1
-
-
1642471947
-
Effect of sandblasting, grinding, polishing and glazing on the flexural strength of two pressable all-ceramic dental materials
-
Albakry, M., Guazzato, M. Swain, M.V. (2004) Effect of sandblasting, grinding, polishing and glazing on the flexural strength of two pressable all-ceramic dental materials. Journal of Dentistry 32 : 91 99.
-
(2004)
Journal of Dentistry
, vol.32
, pp. 91-99
-
-
Albakry, M.1
Guazzato, M.2
Swain, M.V.3
-
2
-
-
0023395756
-
Effect of incompatibility stress on the fit of metal-ceramic crowns
-
Anusavice, K.J. Carroll, J.E. (1987) Effect of incompatibility stress on the fit of metal-ceramic crowns. Journal of Dental Research 66 : 1341 1345.
-
(1987)
Journal of Dental Research
, vol.66
, pp. 1341-1345
-
-
Anusavice, K.J.1
Carroll, J.E.2
-
3
-
-
0018996246
-
Comparative evaluation of ceramic-metal bond tests using finite element stress analysis
-
Anusavice, K.J., Dehoff, P.H. Fairhurst, C.W. (1980) Comparative evaluation of ceramic-metal bond tests using finite element stress analysis. Journal of Dental Research 59 : 608 613.
-
(1980)
Journal of Dental Research
, vol.59
, pp. 608-613
-
-
Anusavice, K.J.1
Dehoff, P.H.2
Fairhurst, C.W.3
-
4
-
-
0024061029
-
Delayed crack development in porcelain due to incompatibility stress
-
Anusavice, K.J., Dehoff, P.H., Gray, A. Lee, R.B. (1988) Delayed crack development in porcelain due to incompatibility stress. Journal of Dental Research 67 : 1086 1091.
-
(1988)
Journal of Dental Research
, vol.67
, pp. 1086-1091
-
-
Anusavice, K.J.1
Dehoff, P.H.2
Gray, A.3
Lee, R.B.4
-
5
-
-
0024693929
-
Influence of tempering and contraction mismatch on crack development in ceramic surfaces
-
Anusavice, K.J., DeHoff, P.H., Hojjatie, B. Gray, A. (1989) Influence of tempering and contraction mismatch on crack development in ceramic surfaces. Journal of Dental Research 68 : 1182 1187.
-
(1989)
Journal of Dental Research
, vol.68
, pp. 1182-1187
-
-
Anusavice, K.J.1
Dehoff, P.H.2
Hojjatie, B.3
Gray, A.4
-
6
-
-
0020841308
-
Thermal shock resistance of porcelain discs
-
Anusavice, K.J., Dehoff, P.H., Twiggs, S.W. Lockwood, P.C. (1983) Thermal shock resistance of porcelain discs. Journal of Dental Research 62 : 1082 1085.
-
(1983)
Journal of Dental Research
, vol.62
, pp. 1082-1085
-
-
Anusavice, K.J.1
Dehoff, P.H.2
Twiggs, S.W.3
Lockwood, P.C.4
-
7
-
-
0026112382
-
Influence of initial flaw size on crack growth in air-tempered porcelain
-
Anusavice, K.J., Gray, A. Shen, C. (1991) Influence of initial flaw size on crack growth in air-tempered porcelain. Journal of Dental Research 70 : 131 136.
-
(1991)
Journal of Dental Research
, vol.70
, pp. 131-136
-
-
Anusavice, K.J.1
Gray, A.2
Shen, C.3
-
8
-
-
0024399223
-
Influence of framework design, contraction mismatch, and thermal history on porcelain checking in fixed partial dentures
-
Anusavice, K.J. Gray, A.E. (1989) Influence of framework design, contraction mismatch, and thermal history on porcelain checking in fixed partial dentures. Dental Materials 5 : 58 63.
