메뉴 건너뛰기




Volumn 69, Issue 1, 2010, Pages 48-53

Determination of resin bond strength to zirconia ceramic surface using different primers

Author keywords

Air abrasion; Bond strength; Silane; Surface treatment; Zirconia ceramic

Indexed keywords

FILTEK Z250; METHACRYLIC ACID DERIVATIVE; METHACRYLOYLOXYDECYL DIHYDROGEN PHOSPHATE; PANAVIA FLUORO; PANAVIA-FLUORO; RESIN; RESIN CEMENT; SILANE DERIVATIVE; TRIMETHOXYSILANE; ZIRCONIUM; ZIRCONIUM OXIDE;

EID: 78650207912     PISSN: 00016357     EISSN: 15023850     Source Type: Journal    
DOI: 10.3109/00016357.2010.517558     Document Type: Article
Times cited : (33)

References (30)
  • 1
    • 50349096922 scopus 로고    scopus 로고
    • The effect of hydrofluoric acid surface treatment and bond strength of a zirconia veneering ceramic
    • Chaiyabutr Y, McGowan S, Phillips KM, Kois JC, Giordano RA. The effect of hydrofluoric acid surface treatment and bond strength of a zirconia veneering ceramic. J Prosthet Dent 2008;100 194-202.
    • (2008) J Prosthet Dent , vol.100 , pp. 194-202
    • Chaiyabutr, Y.1    McGowan, S.2    Phillips, K.M.3    Kois, J.C.4    Giordano, R.A.5
  • 2
    • 42449099988 scopus 로고    scopus 로고
    • Effect of various surface conditioning methods on the adhesion of dual-cure resin cement with MDP functional monomer to zirconia after thermal aging
    • Ozcan M, Nijhuis H, Valandro LF. Effect of various surface conditioning methods on the adhesion of dual-cure resin cement with MDP functional monomer to zirconia after thermal aging. Dent Mater J 2008;27 99-104.
    • (2008) Dent Mater J , vol.27 , pp. 99-104
    • Ozcan, M.1    Nijhuis, H.2    Valandro, L.F.3
  • 3
    • 57749176443 scopus 로고    scopus 로고
    • An in vitro evaluation of the long-term resin bond to a new densely sintered high-purity zirconium-oxide ceramic surface
    • Phark JH, Duarte S Jr, Blatz M, Sadan A. An in vitro evaluation of the long-term resin bond to a new densely sintered high-purity zirconium-oxide ceramic surface. J Prosthet Dent 2009;101 29-38.
    • (2009) J Prosthet Dent , vol.101 , pp. 29-38
    • Phark, J.H.1    Duarte Jr., S.2    Blatz, M.3    Sadan, A.4
  • 5
    • 34250185998 scopus 로고    scopus 로고
    • Effect of loading method on the fracture mechanics of two layered all-ceramic restorative systems
    • Aboushelib MN, de Jager N, Kleverlaan CJ, Feilzer AJ. Effect of loading method on the fracture mechanics of two layered all-ceramic restorative systems. Dent Mater 2007;23 952-9.
    • (2007) Dent Mater , vol.23 , pp. 952-9
    • Aboushelib, M.N.1    De Jager, N.2    Kleverlaan, C.J.3    Feilzer, A.J.4
  • 6
    • 33744789998 scopus 로고    scopus 로고
    • Effect of zirconium-oxide ceramic surface treatments on the bond strength to adhesive resin
    • Atsu SS, Kilicarslan MA, Kucukesmen HC, Aka PS. Effect of zirconium-oxide ceramic surface treatments on the bond strength to adhesive resin. J Prosthet Dent 2006;95 430-6.
    • (2006) J Prosthet Dent , vol.95 , pp. 430-6
    • Atsu, S.S.1    Kilicarslan, M.A.2    Kucukesmen, H.C.3    Aka, P.S.4
  • 7
    • 0031598657 scopus 로고    scopus 로고
    • Bonding to zirconia ceramic: Adhesion methods and their durability
    • PII S01095641980000116
    • Kern M, Wegner SM. Bonding to zirconia ceramic adhesion methods and their durability. Dent Mater 1998;14 64-71. (Pubitemid 128419490)
    • (1998) Dental Materials , vol.14 , Issue.1 , pp. 64-71
    • Kern, M.1    Wegner, S.M.2
  • 8
    • 67649394413 scopus 로고    scopus 로고
    • Effect of surface treatment on the initial bond strength of different luting cements to zirconium oxide ceramic
    • Nothdurft FP, Motter PJ, Pospiech PR. Effect of surface treatment on the initial bond strength of different luting cements to zirconium oxide ceramic. Clin Oral Investig 2009;13 229-35.
    • (2009) Clin Oral Investig , vol.13 , pp. 229-35
    • Nothdurft, F.P.1    Motter, P.J.2    Pospiech, P.R.3
  • 10
