Volumn 10, Issue 11, 2014, Pages 4861-4869

Adhesion determination of dental porcelain to zirconia using the Schwickerath test: Strength vs. fracture energy approach

Author keywords

Adhesion; Porcelain; Schwickerath test; Strain energy release rate; Zirconia

Indexed keywords

BOND STRENGTH (MATERIALS); CRACKS; ENERGY RELEASE RATE; FRACTURE TOUGHNESS; PORCELAIN; STRAIN ENERGY; STRAIN RATE; UNLOADING; ZIRCONIA;

EID: 84908127337     PISSN: 17427061     EISSN: 18787568     Source Type: Journal    
DOI: 10.1016/j.actbio.2014.07.028     Document Type: Article
Times cited : (26)

References (34)
  • 1
    • 77956529457 scopus 로고    scopus 로고
    • Survival probability of zirconia-based fixed dental prostheses up to 5 yr: A systematic review of the literature
    • J.S. Schley, N. Heussen, S. Reich, J. Fischer, K. Haselhuhn, and S. Wolfart Survival probability of zirconia-based fixed dental prostheses up to 5 yr: a systematic review of the literature Eur J Oral Sci 118 2010 443 450
    • (2010) Eur J Oral Sci , vol.118 , pp. 443-450
    • Schley, J.S.1    Heussen, N.2    Reich, S.3    Fischer, J.4    Haselhuhn, K.5    Wolfart, S.6
  • 2
    • 78650487512 scopus 로고    scopus 로고
    • A clinical comparison of zirconia, metal and alumina fixed-prosthesis frameworks veneered with layered or pressed ceramic: A three-year report
    • R.P. Christensen, and B.J. Ploeger A clinical comparison of zirconia, metal and alumina fixed-prosthesis frameworks veneered with layered or pressed ceramic: a three-year report J Am Dent Assoc 141 2010 1317 1329
    • (2010) J Am Dent Assoc , vol.141 , pp. 1317-1329
    • Christensen, R.P.1    Ploeger, B.J.2
  • 3
    • 63349108354 scopus 로고    scopus 로고
    • Failure analysis of clinically failed all-ceramic fixed partial dentures using fractal geometry
    • P. Bulpakdi, B. Taskonak, J. Yan, and J.J. Mecholsky Jr Failure analysis of clinically failed all-ceramic fixed partial dentures using fractal geometry Dent Mater 25 2009 634 640
    • (2009) Dent Mater , vol.25 , pp. 634-640
    • Bulpakdi, P.1    Taskonak, B.2    Yan, J.3    Mecholsky, J.J.4
  • 4
    • 45049088335 scopus 로고    scopus 로고
    • Fractographic analyses of zirconia-based fixed partial dentures
    • B. Taskonak, J. Yan, J.J. Mecholsky Jr, A. Sertgoz, and A. Kocak Fractographic analyses of zirconia-based fixed partial dentures Dent Mater 24 2008 1077 1082
    • (2008) Dent Mater , vol.24 , pp. 1077-1082
    • Taskonak, B.1    Yan, J.2    Mecholsky, J.J.3    Sertgoz, A.4    Kocak, A.5
  • 5
    • 59149092803 scopus 로고    scopus 로고
    • Bridging the gap between clinical failure and laboratory fracture strength tests using a fractographic approach
    • M.N. Aboushelib, A.J. Feilzer, and C.J. Kleverlaan Bridging the gap between clinical failure and laboratory fracture strength tests using a fractographic approach Dent Mater 25 2009 383 391
    • (2009) Dent Mater , vol.25 , pp. 383-391
    • Aboushelib, M.N.1    Feilzer, A.J.2    Kleverlaan, C.J.3
  • 6
    • 4243558954 scopus 로고    scopus 로고
    • DIN EN ISO 9693:1999 (=ISO 9693:1999 = EN ISO 9693:2000-12). Geneva: International Organization for Standardization/Berlin: Beuth Verlag
