1
-
-
84858620918
-
Determination of standard gibbs free energy of formation of chukanovite and purbaix diagrams of iron in carbonated media
-
Azoulay, I., Rémazeilles, C., Refait, P. (2012): Determination of standard Gibbs free energy of formation of chukanovite and Purbaix diagrams of iron in carbonated media. Corrosion Sci, 58, 229-236.
-
(2012)
Corrosion Sci
, vol.58
, pp. 229-236
-
-
Azoulay, I.1
Rémazeilles, C.2
Refait, P.3
-
2
-
-
34548364506
-
Use of three-dimensional parameters in the analysis of crystal structures under compression
-
A. Grzechnik, ed. Transworld Research Network, Trivandrum, Kerela, India
-
Balić-Žunić, T. (2007): Use of three-dimensional parameters in the analysis of crystal structures under compression. in "Pressure-induced phase transitions", A. Grzechnik, ed. Transworld Research Network, Trivandrum, Kerela, India, 157-184.
-
(2007)
Pressure-induced Phase Transitions
, pp. 157-184
-
-
Balić-Žunić, T.1
-
3
-
-
0000526431
-
IVTON - Program for the calculation of geometrical aspects of crystal structures and some crystal chemical applications
-
Balić-Žunić, T. & Makovicky, E. (1996): IVTON - program for the calculation of geometrical aspects of crystal structures and some crystal chemical applications. J. Appl. Crystallogr., 29, 305-306.
-
(1996)
J. Appl. Crystallogr.
, vol.29
, pp. 305-306
-
-
Balić-Žunić, T.1
Makovicky, E.2
-
4
-
-
77954629326
-
1+xSb nanophase and its structure determination using automated electron diffraction tomography
-
1+xSb nanophase and its structure determination using automated electron diffraction tomography. J. Am. Chem. Soc, 132, 9881-9889.
-
(2010)
J. Am. Chem. Soc
, vol.132
, pp. 9881-9889
-
-
Birkel, C.S.1
Mugnaioli, E.2
Gorelik, T.3
Kolb, U.4
Panthoefer, M.5
Tremel, W.6
-
5
-
-
0029278371
-
Physico-chemical characterization of corrosion layers formed on iron in a sodium carbonate-bicarbonate containing environment
-
Blengino, J.M., Keddam, M., Labbe, J.P., Robbiola, L. (1995): Physico-chemical characterization of corrosion layers formed on iron in a sodium carbonate-bicarbonate containing environment. Corrosion Sci., 37, 621-643.
-
(1995)
Corrosion Sci.
, vol.37
, pp. 621-643
-
-
Blengino, J.M.1
Keddam, M.2
Labbe, J.P.3
Robbiola, L.4
-
6
-
-
84945061921
-
Empirical bond-strength-bond-length curves for oxides
-
Brown, I.D. & Shannon, R.D. (1973): Empirical bond-strength-bond- length curves for oxides. Acta Crystallogr., A29, 266-282.
-
(1973)
Acta Crystallogr.
, vol.A29
, pp. 266-282
-
-
Brown, I.D.1
Shannon, R.D.2
-
7
-
-
84859754995
-
SIR2011: A new package for crystal structure determination and refinement
-
Burla, M.C., Caliandro, R., Camalli, M., Carrozzini, B., Cascarano, G.L., Giacovazzo, C., Mallamo, M., Mazzone, A., Polidori, G., Spagna, R. (2012): SIR2011: a new package for crystal structure determination and refinement. J. Appl. Crystallogr., 45, 357-361.
-
(2012)
J. Appl. Crystallogr.
, vol.45
, pp. 357-361
-
-
Burla, M.C.1
Caliandro, R.2
Camalli, M.3
Carrozzini, B.4
Cascarano, G.L.5
Giacovazzo, C.6
Mallamo, M.7
Mazzone, A.8
Polidori, G.9
Spagna, R.10
-
8
-
-
7544239422
-
Clay minerals in the meuse-haute marne underground laboratory (France): Possible influence of organic matter on clay mineral evolution
-
Claret, F., Sakharov, B.A., Drits, V.A., Velde, B., Meunier, A., Griffault, L., Lanson, B. (2004): Clay minerals in the Meuse-Haute Marne underground laboratory (France): possible influence of organic matter on clay mineral evolution. Clays and Clay Minerals, 52, 515-532.
