메뉴 건너뛰기




Volumn 23, Issue 8, 2007, Pages 1018-1029

The biaxial flexural strength and fatigue property of Lava™ Y-TZP dental ceramic

Author keywords

Biaxial flexural strength; Dental ceramic; Fatigue; Hardness; Mechanical properties

Indexed keywords

ANALYSIS OF VARIANCE (ANOVA); BENDING STRENGTH; FATIGUE OF MATERIALS; HARDNESS; WEIBULL DISTRIBUTION; YTTRIA STABILIZED ZIRCONIA;

EID: 34250164925     PISSN: 01095641     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.dental.2006.09.003     Document Type: Article
Times cited : (144)

References (46)
  • 3
    • 33645309086 scopus 로고    scopus 로고
    • Survival rates of IPS empress 2 all-ceramic crowns and fixed partial dentures: results of a 5-year prospective clinical study
    • Marquardt P., and Strub J.R. Survival rates of IPS empress 2 all-ceramic crowns and fixed partial dentures: results of a 5-year prospective clinical study. Quintessence Int 37 (2006) 253-259
    • (2006) Quintessence Int , vol.37 , pp. 253-259
    • Marquardt, P.1    Strub, J.R.2
  • 4
    • 0032015941 scopus 로고    scopus 로고
    • In-Ceram fixed partial dentures: three-year clinical trial results
    • Sorensen J.A., Kang S.K., Torres T.J., and Knode H. In-Ceram fixed partial dentures: three-year clinical trial results. J Calif Dent Assoc 26 (1998) 207-214
    • (1998) J Calif Dent Assoc , vol.26 , pp. 207-214
    • Sorensen, J.A.1    Kang, S.K.2    Torres, T.J.3    Knode, H.4
  • 6
    • 0035351260 scopus 로고    scopus 로고
    • Fracture resistance of lithium disilicate-, alumina-, and zirconia- based three-unit fixed partial dentures: a laboratory study
    • Tinschert J., Natt G., Mautsch W., Augthun M., and Spiekermann H. Fracture resistance of lithium disilicate-, alumina-, and zirconia- based three-unit fixed partial dentures: a laboratory study. Int J Prosthodont 14 (2001) 231-238
    • (2001) Int J Prosthodont , vol.14 , pp. 231-238
    • Tinschert, J.1    Natt, G.2    Mautsch, W.3    Augthun, M.4    Spiekermann, H.5
  • 7
    • 1842783267 scopus 로고    scopus 로고
    • Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part II. Zirconia-based dental ceramics
    • Guazzato M., Albakry M., Ringer S.P., and Swain M.V. Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part II. Zirconia-based dental ceramics. Dent Mater 20 (2005) 449-456
    • (2005) Dent Mater , vol.20 , pp. 449-456
    • Guazzato, M.1    Albakry, M.2    Ringer, S.P.3    Swain, M.V.4
  • 8
    • 0034264517 scopus 로고    scopus 로고
    • Structural reliability of alumina-, feldspar-, leucite-, mica- and zirconia-based ceramics
    • Tinschert J., Zwez D., Marx R., and Anusavice K.J. Structural reliability of alumina-, feldspar-, leucite-, mica- and zirconia-based ceramics. J Dent 28 (2000) 529-535
    • (2000) J Dent , vol.28 , pp. 529-535
    • Tinschert, J.1    Zwez, D.2    Marx, R.3    Anusavice, K.J.4
  • 9
    • 84980204606 scopus 로고
    • Mechanisms of toughening partially stabilized zirconia (PSZ)
    • Porter D.L., and Heuer A.H. Mechanisms of toughening partially stabilized zirconia (PSZ). J Am Ceram Soc 60 (1977) 183-184
    • (1977) J Am Ceram Soc , vol.60 , pp. 183-184
    • Porter, D.L.1    Heuer, A.H.2
  • 10
    • 0032917811 scopus 로고    scopus 로고
    • Review zirconia as a ceramic biomaterial
    • Piconi C., and Maccauro G. Review zirconia as a ceramic biomaterial. Biomaterials 20 (1999) 1-25