-
(1989)
Dental Materials
, vol.5
, pp. 58-63
-
-
Anusavice, K.J.1
Gray, A.E.2
-
9
-
-
0022778429
-
Influence of metal thickness on stress distribution in metal-ceramic crowns
-
Anusavice, K.J., Hojjatie, B. Dehoff, P.H. (1986) Influence of metal thickness on stress distribution in metal-ceramic crowns. Journal of Dental Research 65 : 1173 1178.
-
(1986)
Journal of Dental Research
, vol.65
, pp. 1173-1178
-
-
Anusavice, K.J.1
Hojjatie, B.2
Dehoff, P.H.3
-
10
-
-
0030621975
-
Chemical durability of Dicor and lithia-based glass-ceramics
-
Anusavice, K.J. Zhang, N.Z. (1997) Chemical durability of Dicor and lithia-based glass-ceramics. Dental Materials 13 : 13 19.
-
(1997)
Dental Materials
, vol.13
, pp. 13-19
-
-
Anusavice, K.J.1
Zhang, N.Z.2
-
11
-
-
0032223645
-
Chemical durability of Dicor and fluorocanasite-based glass-ceramics
-
Anusavice, K.J. Zhang, N.Z. (1998) Chemical durability of Dicor and fluorocanasite-based glass-ceramics. Journal of Dental Research 77 : 1553 1559.
-
(1998)
Journal of Dental Research
, vol.77
, pp. 1553-1559
-
-
Anusavice, K.J.1
Zhang, N.Z.2
-
12
-
-
1842527538
-
Fracture strength of all-ceramic crowns luted using two bonding methods
-
Attia, A. Kern, M. (2004) Fracture strength of all-ceramic crowns luted using two bonding methods. Journal of Prosthetic Dentistry 91 : 247 252.
-
(2004)
Journal of Prosthetic Dentistry
, vol.91
, pp. 247-252
-
-
Attia, A.1
Kern, M.2
-
13
-
-
0025617576
-
Influence of test method on failure stress of brittle dental materials
-
Ban, S. Anusavice, K.J. (1990) Influence of test method on failure stress of brittle dental materials. Journal of Dental Research 69 : 1791 1799.
-
(1990)
Journal of Dental Research
, vol.69
, pp. 1791-1799
-
-
Ban, S.1
Anusavice, K.J.2
-
14
-
-
0026824726
-
Effect of loading conditions on bi-axial flexure strength of dental cements
-
Ban, S., Hasegawa, J. Anusavice, K.J. (1992) Effect of loading conditions on bi-axial flexure strength of dental cements. Dental Materials 8 : 100 104.
-
(1992)
Dental Materials
, vol.8
, pp. 100-104
-
-
Ban, S.1
Hasegawa, J.2
Anusavice, K.J.3
-
15
-
-
0033209858
-
Effects of surface finish and fatigue testing on the fracture strength of CAD-CAM and pressed-ceramic crowns
-
Chen, H.Y., Hickel, R., Setcos, J.C. Kunzelmann, K.H. (1999) Effects of surface finish and fatigue testing on the fracture strength of CAD-CAM and pressed-ceramic crowns. Journal of Prosthetic Dentistry 82 : 468 475.
-
(1999)
Journal of Prosthetic Dentistry
, vol.82
, pp. 468-475
-
-
Chen, H.Y.1
Hickel, R.2
Setcos, J.C.3
Kunzelmann, K.H.4
-
16
-
-
22544457618
-
Fate of vital pulps beneath a metal-ceramic crown or a bridge retainer
-
Cheung, G.S., Lai, S.C. Ng, R.P. (2005) Fate of vital pulps beneath a metal-ceramic crown or a bridge retainer. International Endodontics Journal 38 : 521 530.
-
(2005)
International Endodontics Journal
, vol.38
, pp. 521-530
-
-
Cheung, G.S.1
Lai, S.C.2
Ng, R.P.3
-
20
-
-
33645661532
-
A 20-year retrospective survival study of fixed partial dentures
-
De Backer, H., Van Maele, G., De Moor, N., Van den Berghe, L. De Boever, J. (2006) A 20-year retrospective survival study of fixed partial dentures. International Journal of Prosthodontics 19 : 143 153.
