Volumn 25, Issue 1, 2009, Pages 121-128

High-strength CAD/CAM-fabricated veneering material sintered to zirconia copings - A new fabrication mode for all-ceramic restorations

Author keywords

CAD CAM; Chipping; High strength glass ceramic; Veneer cap; Zirconia

Indexed keywords

CERAMIC MATERIALS; CHROMIUM; COBALT; FABRICATION; FRACTURE; GLASS CERAMICS; REGRESSION ANALYSIS; RESTORATION; SETTLING TANKS; SINTERING; TRANSITION METALS; VENEERS;

EID: 57449084616     PISSN: 01095641     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.dental.2008.04.019     Document Type: Article
Times cited : (225)

References (38)
  • 1
    • 34250851683 scopus 로고    scopus 로고
    • Restoration of the upper dental arch using lava all-ceramic crown and bridgework
    • Barnfather K.D., and Brunton P.A. Restoration of the upper dental arch using lava all-ceramic crown and bridgework. Br Dent J 202 (2007) 731-735
    • (2007) Br Dent J , vol.202 , pp. 731-735
    • Barnfather, K.D.1    Brunton, P.A.2
  • 2
    • 5444219837 scopus 로고    scopus 로고
    • Precision of a CAD/CAM technique for the production of Zirconium dioxide copings
    • Coli P., and Karlsson S. Precision of a CAD/CAM technique for the production of Zirconium dioxide copings. Int J Prosthodont 17 (2004) 577-580
    • (2004) Int J Prosthodont , vol.17 , pp. 577-580
    • Coli, P.1    Karlsson, S.2
  • 3
    • 12444332060 scopus 로고    scopus 로고
    • Fracture behavior of lithia disilicate- and leucite-based ceramics
    • Della Bona A., Mecholsky Jr. J.J., and Anusavice K.J. Fracture behavior of lithia disilicate- and leucite-based ceramics. Dent Mater 20 (2004) 956-962
    • (2004) Dent Mater , vol.20 , pp. 956-962
    • Della Bona, A.1    Mecholsky Jr., J.J.2    Anusavice, K.J.3
  • 4
    • 33644686403 scopus 로고    scopus 로고
    • Guidelines for success with zirconia ceramics: the changing standards
    • Devaud V. Guidelines for success with zirconia ceramics: the changing standards. Pract Proced Aesthet Dent 17 (2005) 508-510
    • (2005) Pract Proced Aesthet Dent , vol.17 , pp. 508-510
    • Devaud, V.1
  • 5
    • 0036725232 scopus 로고    scopus 로고
    • Retention of selected core materials to zirconia posts
    • Edelhoff D., and Sorensen J.A. Retention of selected core materials to zirconia posts. Oper Dent 27 (2002) 455-461
    • (2002) Oper Dent , vol.27 , pp. 455-461
    • Edelhoff, D.1    Sorensen, J.A.2
  • 7
    • 27244457971 scopus 로고    scopus 로고
    • All-ceramic full-coverage restorations: concepts and guidelines for material selection
    • quiz 258
    • Raigrodski A.J. All-ceramic full-coverage restorations: concepts and guidelines for material selection. Pract Proced Aesthet Dent 17 (2005) 249-256 quiz 258
    • (2005) Pract Proced Aesthet Dent , vol.17 , pp. 249-256
    • Raigrodski, A.J.1
  • 8
    • 0031993427 scopus 로고    scopus 로고
    • IPS empress crown system: three-year clinical trial results
    • Sorensen J.A., Choi C., Fanuscu M.I., and Mito W.T. IPS empress crown system: three-year clinical trial results. J Calif Dent Assoc 26 (1998) 130-136
    • (1998) J Calif Dent Assoc , vol.26 , pp. 130-136
    • Sorensen, J.A.1    Choi, C.2    Fanuscu, M.I.3    Mito, W.T.4
  • 9
    • 0032015941 scopus 로고    scopus 로고
    • In-ceram fixed partial dentures: three-year clinical trial results
    • Sorensen J.A., Kang S.K., Torres T.J., and Knode H. In-ceram fixed partial dentures: three-year clinical trial results. J Calif Dent Assoc 26 (1998) 207-214
    • (1998) J Calif Dent Assoc , vol.26 , pp. 207-214
    • Sorensen, J.A.1    Kang, S.K.2    Torres, T.J.3    Knode, H.4
  • 12
    • 0035351260 scopus 로고    scopus 로고
    • Fracture resistance of lithium-disilicate-, alumina-, and zirconia-based three-unit fixed partial dentures: a laboratory study
