0029678682
-
Ceramics in dentistry: Historical roots and current perspectives
-
Kelly JR, Nishimura I, Campbell SD. Ceramics in dentistry: historical roots and current perspectives. J Prosthet Dent 1996;75:18-32.
-
(1996)
J Prosthet Dent
, vol.75
, pp. 18-32
-
-
Kelly, J.R.1
Nishimura, I.2
Campbell, S.D.3
-
3
-
-
0030135524
-
Leucite crystallization during processing of a heat-pressed dental ceramic
-
Mackert JR Jr, Russell CM. Leucite crystallization during processing of a heat-pressed dental ceramic. Int J Prosthodont 1996;9:261-5.
-
(1996)
Int J Prosthodont
, vol.9
, pp. 261-265
-
-
Mackert Jr., J.R.1
Russell, C.M.2
-
4
-
-
0029318343
-
Failure of all-ceramic fixed partial dentures in vitro and in vivo: Analysis and modeling
-
Kelly JR, Tesk JA, Sorensen JA. Failure of all-ceramic fixed partial dentures in vitro and in vivo: analysis and modeling. J Dent Res 1995;74:1253-8.
-
(1995)
J Dent Res
, vol.74
, pp. 1253-1258
-
-
Kelly, J.R.1
Tesk, J.A.2
Sorensen, J.A.3
-
6
-
-
0032601521
-
A clinical investigation on three-unit fixed partial dentures fabricated with a lithium disilicate glass-ceramic
-
Sorensen JA, Cruz M, Mito WT, Raffeiner O, Meredith HR, Foser HP. A clinical investigation on three-unit fixed partial dentures fabricated with a lithium disilicate glass-ceramic. Pract Periodontics Aesthet Dent 1999;11:95-106.
-
(1999)
Pract Periodontics Aesthet Dent
, vol.11
, pp. 95-106
-
-
Sorensen, J.A.1
Cruz, M.2
Mito, W.T.3
Raffeiner, O.4
Meredith, H.R.5
Foser, H.P.6
-
7
-
-
0020430381
-
Interproximal periodontal disease - The embrasure as an etiologic factor
-
Nevins M. Interproximal periodontal disease - the embrasure as an etiologic factor. Int J Periodontics Restorative Dent 1982;2:8-27.
-
(1982)
Int J Periodontics Restorative Dent
, vol.2
, pp. 8-27
-
-
Nevins, M.1
-
8
-
-
0033289828
-
Comparing the perception of dentists and lay people to altered dental esthetics
-
Kokich VO Jr, Kiyak HA, Shapiro PA. Comparing the perception of dentists and lay people to altered dental esthetics. J Esthet Dent 1999;11:311-24.
-
(1999)
J Esthet Dent
, vol.11
, pp. 311-324
-
-
Kokich Jr., V.O.1
Kiyak, H.A.2
Shapiro, P.A.3
-
10
-
-
0025224747
-
Three-dimensional finite element analysis of glass-ceramic dental crowns
-
Hojjatie B, Anusavice KJ. Three-dimensional finite element analysis of glass-ceramic dental crowns. J Biomech 1990;23:1157-66.
-
(1990)
J Biomech
, vol.23
, pp. 1157-1166
-
-
Hojjatie, B.1
Anusavice, K.J.2
-
11
-
-
33645286840
-
All-ceramic resin-bonded bridges. A 3-dimensional finite-element analysis study
-
Pospiech P, Rammelsberg P, Goldhofer G, Gernet W. All-ceramic resin-bonded bridges. A 3-dimensional finite-element analysis study. Eur J Oral Sci 1996;104:390-5.
-
(1996)
Eur J Oral Sci
, vol.104
, pp. 390-395
-
-
Pospiech, P.1
Rammelsberg, P.2
Goldhofer, G.3
Gernet, W.4
-
14
-
-
0000357002
-
The phenomena of rupture and flow in solids
-
Griffith AA. The phenomena of rupture and flow in solids. Philos Trans R Soc Lond Series A 1920;221:163.
-
(1920)
Philos Trans R Soc Lond Series A
, vol.221
, pp. 163
-
-
Griffith, A.A.1
-
15
-
-
0013170606
-
Detection of strength-impairing flaws in glass
-
Ernsberger FM. Detection of strength-impairing flaws in glass. Proc Roy Soc Lond Series A 1960;257:213.
-
(1960)
Proc Roy Soc Lond Series A
, vol.257
, pp. 213
-
-
Ernsberger, F.M.1
-
16
-
-
0028709614
-
Fracture surface characterization of clinically failed all-ceramic crowns
-
Thompson JY, Anusavice KJ, Naman A, Morris HF. Fracture surface characterization of clinically failed all-ceramic crowns. J Dent Res 1994;73:1824-32.
