메뉴 건너뛰기




Volumn 12, Issue 1, 1999, Pages 28-37

Effects of Cyclic Loading on the Strength of All-Ceramic Materials

Author keywords

[No Author keywords available]

Indexed keywords

ALUMINUM OXIDE; ALUMINUM SILICATE; IN CERAM; IN-CERAM; IPS EMPRESS CERAMIC; IPS-EMPRESS CERAMIC; LEUCITE;

EID: 0032610772     PISSN: 08932174     EISSN: None     Source Type: Journal    
DOI: None     Document Type: Article
Times cited : (53)

References (29)
  • 1
    • 0026145328 scopus 로고
    • Physiological aging of an all-ceramic restorative material
    • Drummond JL, Novickas D, Lenke JW. Physiological aging of an all-ceramic restorative material. Dent Mater 1991;7:133-137.
    • (1991) Dent Mater , vol.7 , pp. 133-137
    • Drummond, J.L.1    Novickas, D.2    Lenke, J.W.3
  • 7
    • 0027639145 scopus 로고
    • Mechanical fatigue of a feldspathic dental porcelain
    • White SN. Mechanical fatigue of a feldspathic dental porcelain. Dent Mater 1993;9:260-264.
    • (1993) Dent Mater , vol.9 , pp. 260-264
    • White, S.N.1
  • 8
    • 0029364035 scopus 로고
    • Cyclic mechanical fatigue of a feldspathic dental porcelain
    • White SN, Zhao XY, Zhaokun Y, Li ZC. Cyclic mechanical fatigue of a feldspathic dental porcelain. Int J Prosthodont 1995;8:413-420.
    • (1995) Int J Prosthodont , vol.8 , pp. 413-420
    • White, S.N.1    Zhao, X.Y.2    Zhaokun, Y.3    Li, Z.C.4
  • 10
    • 0026891764 scopus 로고
    • Tensile stress in glass-ceramic crowns: Effect of flaws and cement voids
    • Anusavice KJ, Hojjatie B. Tensile stress in glass-ceramic crowns: Effect of flaws and cement voids. Int J Prosthodont 1992; 5:351-358.
    • (1992) Int J Prosthodont , vol.5 , pp. 351-358
    • Anusavice, K.J.1    Hojjatie, B.2
  • 14
    • 0347344165 scopus 로고
    • Fracture mechanics of ceramics
    • Nishida T, Yasuda E (eds). Tokyo: Nikkan Kogyo Shimbun
    • Nishida T, Yasuda E. Fracture mechanics of ceramics. In: Nishida T, Yasuda E (eds). Mechanical Properties of Ceramics [in Japanese]. Tokyo: Nikkan Kogyo Shimbun, 1986:63-95.
    • (1986) Mechanical Properties of Ceramics [in Japanese] , pp. 63-95
    • Nishida, T.1    Yasuda, E.2
  • 15
    • 0025617576 scopus 로고
    • Influence of test method on failure stress of brittle dental materials
    • Ban S, Anusavice KJ. Influence of test method on failure stress of brittle dental materials. J Dent Res 1990;69:1791-1799.
    • (1990) J Dent Res , vol.69 , pp. 1791-1799
    • Ban, S.1    Anusavice, K.J.2
  • 16
    • 0028476223 scopus 로고
    • Fracture strength of all-ceramic crowns
    • Yoshinari M, Derand T. Fracture strength of all-ceramic crowns. Int J Prosthodont 1994;7:329-338.
    • (1994) Int J Prosthodont , vol.7 , pp. 329-338
    • Yoshinari, M.1    Derand, T.2
  • 17
    • 0022702131 scopus 로고
    • Fracture toughness of commercial dental porcelains
    • Morena R, Lockwood PE, Fairhurst CW. Fracture toughness of commercial dental porcelains. Dent Mater 1986;2:58-62.
    • (1986) Dent Mater , vol.2 , pp. 58-62
    • Morena, R.1    Lockwood, P.E.2    Fairhurst, C.W.3
  • 18
    • 0026173831 scopus 로고
    • Cyclic fatigue of ceramic materials: Influence of crack path and fatigue mechanisms