    • (1999) Biomaterials , vol.20 , pp. 1-25
    • Piconi, C.1    Maccauro, G.2
  • 11
    • 3242748246 scopus 로고    scopus 로고
    • Dental ceramic:current thinking and trends
    • Kelly J.R. Dental ceramic:current thinking and trends. Dent Clin N Am 48 (2004) 513-530
    • (2004) Dent Clin N Am , vol.48 , pp. 513-530
    • Kelly, J.R.1
  • 12
    • 0033222358 scopus 로고    scopus 로고
    • The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic
    • Kosmac T., Oblak C., Jevnikar P., Funduk N., and Marion L. The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic. Dent Mater 15 (1999) 426-433
    • (1999) Dent Mater , vol.15 , pp. 426-433
    • Kosmac, T.1    Oblak, C.2    Jevnikar, P.3    Funduk, N.4    Marion, L.5
  • 14
    • 0035280162 scopus 로고    scopus 로고
    • Effect of amount of grinding on flexural strength of dental ceramics
    • Kitazaki H., Takahashi H., Hasegawa S., and Nishimura F. Effect of amount of grinding on flexural strength of dental ceramics. J Med Dent Sci 48 (2001) 7-13
    • (2001) J Med Dent Sci , vol.48 , pp. 7-13
    • Kitazaki, H.1    Takahashi, H.2    Hasegawa, S.3    Nishimura, F.4
  • 15
    • 0033350821 scopus 로고    scopus 로고
    • Low-temperature aging of Y-TZP ceramics
    • Chevalier J. Low-temperature aging of Y-TZP ceramics. J Am Ceram Soc 82 (1999) 2150-2154
    • (1999) J Am Ceram Soc , vol.82 , pp. 2150-2154
    • Chevalier, J.1
  • 16
    • 9944223028 scopus 로고    scopus 로고
    • The Lava system for CAD/CAM production of high-strength precition fixed prosthodontics
    • Sorensen J.A. The Lava system for CAD/CAM production of high-strength precition fixed prosthodontics. Quintessence Dent Technol 26 (2003) 57-67
    • (2003) Quintessence Dent Technol , vol.26 , pp. 57-67
    • Sorensen, J.A.1
  • 17
    • 0036636830 scopus 로고    scopus 로고
    • Mechanical properties of In-Ceram Alumina and In-Ceram Zirconia
    • Guazzato M., Albakry M., Swain M.V., and Ironside J. Mechanical properties of In-Ceram Alumina and In-Ceram Zirconia. Int J Prosthodont 15 (2002) 339-346
    • (2002) Int J Prosthodont , vol.15 , pp. 339-346
    • Guazzato, M.1    Albakry, M.2    Swain, M.V.3    Ironside, J.4
  • 18
    • 0042128629 scopus 로고    scopus 로고
    • Weibull analysis and flexural strength of hot-pressed core and veneered ceramic structure
    • Bona A.D., Anusavice K.J., and DeHoff P.H. Weibull analysis and flexural strength of hot-pressed core and veneered ceramic structure. Dent Mater 19 (2003) 662-669
    • (2003) Dent Mater , vol.19 , pp. 662-669
    • Bona, A.D.1    Anusavice, K.J.2    DeHoff, P.H.3
  • 19
    • 84980128235 scopus 로고
    • Precise tensile properties of ceramic bodies
    • Duckworth W.H. Precise tensile properties of ceramic bodies. J Am Ceram Soc 34 (1951) 1-9
    • (1951) J Am Ceram Soc , vol.34 , pp. 1-9
    • Duckworth, W.H.1
  • 20
    • 84987266075 scopus 로고
    • A statistical distribution function of wide applicability
    • Weibull W. A statistical distribution function of wide applicability. J Appl Mech 18 (1951) 293-297
    • (1951) J Appl Mech , vol.18 , pp. 293-297
    • Weibull, W.1
  • 22
    • 0032610772 scopus 로고    scopus 로고
    • Effects of cyclic loading on the strength of all-ceramic materials
    • Ohyama T., Yoshinari M., and Oda Y. Effects of cyclic loading on the strength of all-ceramic materials. Int J Prosthodont 12 (1999) 28-37
    • (1999) Int J Prosthodont , vol.12 , pp. 28-37
