Volumn 83, Issue 2, 2000, Pages 210-215

Shear bond strength of resin luting cement to glass-infiltrated porous aluminum oxide cores

Author keywords

[No Author keywords available]

Indexed keywords

ALUMINUM OXIDE; BORON DERIVATIVE; DENTIN BONDING AGENT; DIAMOND; GLASS; IN CERAM; IN-CERAM; METHACRYLIC ACID DERIVATIVE; METHACRYLIC ACID METHYL ESTER; PANAVIA EX; PHOSPHATE; RESIN CEMENT; SUPER BOND; SUPER-BOND;

EID: 0034132457     PISSN: 00223913     EISSN: None     Source Type: Journal    
DOI: 10.1016/S0022-3913(00)80014-1     Document Type: Article
Times cited : (48)

References (17)
  • 1
    • 0030254327 scopus 로고    scopus 로고
    • Copy-milled aluminous core ceramic crowns: a clinical report
    • Rinke S., and Huls A. Copy-milled aluminous core ceramic crowns: a clinical report. J Prosthet Dent 76 (1996) 343-346
    • (1996) J Prosthet Dent , vol.76 , pp. 343-346
    • Rinke, S.1    Huls, A.2
  • 2
    • 0029444234 scopus 로고
    • In-Ceram failure behavior and core-veneer interface quality as influenced by residual infiltration glass
    • Carrier D.D., and Kelly J.R. In-Ceram failure behavior and core-veneer interface quality as influenced by residual infiltration glass. J Prosthodont 4 (1995) 237-242
    • (1995) J Prosthodont , vol.4 , pp. 237-242
    • Carrier, D.D.1    Kelly, J.R.2
  • 3
    • 0141697178 scopus 로고
    • Bond strength of resin cement to In-Ceram core materials
    • (IADR Abstracts)
    • (IADR Abstracts). Kraivixien-Vonghantuset R., Pietrobon N., and Nathanson D. Bond strength of resin cement to In-Ceram core materials. J Dent Res 71 (1992) 141
    • (1992) J Dent Res , vol.71 , pp. 141
    • Kraivixien-Vonghantuset, R.1    Pietrobon, N.2    Nathanson, D.3
  • 4
    • 0141973832 scopus 로고
    • Tensile bond strength of two silicoating systems on the AI D ceramics In-Ceram
    • (IADR Abstracts)
    • (IADR Abstracts). Neikes M.J., Kern M., and Stroh J.R. Tensile bond strength of two silicoating systems on the AI D ceramics In-Ceram. J Dent Res 71 (1992) 144
    • (1992) J Dent Res , vol.71 , pp. 144
    • Neikes, M.J.1    Kern, M.2    Stroh, J.R.3
  • 5
    • 0032044383 scopus 로고    scopus 로고
    • Microscopic and energy dispersive xray analysis of surface adaptation of dental cements to dental ceramic surfaces
    • Thompson J.Y., Rapp M.M., and Parker A.J. Microscopic and energy dispersive xray analysis of surface adaptation of dental cements to dental ceramic surfaces. J Prosthet Dent 79 (1998) 378-383
    • (1998) J Prosthet Dent , vol.79 , pp. 378-383
    • Thompson, J.Y.1    Rapp, M.M.2    Parker, A.J.3
  • 6
    • 0029363971 scopus 로고
    • Tensile bond strength of resin luting cement to glass infiltrated porous aluminum oxide cores (In-Ceram)
    • Isidor F., Stokholm R., and Ravnholt G. Tensile bond strength of resin luting cement to glass infiltrated porous aluminum oxide cores (In-Ceram). Eur J Prosthodont Restor Dent 3 (1995) 199-202
    • (1995) Eur J Prosthodont Restor Dent , vol.3 , pp. 199-202
    • Isidor, F.1    Stokholm, R.2    Ravnholt, G.3
  • 8
    • 77949579355 scopus 로고
    • Study of anterior adhesive bridges and splints using newly developed adhesive resins
