메뉴 건너뛰기




Volumn 13, Issue 2, 2009, Pages 229-235

Effect of surface treatment on the initial bond strength of different luting cements to zirconium oxide ceramic

Author keywords

Bond strength; Ceramic; Luting cements; Surface treatment; Zirconia; Zirconium oxide

Indexed keywords

PHOSPHATE; RESIN CEMENT; ZIRCONIUM; ZIRCONIUM OXIDE;

EID: 67649394413     PISSN: 14326981     EISSN: 14363771     Source Type: Journal    
DOI: 10.1007/s00784-008-0222-8     Document Type: Article
Times cited : (71)

References (43)
  • 2
    • 33744789998 scopus 로고    scopus 로고
    • Effect of zirconium-oxide ceramic surface treatments on the bond strength to adhesive resin
    • Atsu SS, Kilicarslan MA, Kucukesmen HC, Aka PS (2006) Effect of zirconium-oxide ceramic surface treatments on the bond strength to adhesive resin. J Prosthet Dent 95:430-436
    • (2006) J Prosthet Dent , vol.95 , pp. 430-436
    • Atsu, S.S.1    Kilicarslan, M.A.2    Kucukesmen, H.C.3    Aka, P.S.4
  • 3
    • 34548648100 scopus 로고    scopus 로고
    • Influence of surface treatment and simulated aging on bond strengths of luting agents to zirconia
    • Blatz MB, Chiche G, Holst S, Sadan A (2007) Influence of surface treatment and simulated aging on bond strengths of luting agents to zirconia. Quintessence Int 38:745-753
    • (2007) Quintessence Int , vol.38 , pp. 745-753
    • Blatz, M.B.1    Chiche, G.2    Holst, S.3    Sadan, A.4
  • 4
    • 0036562709 scopus 로고    scopus 로고
    • Effect of ceramic surface treatment on tensile bond strength to a resin cement
    • Della Bona A, Anusavice KJ, Hood JA (2002) Effect of ceramic surface treatment on tensile bond strength to a resin cement. Int J Prosthodont 15:248-253
    • (2002) Int J Prosthodont , vol.15 , pp. 248-253
    • Della Bona, A.1    Anusavice, K.J.2    Hood, J.A.3
  • 5
    • 0028418727 scopus 로고
    • Shear bond strength of resin bonded ceramic after different try-in procedures
    • Della Bona A, Northeast SE (1994) Shear bond strength of resin bonded ceramic after different try-in procedures. J Dent 22:103-107
    • (1994) J Dent , vol.22 , pp. 103-107
    • Della Bona, A.1    Northeast, S.E.2
  • 6
    • 0029372422 scopus 로고
    • Shear vs. tensile bond strength of resin composite bonded to ceramic
    • Della Bona A, van Noort R (1995) Shear vs. tensile bond strength of resin composite bonded to ceramic. J Dent Res 74:1591-1596
    • (1995) J Dent Res , vol.74 , pp. 1591-1596
    • Della Bona, A.1    van Noort, R.2
  • 7
    • 0034157359 scopus 로고    scopus 로고
    • Bond strength of luting cements to zirconium oxide ceramics
    • Derand P, Derand T (2000) Bond strength of luting cements to zirconium oxide ceramics. Int J Prosthodont 13:131-135
    • (2000) Int J Prosthodont , vol.13 , pp. 131-135
    • Derand, P.1    Derand, T.2
  • 8
    • 0036725232 scopus 로고    scopus 로고
    • Retention of selected core materials to zirconia posts
    • Edelhoff D, Sorensen JA (2002) Retention of selected core materials to zirconia posts. Oper Dent 27:455-461
    • (2002) Oper Dent , vol.27 , pp. 455-461
    • Edelhoff, D.1    Sorensen, J.A.2
  • 9
    • 20444408006 scopus 로고    scopus 로고
    • In vitro retentive strength of zirconium oxide ceramic crowns using different luting agents
    • Ernst CP, Cohnen U, Stender E, Willershausen B (2005) In vitro retentive strength of zirconium oxide ceramic crowns using different luting agents. J Prosthet Dent 93:551-558
    • (2005) J Prosthet Dent , vol.93 , pp. 551-558
    • Ernst, C.P.1    Cohnen, U.2    Stender, E.3    Willershausen, B.4
  • 10
    • 2542639442 scopus 로고    scopus 로고
    • Experimental zirconia abutments for implant-supported single-tooth restorations in esthetically demanding regions: 4 year results of a prospective clinical study
    • Glauser R, Sailer I, Wohlwend A, Studer S, Schibli M, Scharer P (2004) Experimental zirconia abutments for implant-supported single-tooth restorations in esthetically demanding regions: 4 year results of a prospective clinical study. Int J Prosthodont 17:285-290
