Volumn 33, Issue 2, 2006, Pages 117-124

Surface roughness of five different dental ceramic core materials after grinding and polishing

Author keywords

All ceramic crowns; Alumina; Dental ceramics; Dental polishing; Finishing; Lithium disilicate; Y TZP; Zirconia

Indexed keywords

ALLCERAM; ALUMINUM OXIDE; ALUMINUM SILICATE; DENZIR; IN CERAM ALUMINA; IN CERAM ZIRCONIA; IN-CERAM ALUMINA; IN-CERAM ZIRCONIA; IPS EMPRESS CERAMIC; IPS-EMPRESS CERAMIC; VITA MARK II;

EID: 33645356680     PISSN: 0305182X     EISSN: 13652842     Source Type: Journal    
DOI: 10.1111/j.1365-2842.2006.01546.x     Document Type: Article
Times cited : (61)

References (26)
  • 1
    • 0030125754 scopus 로고    scopus 로고
    • Microstructure of a high strength alumina glass composite
    • Hornberger H Marquis PM. Microstructure of a high strength alumina glass composite. J Mater Res. 1996 4 855 858.
    • (1996) J Mater Res. , vol.4 , pp. 855-858
    • Hornberger, H.1    Marquis, P.M.2
  • 3
    • 0035348103 scopus 로고    scopus 로고
    • Flexural strength of Cerec 2 machined and jointed InCeram-Alumina and InCeram-Zirconia bars
    • Apholt W Bindl A Lüthy H Mörmann WH. Flexural strength of Cerec 2 machined and jointed InCeram-Alumina and InCeram-Zirconia bars. Dent Mater. 2001 17 260 267.
    • (2001) Dent Mater. , vol.17 , pp. 260-267
    • Apholt, W.1    Bindl, A.2    Lüthy, H.3    Mörmann, W.H.4
  • 4
    • 0007285056 scopus 로고    scopus 로고
    • A comparison of the microstructure and properties of the IPS Empress 2 and the IPS Empress glass-ceramics
    • Höland W Schweiger M Frank M Rheinberger V. A comparison of the microstructure and properties of the IPS Empress 2 and the IPS Empress glass-ceramics. J Biomed Mater Res. 2000 53 297 303.
    • (2000) J Biomed Mater Res. , vol.53 , pp. 297-303
    • Höland, W.1    Schweiger, M.2    Frank, M.3    Rheinberger, V.4
  • 5
    • 0027546239 scopus 로고
    • A new all-ceramic crown. a dense-sintered, high-purity alumina coping with porcelain
    • Andersson M Odèn A. A new all-ceramic crown. A dense-sintered, high-purity alumina coping with porcelain. Acta Odontol Scand. 1993 51 59 64.
    • (1993) Acta Odontol Scand. , vol.51 , pp. 59-64
    • Andersson, M.1    Odèn, A.2
  • 6
    • 0033157337 scopus 로고    scopus 로고
    • The Decim system for the production of dental restorations
    • Sjölin R Sundh A Bergman M. The Decim system for the production of dental restorations. Int J Comput Dent. 1999 2 197 207.
    • (1999) Int J Comput Dent. , vol.2 , pp. 197-207
    • Sjölin, R.1    Sundh, A.2    Bergman, M.3
  • 7
    • 3242741859 scopus 로고    scopus 로고
    • A comparison of fracture strength of yttrium-oxide-partially-stabilized zirconia ceramic crowns with varying core thickness, shapes and veneer ceramics
    • Sundh A Sjögren G. A comparison of fracture strength of yttrium-oxide-partially-stabilized zirconia ceramic crowns with varying core thickness, shapes and veneer ceramics. J Oral Rehabil. 2004 31 682 688.
    • (2004) J Oral Rehabil. , vol.31 , pp. 682-688
    • Sundh, A.1    Sjögren, G.2
  • 8
    • 16344387546 scopus 로고    scopus 로고
    • Fracture resistance of yttrium oxide partially-stabilized zirconia all-ceramic bridges after veneering and mechanical fatigue testing
    • Sundh A Molin M Sjögren G. Fracture resistance of yttrium oxide partially-stabilized zirconia all-ceramic bridges after veneering and mechanical fatigue testing. Dent Mater. 2005 21 476 482.
    • (2005) Dent Mater. , vol.21 , pp. 476-482
    • Sundh, A.1    Molin, M.2    Sjögren, G.3
  • 9
    • 11844264547 scopus 로고    scopus 로고
    • Influence of surface and heat treatments on the flexural strength of Y-TZP dental ceramic
    • Guazzato M Quach L Albakry M Swain MV. Influence of surface and heat treatments on the flexural strength of Y-TZP dental ceramic. J Dent. 2005 33 9 18.
    • (2005) J Dent. , vol.33 , pp. 9-18