    • Tabat Y., and Amano H. Study of anterior adhesive bridges and splints using newly developed adhesive resins. J Gnathol 4 (1985) 73-85
    • (1985) J Gnathol , vol.4 , pp. 73-85
    • Tabat, Y.1    Amano, H.2
  • 9
    • 0041194819 scopus 로고
    • Adhesive and mechanical properties of a new dental adhesive
    • (abstract)
    • (abstract). Omura J., Yamauchi J., Harada I., and Wada T. Adhesive and mechanical properties of a new dental adhesive. J Dent Res 63 (1984) 233
    • (1984) J Dent Res , vol.63 , pp. 233
    • Omura, J.1    Yamauchi, J.2    Harada, I.3    Wada, T.4
  • 10
    • 0026194688 scopus 로고
    • Bond strength of etched In-Ceram to tooth enamel
    • [in German]
    • [in German]. Pape F.W., Pfeiffer P., and Marx R. Bond strength of etched In-Ceram to tooth enamel. ZWR 100 (1991) 450-453
    • (1991) ZWR , vol.100 , pp. 450-453
    • Pape, F.W.1    Pfeiffer, P.2    Marx, R.3
  • 11
    • 0023413139 scopus 로고
    • Shear strength of the composite bond to etched porcelain
    • Stangel I., Nathanson D., and Hsu C.S. Shear strength of the composite bond to etched porcelain. J Dent Res 66 (1987) 1460-1465
    • (1987) J Dent Res , vol.66 , pp. 1460-1465
    • Stangel, I.1    Nathanson, D.2    Hsu, C.S.3
  • 12
    • 0027605367 scopus 로고
    • Bond strength of composite to etched and sandblasted porcelain
    • Wolf D.M., Powers J.M., and O'Keefe K.L. Bond strength of composite to etched and sandblasted porcelain. Am J Dent 6 (1993) 155-158
    • (1993) Am J Dent , vol.6 , pp. 155-158
    • Wolf, D.M.1    Powers, J.M.2    O'Keefe, K.L.3
  • 13
    • 0028441251 scopus 로고
    • Bonding of resin cements to an aluminous ceramic: a new surface treatment
    • Sadoun M., and Asmussen E. Bonding of resin cements to an aluminous ceramic: a new surface treatment. Dent Mater 10 (1994) 185-189
    • (1994) Dent Mater , vol.10 , pp. 185-189
    • Sadoun, M.1    Asmussen, E.2
  • 15
    • 0029266741 scopus 로고
    • Bonding to glass infiltrated alumina ceramic: adhesive methods and their durability
    • Kern M., and Thompson V.P. Bonding to glass infiltrated alumina ceramic: adhesive methods and their durability. J Prosthet Dent 73 (1995) 240-249
    • (1995) J Prosthet Dent , vol.73 , pp. 240-249
    • Kern, M.1    Thompson, V.P.2
  • 16
    • 0031226791 scopus 로고    scopus 로고
    • Preliminary investigation of a novel retentive system for hydrofluoric acid etch-resistant dental ceramics
    • Wood D.J., Bubb N.L., Millar B.J., and Dunne S.M. Preliminary investigation of a novel retentive system for hydrofluoric acid etch-resistant dental ceramics. J Prosthet Dent 78 (1997) 275-280
    • (1997) J Prosthet Dent , vol.78 , pp. 275-280
    • Wood, D.J.1    Bubb, N.L.2    Millar, B.J.3    Dunne, S.M.4
  • 17
    • 0028435067 scopus 로고
    • Sandblasting and silica coating of a glass-infiltrated alumina ceramic: volume loss, morphology, and changes in the surface composition
    • Kern M., and Thompson V.P. Sandblasting and silica coating of a glass-infiltrated alumina ceramic: volume loss, morphology, and changes in the surface composition. J Prosthet Dent 71 (1994) 453-461
    • (1994) J Prosthet Dent , vol.71 , pp. 453-461
    • Kern, M.1    Thompson, V.P.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.