    • (2004) Int J Prosthodont , vol.17 , pp. 285-290
    • Glauser, R.1    Sailer, I.2    Wohlwend, A.3    Studer, S.4    Schibli, M.5    Scharer, P.6
  • 12
    • 0036517873 scopus 로고    scopus 로고
    • Investigation of the fracture resistance of three types of zirconia posts in all-ceramic post-and-core restorations
    • Jeong SM, Ludwig K, Kern M (2002) Investigation of the fracture resistance of three types of zirconia posts in all-ceramic post-and-core restorations. Int J Prosthodont 15:154-158
    • (2002) Int J Prosthodont , vol.15 , pp. 154-158
    • Jeong, S.M.1    Ludwig, K.2    Kern, M.3
  • 13
    • 0028435067 scopus 로고
    • Sandblasting and silica coating of a glass-infiltrated alumina ceramic: Volume loss, morphology, and changes in the surface composition
    • Kern M, Thompson VP (1994) Sandblasting and silica coating of a glass-infiltrated alumina ceramic: Volume loss, morphology, and changes in the surface composition. J Prosthet Dent 71:453-461
    • (1994) J Prosthet Dent , vol.71 , pp. 453-461
    • Kern, M.1    Thompson, V.P.2
  • 14
    • 0031598657 scopus 로고    scopus 로고
    • Bonding to zirconia ceramic: Adhesion methods and their durability
    • Kern M, Wegner SM (1998) Bonding to zirconia ceramic: Adhesion methods and their durability. Dent Mater 14:64-71
    • (1998) Dent Mater , vol.14 , pp. 64-71
    • Kern, M.1    Wegner, S.M.2
  • 15
    • 5344253044 scopus 로고    scopus 로고
    • In vitro fracture resistance of posterior metal-ceramic and all-ceramic inlay-retained resin-bonded fixed partial dentures
    • Kilicarslan MA, Kedici PS, Kucukesmen HC, Uludag BC (2004) In vitro fracture resistance of posterior metal-ceramic and all-ceramic inlay-retained resin-bonded fixed partial dentures. J Prosthet Dent 92:365-370
    • (2004) J Prosthet Dent , vol.92 , pp. 365-370
    • Kilicarslan, M.A.1    Kedici, P.S.2    Kucukesmen, H.C.3    Uludag, B.C.4
  • 16
    • 25844498493 scopus 로고    scopus 로고
    • The influence of ceramic surface treatments on the tensile bond strength of composite resin to all-ceramic coping materials
    • Kim BK, Bae HE, Shim JS, Lee KW (2005) The influence of ceramic surface treatments on the tensile bond strength of composite resin to all-ceramic coping materials. J Prosthet Dent 94:357-362
    • (2005) J Prosthet Dent , vol.94 , pp. 357-362
    • Kim, B.K.1    Bae, H.E.2    Shim, J.S.3    Lee, K.W.4
  • 17
    • 30344433724 scopus 로고    scopus 로고
    • Effect of thermocycling on bond strength of luting cements to zirconia ceramic
    • Luthy H, Loeffel O, Hammerle CH (2006) Effect of thermocycling on bond strength of luting cements to zirconia ceramic. Dent Mater 22:195-200
    • (2006) Dent Mater , vol.22 , pp. 195-200
    • Luthy, H.1    Loeffel, O.2    Hammerle, C.H.3
  • 19
    • 0024103132 scopus 로고
    • Tensile bond of resin cements to porcelain veneers
    • Nicholls JI (1988) Tensile bond of resin cements to porcelain veneers. J Prosthet Dent 60:443-447
    • (1988) J Prosthet Dent , vol.60 , pp. 443-447
    • Nicholls, J.I.1
  • 20
    • 67649402008 scopus 로고    scopus 로고
    • In vitro Untersuchungen zu vollkeramischen Stiftaufbauten aus Zirkonoxid
    • Nothdurft FP, Gernet W, Pospiech PR (2003) In vitro Untersuchungen zu vollkeramischen Stiftaufbauten aus Zirkonoxid. Dtsch Zahnärztl Z 58:451-456
    • (2003) Dtsch Zahnärztl Z , vol.58 , pp. 451-456
    • Nothdurft, F.P.1    Gernet, W.2    Pospiech, P.R.3
  • 21
    • 33645817180 scopus 로고    scopus 로고
    • Clinical evaluation of pulpless teeth restored with conventionally cemented zirconia posts: A pilot study
    • Nothdurft FP, Pospiech PR (2006) Clinical evaluation of pulpless teeth restored with conventionally cemented zirconia posts: A pilot study. J Prosthet Dent 95:311-314
    • (2006) J Prosthet Dent , vol.95 , pp. 311-314
    • Nothdurft, F.P.1    Pospiech, P.R.2
  • 22
    • 48549085496 scopus 로고    scopus 로고