    • 33847107611 scopus 로고    scopus 로고
    • Panavia F 2.0 bonding to contaminated zirconia ceramic after different cleaning procedures
    • DOI 10.1016/j.dental.2006.03.008, PII S0109564106000856
    • Quaas AC, Yang B, Kern M. Panavia F 2.0 bonding to contaminated zirconia ceramic after different cleaning procedures. Dent Mater 2007;23 506-12. (Pubitemid 46281292)
    • (2007) Dental Materials , vol.23 , Issue.4 , pp. 506-512
    • Quaas, A.C.1    Yang, B.2    Kern, M.3
  • 11
    • 46249132938 scopus 로고    scopus 로고
    • Effects of dental adhesive cement and surface treatment on bond strength and leakage of zirconium oxide ceramics
    • Tsukakoshi M, Shinya A, Gomi H, Lassila LV, Vallittu PK. Effects of dental adhesive cement and surface treatment on bond strength and leakage of zirconium oxide ceramics. Dent Mater J 2008;27 159-71.
    • (2008) Dent Mater J , vol.27 , pp. 159-71
    • Tsukakoshi, M.1    Shinya, A.2    Gomi, H.3    Lassila, L.V.4    Vallittu, P.K.5
  • 12
    • 27744579062 scopus 로고    scopus 로고
    • Bond strength of composite luting cement to zirconia ceramic surfaces
    • DOI 10.1016/j.dental.2005.02.005, PII S0109564105001181
    • Derand T, Molin M, Kvam K. Bond strength of composite luting cement to zirconia ceramic surfaces. Dent Mater 2005; 21 1158-62. (Pubitemid 41606212)
    • (2005) Dental Materials , vol.21 , Issue.12 , pp. 1158-1162
    • Derand, T.1    Molin, M.2    Kvam, K.3
  • 13
    • 70349481496 scopus 로고    scopus 로고
    • Surface conditioning influences zirconia ceramic bonding
    • Kern M, Barloi A, Yang B. Surface conditioning influences zirconia ceramic bonding. J Dent Res 2009;88 817-22.
    • (2009) J Dent Res , vol.88 , pp. 817-22
    • Kern, M.1    Barloi, A.2    Yang, B.3
  • 14
    • 30344433724 scopus 로고    scopus 로고
    • Effect of thermocycling on bond strength of luting cements to zirconia ceramic
    • DOI 10.1016/j.dental.2005.04.016, PII S0109564105001569
    • Luthy H, Loeffel O, Hammerle CH. Effect of thermocycling on bond strength of luting cements to zirconia ceramic. Dent Mater 2006;22 195-200. (Pubitemid 43061319)
    • (2006) Dental Materials , vol.22 , Issue.2 , pp. 195-200
    • Luthy, H.1    Loeffel, O.2    Hammerle, C.H.F.3
  • 15
    • 33845290307 scopus 로고    scopus 로고
    • Durability of the resin bond strength to zirconia ceramic after using different surface conditioning methods
    • DOI 10.1016/j.dental.2005.11.040, PII S0109564105003568
    • Wolfart M, Lehmann F, Wolfart S, Kern M. Durability of the resin bond strength to zirconia ceramic after using different surface conditioning methods. Dent Mater 2007;23 45-50. (Pubitemid 44880064)
    • (2007) Dental Materials , vol.23 , Issue.1 , pp. 45-50
    • Wolfart, M.1    Lehmann, F.2    Wolfart, S.3    Kern, M.4
  • 17
    • 0038644503 scopus 로고    scopus 로고
    • Resin-ceramic bonding a review of the literature
    • Blatz MB, Sadan A, Kern M.Resin-ceramic bonding a review of the literature. J Prosthet Dent 2003;89 268-74.
    • (2003) J Prosthet Dent , vol.89 , pp. 268-74
    • Blatz, M.B.1    Sadan, A.2    Kern, M.3
  • 18
    • 0035404137 scopus 로고    scopus 로고
    • The Effect of Surface Treatment on the Shear Bond Strength of Luting Cement to a Glass-Infiltrated Alumina Ceramic
    • Ozcan M, Alkumru HN, Gemalmaz D. The effect of surface treatment on the shear bond strength of luting cement to a glass-infiltrated alumina ceramic. Int J Prosthodont 2001;14 335-9. (Pubitemid 33692668)
    • (2001) International Journal of Prosthodontics , vol.14 , Issue.4 , pp. 335-339
    • Ozcan, M.1    Alkumru, H.N.2    Gemalmaz, D.3
  • 20
    • 0034202903 scopus 로고    scopus 로고
    • Effects of surface treatments on shear bond strengths between a resin cement and an alumina core
    • Madani M, Chu FC, McDonald AV, Smales RJ. Effects of surface treatments on shear bond strengths between a resin cement and an alumina core. J Prosthet Dent 2000;83 644-7.
