Volumn 44, Issue 4, 2010, Pages 1503-1508

Anodic activation of iron corrosion in clay media under water-saturated conditions at 90 °C: Characterization of the corrosion interface

Author keywords

[No Author keywords available]

Indexed keywords

ANODIC ACTIVATION; CA-DOPED; CORROSION PRODUCTS; EXTERNAL LAYERS; IRON CORROSION; LONG-TERM CORROSION; MAGNETITE LAYERS; MATRIX LAYERS; MINERALOGICAL PROPERTIES; NUCLEAR GLASS; OUTER LAYER; PHYLLOSILICATE; RE-OXIDATION; SATURATED CLAY; SATURATED CONDITIONS; SPECTROSCOPIC TECHNIQUE; UNDER WATER;

EID: 77249151025     PISSN: 0013936X     EISSN: 15205851     Source Type: Journal    
DOI: 10.1021/es9021987     Document Type: Article
Times cited : (85)

References (27)
  • 1
    • 51249114579 scopus 로고    scopus 로고
    • Corrosion issues in nuclear waste disposal
    • Féron, D.; Crusset, D.; Gras, J. M. Corrosion issues in nuclear waste disposal. J. Nucl. Mater. 2008, 379, 16-23.
    • (2008) J. Nucl. Mater , vol.379 , pp. 16-23
    • Féron, D.1    Crusset, D.2    Gras, J.M.3
  • 2
    • 0032030367 scopus 로고    scopus 로고
    • Clay mineralogical investigations related to nuclear waste disposal
    • Madsen, F. T. Clay mineralogical investigations related to nuclear waste disposal. Clay Min. 1998, 33, 109-129.
    • (1998) Clay Min , vol.33 , pp. 109-129
    • Madsen, F.T.1
  • 3
    • 0001146334 scopus 로고    scopus 로고
    • Simulated alteration tests on non-radioactive SON 68 nuclear glass in the presence of corrosion products and environmental materials
    • Jollivet, P.; Minet, Y.; Nicolas, M.; Vernaz, E. Simulated alteration tests on non-radioactive SON 68 nuclear glass in the presence of corrosion products and environmental materials. J. Nucl. Mater. 2000, 281, 231-243.
    • (2000) J. Nucl. Mater , vol.281 , pp. 231-243
    • Jollivet, P.1    Minet, Y.2    Nicolas, M.3    Vernaz, E.4
  • 5
    • 51249084136 scopus 로고    scopus 로고
    • The effect of radiation on the anaerobic corrosion of steel
    • Smart, N. R.; Rance, A. P.; Werme, L. O. The effect of radiation on the anaerobic corrosion of steel. J. Nucl. Mater. 2008, 379, 97-104.
    • (2008) J. Nucl. Mater , vol.379 , pp. 97-104
    • Smart, N.R.1    Rance, A.P.2    Werme, L.O.3
  • 6
    • 17344382736 scopus 로고    scopus 로고
    • Corrosion des surconteneurs de déchets, cas d'un surconteneur en acier faiblement allié.
    • Bataillon, C.; Musy, C.; Roy, M. Corrosion des surconteneurs de déchets, cas d'un surconteneur en acier faiblement allié. J. Phys. IV 2001, 11, 267-274.
    • (2001) J. Phys. IV , vol.11 , pp. 267-274
    • Bataillon, C.1    Musy, C.2    Roy, M.3
  • 7
    • 51449094181 scopus 로고    scopus 로고
    • Corrosion of iron and low alloyed steel within a water saturated brick of clay under anaerobic deep geological disposal conditions: An integrated experiment
    • Martin, F. A.; Bataillon, C.; Schlegel, M. L. Corrosion of iron and low alloyed steel within a water saturated brick of clay under anaerobic deep geological disposal conditions: An integrated experiment. J. Nucl. Mater. 2008, 379, 80-90.
    • (2008) J. Nucl. Mater , vol.379 , pp. 80-90
    • Martin, F.A.1    Bataillon, C.2    Schlegel, M.L.3
  • 8
    • 50549093288 scopus 로고    scopus 로고
    • Metal corrosion and argillite transformation at the water-saturated, high temperature iron-clay interface: A microscopic-scale study
