Volumn 96, Issue 3, 2006, Pages 154-164

In vitro evaluation of low-temperature aging effects and finishing procedures on the flexural strength and structural stability of Y-TZP dental ceramics

Author keywords

[No Author keywords available]

Indexed keywords

YTTRIA STABILIZED TETRAGONAL ZIRCONIA POLYCRYSTALS CERAMIC; YTTRIA-STABILIZED TETRAGONAL ZIRCONIA POLYCRYSTALS CERAMIC; YTTRIUM;

EID: 33748596081     PISSN: 00223913     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.prosdent.2006.08.004     Document Type: Article
Times cited : (170)

References (41)
  • 1
    • 0038727300 scopus 로고    scopus 로고
    • An in vitro study of the compressive load at fracture of Procera AllCeram crowns with varying thickness of veneer porcelain
    • Webber B., McDonald A., and Knowles J. An in vitro study of the compressive load at fracture of Procera AllCeram crowns with varying thickness of veneer porcelain. J Prosthet Dent 89 (2003) 154-160
    • (2003) J Prosthet Dent , vol.89 , pp. 154-160
    • Webber, B.1    McDonald, A.2    Knowles, J.3
  • 2
    • 0035351260 scopus 로고    scopus 로고
    • Fracture resistance of lithium disilicate-, alumina-, and zirconia-based three-unit fixed partial dentures: a laboratory study
    • Tinschert J., Natt G., Mautsch W., Augthum M., and Spiekermann H. Fracture resistance of lithium disilicate-, alumina-, and zirconia-based three-unit fixed partial dentures: a laboratory study. Int J Prosthodont 14 (2001) 231-238
    • (2001) Int J Prosthodont , vol.14 , pp. 231-238
    • Tinschert, J.1    Natt, G.2    Mautsch, W.3    Augthum, M.4    Spiekermann, H.5
  • 3
    • 0026461934 scopus 로고
    • Slip-casting alumina ceramics for crown and bridge restorations
    • Probster L., and Diehl J. Slip-casting alumina ceramics for crown and bridge restorations. Quintessence Int 23 (1992) 25-31
    • (1992) Quintessence Int , vol.23 , pp. 25-31
    • Probster, L.1    Diehl, J.2
  • 5
    • 0035512807 scopus 로고    scopus 로고
    • Use of contact testing in the characterization and design of all-ceramic crownlike layer structures: a review
    • Lawn B.R., Deng Y., and Thompson V.P. Use of contact testing in the characterization and design of all-ceramic crownlike layer structures: a review. J Prosthet Dent 86 (2001) 495-510
    • (2001) J Prosthet Dent , vol.86 , pp. 495-510
    • Lawn, B.R.1    Deng, Y.2    Thompson, V.P.3
  • 6
    • 0028476223 scopus 로고
    • Fracture strength of all-ceramic crowns
    • Yoshinari M., and Derand T. Fracture strength of all-ceramic crowns. Int J Prosthodont 7 (1994) 329-338
    • (1994) Int J Prosthodont , vol.7 , pp. 329-338
    • Yoshinari, M.1    Derand, T.2
  • 7
    • 0035408488 scopus 로고    scopus 로고
    • Five-year evaluation of posterior all-ceramic three-unit (In-Ceram) FPDs
    • Vult von Steyern P., Jonsson O., and Nilner K. Five-year evaluation of posterior all-ceramic three-unit (In-Ceram) FPDs. Int J Prosthodont 14 (2001) 379-384
    • (2001) Int J Prosthodont , vol.14 , pp. 379-384
    • Vult von Steyern, P.1    Jonsson, O.2    Nilner, K.3
  • 9
    • 0029294815 scopus 로고
    • Relative flexural strength of six new ceramic materials
    • Seghi R.R., and Sorensen J.A. Relative flexural strength of six new ceramic materials. Int J Prosthodont 8 (1995) 239-246
    • (1995) Int J Prosthodont , vol.8 , pp. 239-246