    • Tinschert J., Natt G., Mautsch W., Augthun M., and Spiekermann H. Fracture resistance of lithium-disilicate-, alumina-, and zirconia-based three-unit fixed partial dentures: a laboratory study. Int J Prosthodont 14 (2001) 231-238
    • (2001) Int J Prosthodont , vol.14 , pp. 231-238
    • Tinschert, J.1    Natt, G.2    Mautsch, W.3    Augthun, M.4    Spiekermann, H.5
  • 13
    • 33747062117 scopus 로고    scopus 로고
    • Fracture strength of two oxide ceramic crown systems after cyclic pre-loading and thermocycling
    • Vult von Steyern P., Ebbesson S., Holmgren J., Haag P., and Nilner K. Fracture strength of two oxide ceramic crown systems after cyclic pre-loading and thermocycling. J Oral Rehabil 33 (2006) 682-689
    • (2006) J Oral Rehabil , vol.33 , pp. 682-689
    • Vult von Steyern, P.1    Ebbesson, S.2    Holmgren, J.3    Haag, P.4    Nilner, K.5
  • 14
    • 0034264517 scopus 로고    scopus 로고
    • Structural reliability of alumina-, feldspar-, leucite-, mica- and zirconia-based ceramics
    • Tinschert J., Zwez D., Marx R., and Anusavice K.J. Structural reliability of alumina-, feldspar-, leucite-, mica- and zirconia-based ceramics. J Dent 28 (2000) 529-535
    • (2000) J Dent , vol.28 , pp. 529-535
    • Tinschert, J.1    Zwez, D.2    Marx, R.3    Anusavice, K.J.4
  • 15
    • 25144511110 scopus 로고    scopus 로고
    • Microtensile bond strength of different components of core veneered all-ceramic restorations
    • Aboushelib M.N., de Jager N., Kleverlaan C.J., and Feilzer A.J. Microtensile bond strength of different components of core veneered all-ceramic restorations. Dent Mater 21 (2005) 984-991
    • (2005) Dent Mater , vol.21 , pp. 984-991
    • Aboushelib, M.N.1    de Jager, N.2    Kleverlaan, C.J.3    Feilzer, A.J.4
  • 16
    • 33746623731 scopus 로고    scopus 로고
    • Microtensile bond strength of different components of core veneered all-ceramic restorations. Part II. zirconia veneering ceramics
    • Aboushelib M.N., Kleverlaan C.J., and Feilzer A.J. Microtensile bond strength of different components of core veneered all-ceramic restorations. Part II. zirconia veneering ceramics. Dent Mater 22 (2006) 857-863
    • (2006) Dent Mater , vol.22 , pp. 857-863
    • Aboushelib, M.N.1    Kleverlaan, C.J.2    Feilzer, A.J.3
  • 17
    • 33745810915 scopus 로고    scopus 로고
    • All-ceramic 2-5-unit implant-supported reconstructions. A randomized, prospective clinical trial
    • Larsson C., Vult von Steyern P., Sunzel B., and Nilner K. All-ceramic 2-5-unit implant-supported reconstructions. A randomized, prospective clinical trial. Swed Dent J 30 (2006) 45-53
    • (2006) Swed Dent J , vol.30 , pp. 45-53
    • Larsson, C.1    Vult von Steyern, P.2    Sunzel, B.3    Nilner, K.4
  • 18
    • 33749183091 scopus 로고    scopus 로고
    • Prospective clinical study of zirconia posterior fixed partial dentures: 3-year follow-up
    • Sailer I., Feher A., Filser F., Luthy H., Gauckler L.J., Scharer P., et al. Prospective clinical study of zirconia posterior fixed partial dentures: 3-year follow-up. Quintessence Int 37 (2006) 685-693
    • (2006) Quintessence Int , vol.37 , pp. 685-693
    • Sailer, I.1    Feher, A.2    Filser, F.3    Luthy, H.4    Gauckler, L.J.5    Scharer, P.6
  • 19
    • 14844364021 scopus 로고    scopus 로고
    • All-ceramic fixed partial dentures designed according to the DC-Zirkon technique. A 2-year clinical study
    • Vult von Steyern P., Carlson P., and Nilner K. All-ceramic fixed partial dentures designed according to the DC-Zirkon technique. A 2-year clinical study. J Oral Rehabil 32 (2005) 180-187
    • (2005) J Oral Rehabil , vol.32 , pp. 180-187
    • Vult von Steyern, P.1    Carlson, P.2    Nilner, K.3