    • Schlegel, M. L.; Bataillon, C.; Benhamida, K.; Blanc, C.; Menut, D.; Lacour, J.-L. Metal corrosion and argillite transformation at the water-saturated, high temperature iron-clay interface: a microscopic-scale study. Appl. Geochem. 2008, 23, 2619-2633.
    • (2008) Appl. Geochem , vol.23 , pp. 2619-2633
    • Schlegel, M.L.1    Bataillon, C.2    Benhamida, K.3    Blanc, C.4    Menut, D.5    Lacour, J.-L.6
  • 9
    • 13944269844 scopus 로고    scopus 로고
    • Long-term corrosion resistance of metallic reinforcements in concrete - a study of corrosion mechanisms based on archaeological artefacts
    • Chitty, W. J.; Dillmann, P.; L'Hostis, V.; Lombard, C. Long-term corrosion resistance of metallic reinforcements in concrete - a study of corrosion mechanisms based on archaeological artefacts. Corros. Sci. 2005, 47, 1555-1581.
    • (2005) Corros. Sci , vol.47 , pp. 1555-1581
    • Chitty, W.J.1    Dillmann, P.2    L'Hostis, V.3    Lombard, C.4
  • 12
    • 10044274161 scopus 로고    scopus 로고
    • Corrosion of iron archaeological artefacts in soil: Characterisation of the corrosion system
    • Neff, D.; Dillmann, P.; Bellot-Gurlet, L.; Berranger, G. Corrosion of iron archaeological artefacts in soil: characterisation of the corrosion system. Corros. Sci. 2005, 47, 515-535.
    • (2005) Corros. Sci , vol.47 , pp. 515-535
    • Neff, D.1    Dillmann, P.2    Bellot-Gurlet, L.3    Berranger, G.4
  • 13
    • 0002604513 scopus 로고
    • Phase diagrams depicting aqueous solubility of binary mineral systems
    • Lippmann, F. Phase diagrams depicting aqueous solubility of binary mineral systems. Neues Jahrb. Mineral., Abh. 1980, 139, 1-25.
    • (1980) Neues Jahrb. Mineral., Abh , vol.139 , pp. 1-25
    • Lippmann, F.1
  • 15
    • 0019715395 scopus 로고
    • Crystal-structure refinements of magnesite, calcite, rhodochrosite, siderite, smithonite, and dolomite, with discussion of some aspects of the stereochemistry of calcite type carbonates
    • Effenberger, H.; Mereiter, K.; Zemann, J. Crystal-structure refinements of magnesite, calcite, rhodochrosite, siderite, smithonite, and dolomite, with discussion of some aspects of the stereochemistry of calcite type carbonates. Z. Kristallogr. 1981, 156, 233-243.
    • (1981) Z. Kristallogr , vol.156 , pp. 233-243
    • Effenberger, H.1    Mereiter, K.2    Zemann, J.3
  • 16
    • 0038366113 scopus 로고    scopus 로고
    • Corrosion of iron under alternating wet and dry conditions
    • Dunn, D. S.; Bogart, M. B.; Brossia, C. S.; Cragnolino, G. A. Corrosion of iron under alternating wet and dry conditions. Corrosion 2000, 56, 470-481.
    • (2000) Corrosion , vol.56 , pp. 470-481
    • Dunn, D.S.1    Bogart, M.B.2    Brossia, C.S.3    Cragnolino, G.A.4
  • 17
    • 51249124452 scopus 로고    scopus 로고
    • Longterm corrosion behaviour of low-carbon steel in anoxic environment: Characterization of archaeological artefacts
    • Saheb, M.; Neff, D.; Dillmann, P.; Matthiesen, H.; Foy, E. Longterm corrosion behaviour of low-carbon steel in anoxic environment: characterization of archaeological artefacts. J. Nucl. Mater. 2008, 379, 118-123.
    • (2008) J. Nucl. Mater , vol.379 , pp. 118-123
    • Saheb, M.1    Neff, D.2    Dillmann, P.3    Matthiesen, H.4    Foy, E.5
  • 19
    • 33750050312 scopus 로고    scopus 로고
