메뉴 건너뛰기




Volumn 13, Issue 5, 2011, Pages 473-480

Evaluation of self-adhesive resin cement bond strength to yttria-stabilized zirconia ceramic (Y-TZP) using four surface treatments

Author keywords

EDS; Microshear bond strength; Resin cements; SEM; Surface treatment; Yttria stabilized zirconia ceramic

Indexed keywords

ALLOY PRIMER; ALUMINUM OXIDE; BIOMATERIAL; BISPHENOL A BIS(2 HYDROXYPROPYL) ETHER DIMETHACRYLATE; MACROGOL DERIVATIVE; METHACRYLIC ACID DERIVATIVE; METHACRYLOXYPROPYLTRIMETHOXYSILANE; METHACRYLOYLOXYDECYL DIHYDROGEN PHOSPHATE; POLYMETHACRYLIC ACID DERIVATIVE; RELY X UNICEM; RELYX ARC; RESIN CEMENT; ROCATEC; SILANE DERIVATIVE; THIOKETONE; TOOTH CEMENT; WATER; YTTRIA STABILIZED TETRAGONAL ZIRCONIA; YTTRIUM; ZIRCONIUM;

EID: 84856379765     PISSN: 14615185     EISSN: 17579988     Source Type: Journal    
DOI: 10.3290/j.jad.a19820     Document Type: Article
Times cited : (50)