    • Seghi, R.R.1    Sorensen, J.A.2
  • 10
    • 0026149549 scopus 로고
    • The all-porcelain, resin-bonded bridge
    • Kern M., Knode H., and Strubb J.R. The all-porcelain, resin-bonded bridge. Quintessence Int 22 (1991) 257-262
    • (1991) Quintessence Int , vol.22 , pp. 257-262
    • Kern, M.1    Knode, H.2    Strubb, J.R.3
  • 11
    • 0034132550 scopus 로고    scopus 로고
    • Survival of In-Ceram crowns in a private practice: a prospective clinical trial
    • McLaren E.A., and White S.N. Survival of In-Ceram crowns in a private practice: a prospective clinical trial. J Prosthet Dent 83 (2000) 216-222
    • (2000) J Prosthet Dent , vol.83 , pp. 216-222
    • McLaren, E.A.1    White, S.N.2
  • 12
    • 0032917811 scopus 로고    scopus 로고
    • Zirconia as a ceramic material
    • Piconi C., and Maccauro G. Zirconia as a ceramic material. Biomaterials 20 (1999) 1-25
    • (1999) Biomaterials , vol.20 , pp. 1-25
    • Piconi, C.1    Maccauro, G.2
  • 13
    • 0033749719 scopus 로고    scopus 로고
    • A comparison of all-ceramic restorative systems: part 2
    • 43-5
    • Giordano R. A comparison of all-ceramic restorative systems: part 2. Gen Dent 48 (2000) 38-40 43-5
    • (2000) Gen Dent , vol.48 , pp. 38-40
    • Giordano, R.1
  • 14
    • 0036636830 scopus 로고    scopus 로고
    • Mechanical properties of In-Ceram Alumina and In-Ceram Zirconia
    • Guazzato M., Albakry M., Swain M.V., and Ironside J. Mechanical properties of In-Ceram Alumina and In-Ceram Zirconia. Int J Prosthodont 15 (2002) 339-346
    • (2002) Int J Prosthodont , vol.15 , pp. 339-346
    • Guazzato, M.1    Albakry, M.2    Swain, M.V.3    Ironside, J.4
  • 15
    • 2942547986 scopus 로고    scopus 로고
    • Fracture resistance of three all-ceramic restorative systems for posterior applications
    • Pallis K., Griggs J.A., Woody R.D., Guillen G.E., and Miller A.W. Fracture resistance of three all-ceramic restorative systems for posterior applications. J Prosthet Dent 91 (2004) 561-569
    • (2004) J Prosthet Dent , vol.91 , pp. 561-569
    • Pallis, K.1    Griggs, J.A.2    Woody, R.D.3    Guillen, G.E.4    Miller, A.W.5
  • 17
    • 0032690720 scopus 로고    scopus 로고
    • On the degradation of zirconia ceramics during low-temperature annealing in water or water vapor
    • Guo X. On the degradation of zirconia ceramics during low-temperature annealing in water or water vapor. J Physics Chem Solids 60 (1999) 539-546
    • (1999) J Physics Chem Solids , vol.60 , pp. 539-546
    • Guo, X.1
  • 18
    • 0002512802 scopus 로고
    • Review of low temperature degradation in Y-TZPs
    • Tressler R.E., and McNallan M. (Eds), American Ceramics Society, Westerville
    • Lilley E. Review of low temperature degradation in Y-TZPs. In: Tressler R.E., and McNallan M. (Eds). Ceramic transaction: corrosion and corrosive degradation of ceramics (1990), American Ceramics Society, Westerville 387-407
    • (1990) Ceramic transaction: corrosion and corrosive degradation of ceramics , pp. 387-407
    • Lilley, E.1
  • 19
    • 0033350821 scopus 로고    scopus 로고
    • Low-temperature aging of Y-TZP ceramics
    • Chevalier J., Cales B., and Drouin J.M. Low-temperature aging of Y-TZP ceramics. J Am Ceram Soc 82 (1999) 2150-2204
    • (1999) J Am Ceram Soc , vol.82 , pp. 2150-2204
    • Chevalier, J.1    Cales, B.2    Drouin, J.M.3
  • 20
    • 0032182099 scopus 로고    scopus 로고