-
(2004)
Clays and Clay Minerals
, vol.52
, pp. 515-532
-
-
Claret, F.1
Sakharov, B.A.2
Drits, V.A.3
Velde, B.4
Meunier, A.5
Griffault, L.6
Lanson, B.7
-
9
-
-
78650709879
-
Glass-iron-clay interactions in a radioactive waste geological disposal: An integrated laboratory-scale experiment
-
de Combarieu, G., Schlegel, M., Neff, D., Foy, E., Vantelon, D., Barboux, P., Gin, S. (2011): Glass-iron-clay interactions in a radioactive waste geological disposal: an integrated laboratory-scale experiment. Appl. Geochem., 26, 65-79.
-
(2011)
Appl. Geochem.
, vol.26
, pp. 65-79
-
-
De Combarieu, G.1
Schlegel, M.2
Neff, D.3
Foy, E.4
Vantelon, D.5
Barboux, P.6
Gin, S.7
-
11
-
-
27244453007
-
Electron crystallography of zeolite - The MWW family as a test of direct 3D structure determination
-
Dorset, D.L., Roth, W.J., Gilmore, C.J. (2005): Electron crystallography of zeolite - the MWW family as a test of direct 3D structure determination. Acta Crystallogr., A61, 516-527.
-
(2005)
Acta Crystallogr.
, vol.A61
, pp. 516-527
-
-
Dorset, D.L.1
Roth, W.J.2
Gilmore, C.J.3
-
12
-
-
0019715395
-
Crystal structure refinement of magnesite, calcite, rhodochrosite, siderite, smithonite, and dolomite, with discussion of some aspects of the stereochemistry of calcite type carbonates
-
Effenberger, H., Mereiter, K., Zemann, J. (1981): Crystal structure refinement of magnesite, calcite, rhodochrosite, siderite, smithonite, and dolomite, with discussion of some aspects of the stereochemistry of calcite type carbonates. Z. Kristallogr., 156, 233-243.
-
(1981)
Z. Kristallogr.
, vol.156
, pp. 233-243
-
-
Effenberger, H.1
Mereiter, K.2
Zemann, J.3
-
13
-
-
84985407661
-
Ein dem Malachit ähnliches Eisenkarbonat als Korrosionsprodukt von Stahl
-
Erdös, E. & Altorfer, H. (1976): Ein dem Malachit ähnliches Eisenkarbonat als Korrosionsprodukt von Stahl. Werkstoffe und Korrosion, 27, 304-312.
-
(1976)
Werkstoffe und Korrosion
, vol.27
, pp. 304-312
-
-
Erdös, E.1
Altorfer, H.2
-
14
-
-
10744226551
-
ANDRA underground research laboratory: Interpretation of the mineralogical and geochemical data acquired in the callovian-oxfordian formation by investigative drilling
-
Gaucher, E., Robelin, C., Matray, J.M., Négrel, G., Gros, Y., Heitz, J.F., Vinsot, A., Rebours, H., Cassagnabère, A., Bouchet, A. (2004): ANDRA underground research laboratory: interpretation of the mineralogical and geochemical data acquired in the Callovian-Oxfordian formation by investigative drilling. Phys. Chem. Earth, 29, 55-77.
-
(2004)
Phys. Chem. Earth
, vol.29
, pp. 55-77
-
-
Gaucher, E.1
Robelin, C.2
Matray, J.M.3
Négrel, G.4
Gros, Y.5
Heitz, J.F.6
Vinsot, A.7
Rebours, H.8
Cassagnabère, A.9
Bouchet, A.10
-
15
-
-
33847168921
-
Structure solution with three-dimensional sets of precessed electron diffraction intensities
-
Gemmi, M. & Nicolopoulos, S. (2007): Structure solution with three-dimensional sets of precessed electron diffraction intensities. Ultramicroscopy, 107, 483-494.