  • 20
    • 0023967360 scopus 로고
    • Causes of failure following oral rehabilitation: biological versus technical factors
    • Strub J.R., Stiffler S., and Scharer P. Causes of failure following oral rehabilitation: biological versus technical factors. Quintessence Int 19 (1988) 215-222
    • (1988) Quintessence Int , vol.19 , pp. 215-222
    • Strub, J.R.1    Stiffler, S.2    Scharer, P.3
  • 21
    • 29144507753 scopus 로고    scopus 로고
    • Strength and fracture pattern of monolithic CAD/CAM-generated posterior crowns
    • Bindl A., Luthy H., and Mormann W.H. Strength and fracture pattern of monolithic CAD/CAM-generated posterior crowns. Dent Mater 22 (2006) 29-36
    • (2006) Dent Mater , vol.22 , pp. 29-36
    • Bindl, A.1    Luthy, H.2    Mormann, W.H.3
  • 22
    • 33745078246 scopus 로고    scopus 로고
    • Thin-wall ceramic CAD/CAM crown copings: strength and fracture pattern
    • Bindl A., Luthy H., and Mormann W.H. Thin-wall ceramic CAD/CAM crown copings: strength and fracture pattern. J Oral Rehabil 33 (2006) 520-528
    • (2006) J Oral Rehabil , vol.33 , pp. 520-528
    • Bindl, A.1    Luthy, H.2    Mormann, W.H.3
  • 23
    • 2342652157 scopus 로고    scopus 로고
    • Survival rate of mono-ceramic and ceramic-core CAD/CAM-generated anterior crowns over 2-5 years
    • Bindl A., and Mormann W.H. Survival rate of mono-ceramic and ceramic-core CAD/CAM-generated anterior crowns over 2-5 years. Eur J Oral Sci 112 (2004) 197-204
    • (2004) Eur J Oral Sci , vol.112 , pp. 197-204
    • Bindl, A.1    Mormann, W.H.2
  • 25
    • 33746383047 scopus 로고    scopus 로고
    • Marginal accuracy of titanium copings fabricated by casting and CAD/CAM techniques
    • Witkowski S., Komine F., and Gerds T. Marginal accuracy of titanium copings fabricated by casting and CAD/CAM techniques. J Prosthet Dent 96 (2006) 47-52
    • (2006) J Prosthet Dent , vol.96 , pp. 47-52
    • Witkowski, S.1    Komine, F.2    Gerds, T.3
  • 26
    • 2342478568 scopus 로고    scopus 로고
    • Crowns cemented on crown preparations lacking geometric resistance form. Part II: effect of cement
    • Proussaefs P. Crowns cemented on crown preparations lacking geometric resistance form. Part II: effect of cement. J Prosthodont 13 (2004) 36-41
    • (2004) J Prosthodont , vol.13 , pp. 36-41
    • Proussaefs, P.1
  • 27
    • 0028511896 scopus 로고
    • In vitro fracture behavior of ceramic and metal-ceramic restorations
    • Smith T.B., Kelly J.R., and Tesk J.A. In vitro fracture behavior of ceramic and metal-ceramic restorations. J Prosthodont 3 (1994) 138-144
    • (1994) J Prosthodont , vol.3 , pp. 138-144
    • Smith, T.B.1    Kelly, J.R.2    Tesk, J.A.3
  • 28
    • 29144487947 scopus 로고    scopus 로고
    • Load-to-fracture value of different all-ceramic crown systems
    • Snyder M.D., and Hogg K.D. Load-to-fracture value of different all-ceramic crown systems. J Contemp Dent Pract 6 (2005) 54-63
    • (2005) J Contemp Dent Pract , vol.6 , pp. 54-63
    • Snyder, M.D.1    Hogg, K.D.2
  • 29
    • 16344387546 scopus 로고    scopus 로고
    • Fracture resistance of yttrium oxide partially-stabilized zirconia all-ceramic bridges after veneering and mechanical fatigue testing
    • Sundh A., Molin M., and Sjogren G. Fracture resistance of yttrium oxide partially-stabilized zirconia all-ceramic bridges after veneering and mechanical fatigue testing. Dent Mater 21 (2005) 476-482
    • (2005) Dent Mater , vol.21 , pp. 476-482
    • Sundh, A.1    Molin, M.2    Sjogren, G.3
  • 30
    • 0027655860 scopus 로고
    • The fracture resistance of all-ceramic crowns on supporting structures with different elastic moduli
    • Scherrer S.S., and de Rijk W.G. The fracture resistance of all-ceramic crowns on supporting structures with different elastic moduli. Int J Prosthodont 6 (1993) 462-467