References (36)
  • 1
  • 2
    • 41449099480 scopus 로고    scopus 로고
    • Effect of conditioning methods on the microtensile bond strength of phosphate monomer- based cement on zirconia ceramic in dry and aged conditions
    • Amaral R, Özcan M, Valandro LF, Balducci I, Bottino MA. Effect of conditioning methods on the microtensile bond strength of phosphate monomer- based cement on zirconia ceramic in dry and aged conditions. J Biomed Mater Res B Appl Biomater 2008; 85: 1-9.
    • (2008) J Biomed Mater Res B Appl Biomater , vol.85 , pp. 1-9
    • Amaral, R.1    Özcan, M.2    Valandro, L.F.3    Balducci, I.4    Bottino, M.A.5
  • 3
    • 77952423955 scopus 로고    scopus 로고
    • In vitro comparative bond strength of contemporary self-adhesive resin cements to zirconium oxide ceramic with and without air-particle abrasion
    • Blatz MB, Phark JH, Özer F, Mante FK, Saleh N, Bergler M, Sadan A. In vitro comparative bond strength of contemporary self-adhesive resin cements to zirconium oxide ceramic with and without air-particle abrasion. Clin Oral Investig 2010; 14: 187-192.
    • (2010) Clin Oral Investig , vol.14 , pp. 187-192
    • Blatz, M.B.1    Phark, J.H.2    Özer, F.3    Mante, F.K.4    Saleh, N.5    Bergler, M.6    Sadan, A.7
  • 4
    • 0038644503 scopus 로고    scopus 로고
    • Resin-ceramic bonding: A review of the literature
    • Blatz MB, Sadan A, Kern M. Resin-ceramic bonding: a review of the literature. J Prosthet Dent 2003; 89: 268-274.
    • (2003) J Prosthet Dent , vol.89 , pp. 268-274
    • Blatz, M.B.1    Sadan, A.2    Kern, M.3
  • 5
    • 0036593234 scopus 로고    scopus 로고
    • Long-term clinical success of all-ceramic posterior restorations
    • Blatz MB. Long-term clinical success of all-ceramic posterior restorations. Quintessence Int 2002; 33: 415-426.
    • (2002) Quintessence Int , vol.33 , pp. 415-426
    • Blatz, M.B.1
  • 6
    • 0036490134 scopus 로고    scopus 로고
    • Are adhesive technologies needed to support ceramics? An assessment of the current evidence
    • Burke FJ, Fleming GJ, Nathanson D, Marquis PM. Are adhesive technologies needed to support ceramics? An assessment of the current evidence. J Adhes Dent 2002; 4: 7-22.
    • (2002) J Adhes Dent , vol.4 , pp. 7-22
    • Burke, F.J.1    Fleming, G.J.2    Nathanson, D.3    Marquis, P.M.4
  • 9
    • 50349096922 scopus 로고    scopus 로고
    • The effect of hydrofluoric acid surface treatment and bond strength of a zirconia veneering ceramic
    • Chaiyabutr Y, McGowan S, Phillips KM, Kois JC, Giordano RA, The effect of hydrofluoric acid surface treatment and bond strength of a zirconia veneering ceramic. J Prosthet Dent 2008;100: 194-202.
    • (2008) J Prosthet Dent , vol.100 , pp. 194-202
    • Chaiyabutr, Y.1    McGowan, S.2    Phillips, K.M.3    Kois, J.C.4    Giordano, R.A.5
  • 10
    • 0024546336 scopus 로고
    • Mechanical properties and short-therm in-vivo evaluation of yttrium-oxide-partially-stabilized zirconia
    • Christel P, Meunier A, Heller M, Torre JP, Peille CN. Mechanical properties and short-therm in-vivo evaluation of yttrium-oxide-partially-stabilized zirconia. J Biomed Mater Res 1989; 23: 45-61.
    • (1989) J Biomed Mater Res , vol.23 , pp. 45-61
    • Christel, P.1    Meunier, A.2    Heller, M.3    Torre, J.P.4    Peille, C.N.5
  • 11
    • 58149229394 scopus 로고    scopus 로고
    • Influence of surface treatments and resin cement selection on bonding to densely-sintered zirconium-oxide ceramic
    • de Oyagüe RC, Monticelli F, Toledano M, Osorio E, Ferrari M, Osorio R. Influence of surface treatments and resin cement selection on bonding to densely-sintered zirconium-oxide ceramic. Dent Mater 2009; 25: 172-179.
    • (2009) Dent Mater , vol.25 , pp. 172-179
    • de Oyagüe, R.C.1    Monticelli, F.2    Toledano, M.3    Osorio, E.4    Ferrari, M.5    Osorio, R.6
  • 12
    • 0034157359 scopus 로고    scopus 로고
    • Bond strength of luting cements to zirconium oxide ceramics