-
(2006)
International Journal of Prosthodontics
, vol.19
, pp. 143-153
-
-
De Backer, H.1
Van Maele, G.2
De Moor, N.3
Van Den Berghe, L.4
De Boever, J.5
-
21
-
-
4344684951
-
Clinical performance of a lithia disilicate-based core ceramic for three-unit posterior FPDs
-
Esquivel-Upshaw, J.F., Anusavice, K.J., Young, H., Jones, J. Gibbs, C. (2004) Clinical performance of a lithia disilicate-based core ceramic for three-unit posterior FPDs. International Journal of Prosthodontics 17 : 469 475.
-
(2004)
International Journal of Prosthodontics
, vol.17
, pp. 469-475
-
-
Esquivel-Upshaw, J.F.1
Anusavice, K.J.2
Young, H.3
Jones, J.4
Gibbs, C.5
-
22
-
-
0019037466
-
Thermal expansion of dental alloys and porcelains
-
Fairhurst, C.W., Anusavice, K.J., Hashinger, D.T., Ringle, R.D. Twiggs, S.W. (1980) Thermal expansion of dental alloys and porcelains. Journal of Biomedical Materials Research 14 : 435 446.
-
(1980)
Journal of Biomedical Materials Research
, vol.14
, pp. 435-446
-
-
Fairhurst, C.W.1
Anusavice, K.J.2
Hashinger, D.T.3
Ringle, R.D.4
Twiggs, S.W.5
-
23
-
-
0027639110
-
Dynamic fatigue of feldspathic porcelain
-
Fairhurst, C.W., Lockwood, P.E., Ringle, R.D. Twiggs, S.W. (1993) Dynamic fatigue of feldspathic porcelain. Dental Materials 9 : 269 273.
-
(1993)
Dental Materials
, vol.9
, pp. 269-273
-
-
Fairhurst, C.W.1
Lockwood, P.E.2
Ringle, R.D.3
Twiggs, S.W.4
-
24
-
-
0037364513
-
Lifetime prediction of all-ceramic bridges by computational methods
-
Fischer, H., Weber, M. Marx, R. (2003) Lifetime prediction of all-ceramic bridges by computational methods. Journal of Dental Research 82 : 238 242.
-
(2003)
Journal of Dental Research
, vol.82
, pp. 238-242
-
-
Fischer, H.1
Weber, M.2
Marx, R.3
-
26
-
-
0029258806
-
Perspectives on strength
-
Kelly, J.R. (1995) Perspectives on strength. Dental Materials 11 : 103 110.
-
(1995)
Dental Materials
, vol.11
, pp. 103-110
-
-
Kelly, J.R.1
-
27
-
-
0033146116
-
Clinically relevant approach to failure testing of all-ceramic restorations
-
Kelly, J.R. (1999) Clinically relevant approach to failure testing of all-ceramic restorations. Journal of Prosthetic Dentistry 81 : 652 661.
-
(1999)
Journal of Prosthetic Dentistry
, vol.81
, pp. 652-661
-
-
Kelly, J.R.1
-
29
-
-
0025492382
-
Fracture surface analysis of dental ceramics: Clinically failed restorations
-
Kelly, J.R., Giordano, R., Pober, R. Cima, M.J. (1990) Fracture surface analysis of dental ceramics: clinically failed restorations. International Journal of Prosthodontics 3 : 430 440.
-
(1990)
International Journal of Prosthodontics
, vol.3
, pp. 430-440
-
-
Kelly, J.R.1
Giordano, R.2
Pober, R.3
Cima, M.J.4
-
30
-
-
0029318343
-
Failure of all-ceramic fixed partial dentures in vitro and in vivo: Analysis and modeling
-
Kelly, J.R., Tesk, J.A. Sorensen, J.A. (1995) Failure of all-ceramic fixed partial dentures in vitro and in vivo: analysis and modeling. Journal of Dental Research 74 : 1253 1258.