-
(2007)
Ultramicroscopy
, vol.107
, pp. 483-494
-
-
Gemmi, M.1
Nicolopoulos, S.2
-
17
-
-
80053345842
-
A new hydrous al-bearing pyroxene as a water carrier in subduction zones
-
Gemmi, M., Fischer, J., Merlini, M., Poli, S., Fumagalli, P., Mugnaioli, E., Kolb, U. (2011): A new hydrous Al-bearing pyroxene as a water carrier in subduction zones. Earth Planet. Sci. Lett., 310, 422-428.
-
(2011)
Earth Planet. Sci. Lett.
, vol.310
, pp. 422-428
-
-
Gemmi, M.1
Fischer, J.2
Merlini, M.3
Poli, S.4
Fumagalli, P.5
Mugnaioli, E.6
Kolb, U.7
-
18
-
-
84859042942
-
On the structural relations of malachite. I. The rosasite and ludwigite structure families
-
Girgsdies, F. & Behrens, M. (2012): On the structural relations of malachite. I. The rosasite and ludwigite structure families. Acta Crystallogr., B68, 107-117.
-
(2012)
Acta Crystallogr.
, vol.B68
, pp. 107-117
-
-
Girgsdies, F.1
Behrens, M.2
-
19
-
-
80052181605
-
Synthesis and structure determination of the hierarchical meso-microporous zeolite ITQ-43
-
Jiang, J., Jorda, J.L., Yu, J., Baumes, L.A., Mugnaioli, E., Diaz-Cabanas, M.J., Kolb, U., Corma, A. (2011): Synthesis and structure determination of the hierarchical meso-microporous zeolite ITQ-43. Science, 333, 1131-1134.
-
(2011)
Science
, vol.333
, pp. 1131-1134
-
-
Jiang, J.1
Jorda, J.L.2
Yu, J.3
Baumes, L.A.4
Mugnaioli, E.5
Diaz-Cabanas, M.J.6
Kolb, U.7
Corma, A.8
-
20
-
-
78650462952
-
Effect of a thermal gradient on iron-clay interactions
-
Jodin-Caumon, M.C., Mosser-Ruck, R., Rousset, D., Randi, A., Cathelineau, M., Michau, N. (2010): Effect of a thermal gradient on iron-clay interactions. Clays and Clay Minerals, 58, 667-681.
-
(2010)
Clays and Clay Minerals
, vol.58
, pp. 667-681
-
-
Jodin-Caumon, M.C.1
Mosser-Ruck, R.2
Rousset, D.3
Randi, A.4
Cathelineau, M.5
Michau, N.6
-
21
-
-
84871242576
-
Mineralogical evolution of a claystone after reaction with iron under thermal gradient
-
Jodin-Caumon, M.C., Mosser-Ruck, R., Randi, A., Pierron, O., Cathelineau, M., Michau, N. (2012): Mineralogical evolution of a claystone after reaction with iron under thermal gradient. Clays and Clay Minerals, 60, 443-455.
-
(2012)
Clays and Clay Minerals
, vol.60
, pp. 443-455
-
-
Jodin-Caumon, M.C.1
Mosser-Ruck, R.2
Randi, A.3
Pierron, O.4
Cathelineau, M.5
Michau, N.6
-
22
-
-
17644372420
-
Longevity of granular iron in groundwater treatment processes: Corrosion product development
-
Kohn, T., Livi, A.L., Roberts, P., Vikesland, P. (2005): Longevity of granular iron in groundwater treatment processes: corrosion product development. Environ. Sci. Technol., 39, 2867-2879.
-
(2005)
Environ. Sci. Technol.
, vol.39
, pp. 2867-2879
-
-
Kohn, T.1
Livi, A.L.2
Roberts, P.3
Vikesland, P.4
-
23
-
-
33847173656
-
Towards automated diffraction tomography: Part I - Data acquisition
-
Kolb, U., Gorelik, T., Kübel, C., Otten, M.T. (2007): Towards automated diffraction tomography: Part I - Data acquisition. Ultramicroscopy, 107, 507-513.
-
(2007)
Ultramicroscopy
, vol.107
, pp. 507-513
-
-
Kolb, U.1
Gorelik, T.2
Kübel, C.3
Otten, M.T.4
-
24
-
-
45449103253
-
Towards automated diffraction tomography. Part II - Cell parameter determination
-
Kolb, U., Gorelik, T., Otten, M.T. (2008): Towards automated diffraction tomography. Part II - Cell parameter determination. Ultramicroscopy, 108, 763-772.