    • DIN EN ISO 9693:1999 (=ISO 9693:1999 = EN ISO 9693:2000-12). Metal-ceramic dental restorative systems. Geneva: International Organization for Standardization/Berlin: Beuth Verlag.
    • Metal-ceramic Dental Restorative Systems
  • 9
    • 46249127868 scopus 로고    scopus 로고
    • Effect of zirconia surface treatments on the shear strength of zirconia/veneering ceramic composites
    • J. Fischer, P. Grohmann, and B. Stawarczyk Effect of zirconia surface treatments on the shear strength of zirconia/veneering ceramic composites Dent Mater J 27 2008 448 454
    • (2008) Dent Mater J , vol.27 , pp. 448-454
    • Fischer, J.1    Grohmann, P.2    Stawarczyk, B.3
  • 10
    • 60449083274 scopus 로고    scopus 로고
    • Impact of thermal misfit on shear strength of veneering ceramic/zirconia composites
    • J. Fischer, B. Stawarzcyk, A. Trottmann, and C.H. Hämmerle Impact of thermal misfit on shear strength of veneering ceramic/zirconia composites Dent Mater 25 2009 419 423
    • (2009) Dent Mater , vol.25 , pp. 419-423
    • Fischer, J.1    Stawarzcyk, B.2    Trottmann, A.3    Hämmerle, C.H.4
  • 11
    • 34250636079 scopus 로고    scopus 로고
    • Which mechanical and physical testing methods are relevant for predicting the clinical performance of ceramic-based dental prostheses?
    • K.J. Anusavice, K. Kakar, and N. Ferree Which mechanical and physical testing methods are relevant for predicting the clinical performance of ceramic-based dental prostheses? Clin Oral Implants Res 18 Suppl. 3 2007 218 231
    • (2007) Clin Oral Implants Res , vol.18 , pp. 218-231
    • Anusavice, K.J.1    Kakar, K.2    Ferree, N.3
  • 12
    • 41849125937 scopus 로고    scopus 로고
    • Flexural strength of veneering ceramics for zirconia
    • J. Fischer, B. Stawarczyk, and C.H. Hämmerle Flexural strength of veneering ceramics for zirconia J Dent 36 2008 316 321
    • (2008) J Dent , vol.36 , pp. 316-321
    • Fischer, J.1    Stawarczyk, B.2    Hämmerle, C.H.3
  • 13
    • 0018996246 scopus 로고
    • Comparative evaluation of ceramic-metal bond tests using finite element stress analysis
    • K.J. Anusavice, P.H. Dehoff, and C.W. Fairhurst Comparative evaluation of ceramic-metal bond tests using finite element stress analysis J Dent Res 59 1980 608 613
    • (1980) J Dent Res , vol.59 , pp. 608-613
    • Anusavice, K.J.1    Dehoff, P.H.2    Fairhurst, C.W.3
  • 14
    • 14844355576 scopus 로고    scopus 로고
    • The influence of Goldbonder and pre-heat treatment on the adhesion of titanium alloy and porcelain
    • K. Yamada, T. Onizuka, K. Endo, H. Ohno, and M.V. Swain The influence of Goldbonder and pre-heat treatment on the adhesion of titanium alloy and porcelain J Oral Rehabil 32 2005 213 220
    • (2005) J Oral Rehabil , vol.32 , pp. 213-220
    • Yamada, K.1    Onizuka, T.2    Endo, K.3    Ohno, H.4    Swain, M.V.5
  • 15
    • 0024621114 scopus 로고
    • A test specimen for determining the fracture resistance of biomaterial surfaces
    • P.G. Charalambides, J. Lund, A.G. Evans, and R.M. McMeeking A test specimen for determining the fracture resistance of biomaterial surfaces J Appl Mech 56 1989 77 82