-
(1994)
J Dent Res
, vol.73
, pp. 1824-1832
-
-
Thompson, J.Y.1
Anusavice, K.J.2
Naman, A.3
Morris, H.F.4
-
17
-
-
0035318605
-
Tooth preparations for complete crowns: An art form based on scientific principles
-
Goodacre CJ, Campagni WV, Aquilino SA. Tooth preparations for complete crowns: an art form based on scientific principles. J Prosthet Dent 2001;85:363-76.
-
(2001)
J Prosthet Dent
, vol.85
, pp. 363-376
-
-
Goodacre, C.J.1
Campagni, W.V.2
Aquilino, S.A.3
-
18
-
-
0029444234
-
In-Ceram failure behavior and core-veneer interface quality as influenced by residual infiltration glass
-
Carrier DD, Kelly JR. In-Ceram failure behavior and core-veneer interface quality as influenced by residual infiltration glass. J Prosthodont 1995;4:237-42.
-
(1995)
J Prosthodont
, vol.4
, pp. 237-242
-
-
Carrier, D.D.1
Kelly, J.R.2
-
19
-
-
0032608003
-
Survival of Dicor glass-ceramic dental restorations over 14 years: Part 1. Survival of Dicor complete coverage restorations and effect of internal surface acid etching, tooth position, gender, and age
-
Malament KA, Socransky SS. Survival of Dicor glass-ceramic dental restorations over 14 years: Part 1. Survival of Dicor complete coverage restorations and effect of internal surface acid etching, tooth position, gender, and age. J Prosthet Dent 1999;81:23-32.
-
(1999)
J Prosthet Dent
, vol.81
, pp. 23-32
-
-
Malament, K.A.1
Socransky, S.S.2
-
20
-
-
0033146045
-
Survival of Dicor glass-ceramic dental restorations over 14 years. Part II: Effect of thickness of Dicor material and design of tooth preparation
-
Malament KA, Socransky SS. Survival of Dicor glass-ceramic dental restorations over 14 years. Part II: effect of thickness of Dicor material and design of tooth preparation. J Prosthet Dent 1999;81:662-7.
-
(1999)
J Prosthet Dent
, vol.81
, pp. 662-667
-
-
Malament, K.A.1
Socransky, S.S.2
-
22
-
-
0033146116
-
Clinically relevant approach to failure testing of all-ceramic restorations
-
Kelly JR. Clinically relevant approach to failure testing of all-ceramic restorations. J Prosthet Dent 1999;8:652-61.
-
(1999)
J Prosthet Dent
, vol.8
, pp. 652-661
-
-
Kelly, J.R.1
-
24
-
-
0033088886
-
Maximising the fracture resistance of dentine-bonded all-ceramic crowns
-
Burke FJ. Maximising the fracture resistance of dentine-bonded all-ceramic crowns. J Dent 1999;27:169-73.
-
(1999)
J Dent
, vol.27
, pp. 169-173
-
-
Burke, F.J.1
-
25
-
-
0033129355
-
Mechanical properties of dental luting cements
-
Li ZC, White SN. Mechanical properties of dental luting cements. J Prosthet Dent 1999;81:597-609.
-
(1999)
J Prosthet Dent
, vol.81
, pp. 597-609
-
-
Li, Z.C.1
White, S.N.2
-
27
-
-
0034264517
-
Structural reliability of alumina-, feldspar-, leucite-, mica- and zirconia-based ceramics
-
Tinschert J, Zwez D, Marx R, Anusavice KJ. Structural reliability of alumina-, feldspar-, leucite-, mica- and zirconia-based ceramics. J Dent 2000;28:529-35.
-
(2000)
J Dent
, vol.28
, pp. 529-535
-
-
Tinschert, J.1
Zwez, D.2
Marx, R.3
Anusavice, K.J.4
-
28
-
-
0029294815
-
Relative flexural strength of six new ceramic materials
-
Seghi RR, Sorensen JA. Relative flexural strength of six new ceramic materials. Int J Prosthodont 1995;8:239-46.
-
(1995)
Int J Prosthodont
, vol.8
, pp. 239-246
-
-
Seghi, R.R.1
Sorensen, J.A.2
-
30
-
-
0027661848
-
Effect of acid etching on the flexural strength of a feldspathic porcelain and a castable glass ceramic
-
Yen TW, Blackman RB, Baez RJ. Effect of acid etching on the flexural strength of a feldspathic porcelain and a castable glass ceramic. J Prosthet Dent 1993;70:224-33.
-
(1993)
J Prosthet Dent
, vol.70
, pp. 224-233
-
-
Yen, T.W.1
Blackman, R.B.2
Baez, R.J.3
-
31
-
-
0028369111
-
Effect of surface etching on the flexure strength and fracture toughness of Dicor disks containing controlled flaws
-
Thompson JY, Anusavice KJ. Effect of surface etching on the flexure strength and fracture toughness of Dicor disks containing controlled flaws. J Dent Res 1994;73:505-10.
-
(1994)
J Dent Res
, vol.73
, pp. 505-510
-
-