-
(2008)
Ultramicroscopy
, vol.108
, pp. 763-772
-
-
Kolb, U.1
Gorelik, T.2
Otten, M.T.3
-
25
-
-
79957984260
-
Automated electron diffraction tomography - A new tool for nano crystal structure analysis
-
Kolb, U., Mugnaioli, E., Gorelik, T.E. (2011): Automated electron diffraction tomography - a new tool for nano crystal structure analysis. Cryst. Res. and Technol, 46, 542-554.
-
(2011)
Cryst. Res. and Technol
, vol.46
, pp. 542-554
-
-
Kolb, U.1
Mugnaioli, E.2
Gorelik, T.E.3
-
26
-
-
14944358469
-
Ferrous hydroxyl carbonate is a stable transformation product of biogenic magnetite
-
Kukkadapu, R.K., Zachara, J.M., Fredrickson, J.K., Kennedy, D.W., Dohnalkova, A.C., McCready, D.E. (2005): Ferrous hydroxyl carbonate is a stable transformation product of biogenic magnetite. Am. Mineral., 90, 510-515.
-
(2005)
Am. Mineral.
, vol.90
, pp. 510-515
-
-
Kukkadapu, R.K.1
Zachara, J.M.2
Fredrickson, J.K.3
Kennedy, D.W.4
Dohnalkova, A.C.5
McCready, D.E.6
-
27
-
-
84861415030
-
Experimental investigation of smectite interaction with metal iron at 80°C: Structural characterization of newly formed fe-rich phyllosilicates
-
Lanson, B., Lantenois, S., Van Aken, P.A., Bauer, A., Plançon, A. (2012): Experimental investigation of smectite interaction with metal iron at 80°C: structural characterization of newly formed Fe-rich phyllosilicates. Am. Mineral., 97, 864-871.
-
(2012)
Am. Mineral.
, vol.97
, pp. 864-871
-
-
Lanson, B.1
Lantenois, S.2
Van Aken, P.A.3
Bauer, A.4
Plançon, A.5
-
29
-
-
30144444894
-
Experimental study of smetite interaction with metal fe at low temperature: 1. Smectite destabilization
-
Lantenois, S., Lanson, B., Muller, F., Bauer, A., Jullien, M., Plançon, A. (2005): Experimental study of smetite interaction with metal Fe at low temperature: 1. Smectite destabilization. Clays and Clay Minerals, 53, 597-612.
-
(2005)
Clays and Clay Minerals
, vol.53
, pp. 597-612
-
-
Lantenois, S.1
Lanson, B.2
Muller, F.3
Bauer, A.4
Jullien, M.5
Plançon, A.6
-
30
-
-
77955654264
-
Iron hydroxyl carbonate formation in zerovalent iron permeable reactive barriers: Characterization and evaluation of phase stability
-
Lee, T.R. & Wilkin, R.T. (2010): Iron hydroxyl carbonate formation in zerovalent iron permeable reactive barriers: characterization and evaluation of phase stability. J. Contam. Hydrol., 116, 47-57.
-
(2010)
J. Contam. Hydrol.
, vol.116
, pp. 47-57
-
-
Lee, T.R.1
Wilkin, R.T.2
-
31
-
-
0001645947
-
New measure of distortion for coordination polyhedra
-
Makovicky, E. & Balic-Zunic, T. (1998): New measure of distortion for coordination polyhedra. Acta Crystallogr., B54, 766-773.
-
(1998)
Acta Crystallogr.
, vol.B54
, pp. 766-773
-
-
Makovicky, E.1
Balic-Zunic, T.2
-
32
-
-
82055197100
-
VESTA 3 for three-dimensional visualization of crystal, volumetric and morphology data
-
Momma, K. & Izumi, F. (2011): VESTA 3 for three-dimensional visualization of crystal, volumetric and morphology data. J. Appl. Crystallogr., 44, 1272-1276.
