Volumn 11, Issue 1, 1998, Pages 27-32

Influence of Glass-Ceramic Thickness on Hertzian and Bulk Fracture Mechanisms

Author keywords

[No Author keywords available]

Indexed keywords

DICOR CERAMIC; GLASS IONOMER; RESIN CEMENT;

EID: 0031619605     PISSN: 08932174     EISSN: None     Source Type: Journal    
DOI: None     Document Type: Article
Times cited : (46)

References (8)
  • 1
    • 0027655860 scopus 로고
    • The fracture resistance of all-ceramic crowns on supporting structures with different elastic moduli
    • Scherrer SS, de Rijk WG. The fracture resistance of all-ceramic crowns on supporting structures with different elastic moduli. Int J Prosthodont 1993;6:462-467.
    • (1993) Int J Prosthodont , vol.6 , pp. 462-467
    • Scherrer, S.S.1    De Rijk, W.G.2
  • 2
    • 0026891764 scopus 로고
    • Tensile stress in glass-ceramic crowns: Effect of flaws and cement voids
    • Anusavice KJ, Hojjatie B. Tensile stress in glass-ceramic crowns: Effect of flaws and cement voids. Int J Prosthodont 1992;5:351-358.
    • (1992) Int J Prosthodont , vol.5 , pp. 351-358
    • Anusavice, K.J.1    Hojjatie, B.2
  • 3
    • 0025492382 scopus 로고
    • Fracture-surface analysis of dental ceramics: Clinically failed restorations
    • Kelly JR, Giordano R, Pober R, Cima MJ. Fracture-surface analysis of dental ceramics: Clinically failed restorations. Int J Prosthodont 1990;3:430-440.
    • (1990) Int J Prosthodont , vol.3 , pp. 430-440
    • Kelly, J.R.1    Giordano, R.2    Pober, R.3    Cima, M.J.4
  • 4
    • 0028709614 scopus 로고
    • Fracture surface characterization of clinically failed all-ceramic crowns
    • Thompson JY, Anusavice KJ, Naman A, Morris HF. Fracture surface characterization of clinically failed all-ceramic crowns. J Dent Res 1994;73:1824-1832.
    • (1994) J Dent Res , vol.73 , pp. 1824-1832
    • Thompson, J.Y.1    Anusavice, K.J.2    Naman, A.3    Morris, H.F.4
  • 5
    • 0030154926 scopus 로고    scopus 로고
    • Contact damage as a failure mode during in vitro testing
    • Harvey CK, Kelly JR. Contact damage as a failure mode during in vitro testing. I Prosthodont 1996;5:95-100.
    • (1996) I Prosthodont , vol.5 , pp. 95-100
    • Harvey, C.K.1    Kelly, J.R.2
  • 6
    • 0026955496 scopus 로고
    • The effect of crown length on the fracture resistance of posterior porcelain and glass-ceramic systems
    • Scherrer SS, de Rijk WG. The effect of crown length on the fracture resistance of posterior porcelain and glass-ceramic systems. Int J Prosthodont 1992;5:550-557.
    • (1992) Int J Prosthodont , vol.5 , pp. 550-557
    • Scherrer, S.S.1    De Rijk, W.G.2
  • 7
    • 0142261200 scopus 로고
    • Clinical application of bonded Dicor crowns: A two-year report
    • Malament KA, Grossman DG. Clinical application of bonded Dicor crowns: A two-year report [abstract 1523]. J Dent Res 1990;69:299.
    • (1990) J Dent Res , vol.69 , pp. 299
    • Malament, K.A.1    Grossman, D.G.2
  • 8
    • 1842695586 scopus 로고
    • Photoelastic examination of bonded crown interfaces
    • Grossman DF. Photoelastic examination of bonded crown interfaces [abstract 719]. J Dent Res 1989;68:271.
    • (1989) J Dent Res , vol.68 , pp. 271
    • Grossman, D.F.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.