Volumn 23, Issue 8, 2007, Pages 952-959

Effect of loading method on the fracture mechanics of two layered all-ceramic restorative systems

Author keywords

Ceramic structure; Dental restorative materials; Fracture mechanism; Mechanical test; Scanning electron microscopy; Zirconia

Indexed keywords

CERAMIC MATERIALS; ENERGY ABSORPTION; FINITE ELEMENT METHOD; FRACTOGRAPHY; FRACTURE MECHANICS; MECHANICAL TESTING; SCANNING ELECTRON MICROSCOPY;

EID: 34250185998     PISSN: 01095641     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.dental.2006.06.036     Document Type: Article
Times cited : (103)

References (33)
  • 2
    • 0000653434 scopus 로고
    • The reinforcement of dental porcelain with ceramic oxides
    • McLean J.W., and Hughes T.H. The reinforcement of dental porcelain with ceramic oxides. Br Dent J 119 (1965) 251-267
    • (1965) Br Dent J , vol.119 , pp. 251-267
    • McLean, J.W.1    Hughes, T.H.2
  • 3
    • 0036134528 scopus 로고    scopus 로고
    • Fracture toughness of dental ceramics: comparison of bending and indentation method
    • Fischer H., and Marx R. Fracture toughness of dental ceramics: comparison of bending and indentation method. Dent Mater 18 (2002) 12-19
    • (2002) Dent Mater , vol.18 , pp. 12-19
    • Fischer, H.1    Marx, R.2
  • 4
    • 0036206982 scopus 로고    scopus 로고
    • Characterization of damage modes in dental ceramic bilayer structures
    • Deng Y., Lawn B.R., and Lioyd I.K. Characterization of damage modes in dental ceramic bilayer structures. J Biomed Mater Res 63 (2001) 137-145
    • (2001) J Biomed Mater Res , vol.63 , pp. 137-145
    • Deng, Y.1    Lawn, B.R.2    Lioyd, I.K.3
  • 5
    • 3242741859 scopus 로고    scopus 로고
    • A comparison of fracture strength of yttrium-oxide-partially-stabilized zirconia ceramic crowns with varying core thickness, shapes and veneer ceramics
    • Sundh A., and Sjogren G. A comparison of fracture strength of yttrium-oxide-partially-stabilized zirconia ceramic crowns with varying core thickness, shapes and veneer ceramics. J Oral Rehabil 31 (2004) 682-688
    • (2004) J Oral Rehabil , vol.31 , pp. 682-688
    • Sundh, A.1    Sjogren, G.2
  • 6
    • 0036962147 scopus 로고    scopus 로고
    • Review phase transitions in zirconium dioxide and related materials for high performance engineering ceramics
    • Bocanegra-Bernal M.H., and Diaz dela Torre S. Review phase transitions in zirconium dioxide and related materials for high performance engineering ceramics. J Mater Sci 37 (2002) 4947-4971
    • (2002) J Mater Sci , vol.37 , pp. 4947-4971
    • Bocanegra-Bernal, M.H.1    Diaz dela Torre, S.2
  • 7
    • 0034188519 scopus 로고    scopus 로고
    • Mechanical property evaluation of pressable restorative ceramics
    • Drummond J.L., King T.J., Bapna M.S., and Koperski R.D. Mechanical property evaluation of pressable restorative ceramics. Dent Mater 16 (2000) 226-233
    • (2000) Dent Mater , vol.16 , pp. 226-233
    • Drummond, J.L.1    King, T.J.2    Bapna, M.S.3    Koperski, R.D.4
  • 8
    • 0031279525 scopus 로고    scopus 로고
    • Impact velocities of the teeth after a sudden unloading at various initial bite forces, degrees of mouth opening, and distances of travel
    • Nagashima T., Slager G.E., Otten E., Broekhuijsen M.L., and van Willigen J.D. Impact velocities of the teeth after a sudden unloading at various initial bite forces, degrees of mouth opening, and distances of travel. J Dent Res 76 (1997) 1751-1759
    • (1997) J Dent Res , vol.76 , pp. 1751-1759
    • Nagashima, T.1    Slager, G.E.2    Otten, E.3    Broekhuijsen, M.L.4    van Willigen, J.D.5
  • 10
    • 0034264517 scopus 로고    scopus 로고
    • Structural reliability of alumina-, feldspar-, leucite-, mica- and zirconia-based ceramics
    • Tinschert J., Zwez D., Marx R., and Anusavice K.J. Structural reliability of alumina-, feldspar-, leucite-, mica- and zirconia-based ceramics. J Dent 28 (2000) 529-535