-
(2011)
J. Appl. Crystallogr.
, vol.44
, pp. 1272-1276
-
-
Momma, K.1
Izumi, F.2
-
33
-
-
77953299372
-
Effects of temperature, pH, and iron/clay and liquid/clay ratios on experimental conversion of dioctahedral smectite to berthierine, chlorite, vermiculite, or saponite
-
Mosser-Ruck, R., Cathelineau, M., Guillaume, D., Charpentier, D. (2010): Effects of temperature, pH, and iron/clay and liquid/clay ratios on experimental conversion of dioctahedral smectite to berthierine, chlorite, vermiculite, or saponite. Clays and Clay Minerals, 58, 280-291.
-
(2010)
Clays and Clay Minerals
, vol.58
, pp. 280-291
-
-
Mosser-Ruck, R.1
Cathelineau, M.2
Guillaume, D.3
Charpentier, D.4
-
34
-
-
84869080789
-
Applications of automated diffraction tomography (ADT) on nanocrystalline porous materials
-
Mugnaioli, E. & Kolb, U. (2013): Applications of automated diffraction tomography (ADT) on nanocrystalline porous materials. Microporous and Mesoporous Materials, 166, 93-101.
-
(2013)
Microporous and Mesoporous Materials
, vol.166
, pp. 93-101
-
-
Mugnaioli, E.1
Kolb, U.2
-
35
-
-
63449136077
-
Ab initio structure solution from electron diffraction data obtained by a combination of automated diffraction tomography and precession technique
-
Mugnaioli, E., Gorelik, T., Kolb, U. (2009): Ab initio structure solution from electron diffraction data obtained by a combination of automated diffraction tomography and precession technique. Ultramicroscopy, 109, 758-765.
-
(2009)
Ultramicroscopy
, vol.109
, pp. 758-765
-
-
Mugnaioli, E.1
Gorelik, T.2
Kolb, U.3
-
36
-
-
3042785174
-
The effect of bicarbonate/carbonate ions on the formation of iron rust
-
Music, S., Nowik, I., Rustic, M., Orehovec, Z., Popovic, S. (2004): The effect of bicarbonate/carbonate ions on the formation of iron rust. Croat. Chem. Acta, 77, 141-151.
-
(2004)
Croat. Chem. Acta
, vol.77
, pp. 141-151
-
-
Music, S.1
Nowik, I.2
Rustic, M.3
Orehovec, Z.4
Popovic, S.5
-
37
-
-
0001592103
-
Mounting an individual submicrometer sized crystal
-
Neder, R.B., Burghammer, M., Grasl, T., Schulz, H. (1996): Mounting an individual submicrometer sized crystal. Z Kristallogr., 211, 365-367.
-
(1996)
Z Kristallogr.
, vol.211
, pp. 365-367
-
-
Neder, R.B.1
Burghammer, M.2
Grasl, T.3
Schulz, H.4
-
38
-
-
0032702503
-
Refinement of the kaolinite structure from single-crystal synchrotron data
-
Neder, R.B., Burghammer, M., Grasl, T., Schulz, H., Bram, A., Fieldler, S. (1999): Refinement of the kaolinite structure from single-crystal synchrotron data. Clays and Clay Minerals, 47, 487-494.
-
(1999)
Clays and Clay Minerals
, vol.47
, pp. 487-494
-
-
Neder, R.B.1
Burghammer, M.2
Grasl, T.3
Schulz, H.4
Bram, A.5
Fieldler, S.6
-
39
-
-
79952122430
-
Corrosion behaviour of carbon steel for overpack in groundwater containing bicarbonate ions
-
Nishimura, T. & Dong, J. (2009): Corrosion behaviour of carbon steel for overpack in groundwater containing bicarbonate ions. J. Power and Energ. Syst., 3, 23-30.
-
(2009)
J. Power and Energ. Syst.
, vol.3
, pp. 23-30
-
-
Nishimura, T.1
Dong, J.2
-
40
-
-
38049026895
-
2, a new mineral from the weathered iron meteorite dronino
-
2, a new mineral from the weathered iron meteorite Dronino. Eur. J. Mineral, 19, 891-898.