-
(1995)
Journal of Dental Research
, vol.74
, pp. 1253-1258
-
-
Kelly, J.R.1
Tesk, J.A.2
Sorensen, J.A.3
-
31
-
-
0029297598
-
Marginal ditching and staining as a predictor of secondary caries around amalgam restorations: A clinical and microbiological study
-
Kidd, E.A., Joyston-Bechal, S. Beighton, D. (1995) Marginal ditching and staining as a predictor of secondary caries around amalgam restorations: a clinical and microbiological study. Journal of Dental Research 74 : 1206 1211.
-
(1995)
Journal of Dental Research
, vol.74
, pp. 1206-1211
-
-
Kidd, E.A.1
Joyston-Bechal, S.2
Beighton, D.3
-
33
-
-
0031203090
-
Longevity of fixed partial dentures
-
Libby, G., Arcuri, M.R., LaVelle, W.E. Hebl, L. (1997) Longevity of fixed partial dentures. Journal of Prosthetic Dentistry 78 : 127 131.
-
(1997)
Journal of Prosthetic Dentistry
, vol.78
, pp. 127-131
-
-
Libby, G.1
Arcuri, M.R.2
Lavelle, W.E.3
Hebl, L.4
-
34
-
-
0026856133
-
Fatigue life of porcelain repair systems
-
Llobell, A., Nicholls, J.I., Kois, J.C. Daly, C.H. (1992) Fatigue life of porcelain repair systems. International Journal of Prosthodontics 5 : 205 213.
-
(1992)
International Journal of Prosthodontics
, vol.5
, pp. 205-213
-
-
Llobell, A.1
Nicholls, J.I.2
Kois, J.C.3
Daly, C.H.4
-
35
-
-
0034327953
-
Prospective clinical 5-year study of ceramic-veneered titanium restorations with the Procera system
-
Lövgren, R., Andersson, B., Carlsson, G.E. Odman, P. (2000) Prospective clinical 5-year study of ceramic-veneered titanium restorations with the Procera system. Journal of Prosthetic Dentistry 84 : 514 521.
-
(2000)
Journal of Prosthetic Dentistry
, vol.84
, pp. 514-521
-
-
Lövgren, R.1
Andersson, B.2
Carlsson, G.E.3
Odman, P.4
-
36
-
-
0026115101
-
Quantitative X-ray diffraction determination of leucite thermal instability in dental porcelain
-
Mackert, J.R. Evans, A.L. (1991a) Quantitative X-ray diffraction determination of leucite thermal instability in dental porcelain. Journal of the American Ceramic Society 74 : 450 453.
-
(1991)
Journal of the American Ceramic Society
, vol.74
, pp. 450-453
-
-
MacKert, J.R.1
Evans, A.L.2
-
37
-
-
0026112383
-
Effect of cooling rate on leucite volume fraction in dental porcelains
-
Mackert, J.R. Jr. Evans, A.L. (1991b) Effect of cooling rate on leucite volume fraction in dental porcelains. Journal of Dental Research 70 : 137 139.
-
(1991)
Journal of Dental Research
, vol.70
, pp. 137-139
-
-
Mackert Jr., J.R.1
Evans, A.L.2
-
38
-
-
0030307204
-
Microcracks in dental porcelain and their behavior during multiple firing
-
Mackert, J.R. Jr. Williams, A.L. (1996) Microcracks in dental porcelain and their behavior during multiple firing. Journal of Dental Research 75 : 1484 1490.
-
(1996)
Journal of Dental Research
, vol.75
, pp. 1484-1490
-
-
Mackert Jr., J.R.1
Williams, A.L.2
-
39
-
-
33645309086
-
Survival rates of IPS empress 2 all-ceramic crowns and fixed partial dentures: Results of a 5-year prospective clinical study
-
Marquardt, P. Strub, J.R. (2006) Survival rates of IPS empress 2 all-ceramic crowns and fixed partial dentures: results of a 5-year prospective clinical study. Quintessence International 37 : 253 259.