    • Ohyama, T.1    Yoshinari, M.2    Oda, Y.3
  • 23
    • 34250198706 scopus 로고    scopus 로고
    • ISO 6872. International standard for dental ceramic. 2nd ed.; 1995.
  • 24
    • 34250159535 scopus 로고    scopus 로고
    • BSI ENV 843-4. Advanced technical ceramics. Monolithic ceramics. Mechanical properties at room temperatures. Vickers, Knoop and Rockwell superficial hardness tests; 1995.
  • 25
    • 34250178134 scopus 로고    scopus 로고
    • Coelho AA. TOPAS-Academic.; 2004.
  • 26
    • 0000420004 scopus 로고
    • Crystal structure of tetragonal ZrO2
    • Teufer G. Crystal structure of tetragonal ZrO2. Acta Crystallogr 15 (1962) 1187
    • (1962) Acta Crystallogr , vol.15 , pp. 1187
    • Teufer, G.1
  • 29
    • 0036886280 scopus 로고    scopus 로고
    • Transformation-toughened zirconia for dental inlays, crowns and bridges:chemical stability and effect of low-temperature aging on flexural strength and surface structure
    • Ardlin B.I. Transformation-toughened zirconia for dental inlays, crowns and bridges:chemical stability and effect of low-temperature aging on flexural strength and surface structure. Dent Mater 18 (2002) 590-595
    • (2002) Dent Mater , vol.18 , pp. 590-595
    • Ardlin, B.I.1
  • 30
    • 0029258587 scopus 로고
    • Predicting lifetimes of materials and material structures
    • Ritter J.E. Predicting lifetimes of materials and material structures. Dent Mater 11 (1995) 142-146
    • (1995) Dent Mater , vol.11 , pp. 142-146
    • Ritter, J.E.1
  • 31
    • 0020932657 scopus 로고
    • Fracture statics of multiple flaw distribution
    • Plenum Press, New York p. 365-86
    • Johnson C.A. Fracture statics of multiple flaw distribution. In fracture mechanics of ceramics, vol. 5 (1983), Plenum Press, New York p. 365-86
    • (1983) In fracture mechanics of ceramics, vol. 5
    • Johnson, C.A.1
  • 32
    • 0016549634 scopus 로고
    • Phase relationships in the zirconia-yttria system
    • Scott H.G. Phase relationships in the zirconia-yttria system. J Mater Sci 10 (1975) 1527-1535
    • (1975) J Mater Sci , vol.10 , pp. 1527-1535
    • Scott, H.G.1
  • 33
    • 34250212220 scopus 로고    scopus 로고
    • The influence of surface modification techniques on the performance of a Y-TZP dental ceramic
    • Curtis A.R., Wright A.J., and Fleming G.J.P. The influence of surface modification techniques on the performance of a Y-TZP dental ceramic. J Dent (2005) 1-12
    • (2005) J Dent , pp. 1-12
    • Curtis, A.R.1    Wright, A.J.2    Fleming, G.J.P.3
  • 34
  • 35
    • 28944447516 scopus 로고    scopus 로고
    • Influence of surface finish and residual stresses on the aging sensitivity of biomedical grade zirconia
    • Deville S., Chevalier J., and Gremillard L. Influence of surface finish and residual stresses on the aging sensitivity of biomedical grade zirconia. Biomaterials 27 (2006) 2186-2192
    • (2006) Biomaterials , vol.27 , pp. 2186-2192
    • Deville, S.1    Chevalier, J.2    Gremillard, L.3
  • 36
    • 0028434170 scopus 로고
    • Long-term in vivo and in vitro aging of a zirconia ceramic in orthopaedy
    • Cales B., Stefani Y., and Lilley E. Long-term in vivo and in vitro aging of a zirconia ceramic in orthopaedy. J Biomed Mater Res 28 (1994) 619-624
    • (1994) J Biomed Mater Res , vol.28 , pp. 619-624
    • Cales, B.1    Stefani, Y.2    Lilley, E.3
  • 37
    • 4644309900 scopus 로고    scopus 로고