-
(2007)
Eur. J. Mineral
, vol.19
, pp. 891-898
-
-
Pekov, I.V.1
Perchiazzi, N.2
Merlino, S.3
Vyacheslav, N.K.4
Zadov, A.5
-
41
-
-
33846022968
-
Crystal structure determination and rietveld refinement of rosasite and mcguinnessite
-
Perchiazzi, N. (2006): Crystal structure determination and Rietveld refinement of rosasite and mcguinnessite. Z Kristallogr., 23, 505-510.
-
(2006)
Z Kristallogr.
, vol.23
, pp. 505-510
-
-
Perchiazzi, N.1
-
42
-
-
33846009127
-
The malachite-rosaite group: Crystal structure of glaukosphaerite and pokrovskite
-
Perchiazzi, N. & Merlino, S. (2006): The malachite-rosaite group: crystal structure of glaukosphaerite and pokrovskite. Eur. J. Mineral, 18, 787-792.
-
(2006)
Eur. J. Mineral
, vol.18
, pp. 787-792
-
-
Perchiazzi, N.1
Merlino, S.2
-
43
-
-
33847414488
-
Towards a link between the energetic heterogeneities of the edge of smectites and their stability in the context of metallic corrosion
-
Perronnet, M., Villiéras, F., Jullien, M., Razafitianamaharavo, A., Raynal, J., Bonnin, D. (2007): Towards a link between the energetic heterogeneities of the edge of smectites and their stability in the context of metallic corrosion. Geochim. Cosmochim. Acta, 71, 1463-1479.
-
(2007)
Geochim. Cosmochim. Acta
, vol.71
, pp. 1463-1479
-
-
Perronnet, M.1
Villiéras, F.2
Jullien, M.3
Razafitianamaharavo, A.4
Raynal, J.5
Bonnin, D.6
-
44
-
-
4444221565
-
UCSF chimera - A visualization system for exploratory research and analysis
-
Pettersen, F.F., Goddard, T.D., Huanq, C.C., Couch, G.S., Greenblatt, D.M., Menq, E.C., Ferrin, T.E. (2004): UCSF Chimera - a visualization system for exploratory research and analysis. J. Comput. Chem., 25, 1605-1612.
-
(2004)
J. Comput. Chem.
, vol.25
, pp. 1605-1612
-
-
Pettersen, F.F.1
Goddard, T.D.2
Huanq, C.C.3
Couch, G.S.4
Greenblatt, D.M.5
Menq, E.C.6
Ferrin, T.E.7
-
45
-
-
84886795906
-
A multi-technique characterization of cronstedtite synthesized by iron-clay interaction in a step by step cooling procedure
-
Pignatelli, I., Mugnaioli, E., Hybler, J., Mosser-Ruck, R., Cathelineau, M., Michau, N. (2013): A multi-technique characterization of cronstedtite synthesized by iron-clay interaction in a step by step cooling procedure. Clays and Clay Minerals, 61, 277-289.
-
(2013)
Clays and Clay Minerals
, vol.61
, pp. 277-289
-
-
Pignatelli, I.1
Mugnaioli, E.2
Hybler, J.3
Mosser-Ruck, R.4
Cathelineau, M.5
Michau, N.6
-
46
-
-
30844454926
-
3/NaCl electrolytes: Role of fe(II)-containing compounds
-
3/NaCl electrolytes: role of Fe(II)-containing compounds. Corrosion Sci, 48, 709-726.
-
(2006)
Corrosion Sci
, vol.48
, pp. 709-726
-
-
Refass, M.1
Sabot, R.2
Savall, C.3
Jeannin, M.4
Creus, J.5
Refait, Ph.6
-
47
-
-
60349118492
-
3 (chukanovite) as iron product: Synthesis and study by fourier transform infrared spectroscopy
-
3 (chukanovite) as iron product: synthesis and study by Fourier Transform Infrared Spectroscopy. Polyhedron, 28, 749-756.
-
(2009)
Polyhedron
, vol.28
, pp. 749-756
-
-
Rémazeilles, C.1
Refait, P.2
-
48
-
-
84872022240
-
Berthierine-like mineral formation and stability during the interaction of kaolinite with metallic iron at 90 °C under anoxic and oxic conditions
-
Rivard, C, Pelletier, M., Michau, N., Razafitianamaharavo, A., Bihannic, I., Abdelmoula, M., Ghanbaja, J., Villiéras, F. (2013): Berthierine-like mineral formation and stability during the interaction of kaolinite with metallic iron at 90 °C under anoxic and oxic conditions. Am. Mineral, 98, 163-180.