    • (1989) J Appl Mech , vol.56 , pp. 77-82
    • Charalambides, P.G.1    Lund, J.2    Evans, A.G.3    McMeeking, R.M.4
  • 16
    • 0030699144 scopus 로고    scopus 로고
    • Evaluation of the strain energy release rate for the fracture of titanium-porcelain interfacial bonding
    • H.G. Chung, M.V. Swain, and T. Mori Evaluation of the strain energy release rate for the fracture of titanium-porcelain interfacial bonding Biomaterials 18 1997 1553 1557
    • (1997) Biomaterials , vol.18 , pp. 1553-1557
    • Chung, H.G.1    Swain, M.V.2    Mori, T.3
  • 17
    • 0033222608 scopus 로고    scopus 로고
    • New approach for evaluating metal-porcelain interfacial bonding
    • N. Suansuwan, and M.V. Swain New approach for evaluating metal-porcelain interfacial bonding Int J Prosthodont 12 1999 547 552
    • (1999) Int J Prosthodont , vol.12 , pp. 547-552
    • Suansuwan, N.1    Swain, M.V.2
  • 18
    • 84908134523 scopus 로고    scopus 로고
    • Verbundfestigkeit verschiedener Verblendkeramiken zu Zirkonoxid. Bond strength of veneering ceramics to zirconia
    • Kosyfaki P, Swain MV, Fischer J, Witkowski S, Strub JR. Verbundfestigkeit verschiedener Verblendkeramiken zu Zirkonoxid. Bond strength of veneering ceramics to zirconia. Dtsch Zahnärztl Z 2013; 68: 678-694.
    • (2013) Dtsch Zahnärztl Z , vol.68 , pp. 678-694
    • Kosyfaki, P.1    Swain, M.V.2    Fischer, J.3    Witkowski, S.4    Strub, J.R.5
  • 20
    • 0003902029 scopus 로고    scopus 로고
    • Mechanical engineering design
    • R.G. Budynas, K.J. Nisbett, 8th ed. McGraw-Hill Primis New York
    • J.E. Shigley Mechanical engineering design R.G. Budynas, K.J. Nisbett, Shigley's mechanical engineering design 8th ed. 2002 McGraw-Hill Primis New York 144 184
    • (2002) Shigley's Mechanical Engineering Design , pp. 144-184
    • Shigley, J.E.1
  • 22
    • 0023990770 scopus 로고
    • Prüfung der Biegefestigkeit von Metall-Keramik-Verbund-Systemen bei Verwendung von verschiedenen Dentallegierungen
    • H.F. Kappert, R. Becker, and W. Pollocek Prüfung der Biegefestigkeit von Metall-Keramik-Verbund-Systemen bei Verwendung von verschiedenen Dentallegierungen Dtsch Zahnärztl Z 43 1988 445 452
    • (1988) Dtsch Zahnärztl Z , vol.43 , pp. 445-452
    • Kappert, H.F.1    Becker, R.2    Pollocek, W.3
  • 23
    • 0024116246 scopus 로고
    • Zur Festigkeit des metallkeramischen Verbundes bei der Biegeprufung
    • S. Schwarz, J. Lenz, and H. Schwickerath Zur Festigkeit des metallkeramischen Verbundes bei der Biegeprufung Dtsch Zahnarztl Z 43 1988 1152 1158
    • (1988) Dtsch Zahnarztl Z , vol.43 , pp. 1152-1158
    • Schwarz, S.1    Lenz, J.2    Schwickerath, H.3
  • 24
    • 71149121504 scopus 로고
    • Mixed mode cracking in layered materials
    • J.W. Hutchinson, T. Wu, Academic Press New York
    • J.W. Hutchinson, and Z. Suo Mixed mode cracking in layered materials J.W. Hutchinson, T. Wu, Advances in applied mechanics 1992 Academic Press New York 63 191
    • (1992) Advances in Applied Mechanics , pp. 63-191
    • Hutchinson, J.W.1    Suo, Z.2
  • 25
    • 33749179816 scopus 로고    scopus 로고