    • 2 polycrystals of various grain sizes during low-temperature aging in water
    • 2 polycrystals of various grain sizes during low-temperature aging in water. J Am Ceram Soc 81 (1998) 2687-2778
    • (1998) J Am Ceram Soc , vol.81 , pp. 2687-2778
    • Li, J.-F.1    Watanabe, R.2
  • 21
    • 0029237462 scopus 로고
    • Environmental degradation of zirconia ceramics
    • Lawson S. Environmental degradation of zirconia ceramics. J Eur Ceram Soc 15 (1995) 485-502
    • (1995) J Eur Ceram Soc , vol.15 , pp. 485-502
    • Lawson, S.1
  • 22
    • 0942278176 scopus 로고    scopus 로고
    • Delay of tetragonal-to-monoclinic transition in water vapour due to nanostructural effect
    • Boulc'h F., Dessemond L., and Djurado E. Delay of tetragonal-to-monoclinic transition in water vapour due to nanostructural effect. J Eur Ceram Soc 24 (2004) 1181-1185
    • (2004) J Eur Ceram Soc , vol.24 , pp. 1181-1185
    • Boulc'h, F.1    Dessemond, L.2    Djurado, E.3
  • 23
    • 0141460499 scopus 로고    scopus 로고
    • Low-temperature ageing of zirconia-toughened alumina ceramics and its implication in biomedical implants
    • Deville S., Chevalier J., Fantozzi G., Bartolome J.F., Requena J., Moya J.S., et al. Low-temperature ageing of zirconia-toughened alumina ceramics and its implication in biomedical implants. J Eur Ceram Soc 23 (2003) 2975-2982
    • (2003) J Eur Ceram Soc , vol.23 , pp. 2975-2982
    • Deville, S.1    Chevalier, J.2    Fantozzi, G.3    Bartolome, J.F.4    Requena, J.5    Moya, J.S.6
  • 24
    • 0042911602 scopus 로고    scopus 로고
    • Hydrothermal degradation of cubic zirconia
    • Guo X., and He J. Hydrothermal degradation of cubic zirconia. Acta Mater 51 (2003) 5123-5130
    • (2003) Acta Mater , vol.51 , pp. 5123-5130
    • Guo, X.1    He, J.2
  • 25
    • 0024546336 scopus 로고
    • Mechanical properties and short-term in-vivo evaluation of yttrium-oxide-partially-stabilized zirconia
    • Christel P., Meunier A., Heller M., Torre J.P., and Peille C.N. Mechanical properties and short-term in-vivo evaluation of yttrium-oxide-partially-stabilized zirconia. J Biomed Mater Res 23 (1989) 45-61
    • (1989) J Biomed Mater Res , vol.23 , pp. 45-61
    • Christel, P.1    Meunier, A.2    Heller, M.3    Torre, J.P.4    Peille, C.N.5
  • 27
    • 0033771089 scopus 로고    scopus 로고
    • Zirconia as a sliding material. Histologic, laboratory, and clinical data
    • Cales B. Zirconia as a sliding material. Histologic, laboratory, and clinical data. Clin Orthop Relat Res 379 (2000) 94-112
    • (2000) Clin Orthop Relat Res , vol.379 , pp. 94-112
    • Cales, B.1
  • 28
    • 0035348103 scopus 로고    scopus 로고
    • Flexural strength of Cerec 2 machined and jointed InCeram-Alumina and InCeram-Zirconia bars
    • Apholt W., Bindl A., Luthy H., and Mormann W.H. Flexural strength of Cerec 2 machined and jointed InCeram-Alumina and InCeram-Zirconia bars. Dent Mater 17 (2001) 260-267
    • (2001) Dent Mater , vol.17 , pp. 260-267
    • Apholt, W.1    Bindl, A.2    Luthy, H.3    Mormann, W.H.4
  • 30
    • 0036886280 scopus 로고    scopus 로고
    • Transformation-toughened zirconia for dental inlays, crowns and bridges: chemical stability and effect of low-temperature aging on flexural strength and surface structure