    • Raman imaging of ancient rust scales on archaeological iron artefacts for long-term atmospheric corrosion mechanisms study
    • Neff, D.; Bellot-Gurlet, L.; Dillmann, P.; Reguer, S.; Legrand, L. Raman imaging of ancient rust scales on archaeological iron artefacts for long-term atmospheric corrosion mechanisms study. J. Raman Spectrosc. 2006, 37, 1228-1237.
    • (2006) J. Raman Spectrosc , vol.37 , pp. 1228-1237
    • Neff, D.1    Bellot-Gurlet, L.2    Dillmann, P.3    Reguer, S.4    Legrand, L.5
  • 20
    • 33947157819 scopus 로고    scopus 로고
    • Iron corrosion in Callovo-Oxfordian argilite: From experiments to thermodynamic/ kinetic modelling
    • de Combarieu, G.; Barboux, P.; Minet, Y. Iron corrosion in Callovo-Oxfordian argilite: From experiments to thermodynamic/ kinetic modelling. Phys. Chem. Earth 2007, 32, 346-358.
    • (2007) Phys. Chem. Earth , vol.32 , pp. 346-358
    • de Combarieu, G.1    Barboux, P.2    Minet, Y.3
  • 21
    • 60349118492 scopus 로고    scopus 로고
    • 3 (chukanovite) as iron corrosion product: Synthesis and study by Fourier Transform Infrared Spectroscopy
    • 3 (chukanovite) as iron corrosion product: Synthesis and study by Fourier Transform Infrared Spectroscopy. Polyhedron 2009, 28, 749-756.
    • (2009) Polyhedron , vol.28 , pp. 749-756
    • Remazeilles, C.1    Refait, P.2
  • 22
    • 0022178921 scopus 로고
    • Partitioning of divalent transition elements between octahedral sheets of trioctahedral smectites and water
    • Decarreau, A. Partitioning of divalent transition elements between octahedral sheets of trioctahedral smectites and water. Geochim. Cosmochim. Acta 1985, 49, 1537-1544.
    • (1985) Geochim. Cosmochim. Acta , vol.49 , pp. 1537-1544
    • Decarreau, A.1
  • 24
    • 33746382233 scopus 로고    scopus 로고
    • Modelling iron-clay interactions in deep geological disposal conditions
    • Bildstein, O.; Trotignon, L.; Perronnet, M.; Jullien, M. Modelling iron-clay interactions in deep geological disposal conditions. Phys. Chem. Earth 2006, 31, 618-625.
    • (2006) Phys. Chem. Earth , vol.31 , pp. 618-625
    • Bildstein, O.1    Trotignon, L.2    Perronnet, M.3    Jullien, M.4
  • 25
    • 41149138802 scopus 로고    scopus 로고
    • Cation exchanged Fe(II) and Sr compared to other divalent cations (Ca, Mg) in the bure Callovian-Oxfordian formation: Implications for porewater composition modelling
    • Tournassat, C.; Lerouge, C.; Blanc, P.; Brendlé, J.; Greneche, J. M.; Touzelet, S.; Gaucher, E. C. Cation exchanged Fe(II) and Sr compared to other divalent cations (Ca, Mg) in the bure Callovian-Oxfordian formation: Implications for porewater composition modelling. Appl. Geochem. 2008, 23, 641-654.
    • (2008) Appl. Geochem , vol.23 , pp. 641-654
    • Tournassat, C.1    Lerouge, C.2    Blanc, P.3    Brendlé, J.4    Greneche, J.M.5    Touzelet, S.6    Gaucher, E.C.7
  • 26
    • 31644440157 scopus 로고    scopus 로고
    • Evidence for the nucleation and epitaxial growth of Zn phyllosilicate on montmorillonite
    • Schlegel, M. L.; Manceau, A. Evidence for the nucleation and epitaxial growth of Zn phyllosilicate on montmorillonite. Geochim. Cosmochim. Acta 2006, 70, 901-917.
    • (2006) Geochim. Cosmochim. Acta , vol.70 , pp. 901-917
    • Schlegel, M.L.1    Manceau, A.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.