    • Horibe S, Hirahara R. Cyclic fatigue of ceramic materials: Influence of crack path and fatigue mechanisms. Acta Metall Mater 1991;39:1309-1317.
    • (1991) Acta Metall Mater , vol.39 , pp. 1309-1317
    • Horibe, S.1    Hirahara, R.2
  • 19
    • 0026190299 scopus 로고
    • Crack propagation behavior of sintered silicon nitride under cyclic loads
    • Kishimoto H, Ueno A, Kawamoto H. Crack propagation behavior of sintered silicon nitride under cyclic loads. JSME Int J 1991;34:361-366.
    • (1991) JSME Int J , vol.34 , pp. 361-366
    • Kishimoto, H.1    Ueno, A.2    Kawamoto, H.3
  • 20
    • 0025492382 scopus 로고
    • Fracture surface analysis of dental ceramics: Clinically failed restorations
    • Kelly JR, Giordano R, Pober R, Cima MJ. Fracture surface analysis of dental ceramics: Clinically failed restorations. Int J Prosthodont 1990;3:430-440.
    • (1990) Int J Prosthodont , vol.3 , pp. 430-440
    • Kelly, J.R.1    Giordano, R.2    Pober, R.3    Cima, M.J.4
  • 21
    • 0028709614 scopus 로고
    • Fracture surface characterization of clinically failed all-ceramic crowns
    • Thompson JY, Anusavice KJ, Naman A, Morris HF. Fracture surface characterization of clinically failed all-ceramic crowns. J Dent Res 1994;73:1824-1832.
    • (1994) J Dent Res , vol.73 , pp. 1824-1832
    • Thompson, J.Y.1    Anusavice, K.J.2    Naman, A.3    Morris, H.F.4
  • 22
    • 0026149549 scopus 로고
    • The all-porcelain, resin-bonded bridge
    • Kern M, Knode H, Strubb JR. The all-porcelain, resin-bonded bridge. Quintessence Int 1991;22:257-262.
    • (1991) Quintessence Int , vol.22 , pp. 257-262
    • Kern, M.1    Knode, H.2    Strubb, J.R.3
  • 23
    • 0027604308 scopus 로고
    • Survival rate of In-Ceram restorations
    • Pröbster L. Survival rate of In-Ceram restorations. Int J Prosthodont 1993;6:259-263.
    • (1993) Int J Prosthodont , vol.6 , pp. 259-263
    • Pröbster, L.1
  • 24
    • 0026209170 scopus 로고
    • Stiftkernaufbauten aus In-Ceram: Direkte und indirekte Methode
    • Kern M, Knode H. Stiftkernaufbauten aus In-Ceram: Direkte und indirekte Methode. Quintessenz Zahntech 1991;17:917-925.
    • (1991) Quintessenz Zahntech , vol.17 , pp. 917-925
    • Kern, M.1    Knode, H.2
  • 25
    • 0029436750 scopus 로고
    • Zirconia posts: A new all-ceramic concept for nonvital abutment teeth
    • Meyenberg KH, Luthy H, Schärer P. Zirconia posts: A new all-ceramic concept for nonvital abutment teeth. J Esthet Dent 1995;7:73-80.
    • (1995) J Esthet Dent , vol.7 , pp. 73-80
    • Meyenberg, K.H.1    Luthy, H.2    Schärer, P.3
  • 26
    • 0031129277 scopus 로고    scopus 로고
    • Clinical experience with Empress crowns
    • Fradeani M, Aquilano A. Clinical experience with Empress crowns. Int J Prosthodont 1997;10:241-247.
    • (1997) Int J Prosthodont , vol.10 , pp. 241-247
    • Fradeani, M.1    Aquilano, A.2
  • 28
    • 0030095844 scopus 로고    scopus 로고
    • Four year clinical study of glass-infiltrated, sintered alumina crowns
    • Pröbster L. Four year clinical study of glass-infiltrated, sintered alumina crowns. J Oral Rehabil 1996;23:147-151.
    • (1996) J Oral Rehabil , vol.23 , pp. 147-151
    • Pröbster, L.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.