    • Ardlin B.I. Transformation-toughened zirconia for dental inlays, crowns and bridges: chemical stability and effect of low-temperature aging on flexural strength and surface structure. Dent Mater 18 (2002) 590-595
    • (2002) Dent Mater , vol.18 , pp. 590-595
    • Ardlin, B.I.1
  • 32
  • 33
    • 11844264547 scopus 로고    scopus 로고
    • Influence of surface and heat treatments on the flexural strength of Y-TZP dental ceramic
    • Guazzato M., Quach L., Albakry M., and Swain M.V. Influence of surface and heat treatments on the flexural strength of Y-TZP dental ceramic. J Dent 33 (2005) 9-18
    • (2005) J Dent , vol.33 , pp. 9-18
    • Guazzato, M.1    Quach, L.2    Albakry, M.3    Swain, M.V.4
  • 34
    • 0034264517 scopus 로고    scopus 로고
    • Structural reliability of alumina-, feldspar-, leucite-, mica- and zirconia-based ceramics
    • Tinschert J., Zwez D., Marx R., and Anusavice K.J. Structural reliability of alumina-, feldspar-, leucite-, mica- and zirconia-based ceramics. J Dent 28 (2000) 529-535
    • (2000) J Dent , vol.28 , pp. 529-535
    • Tinschert, J.1    Zwez, D.2    Marx, R.3    Anusavice, K.J.4
  • 36
    • 0028434170 scopus 로고
    • Long-term in vivo and in vitro aging of a zirconia ceramic used in orthopaedy
    • Cales B., Stefani Y., and Lilley E. Long-term in vivo and in vitro aging of a zirconia ceramic used in orthopaedy. J Biomed Mater Res 28 (1994) 619-624
    • (1994) J Biomed Mater Res , vol.28 , pp. 619-624
    • Cales, B.1    Stefani, Y.2    Lilley, E.3
  • 37
    • 1842783267 scopus 로고    scopus 로고
    • Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part II. Zirconia-based dental ceramics
    • Guazzato M., Albakry M., Ringer S.P., and Swain M.V. Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part II. Zirconia-based dental ceramics. Dent Mater 20 (2004) 449-456
    • (2004) Dent Mater , vol.20 , pp. 449-456
    • Guazzato, M.1    Albakry, M.2    Ringer, S.P.3    Swain, M.V.4
  • 38
    • 0142029958 scopus 로고    scopus 로고
    • Effects of acid hydrolysis and mechanical polishing on surface residual stresses of low-fusing dental ceramics
    • Alkhiary Y.M., Morgano S.M., and Giordano R.A. Effects of acid hydrolysis and mechanical polishing on surface residual stresses of low-fusing dental ceramics. J Prosthet Dent 90 (2003) 133-142
    • (2003) J Prosthet Dent , vol.90 , pp. 133-142
    • Alkhiary, Y.M.1    Morgano, S.M.2    Giordano, R.A.3
  • 39
    • 0037333013 scopus 로고    scopus 로고
    • Transformation-induced damping behaviour of Y-TZP zirconia ceramics
    • Roebben G., Basu B., Vleugels J., and Van der Biest O. Transformation-induced damping behaviour of Y-TZP zirconia ceramics. J Eur Ceram Soc 23 (2003) 481-489
    • (2003) J Eur Ceram Soc , vol.23 , pp. 481-489
    • Roebben, G.1    Basu, B.2    Vleugels, J.3    Van der Biest, O.4
  • 40
    • 0033814141 scopus 로고    scopus 로고
    • Exhaustive Soxhlet extraction for the complete removal of residual compounds to provide a nonleaching silicane elastomer
    • Gruber A.D., Widenhouse C.W., Mathes S., and Gruber R.P. Exhaustive Soxhlet extraction for the complete removal of residual compounds to provide a nonleaching silicane elastomer. J Biomed Mater Res 53 (2000) 445-448
    • (2000) J Biomed Mater Res , vol.53 , pp. 445-448
    • Gruber, A.D.1    Widenhouse, C.W.2    Mathes, S.3    Gruber, R.P.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.