    • Transverse fracture of brittle bilayers: Relevance to failure of all-ceramic dental crowns
    • J.W. Kim, S. Bhowmick, I. Hermann, and B.R. Lawn Transverse fracture of brittle bilayers: relevance to failure of all-ceramic dental crowns J Biomed Mater Res B Appl Biomater 79 2006 58 65
    • (2006) J Biomed Mater Res B Appl Biomater , vol.79 , pp. 58-65
    • Kim, J.W.1    Bhowmick, S.2    Hermann, I.3    Lawn, B.R.4
  • 26
    • 75049083048 scopus 로고    scopus 로고
    • Review of the fracture toughness approach
    • K.J. Söderholm Review of the fracture toughness approach Dent Mater 26 2010 e63 77
    • (2010) Dent Mater , vol.26 , pp. 63-77
    • Söderholm, K.J.1
  • 28
    • 0043071591 scopus 로고    scopus 로고
    • Adhesion of porcelain to titanium and a titanium alloy
    • N. Suansuwan, and M.V. Swain Adhesion of porcelain to titanium and a titanium alloy J Dent 31 2003 509 518
    • (2003) J Dent , vol.31 , pp. 509-518
    • Suansuwan, N.1    Swain, M.V.2
  • 29
    • 80053642176 scopus 로고    scopus 로고
    • Pressed ceramics onto zirconia. Part 2. Indentation fracture and influence of cooling rate on residual stresses
    • J.E. Choi, J.N. Waddell, and M.V. Swain Pressed ceramics onto zirconia. Part 2. Indentation fracture and influence of cooling rate on residual stresses Dent Mater 27 2011 1111 1118
    • (2011) Dent Mater , vol.27 , pp. 1111-1118
    • Choi, J.E.1    Waddell, J.N.2    Swain, M.V.3
  • 30
    • 84869890189 scopus 로고    scopus 로고
    • Effect of thermal expansion mismatch on the Y-TZP/veneer interfacial adhesion determined by strain energy release rate
    • G. Göstemeyer, M. Jendras, L. Borchers, F.W. Bach, M. Stiesch, and P. Kohorst Effect of thermal expansion mismatch on the Y-TZP/veneer interfacial adhesion determined by strain energy release rate J Prosthodont Res 56 2012 93 101
    • (2012) J Prosthodont Res , vol.56 , pp. 93-101
    • Göstemeyer, G.1    Jendras, M.2    Borchers, L.3    Bach, F.W.4    Stiesch, M.5    Kohorst, P.6
  • 32
    • 0022679706 scopus 로고
    • R-curve behavior from transformation toughening
    • R-curve behavior from transformation toughening J Am Ceramic Soc 69 1986 226 239
    • (1986) J Am Ceramic Soc , vol.69 , pp. 226-239
    • Burns, S.J.1    Swain, M.V.2
  • 33
    • 0348158990 scopus 로고
    • Residual stress effects on fracture toughness measurements
    • D. Francois, Pergamon Press Oxford
    • L.M. Barker Residual stress effects on fracture toughness measurements D. Francois, Advances in fracture research, ICF5, Cannes, France 1981 Pergamon Press Oxford 2563 2570
    • (1981) Advances in Fracture Research, ICF5, Cannes, France , pp. 2563-2570
    • Barker, L.M.1
  • 34
    • 0032106909 scopus 로고    scopus 로고
    • Thermal stresses in metal-ceramic specimens for the ISO crack initiation test (three-point flexure bond test)
    • J. Lenz, and S. Kessel Thermal stresses in metal-ceramic specimens for the ISO crack initiation test (three-point flexure bond test) Dent Mater 14 1998 277 280
    • (1998) Dent Mater , vol.14 , pp. 277-280
    • Lenz, J.1    Kessel, S.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.