    • Dérand P, Dérand T. Bond strength of luting cements to zirconium oxide ceramics. Int J Prosthodont 2000; 13: 131-135.
    • (2000) Int J Prosthodont , vol.13 , pp. 131-135
    • Dérand, P.1    Dérand, T.2
  • 13
    • 33748210816 scopus 로고    scopus 로고
    • Chemical analysis and bonding reaction of RelyX Unicem and Bifix composites - a comparative study
    • Gerth HU, Dammaschke T, Züchner H, Schäfer E. Chemical analysis and bonding reaction of RelyX Unicem and Bifix composites - a comparative study. Dent Mater 2006; 22: 934-941.
    • (2006) Dent Mater , vol.22 , pp. 934-941
    • Gerth, H.U.1    Dammaschke, T.2    Züchner, H.3    Schäfer, E.4
  • 14
    • 11844264547 scopus 로고    scopus 로고
    • Influence of surface and heat treatments on the flexural strength of YTZP dental ceramic
    • Guazzato M, Quach L, Albakry M, Swain MV. Influence of surface and heat treatments on the flexural strength of YTZP dental ceramic. J Dent 2005; 33: 9-18.
    • (2005) J Dent , vol.33 , pp. 9-18
    • Guazzato, M.1    Quach, L.2    Albakry, M.3    Swain, M.V.4
  • 15
    • 0031598657 scopus 로고    scopus 로고
    • Bonding to zirconia ceramic: Adhesion methods and their durability
    • Kern M, Wegner SM. Bonding to zirconia ceramic: adhesion methods and their durability. Dent Mater 1998; 14: 64-71.
    • (1998) Dent Mater , vol.14 , pp. 64-71
    • Kern, M.1    Wegner, S.M.2
  • 17
    • 70349492788 scopus 로고    scopus 로고
    • Durability of resin bonding to zirconia ceramic using different primers
    • Lehmann F, Kern M. Durability of resin bonding to zirconia ceramic using different primers. J Adhes Dent 2009; 11: 479-483.
    • (2009) J Adhes Dent , vol.11 , pp. 479-483
    • Lehmann, F.1    Kern, M.2
  • 19
    • 0033301391 scopus 로고    scopus 로고
    • Zirconia-TZP and alumina-advanced technologies for the manufacturing of single crowns
    • Luthardt RG, Sandkuhl O, Reitz B. Zirconia-TZP and alumina-advanced technologies for the manufacturing of single crowns. Eur J Prosthodont Restor Dent 1999; 7: 113-119.
    • (1999) Eur J Prosthodont Restor Dent , vol.7 , pp. 113-119
    • Luthardt, R.G.1    Sandkuhl, O.2    Reitz, B.3
  • 20
    • 46049106410 scopus 로고    scopus 로고
    • Microshear bond strength of resin bonding systems to machinable ceramic with different surface treatments
    • Meng X, Yoshida K, Atsuta M. Microshear bond strength of resin bonding systems to machinable ceramic with different surface treatments. J Adhes Dent 2008; 10: 189-196.
    • (2008) J Adhes Dent , vol.10 , pp. 189-196
    • Meng, X.1    Yoshida, K.2    Atsuta, M.3
  • 21
    • 67649394413 scopus 로고    scopus 로고
    • Effect of surface treatment on the initial bond strength of different luting cements to zirconium oxide ceramic
    • Nothdurft FP, Motter PJ, Pospiech PR. Effect of surface treatment on the initial bond strength of different luting cements to zirconium oxide ceramic. Clin Oral Investig 2009; 13: 229-235.
    • (2009) Clin Oral Investig , vol.13 , pp. 229-235
    • Nothdurft, F.P.1    Motter, P.J.2    Pospiech, P.R.3
  • 23
    • 57749176443 scopus 로고    scopus 로고
    • An in vitro evaluation of the longterm resin bond to a new densely sintered high-purity zirconium-oxide ceramic surface
    • Phark JH, Duarte S, Blatz M, Sadan A. An in vitro evaluation of the longterm resin bond to a new densely sintered high-purity zirconium-oxide ceramic surface. J Prosthet Dent 2009; 101: 29-38.
    • (2009) J Prosthet Dent , vol.101 , pp. 29-38
    • Phark, J.H.1    Duarte, S.2    Blatz, M.3    Sadan, A.4
  • 24
    • 0032917811 scopus 로고    scopus 로고
    • Zirconia as a ceramic biomaterial
    • Piconi C, Maccauro G. Zirconia as a ceramic biomaterial. Biomaterials 1999; 20: 1-25.
    • (1999) Biomaterials , vol.20 , pp. 1-25
    • Piconi, C.1    Maccauro, G.2
  • 25
    • 19744367539 scopus 로고    scopus 로고
    • The shear bond strength between luting cements and zirconia ceramics after two pre-treatments