-
(2006)
Quintessence International
, vol.37
, pp. 253-259
-
-
Marquardt, P.1
Strub, J.R.2
-
40
-
-
0034156886
-
Secondary caries: A literature review with case reports
-
Mjör, I.A. Toffenetti, F. (2000) Secondary caries: a literature review with case reports. Quintessence International 31 : 165 179.
-
(2000)
Quintessence International
, vol.31
, pp. 165-179
-
-
Mjör, I.A.1
Toffenetti, F.2
-
41
-
-
0022501121
-
Fatigue of dental ceramics in a simulated oral environment
-
Morena, R., Beaudreau, G.M., Lockwood, P.E., Evans, A.L. Fairhurst, C.W. (1986) Fatigue of dental ceramics in a simulated oral environment. Journal of Dental Research 65 : 993 997.
-
(1986)
Journal of Dental Research
, vol.65
, pp. 993-997
-
-
Morena, R.1
Beaudreau, G.M.2
Lockwood, P.E.3
Evans, A.L.4
Fairhurst, C.W.5
-
42
-
-
0028433110
-
Fatigue characteristics of a high-strength porcelain
-
Myers, M.L., Ergle, J.W., Fairhurst, C.W. Ringle, R.D. (1994a) Fatigue characteristics of a high-strength porcelain. International Journal of Prosthodontics 7 : 253 257.
-
(1994)
International Journal of Prosthodontics
, vol.7
, pp. 253-257
-
-
Myers, M.L.1
Ergle, J.W.2
Fairhurst, C.W.3
Ringle, R.D.4
-
43
-
-
0028541650
-
Fatigue failure parameters of IPS-Empress porcelain
-
Myers, M.L., Ergle, J.W., Fairhurst, C.W. Ringle, R.D. (1994b) Fatigue failure parameters of IPS-Empress porcelain. International Journal of Prosthodontics 7 : 549 553.
-
(1994)
International Journal of Prosthodontics
, vol.7
, pp. 549-553
-
-
Myers, M.L.1
Ergle, J.W.2
Fairhurst, C.W.3
Ringle, R.D.4
-
45
-
-
0036716828
-
Influence of connector design on fracture probability of ceramic fixed-partial dentures
-
Oh, W., Götzen, N. Anusavice, K.J. (2002) Influence of connector design on fracture probability of ceramic fixed-partial dentures. Journal of Dental Research 81 : 623 627.
-
(2002)
Journal of Dental Research
, vol.81
, pp. 623-627
-
-
Oh, W.1
Götzen, N.2
Anusavice, K.J.3
-
46
-
-
0036560045
-
Effect of connector design on the fracture resistance of all-ceramic fixed partial dentures
-
Oh, W.S. Anusavice, K.J. (2002) Effect of connector design on the fracture resistance of all-ceramic fixed partial dentures. Journal of Prosthetic Dentistry 87 : 536 542.
-
(2002)
Journal of Prosthetic Dentistry
, vol.87
, pp. 536-542
-
-
Oh, W.S.1
Anusavice, K.J.2
-
48
-
-
0037812257
-
A long-term retrospective and clinical follow-up study of In-Ceram alumina FPDs
-
Olsson, K.G., Furst, B., Andersson, B. Carlsson, G.E. (2003) A long-term retrospective and clinical follow-up study of In-Ceram alumina FPDs. International Journal of Prosthodontics 16 : 150 156.
-
(2003)
International Journal of Prosthodontics
, vol.16
, pp. 150-156
-
-
Olsson, K.G.1
Furst, B.2
Andersson, B.3
Carlsson, G.E.4
-
49
-
-
84868264331
-
-
The relation between gap size, microbial accumulation and the structural features of natural caries in extracted teeth with class I amalgam restorations. A stereo- and polarized light microscopic study. Thesis, University of Copenhagen.
-
Özer, L. (1997) The relation between gap size, microbial accumulation and the structural features of natural caries in extracted teeth with class I amalgam restorations. A stereo- and polarized light microscopic study. Thesis, University of Copenhagen.