    • (1993) Int J Prosthodont , vol.6 , pp. 462-467
    • Scherrer, S.S.1    de Rijk, W.G.2
  • 31
    • 0034280714 scopus 로고    scopus 로고
    • In vitro fracture force and marginal adaptation of ceramic crowns fixed on natural and artificial teeth
    • Rosentritt M., Plein T., Kolbeck C., Behr M., and Handel G. In vitro fracture force and marginal adaptation of ceramic crowns fixed on natural and artificial teeth. Int J Prosthodont 13 (2000) 387-391
    • (2000) Int J Prosthodont , vol.13 , pp. 387-391
    • Rosentritt, M.1    Plein, T.2    Kolbeck, C.3    Behr, M.4    Handel, G.5
  • 32
    • 7444265287 scopus 로고    scopus 로고
    • In vitro fracture strength of teeth restored with different all-ceramic crown systems
    • Potiket N., Chiche G., and Finger I.M. In vitro fracture strength of teeth restored with different all-ceramic crown systems. J Prosthet Dent 92 (2004) 491-495
    • (2004) J Prosthet Dent , vol.92 , pp. 491-495
    • Potiket, N.1    Chiche, G.2    Finger, I.M.3
  • 33
    • 0029258587 scopus 로고
    • Predicting lifetimes of materials and material structures
    • Ritter J.E. Predicting lifetimes of materials and material structures. Dent Mater 11 (1995) 142-146
    • (1995) Dent Mater , vol.11 , pp. 142-146
    • Ritter, J.E.1
  • 34
    • 38549111908 scopus 로고    scopus 로고
    • Fatigue and fracture properties of yttria partially stabilized zirconia crown systems
    • Tsalouchou E., Cattell M.J., Knowles J.C., Pittayachawan P., and McDonald A. Fatigue and fracture properties of yttria partially stabilized zirconia crown systems. Dent Mater 24 (2008) 308-318
    • (2008) Dent Mater , vol.24 , pp. 308-318
    • Tsalouchou, E.1    Cattell, M.J.2    Knowles, J.C.3    Pittayachawan, P.4    McDonald, A.5
  • 35
    • 0029318343 scopus 로고
    • Failure of all-ceramic fixed partial dentures in vitro and in vivo: analysis and modeling
    • Kelly J.R., Tesk J.A., and Sorensen J.A. Failure of all-ceramic fixed partial dentures in vitro and in vivo: analysis and modeling. J Dent Res 74 (1995) 1253-1258
    • (1995) J Dent Res , vol.74 , pp. 1253-1258
    • Kelly, J.R.1    Tesk, J.A.2    Sorensen, J.A.3
  • 36
    • 33749677224 scopus 로고    scopus 로고
    • The efficacy of posterior three-unit zirconium-oxide-based ceramic fixed partial dental prostheses: a prospective clinical pilot study
    • Raigrodski A.J., Chiche G.J., Potiket N., Hochstedler J.L., Mohamed S.E., Billiot S., et al. The efficacy of posterior three-unit zirconium-oxide-based ceramic fixed partial dental prostheses: a prospective clinical pilot study. J Prosthet Dent 96 (2006) 237-244
    • (2006) J Prosthet Dent , vol.96 , pp. 237-244
    • Raigrodski, A.J.1    Chiche, G.J.2    Potiket, N.3    Hochstedler, J.L.4    Mohamed, S.E.5    Billiot, S.6
  • 37
    • 34250653055 scopus 로고    scopus 로고
    • Five-year clinical results of zirconia frameworks for posterior fixed partial dentures
    • Sailer I., Feher A., Filser F., Gauckler L.J., Luthy H., and Hammerle C.H. Five-year clinical results of zirconia frameworks for posterior fixed partial dentures. Int J Prosthodont 20 (2007) 383-388
    • (2007) Int J Prosthodont , vol.20 , pp. 383-388
    • Sailer, I.1    Feher, A.2    Filser, F.3    Gauckler, L.J.4    Luthy, H.5    Hammerle, C.H.6
  • 38
    • 0033146116 scopus 로고    scopus 로고
    • Clinically relevant approach to failure testing of all-ceramic restorations
    • Kelly J.R. Clinically relevant approach to failure testing of all-ceramic restorations. J Prosthet Dent 81 (1999) 652-661
    • (1999) J Prosthet Dent , vol.81 , pp. 652-661
    • Kelly, J.R.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.