceramic Procera. Dent Mater 2004;20:498-508.
    • (2004) Dent. Mater. , vol.20 , pp. 498-508
    • Hummel, M.1    Kern, M.2
  • 26
    • 1942456928 scopus 로고    scopus 로고
    • In vitro evaluation of shear bond strengths of resin to densely-sintered high-purity zirconium-oxide ceramic after long-term storage and thermal cycling
    • Blatz MB, Sadan A, Martin J, Lang B. In vitro evaluation of shear bond strengths of resin to densely-sintered high-purity zirconium-oxide ceramic after long-term storage and thermal cycling. J Prosthet Dent 2004;91:356-62.
    • (2004) J. Prosthet Dent. , vol.91 , pp. 356-362
    • Blatz, M.B.1    Sadan, A.2    Martin, J.3    Lang, B.4
  • 27
    • 4444297012 scopus 로고    scopus 로고
    • In vitro shear bond strength of cementing agents to fixed prosthodontic restorative materials
    • Piwowarczyk A, Lauer HC, Sorensen JA. In vitro shear bond strength of cementing agents to fixed prosthodontic restorative materials. J Prosthet Dent 2004;92:265-73.
    • (2004) J. Prosthet Dent. , vol.92 , pp. 265-273
    • Piwowarczyk, A.1    Lauer, H.C.2    Sorensen, J.A.3
  • 30
    • 0031991726 scopus 로고    scopus 로고
    • Shear bond strength of a resin cement to densely sintered high-purity alumina with various surface conditions
    • Awliya W, Oden A, Yaman P, Dennison JB, Razzoog ME. Shear bond strength of a resin cement to densely sintered high-purity alumina with various surface conditions. Acta Odontol Scand 1998;56:9-13.
    • (1998) Acta Odontol. Scand. , vol.56 , pp. 9-13
    • Awliya, W.1    Oden, A.2    Yaman, P.3    Dennison, J.B.4    Razzoog, M.E.5


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.