    • Guazzato, M.1    Quach, L.2    Albakry, M.3    Swain, M.V.4
  • 10
    • 0029334452 scopus 로고
    • Effect of surface finish on the flexural strength of feldspathic and aluminous dental ceramics
    • Giordano R Cima M Pober R. Effect of surface finish on the flexural strength of feldspathic and aluminous dental ceramics. Int J Prosthodont. 1995 8 311 319.
    • (1995) Int J Prosthodont. , vol.8 , pp. 311-319
    • Giordano, R.1    Cima, M.2    Pober, R.3
  • 12
    • 0029692286 scopus 로고    scopus 로고
    • Effects of grinding, polishing, and overglazing on the flexure strength of a high-leucite feldspathic porcelain
    • Williamson RT Kovarik RE Mitchell RJ. Effects of grinding, polishing, and overglazing on the flexure strength of a high-leucite feldspathic porcelain. Int J Prosthodont. 1996 9 30 37.
    • (1996) Int J Prosthodont. , vol.9 , pp. 30-37
    • Williamson, R.T.1    Kovarik, R.E.2    Mitchell, R.J.3
  • 13
    • 0018987284 scopus 로고
    • An evaluation of postadjustment polishing techniques for porcelain denture teeth
    • Schlissel ER Newitter DA Renner RR Gwinnett AJ. An evaluation of postadjustment polishing techniques for porcelain denture teeth. J Prosthet Dent. 1980 43 258 265.
    • (1980) J Prosthet Dent. , vol.43 , pp. 258-265
    • Schlissel, E.R.1    Newitter, D.A.2    Renner, R.R.3    Gwinnett, A.J.4
  • 14
    • 84985773484 scopus 로고
    • Comparison of two different methods of polishing porcelain
    • Bessing C Wiktorsson Å. Comparison of two different methods of polishing porcelain. Scand J Dent Res. 1983 91 482 487.
    • (1983) Scand J Dent Res. , vol.91 , pp. 482-487
    • Bessing, C.1    Wiktorsson, Å.2
  • 16
    • 0036514540 scopus 로고    scopus 로고
    • Finishing and polishing of a hybrid composite and a heat-pressed glass ceramic
    • Jung M. Finishing and polishing of a hybrid composite and a heat-pressed glass ceramic. Oper Dent. 2002 27 175 183.
    • (2002) Oper Dent. , vol.27 , pp. 175-183
    • Jung, M.1
  • 19
    • 0028394042 scopus 로고
    • Wear of CAD/CAM ceramic inlays: Restorations, opposing cuSPS, and luting cements
    • Krejci I Lutz F Reimer M. Wear of CAD/CAM ceramic inlays: restorations, opposing cuSPS, and luting cements. Quintessence Int. 1994 25 199 207.
    • (1994) Quintessence Int. , vol.25 , pp. 199-207
    • Krejci, I.1    Lutz, F.2    Reimer, M.3
  • 20
    • 1842841840 scopus 로고    scopus 로고
    • A 10-year prospective evaluation of CAD/CAM-manufactured (Cerec) ceramic inlays cemented with a chemically cured or a dual-cured resin composite
    • Sjögren G Molin M van Dijken JWV. A 10-year prospective evaluation of CAD/CAM-manufactured (Cerec) ceramic inlays cemented with a chemically cured or a dual-cured resin composite. Int J Prosthodont. 2004 17 241 246.
    • (2004) Int J Prosthodont. , vol.17 , pp. 241-246
    • Sjögren, G.1    Molin, M.2    Van Dijken, J.W.V.3
  • 21
  • 23
    • 0028368940 scopus 로고
    • Surface roughness of two polished ceramic materials
    • Scurria MS Powers JM. Surface roughness of two polished ceramic materials. J Prosthet Dent. 1994 71 174 177.
    • (1994) J Prosthet Dent. , vol.71 , pp. 174-177
    • Scurria, M.S.1    Powers, J.M.2
  • 24
    • 0029297806 scopus 로고
    • Surface roughness of opalescent porcelains after polishing
    • Ward MT Tate WH Powers JM. Surface roughness of opalescent porcelains after polishing. Oper Dent. 1995 20 106 110.
    • (1995) Oper Dent. , vol.20 , pp. 106-110
    • Ward, M.T.1    Tate, W.H.2    Powers, J.M.3
  • 26
    • 0026133066 scopus 로고
    • Abrasion of human enamel by different ceramics in vitro
    • Seghi RR Rosenstiel SF Bauer P. Abrasion of human enamel by different ceramics in vitro. J Dent Res. 1991 70 221 225.
    • (1991) J Dent Res. , vol.70 , pp. 221-225
    • Seghi, R.R.1    Rosenstiel, S.F.2    Bauer, P.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.