-
(2013)
Am. Mineral
, vol.98
, pp. 163-180
-
-
Rivard, C.1
Pelletier, M.2
Michau, N.3
Razafitianamaharavo, A.4
Bihannic, I.5
Abdelmoula, M.6
Ghanbaja, J.7
Villiéras, F.8
-
49
-
-
33845267905
-
Quadratic elongation: A quantitative measure of distortion in coordination polyhedral
-
Robinson, K., Gibbs, G.V., Ribbe, P.H. (1971): Quadratic elongation: a quantitative measure of distortion in coordination polyhedral. Science, 172, 567-570.
-
(1971)
Science
, vol.172
, pp. 567-570
-
-
Robinson, K.1
Gibbs, G.V.2
Ribbe, P.H.3
-
51
-
-
77951810644
-
2O, solved by conventional and automated electron diffraction
-
2O, solved by conventional and automated electron diffraction. Mineral Mag., 74, 159-177.
-
(2010)
Mineral Mag.
, vol.74
, pp. 159-177
-
-
Rozhdestvenskaya, I.1
Mugnaioli, E.2
Czank, M.3
Depmeier, W.4
Kolb, U.5
Reinholdt, A.6
Weirich, T.7
-
53
-
-
51249124452
-
Long-term corrosion behaviour of low-carbon steel in anoxic environment: Characterisation of archaeological artefacts
-
Saheb, M., Neff, D., Dillmann, P., Matthiesen, H., Foy, E. (2008): Long-term corrosion behaviour of low-carbon steel in anoxic environment: characterisation of archaeological artefacts. J. Nucl. Mater., 379, 118-123.
-
(2008)
J. Nucl. Mater.
, vol.379
, pp. 118-123
-
-
Saheb, M.1
Neff, D.2
Dillmann, P.3
Matthiesen, H.4
Foy, E.5
-
54
-
-
60349124355
-
Multisecular corrosion behaviour of low carbon steel in anoxic soil: Characterisation of corrosion system on archaeological artefacts
-
Saheb, M., Neff, D., Dillmann, P., Matthiesen, H., Foy, E., Bellot-Gurlet, L. (2009): Multisecular corrosion behaviour of low carbon steel in anoxic soil: characterisation of corrosion system on archaeological artefacts. Mater. Corrosion, 60, 99-105.
-
(2009)
Mater. Corrosion
, vol.60
, pp. 99-105
-
-
Saheb, M.1
Neff, D.2
Dillmann, P.3
Matthiesen, H.4
Foy, E.5
Bellot-Gurlet, L.6
-
55
-
-
78649448388
-
Iron corrosion in an anoxic soil: Comparison between thermodynamic modelling and ferrous archaeological artefacts characterised along with the local in situ geochemical conditions
-
Saheb, M., Descostes, M., Neff, D., Matthiesen, H., Michelin, A., Dillmann, P. (2010): Iron corrosion in an anoxic soil: comparison between thermodynamic modelling and ferrous archaeological artefacts characterised along with the local in situ geochemical conditions. Appl. Geochem., 25, 1937-1948.
-
(2010)
Appl. Geochem.
, vol.25
, pp. 1937-1948
-
-
Saheb, M.1
Descostes, M.2
Neff, D.3
Matthiesen, H.4
Michelin, A.5
Dillmann, P.6
-
56
-
-
79955668014
-
Raman study of a deuterated iron hydroxycarbonate to assess long-term corrosion mechanism in anoxic soils
-
Saheb, M., Neff, D., Bellot-Gurlet, L., Dillmann, P. (2011): Raman study of a deuterated iron hydroxycarbonate to assess long-term corrosion mechanism in anoxic soils. J. Raman Spectrosc, 42, 1100-1108.