    • Comparison of resin cement adhesion to Y-TZP ceramic following manufacturers' instructions of the cements only
    • Ozcan M, Kerkdijk S, Valandro LF (2008) Comparison of resin cement adhesion to Y-TZP ceramic following manufacturers' instructions of the cements only. Clin Oral Investig 12:279-282
    • (2008) Clin Oral Investig , vol.12 , pp. 279-282
    • Ozcan, M.1    Kerkdijk, S.2    Valandro, L.F.3
  • 23
    • 0141727597 scopus 로고    scopus 로고
    • Effect of surface conditioning methods on the bond strength of luting cement to ceramics
    • Ozcan M, Vallittu PK (2003) Effect of surface conditioning methods on the bond strength of luting cement to ceramics. Dent Mater 19:725-731
    • (2003) Dent Mater , vol.19 , pp. 725-731
    • Ozcan, M.1    Vallittu, P.K.2
  • 25
    • 5444257231 scopus 로고    scopus 로고
    • Clinical success of zirconium oxide posts with resin composite or glass-ceramic cores in endodontically treated teeth: A 4 year retrospective study
    • Paul SJ, Werder P (2004) Clinical success of zirconium oxide posts with resin composite or glass-ceramic cores in endodontically treated teeth: a 4 year retrospective study. Int J Prosthodont 17:524-528
    • (2004) Int J Prosthodont , vol.17 , pp. 524-528
    • Paul, S.J.1    Werder, P.2
  • 26
    • 19744367539 scopus 로고    scopus 로고
    • The shear bond strength between luting cements and zirconia ceramics after two pre-treatments
    • Piwowarczyk A, Lauer HC, Sorensen JA (2005) The shear bond strength between luting cements and zirconia ceramics after two pre-treatments. Oper Dent 30:382-388
    • (2005) Oper Dent , vol.30 , pp. 382-388
    • Piwowarczyk, A.1    Lauer, H.C.2    Sorensen, J.A.3
  • 27
    • 7444265287 scopus 로고    scopus 로고
    • In vitro fracture strength of teeth restored with different all-ceramic crown systems
    • Potiket N, Chiche G, Finger IM (2004) In vitro fracture strength of teeth restored with different all-ceramic crown systems. J Prosthet Dent 92:491-495
    • (2004) J Prosthet Dent , vol.92 , pp. 491-495
    • Potiket, N.1    Chiche, G.2    Finger, I.M.3
  • 28
    • 9944229063 scopus 로고    scopus 로고
    • Contemporary materials and technologies for all-ceramic fixed partial dentures: A review of the literature
    • Raigrodski AJ (2004) Contemporary materials and technologies for all-ceramic fixed partial dentures: A review of the literature. J Prosthet Dent 92:557-562
    • (2004) J Prosthet Dent , vol.92 , pp. 557-562
    • Raigrodski, A.J.1
  • 29
    • 0141828932 scopus 로고    scopus 로고
    • Bond strength of resin cement to dentin and to surface-treated posts of titanium alloy, glass fiber, and zirconia
    • Sahafi A, Peutzfeldt A, Asmussen E, Gotfredsen K (2003) Bond strength of resin cement to dentin and to surface-treated posts of titanium alloy, glass fiber, and zirconia. J Adhes Dent 5:153-162
    • (2003) J Adhes Dent , vol.5 , pp. 153-162
    • Sahafi, A.1    Peutzfeldt, A.2    Asmussen, E.3    Gotfredsen, K.4
  • 31
    • 0035351260 scopus 로고    scopus 로고
    • Fracture resistance of lithium disilicate-, alumina-, and zirconia-based three-unit fixed partial dentures: A laboratory study
    • Tinschert J, Natt G, Mautsch W, Augthun M, Spiekermann H (2001) Fracture resistance of lithium disilicate-, alumina-, and zirconia-based three-unit fixed partial dentures: A laboratory study. Int J Prosthodont 14:231-238
    • (2001) Int J Prosthodont , vol.14 , pp. 231-238
    • Tinschert, J.1    Natt, G.2    Mautsch, W.3    Augthun, M.4    Spiekermann, H.5
  • 32
    • 33845465853 scopus 로고    scopus 로고
    • Effect of surface condition of dental zirconia ceramic (Denzir) on bonding
    • Uo M, Sjogren G, Sundh A, Goto M, Watari F, Bergman M (2006) Effect of surface condition of dental zirconia ceramic (Denzir) on bonding. Dent Mater J 25:626-631
    • (2006) Dent Mater J , vol.25 , pp. 626-631
    • Uo, M.1    Sjogren, G.2    Sundh, A.3    Goto, M.4    Watari, F.5    Bergman, M.6
  • 33
    • 21444455550 scopus 로고    scopus 로고