    • Fatigue and damage tolerance of Y-TZP ceramics in layered biomechanical systems
    • Zhang Y., Pajares A., and Lawn B.R. Fatigue and damage tolerance of Y-TZP ceramics in layered biomechanical systems. J Biomed Mater Res B Appl Biomater 71 (2004) 166-171
    • (2004) J Biomed Mater Res B Appl Biomater , vol.71 , pp. 166-171
    • Zhang, Y.1    Pajares, A.2    Lawn, B.R.3
  • 38
    • 0031083224 scopus 로고    scopus 로고
    • Relationships between static chemical and cyclic mechanical fatigue in a feldspathic porcelain
    • White S.N., Li Z.C., Yu Z., and Kipnis V. Relationships between static chemical and cyclic mechanical fatigue in a feldspathic porcelain. Dent Mater 13 (1997) 103-110
    • (1997) Dent Mater , vol.13 , pp. 103-110
    • White, S.N.1    Li, Z.C.2    Yu, Z.3    Kipnis, V.4
  • 39
    • 0038378501 scopus 로고    scopus 로고
    • Fracture toughness and hardness evaluation of three pressable all-ceramic dental materials
    • Albakry M., Guazzato M., and Swain M.V. Fracture toughness and hardness evaluation of three pressable all-ceramic dental materials. J Dent 31 (2003) 181-188
    • (2003) J Dent , vol.31 , pp. 181-188
    • Albakry, M.1    Guazzato, M.2    Swain, M.V.3
  • 40
    • 33846490999 scopus 로고    scopus 로고
    • Mechanical properties of dental materials
    • Anusavice K.J. (Ed), Saunders, Philadelphia, PA
    • Anusavice K.J. Mechanical properties of dental materials. In: Anusavice K.J. (Ed). Phillips' science of dental materials. 11th ed. (2003), Saunders, Philadelphia, PA 93
    • (2003) Phillips' science of dental materials. 11th ed. , pp. 93
    • Anusavice, K.J.1
  • 42
    • 3042833035 scopus 로고    scopus 로고
    • Maximal bite forces in healthy young adults are predicted by surface electromyography
    • Ferrario V.F., Sforza C., Zanotti G., and Tartaglia G.M. Maximal bite forces in healthy young adults are predicted by surface electromyography. J Dent 32 (2004) 451-457
    • (2004) J Dent , vol.32 , pp. 451-457
    • Ferrario, V.F.1    Sforza, C.2    Zanotti, G.3    Tartaglia, G.M.4
  • 43
    • 0037362701 scopus 로고    scopus 로고
    • Association between masticatory performance and maximal occlusal force in young men
    • Okiyama S., Ikebe K., and Nokubi T. Association between masticatory performance and maximal occlusal force in young men. J Oral Rehabil 30 (2003) 278-282
    • (2003) J Oral Rehabil , vol.30 , pp. 278-282
    • Okiyama, S.1    Ikebe, K.2    Nokubi, T.3
  • 45
    • 34250217876 scopus 로고    scopus 로고
    • Effect of mechanical cycling on the flexural strength of densely sintered ceramics
    • Itinoche K.M., Ozcan M., Bottino M.A., and Oyafuso D. Effect of mechanical cycling on the flexural strength of densely sintered ceramics. Dent Mater 21 (2006) 1-6
    • (2006) Dent Mater , vol.21 , pp. 1-6
    • Itinoche, K.M.1    Ozcan, M.2    Bottino, M.A.3    Oyafuso, D.4
  • 46
    • 16344387546 scopus 로고    scopus 로고
    • Fracture resistance of yttrium oxide partially stabilized zirconia all-ceramic bridges after veneering and mechanical fatigue testing
    • Sundh A., Molin M., and Sjogren G. Fracture resistance of yttrium oxide partially stabilized zirconia all-ceramic bridges after veneering and mechanical fatigue testing. Dent Mater 21 (2005) 476-482
    • (2005) Dent Mater , vol.21 , pp. 476-482
    • Sundh, A.1    Molin, M.2    Sjogren, G.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.