-
(2011)
J. Raman Spectrosc
, vol.42
, pp. 1100-1108
-
-
Saheb, M.1
Neff, D.2
Bellot-Gurlet, L.3
Dillmann, P.4
-
57
-
-
84866340512
-
Structure characterization of hard materials by precession electron diffraction and automatic diffraction tomography: 6H-sic semiconductor and ni1 + xTe1 embedded nanodomains
-
Sarakinou, E., Mugnaioli, E., Lioutas, C.B., Vouroutzis, N., Frangis, N., Kolb, U., Nikolopoulos, S. (2012): Structure characterization of hard materials by precession electron diffraction and automatic diffraction tomography: 6H-SiC semiconductor and Ni1 + xTe1 embedded nanodomains. Semiconductor Sci. Technol, 27, 105003-105009.
-
(2012)
Semiconductor Sci. Technol
, vol.27
, pp. 105003-105009
-
-
Sarakinou, E.1
Mugnaioli, E.2
Lioutas, C.B.3
Vouroutzis, N.4
Frangis, N.5
Kolb, U.6
Nikolopoulos, S.7
-
58
-
-
50549093288
-
Metal corrosion and argillite transformation at the water-saturated high-temperature iron-clay interface: A microscopic-scale study
-
Schlegel, ML., Bataillon, C, Benhamida, K., Blanc, C, Menut, D., Lacour, J. (2008): Metal corrosion and argillite transformation at the water-saturated high-temperature iron-clay interface: a microscopic-scale study. Appl. Geochem, 23, 2619-2633.
-
(2008)
Appl. Geochem
, vol.23
, pp. 2619-2633
-
-
Schlegel, M.L.1
Bataillon, C.2
Benhamida, K.3
Blanc, C.4
Menut, D.5
Lacour, J.6
-
59
-
-
77249151025
-
Anodic activation of iron corrosion in clay media under water-saturated conditions at 90° C: Characterization of the corrosion interface
-
Schlegel, M.L., Bataillon, C, Blanc, C, Pret, D., Foy, E. (2010): Anodic activation of iron corrosion in clay media under water-saturated conditions at 90° C: characterization of the corrosion interface. Environ. Sci. Technol, 44, 1503-1508.
-
(2010)
Environ. Sci. Technol
, vol.44
, pp. 1503-1508
-
-
Schlegel, M.L.1
Bataillon, C.2
Blanc, C.3
Pret, D.4
Foy, E.5
-
60
-
-
84865270221
-
Application of clustering techniques to electron-diffraction data: Determination of unit-cell parameters
-
Schlitt, S., Gorelik, T.E., Stewart, A.A., Schömer, E., Raasch, T., Kolb, U. (2012): Application of clustering techniques to electron-diffraction data: determination of unit-cell parameters. Acta Crystallogr., A68, 536-546.
-
(2012)
Acta Crystallogr.
, vol.A68
, pp. 536-546
-
-
Schlitt, S.1
Gorelik, T.E.2
Stewart, A.A.3
Schömer, E.4
Raasch, T.5
Kolb, U.6
-
63
-
-
0028401583
-
Double conical beam-rocking system for measurement of integrated electron diffraction intensities
-
Vincent, R. & Midgley, P.A. (1994): Double conical beam-rocking system for measurement of integrated electron diffraction intensities. Ultramicroscopy, 53, 271-282.
-
(1994)
Ultramicroscopy
, vol.53
, pp. 271-282
-
-
Vincent, R.1
Midgley, P.A.2
-
64
-
-
30944452356
-
The effect of iron on montmorillonite stability. (II) experimental investigation
-
Wilson, J., Cressey, G., Cressey, B., Cuadros, J., Ragnarsdottir, V.K., Savage, D., Shibata, M. (2006): The effect of iron on montmorillonite stability. (II) Experimental investigation. Geochim. Cosmochim. Acta, 70, 323-336.
-
(2006)
Geochim. Cosmochim. Acta
, vol.70
, pp. 323-336
-
-
Wilson, J.1
Cressey, G.2
Cressey, B.3
Cuadros, J.4
Ragnarsdottir, V.K.5
Savage, D.6
Shibata, M.7
-
65
-
-
33845884085
-
3, durch Neutronenbeugung
-
3, durch Neutronenbeugung. Z Kristallogr., 145, 412-426.
-
(1977)
Z Kristallogr.
, vol.145
, pp. 412-426
-
-
Zigan, F.1
Joswig, W.2
Schuster, H.D.3
Mason, S.A.4
|