    • All-ceramic fixed partial dentures. Studies on aluminum oxide- and zirconium dioxide-based ceramic systems
    • Vult von Steyern P (2005) All-ceramic fixed partial dentures. Studies on aluminum oxide- and zirconium dioxide-based ceramic systems. Swed Dent J Suppl:1-69
    • (2005) Swed Dent J , Issue.SUPPL. , pp. 1-69
    • Vult von Steyern, P.1
  • 34
    • 14844364021 scopus 로고    scopus 로고
    • All-ceramic fixed partial dentures designed according to the DC-Zirkon technique. A 2 year clinical study
    • Vult von Steyern P, Carlson P, Nilner K (2005) All-ceramic fixed partial dentures designed according to the DC-Zirkon technique. A 2 year clinical study. J Oral Rehabil 32:180-187
    • (2005) J Oral Rehabil , vol.32 , pp. 180-187
    • Vult von Steyern, P.1    Carlson, P.2    Nilner, K.3
  • 35
    • 33747062117 scopus 로고    scopus 로고
    • Fracture strength of two oxide ceramic crown systems after cyclic pre-loading and thermocycling
    • Vult von Steyern P, Ebbesson S, Holmgren J, Haag P, Nilner K (2006) Fracture strength of two oxide ceramic crown systems after cyclic pre-loading and thermocycling. J Oral Rehabil 33:682-689
    • (2006) J Oral Rehabil , vol.33 , pp. 682-689
    • Vult von Steyern, P.1    Ebbesson, S.2    Holmgren, J.3    Haag, P.4    Nilner, K.5
  • 36
    • 0036561939 scopus 로고    scopus 로고
    • Effect of different artificial aging conditions on ceramic-composite bond strength
    • Wegner SM, Gerdes W, Kern M (2002) Effect of different artificial aging conditions on ceramic-composite bond strength. Int J Prosthodont 15:267-272
    • (2002) Int J Prosthodont , vol.15 , pp. 267-272
    • Wegner, S.M.1    Gerdes, W.2    Kern, M.3
  • 37
    • 0034208413 scopus 로고    scopus 로고
    • Long-term resin bond strength to zirconia ceramic
    • Wegner SM, Kern M (2000) Long-term resin bond strength to zirconia ceramic. J Adhes Dent 2:139-147
    • (2000) J Adhes Dent , vol.2 , pp. 139-147
    • Wegner, S.M.1    Kern, M.2
  • 38
    • 29244474632 scopus 로고    scopus 로고
    • A new design for all-ceramic inlay-retained fixed partial dentures: A report of 2 cases
    • Wolfart S, Kern M (2006) A new design for all-ceramic inlay-retained fixed partial dentures: A report of 2 cases. Quintessence Int 37:27-33
    • (2006) Quintessence Int , vol.37 , pp. 27-33
    • Wolfart, S.1    Kern, M.2
  • 40
    • 0141923180 scopus 로고    scopus 로고
    • In vivo fracture resistance of implant-supported all-ceramic restorations
    • Yildirim M, Fischer H, Marx R, Edelhoff D (2003) In vivo fracture resistance of implant-supported all-ceramic restorations. J Prosthet Dent 90:325-331
    • (2003) J Prosthet Dent , vol.90 , pp. 325-331
    • Yildirim, M.1    Fischer, H.2    Marx, R.3    Edelhoff, D.4
  • 41
    • 0033146141 scopus 로고    scopus 로고
    • Adhesive primers for bonding cobalt-chromium alloy to resin
    • Yoshida K, Kamada K, Atsuta M (1999) Adhesive primers for bonding cobalt-chromium alloy to resin. J Oral Rehabil 26:475-478
    • (1999) J Oral Rehabil , vol.26 , pp. 475-478
    • Yoshida, K.1    Kamada, K.2    Atsuta, M.3
  • 42
    • 33645419309 scopus 로고    scopus 로고
    • Bonding of dual-cured resin cement to zirconia ceramic using phosphate acid ester monomer and zirconate coupler
    • Yoshida K, Tsuo Y, Atsuta M (2006) Bonding of dual-cured resin cement to zirconia ceramic using phosphate acid ester monomer and zirconate coupler. J Biomed Mater Res B Appl Biomater 77:28-33
    • (2006) J Biomed Mater Res B Appl Biomater , vol.77 , pp. 28-33
    • Yoshida, K.1    Tsuo, Y.2    Atsuta, M.3
  • 43
    • 7944226113 scopus 로고    scopus 로고
    • Zirconate coupling agent for bonding resin luting cement to pure zirconium
    • Yoshida K, Yamashita M, Atsuta M (2004) Zirconate coupling agent for bonding resin luting cement to pure zirconium. Am J Dent 17:249-252
    • (2004) Am J Dent , vol.17 , pp. 249-252
    • Yoshida, K.1    Yamashita, M.2    Atsuta, M.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.