-
(1997)
-
-
Özer, L.1
-
50
-
-
84868264267
-
The relation between gap size, microbial accumulation and the structural features of natural caries in extracted teeth with class i amalgam restorations: A stereo- and polarized microscopic study
-
Özer, L. (1998) The relation between gap size, microbial accumulation and the structural features of natural caries in extracted teeth with class I amalgam restorations: a stereo- and polarized microscopic study. Tandlægebladet 102 (NR6) : 318 319.
-
(1998)
Tandlægebladet
, vol.102
, Issue.6
, pp. 318-319
-
-
Özer, L.1
-
51
-
-
0346641397
-
What is known about caries in relation to restorations as a reason for replacement? A review
-
Özer, L. Thylstrup, A. (1995) What is known about caries in relation to restorations as a reason for replacement? A review. Advances in Dental Research 9 : 394 402.
-
(1995)
Advances in Dental Research
, vol.9
, pp. 394-402
-
-
Özer, L.1
Thylstrup, A.2
-
52
-
-
0033222301
-
The fatigue strength of the interface between Ag-Pd alloy and hydrothermal ceramic
-
Poljak-Guberina, R., Catovic, A., Jerolimov, V., Franz, M. Bergman, V. (1999) The fatigue strength of the interface between Ag-Pd alloy and hydrothermal ceramic. Dental Materials 15 : 417 420.
-
(1999)
Dental Materials
, vol.15
, pp. 417-420
-
-
Poljak-Guberina, R.1
Catovic, A.2
Jerolimov, V.3
Franz, M.4
Bergman, V.5
-
53
-
-
0032054204
-
Dynamic fatigue and degradation in solution of hydroxyapatite ceramics
-
Raynaud, S., Champion, E., Bernache-Assolant, D. Tetard, D. (1998) Dynamic fatigue and degradation in solution of hydroxyapatite ceramics. Journal of Materials Science: Materials in Medicine 9 : 221 227.
-
(1998)
Journal of Materials Science: Materials in Medicine
, vol.9
, pp. 221-227
-
-
Raynaud, S.1
Champion, E.2
Bernache-Assolant, D.3
Tetard, D.4
-
54
-
-
33746913496
-
Metal-ceramic failure in noble metal crowns: 7-year results of a prospective clinical trial in private practices
-
Reitemeier, B., Hansel, K., Kastner, C. Walter, M.H. (2006) Metal-ceramic failure in noble metal crowns: 7-year results of a prospective clinical trial in private practices. International Journal of Prosthodontics 19 : 397 399.
-
(2006)
International Journal of Prosthodontics
, vol.19
, pp. 397-399
-
-
Reitemeier, B.1
Hansel, K.2
Kastner, C.3
Walter, M.H.4
-
55
-
-
0032040119
-
Meta-analysis of fixed partial denture survival: Prostheses and abutments
-
Scurria, M.S., Bader, J.D. Shugars, D.A. (1998) Meta-analysis of fixed partial denture survival: prostheses and abutments. Journal of Prosthetic Dentistry 79 : 459 464.
-
(1998)
Journal of Prosthetic Dentistry
, vol.79
, pp. 459-464
-
-
Scurria, M.S.1
Bader, J.D.2
Shugars, D.A.3
-
56
-
-
84889106325
-
Stress and reliability analysis of a metal-ceramic dental crown
-
In. Pittsburgh, PA: NASA Lewis Research Center.
-
Sokolowski, T.M., Hojjatie, B., Nemeth, N.N. Anusavice, K.J. (1996a) Stress and reliability analysis of a metal-ceramic dental crown. In Proceedings of ANSYS Conference and Exposition, 1 18. Pittsburgh, PA : NASA Lewis Research Center.
-
(1996)
Proceedings of ANSYS Conference and Exposition
, pp. 1-18
-
-
Sokolowski, T.M.1
Hojjatie, B.2
Nemeth, N.N.3
Anusavice, K.J.4
-
57
-
-
34250758350
-
Stress and reliability analysis of a metal-ceramic dental crown
-
Sokolowski, T.M., Hojjatie, B., Nemeth, N.N. Anusavice, K.J. (1996b) Stress and reliability analysis of a metal-ceramic dental crown. NASA Technical Memorandum 107178 : 1 18.