    • Piwowarczyk A, Lauer HC, Sorensen JA. The shear bond strength between luting cements and zirconia ceramics after two pre-treatments. Oper Dent 2005; 30: 382-388.
    • (2005) Oper Dent , vol.30 , pp. 382-388
    • Piwowarczyk, A.1    Lauer, H.C.2    Sorensen, J.A.3
  • 27
    • 84995795451 scopus 로고    scopus 로고
    • (RelyX Unicem_TPP_EBU_1108_02_15.pdf); 3M ESPE internal data
    • RelyX Unicem - Technical Product Profile (RelyX Unicem_TPP_EBU_1108_02_15.pdf); 3M ESPE internal data.
    • RelyX Unicem - Technical Product Profile
  • 28
    • 46249121351 scopus 로고    scopus 로고
    • Mechanical properties of dental zirconia ceramics changed with sandblasting and heat treatment
    • Sato H, Yamada K, Pezzotti G, Nawa M, Ban S. Mechanical properties of dental zirconia ceramics changed with sandblasting and heat treatment. Dent Mater J 2008; 27: 408-414.
    • (2008) Dent Mater J , vol.27 , pp. 408-414
    • Sato, H.1    Yamada, K.2    Pezzotti, G.3    Nawa, M.4    Ban, S.5
  • 29
    • 0036635362 scopus 로고    scopus 로고
    • Micro-shear bond strength of dualcured resin cement to glass ceramics
    • Shimada Y, Yamaguchi S, Tagami J. Micro-shear bond strength of dualcured resin cement to glass ceramics. Dent Mater 2002; 18: 380-388.
    • (2002) Dent Mater , vol.18 , pp. 380-388
    • Shimada, Y.1    Yamaguchi, S.2    Tagami, J.3
  • 30
    • 33745743170 scopus 로고    scopus 로고
    • Bond strength of a resin cement to high-alumina and zirconia-reinforced ceramics: The effect of surface conditioning
    • Valandro LF, Özcan M, Bottino MC, Bottino MA, Scotti R, Bona AD. Bond strength of a resin cement to high-alumina and zirconia-reinforced ceramics: The effect of surface conditioning. J Adhes Dent 2006; 8: 175-181.
    • (2006) J Adhes Dent , vol.8 , pp. 175-181
    • Valandro, L.F.1    Özcan, M.2    Bottino, M.C.3    Bottino, M.A.4    Scotti, R.5    Bona, A.D.6
  • 31
    • 0039415468 scopus 로고    scopus 로고
    • Development of a new adhesive material and its properties
    • Gettleman L, Vrijhoef MMA, Uchiyama Y (eds), June 24
    • Wada T, Development of a new adhesive material and its properties. In: Gettleman L, Vrijhoef MMA, Uchiyama Y (eds). Proceedings of the international symposium on adhesive prosthodontics. June 24, 198: 9-18.
    • Proceedings of the international symposium on adhesive prosthodontics , vol.198 , pp. 9-18
    • Wada, T.1
  • 32
    • 40749115551 scopus 로고    scopus 로고
    • Strength influencing variables on CAD/CAM zirconia frameworks
    • Wang H, Aboushelib MN, Feilzer AJ. Strength influencing variables on CAD/CAM zirconia frameworks. Dent Mater 2008; 24: 633-638.
    • (2008) Dent Mater , vol.24 , pp. 633-638
    • Wang, H.1    Aboushelib, M.N.2    Feilzer, A.J.3
  • 33
    • 0034208413 scopus 로고    scopus 로고
    • Long-term resin bond strength to zirconia ceramic
    • Wegner SM, Kern M. Long-term resin bond strength to zirconia ceramic. J Adhes Dent 2000; 2: 139-147.
    • (2000) J Adhes Dent , vol.2 , pp. 139-147
    • Wegner, S.M.1    Kern, M.2
  • 34
    • 33845290307 scopus 로고    scopus 로고
    • Durability of the resin bond strength to zirconia ceramic after using different surface conditioning methods
    • Wolfart M, Lehmann F, Wolfart S, Kern M. Durability of the resin bond strength to zirconia ceramic after using different surface conditioning methods. Dent Mater 2007; 23: 45-50.
    • (2007) Dent Mater , vol.23 , pp. 45-50
    • Wolfart, M.1    Lehmann, F.2    Wolfart, S.3    Kern, M.4
  • 35
    • 71349083001 scopus 로고    scopus 로고
    • Influence of air-abrasion on zirconia ceramic bonding using an adhesive composite resin
    • Yang B, Barloi A, Kern M. Influence of air-abrasion on zirconia ceramic bonding using an adhesive composite resin. Dent Mater 2010; 26: 44-50.
    • (2010) Dent Mater , vol.26 , pp. 44-50
    • Yang, B.1    Barloi, A.2    Kern, M.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.