    • (2000) J Dent , vol.28 , pp. 529-535
    • Tinschert, J.1    Zwez, D.2    Marx, R.3    Anusavice, K.J.4
  • 11
    • 12444332060 scopus 로고    scopus 로고
    • Fracture behavior of lithia disilicate- and leucite-based ceramics
    • Della Bona A., Mecholsky J., John J., and Anusavice K.J. Fracture behavior of lithia disilicate- and leucite-based ceramics. Dent Mater 20 (2004) 956-962
    • (2004) Dent Mater , vol.20 , pp. 956-962
    • Della Bona, A.1    Mecholsky, J.2    John, J.3    Anusavice, K.J.4
  • 12
  • 13
    • 0029258584 scopus 로고
    • Fractography: determining the sites of fracture initiation
    • Mecholsky J. Fractography: determining the sites of fracture initiation. Dent Mater 11 (1995) 113-116
    • (1995) Dent Mater , vol.11 , pp. 113-116
    • Mecholsky, J.1
  • 14
    • 25144475575 scopus 로고    scopus 로고
    • Quinn JB, Quinn GD, Kelly JR, Scherrer SS. Fractographic analyses of three ceramic whole crown restoration failures. Dent Mater; 2005.
  • 15
    • 0034230609 scopus 로고    scopus 로고
    • Influence of relative layer height and testing method on the failure mode and origin in a bilayered dental ceramic composite
    • Thompson G. Influence of relative layer height and testing method on the failure mode and origin in a bilayered dental ceramic composite. Dent Mater 16 (2000) 235-243
    • (2000) Dent Mater , vol.16 , pp. 235-243
    • Thompson, G.1
  • 16
    • 0024760939 scopus 로고
    • Fracture-surface analysis of dental ceramics
    • Kelly J., Campbell S., and Bowen H. Fracture-surface analysis of dental ceramics. J Prosthet Dent 62 (1989) 536-541
    • (1989) J Prosthet Dent , vol.62 , pp. 536-541
    • Kelly, J.1    Campbell, S.2    Bowen, H.3
  • 17
    • 0034174580 scopus 로고    scopus 로고
    • Role of adhesive interlayer in transverse fracture of brittle layer structure
    • Chai H., and Lawn B. Role of adhesive interlayer in transverse fracture of brittle layer structure. J Mater Res 15 (2000) 1017-1023
    • (2000) J Mater Res , vol.15 , pp. 1017-1023
    • Chai, H.1    Lawn, B.2
  • 18
    • 0028709614 scopus 로고
    • Fracture surface characterization of clinically failed all-ceramic crowns
    • Thompson J.Y., Anusavice K.J., Naman A., and Morris H.F. Fracture surface characterization of clinically failed all-ceramic crowns. J Dent Res 73 (1994) 1824-1832
    • (1994) J Dent Res , vol.73 , pp. 1824-1832
    • Thompson, J.Y.1    Anusavice, K.J.2    Naman, A.3    Morris, H.F.4
  • 19
    • 0031598699 scopus 로고    scopus 로고
    • Role of microstructure on contact damage and strength degradation of micaceous glass-ceramics
    • Peterson I.M., Wuttiphan S., Lawn B.R., and Chyung K. Role of microstructure on contact damage and strength degradation of micaceous glass-ceramics. Dent Mater 14 (1998) 80-89
    • (1998) Dent Mater , vol.14 , pp. 80-89
    • Peterson, I.M.1    Wuttiphan, S.2    Lawn, B.R.3    Chyung, K.4
  • 21
    • 0035512807 scopus 로고    scopus 로고
    • Use of contact testing in the characterization and design of all-ceramic crown like layer structures: a review
    • Lawn B., Deng Y., and Thompson V. Use of contact testing in the characterization and design of all-ceramic crown like layer structures: a review. J Prosth Dent 86 (2001) 495-510
    • (2001) J Prosth Dent , vol.86 , pp. 495-510
    • Lawn, B.1    Deng, Y.2    Thompson, V.3
  • 22
    • 25144511110 scopus 로고    scopus 로고
    • Microtensile bond strength of different components of core veneered all-ceramic restorations
    • Aboushelib M.N., de Jager N., Kleverlaan C.J., and Feilzer A.J. Microtensile bond strength of different components of core veneered all-ceramic restorations. Dent Mater 21 (2005) 984-991
    • (2005) Dent Mater , vol.21 , pp. 984-991
    • Aboushelib, M.N.1    de Jager, N.2    Kleverlaan, C.J.3    Feilzer, A.J.4
  • 24
    • 2942547986 scopus 로고    scopus 로고