-
(1996)
NASA Technical Memorandum
, Issue.107178
, pp. 1-18
-
-
Sokolowski, T.M.1
Hojjatie, B.2
Nemeth, N.N.3
Anusavice, K.J.4
-
59
-
-
12244286788
-
A systematic review of the survival and complication rates of fixed partial dentures (FPDs) after an observation period of at least 5 years
-
Tan, K., Pjetursson, B.E., Lang, N.P. Chan, E.S. (2004) A systematic review of the survival and complication rates of fixed partial dentures (FPDs) after an observation period of at least 5 years. Clinical Oral Implants Research 15 : 654 666.
-
(2004)
Clinical Oral Implants Research
, vol.15
, pp. 654-666
-
-
Tan, K.1
Pjetursson, B.E.2
Lang, N.P.3
Chan, E.S.4
-
60
-
-
0028709614
-
Fracture surface characterization of clinically failed all-ceramic crowns
-
Thompson, J.Y., Anusavice, K.J., Naman, A. Morris, H.F. (1994) Fracture surface characterization of clinically failed all-ceramic crowns. Journal of Dental Research 73 : 1824 1832.
-
(1994)
Journal of Dental Research
, vol.73
, pp. 1824-1832
-
-
Thompson, J.Y.1
Anusavice, K.J.2
Naman, A.3
Morris, H.F.4
-
61
-
-
0031619605
-
Influence of glass-ceramic thickness on Hertzian and bulk fracture mechanisms
-
Tsai, Y.L., Petsche, P.E., Anusavice, K.J. Yang, M.C. (1998) Influence of glass-ceramic thickness on Hertzian and bulk fracture mechanisms. International Journal of Prosthodontics 11 : 27 32.
-
(1998)
International Journal of Prosthodontics
, vol.11
, pp. 27-32
-
-
Tsai, Y.L.1
Petsche, P.E.2
Anusavice, K.J.3
Yang, M.C.4
-
62
-
-
0029331263
-
Cyclic fatigue of a model feldspathic porcelain
-
Twiggs, S.W., Fairhurst, C.W., Lockwood, P.E. Ringle, R.D. (1995) Cyclic fatigue of a model feldspathic porcelain. Dental Materials 11 : 273 276.
-
(1995)
Dental Materials
, vol.11
, pp. 273-276
-
-
Twiggs, S.W.1
Fairhurst, C.W.2
Lockwood, P.E.3
Ringle, R.D.4
-
64
-
-
0033070380
-
Six-year follow-up of titanium and high-gold porcelain-fused-to-metal fixed partial dentures
-
Walter, M., Reppel, P.D., Böning, K. Freesmeyer, W.B. (1999) Six-year follow-up of titanium and high-gold porcelain-fused-to-metal fixed partial dentures. Journal of Oral Rehabilitation 26 : 91 96.
-
(1999)
Journal of Oral Rehabilitation
, vol.26
, pp. 91-96
-
-
Walter, M.1
Reppel, P.D.2
Böning, K.3
Freesmeyer, W.B.4
-
65
-
-
0027639145
-
Mechanical fatigue of a feldspathic dental porcelain
-
White, S.N. (1993) Mechanical fatigue of a feldspathic dental porcelain. Dental Materials 9 : 260 264.
-
(1993)
Dental Materials
, vol.9
, pp. 260-264
-
-
White, S.N.1
-
66
-
-
0029692286
-
Effects of grinding, polishing, and overglazing on the flexure strength of a high-leucite feldspathic porcelain
-
Williamson, R.T., Kovarik, R.E. Mitchell, R.J. (1996) Effects of grinding, polishing, and overglazing on the flexure strength of a high-leucite feldspathic porcelain. International Journal of Prosthodontics 9 : 30 37.
-
(1996)
International Journal of Prosthodontics
, vol.9
, pp. 30-37
-
-
Williamson, R.T.1
Kovarik, R.E.2