    • (2000) J Prosthet Dent , vol.83 , pp. 644-7
    • Madani, M.1    Chu, F.C.2    McDonald, A.V.3    Smales, R.J.4
  • 21
    • 34447643377 scopus 로고    scopus 로고
    • The effect of five silane coupling agents on the bond strength of a luting cement to a silica-coated titanium
    • Matinlinna JP, Lassila LV, Vallittu PK. The effect of five silane coupling agents on the bond strength of a luting cement to a silica-coated titanium. Dent Mater 2007;23 1173-80.
    • (2007) Dent Mater , vol.23 , pp. 1173-80
    • Matinlinna, J.P.1    Lassila, L.V.2    Vallittu, P.K.3
  • 22
    • 33746653356 scopus 로고    scopus 로고
    • Evaluation of resin adhesion to zirconia ceramic using some organosilanes
    • DOI 10.1016/j.dental.2005.11.035, PII S0109564105002940
    • Matinlinna JP, Heikkinen T, Ozcan M, Lassila LV, Vallittu PK. Evaluation of resin adhesion to zirconia ceramic using some organosilanes. Dent Mater 2006;22 824-31. (Pubitemid 44148808)
    • (2006) Dental Materials , vol.22 , Issue.9 , pp. 824-831
    • Matinlinna, J.P.1    Heikkinen, T.2    Ozcan, M.3    Lassila, L.V.J.4    Vallittu, P.K.5
  • 23
    • 4644275580 scopus 로고    scopus 로고
    • The effect of a 3-methacryloxypropyltrimethoxysilane and vinyltriisopropoxysilane blend and tris(3-trimethoxysilyl-propyl)isocyanurate on the shear bond strength of composite resin to titanium metal
    • Matinlinna JP, Ozcan M, Lassila LV, Vallittu PK. The effect of a 3-methacryloxypropyltrimethoxysilane and vinyltriisopropoxysilane blend and tris(3-trimethoxysilyl-propyl)isocyanurate on the shear bond strength of composite resin to titanium metal. Dent Mater 2004;20 804-13.
    • (2004) Dent Mater , vol.20 , pp. 804-13
    • Matinlinna, J.P.1    Ozcan, M.2    Lassila, L.V.3    Vallittu, P.K.4
  • 26
    • 0034208413 scopus 로고    scopus 로고
    • Long-term resin bond strength to zirconia ceramic
    • Wegner SM, Kern M. Long-term resin bond strength to zirconia ceramic. J Adhes Dent 2000;2 139-47.
    • (2000) J Adhes Dent , vol.2 , pp. 139-47
    • Wegner, S.M.1    Kern, M.2
  • 27
    • 56849124974 scopus 로고    scopus 로고
    • Effect of surface treatments and aging in water on bond strength to zirconia
    • Lindgren J, Smeds J, Sjogren G. Effect of surface treatments and aging in water on bond strength to zirconia. Oper Dent 2008;33 675-81.
    • (2008) Oper Dent , vol.33 , pp. 675-81
    • Lindgren, J.1    Smeds, J.2    Sjogren, G.3
  • 28
    • 58149229394 scopus 로고    scopus 로고
    • Influence of surface treatments and resin cement selection on bonding to densely-sintered zirconium-oxide ceramic
    • de Oyague RC, Monticelli F, Toledano M, Osorio E, Ferrari M, Osorio R. Influence of surface treatments and resin cement selection on bonding to densely-sintered zirconium-oxide ceramic. Dent Mater 2009;25 172-9.
    • (2009) Dent Mater , vol.25 , pp. 172-9
    • De Oyague, R.C.1    Monticelli, F.2    Toledano, M.3    Osorio, E.4    Ferrari, M.5    Osorio, R.6
  • 29
    • 57449106111 scopus 로고    scopus 로고
    • Effect of testing methods on the bond strength of resin to zirconia-alumina ceramic microtensile versus shear test
    • Valandro LF, Ozcan M, Amaral R, Vanderlei A, Bottino MA. Effect of testing methods on the bond strength of resin to zirconia-alumina ceramic microtensile versus shear test. Dent Mater J 2008;27 849-55.
    • (2008) Dent Mater J , vol.27 , pp. 849-55
    • Valandro, L.F.1    Ozcan, M.2    Amaral, R.3    Vanderlei, A.4    Bottino, M.A.5
  • 30
    • 77950351197 scopus 로고    scopus 로고
    • In vitro evaluation of shear bond strength of veneering ceramics to zirconia
    • Ozkurt Z, Kazazoglu E, Unal A. In vitro evaluation of shear bond strength of veneering ceramics to zirconia. Dent Mater J 2010;29 138-46.
    • (2010) Dent Mater J , vol.29 , pp. 138-146
    • Ozkurt, Z.1    Kazazoglu, E.2    Unal, A.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.