    • Fracture resistance of three all-ceramic restorative systems for posterior applications
    • Pallis K., Griggs J.A., Woody R.D., Guillen G.E., and Miller A.W. Fracture resistance of three all-ceramic restorative systems for posterior applications. J Prosthet Dent 91 (2004) 561-569
    • (2004) J Prosthet Dent , vol.91 , pp. 561-569
    • Pallis, K.1    Griggs, J.A.2    Woody, R.D.3    Guillen, G.E.4    Miller, A.W.5
  • 25
    • 0030154870 scopus 로고    scopus 로고
    • Impact resistance of crowned endodontically treated central incisors with internal composite cores
    • Cathro P.R., Chandler N.P., and Hood J.A.A. Impact resistance of crowned endodontically treated central incisors with internal composite cores. Endod Dent Traumatol 12 (1996) 124-128
    • (1996) Endod Dent Traumatol , vol.12 , pp. 124-128
    • Cathro, P.R.1    Chandler, N.P.2    Hood, J.A.A.3
  • 26
    • 0032107537 scopus 로고    scopus 로고
    • Comparison of three fracture toughness testing techniques using a dental glass and a dental ceramic
    • Scherrer S.S., Denry I.L., and Wiskott H.W. Comparison of three fracture toughness testing techniques using a dental glass and a dental ceramic. Dent Mater 14 (1998) 246-255
    • (1998) Dent Mater , vol.14 , pp. 246-255
    • Scherrer, S.S.1    Denry, I.L.2    Wiskott, H.W.3
  • 27
    • 0038149964 scopus 로고    scopus 로고
    • IC) of hot-pressed core ceramics based fractographic analysis of fractured ceramic FPDs
    • IC) of hot-pressed core ceramics based fractographic analysis of fractured ceramic FPDs. Int J Prosthodont 16 (2003) 135-140
    • (2003) Int J Prosthodont , vol.16 , pp. 135-140
    • Oh, W.1    Park, J.2    Anusavice, K.J.3
  • 28
    • 0038378501 scopus 로고    scopus 로고
    • Fracture toughness and hardness evaluation of three pressable all-ceramic dental materials
    • Albakry M., Guazzato M., and Swain M.V. Fracture toughness and hardness evaluation of three pressable all-ceramic dental materials. J Dent 31 (2003) 181-188
    • (2003) J Dent , vol.31 , pp. 181-188
    • Albakry, M.1    Guazzato, M.2    Swain, M.V.3
  • 29
    • 11844264547 scopus 로고    scopus 로고
    • Influence of surface and heat treatments on the flexural strength of Y-TZP dental ceramic
    • Guazzato M., Quach L., Albakry M., and Swain M.V. Influence of surface and heat treatments on the flexural strength of Y-TZP dental ceramic. J Dent 33 (2005) 9-18
    • (2005) J Dent , vol.33 , pp. 9-18
    • Guazzato, M.1    Quach, L.2    Albakry, M.3    Swain, M.V.4
  • 31
    • 3042833035 scopus 로고    scopus 로고
    • Maximal bite forces in healthy young adults as predicted by surface electromyography
    • Ferrario V.F., Sforza C., Zanotti G., and Tartaglia G.M. Maximal bite forces in healthy young adults as predicted by surface electromyography. J Dent 32 (2004) 451-457
    • (2004) J Dent , vol.32 , pp. 451-457
    • Ferrario, V.F.1    Sforza, C.2    Zanotti, G.3    Tartaglia, G.M.4
  • 32
    • 13444311681 scopus 로고    scopus 로고
    • The influence of design parameters on the FEA-determined stress distribution in CAD-CAM produced all-ceramic dental crowns
    • De Jager N., Pallav P., and Feilzer A.J. The influence of design parameters on the FEA-determined stress distribution in CAD-CAM produced all-ceramic dental crowns. Dent Mater 21 (2005) 242-251
    • (2005) Dent Mater , vol.21 , pp. 242-251
    • De Jager, N.1    Pallav, P.2    Feilzer, A.J.3
  • 33
    • 0036834319 scopus 로고    scopus 로고
    • Finite element analysis studies of a metal-ceramic crown on a first premolar tooth
    • Proos K.A., Swain M.V., Ironside J., and Steven G.P. Finite element analysis studies of a metal-ceramic crown on a first premolar tooth. Int J Prosthodont 15 (2002) 521-527
    • (2002) Int J Prosthodont , vol.15 , pp. 521-527
    • Proos, K.A.1    Swain, M.V.2    Ironside, J.3    Steven, G.P.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.