Volumn 91, Issue 8, 2012, Pages 800-804

Fatigue strength of Ce-TZP/Al2O3 nanocomposite with different surfaces

Author keywords

bi axial flexure strength; dental composite; dental implant; dental restorations; surface treatment; zirconia

Indexed keywords

ALUMINUM OXIDE; BIOMATERIAL; CE TZP AL2O3; CE-TZP-AL2O3; CERIUM; DENTAL MATERIAL; HYDROFLUORIC ACID; NANOCOMPOSITE; RESIN; WATER; YTTRIA STABILIZED TETRAGONAL ZIRCONIA; YTTRIUM; ZIRCONIUM;

EID: 84864148577     PISSN: 00220345     EISSN: 15440591     Source Type: Journal    
DOI: 10.1177/0022034512452277     Document Type: Article
Times cited : (40)

References (28)
  • 1
    • 68549122693 scopus 로고    scopus 로고
    • Are ceramic implants a viable alternative to titanium implants? A systematic literature review
    • Andreiotelli M, Wenz HJ, Kohal RJ. Are ceramic implants a viable alternative to titanium implants? A systematic literature review. Clin Oral Implants Res. 2009 ; 20 (Suppl 4). 32-47
    • (2009) Clin Oral Implants Res , vol.20 , Issue.SUPPL. 4 , pp. 32-47
    • Andreiotelli, M.1    Wenz, H.J.2    Kohal, R.J.3
  • 2
    • 53549109459 scopus 로고    scopus 로고
    • Reliability and properties of core materials for all-ceramic dental restorations
    • Ban S. Reliability and properties of core materials for all-ceramic dental restorations. Jpn Dent Sci Rev. 2008 ; 44: 3-21
    • (2008) Jpn Dent Sci Rev , vol.44 , pp. 3-21
    • Ban, S.1
  • 3
    • 0025617576 scopus 로고
    • Influence of test method on failure stress of brittle dental materials
    • Ban S, Anusavice KJ. Influence of test method on failure stress of brittle dental materials. J Dent Res. 1990 ; 69: 1791-1799
    • (1990) J Dent Res , vol.69 , pp. 1791-1799
    • Ban, S.1    Anusavice, K.J.2
  • 4
    • 46749123800 scopus 로고    scopus 로고
    • Fracture toughness, strength and slow crack growth in a ceria stabilized zirconia-alumina nanocomposite for medical applications
    • Benzaid R, Chevalier J, Saadaoui M, Fantozzi G, Nawa M, Diaz LA, et al. Fracture toughness, strength and slow crack growth in a ceria stabilized zirconia-alumina nanocomposite for medical applications. Biomaterials. 2008 ; 29: 3636-3641
    • (2008) Biomaterials , vol.29 , pp. 3636-3641
    • Benzaid, R.1    Chevalier, J.2    Saadaoui, M.3    Fantozzi, G.4    Nawa, M.5    Diaz, L.A.6
  • 5
    • 0033225415 scopus 로고    scopus 로고
    • Subcritical crack propagation in 3Y-TZP ceramics: Static and cyclic fatigue
    • Chevalier J, Olagnon C, Fantozzi G. Subcritical crack propagation in 3Y-TZP ceramics: static and cyclic fatigue. J Am Ceram Soc. 1999 ; 82: 3129-3138 (Pubitemid 30519410)
    • (1999) Journal of the American Ceramic Society , vol.82 , Issue.11 , pp. 3129-3138
    • Chevalier, J.1    Olagnon, C.2    Fantozzi, G.3
  • 7
    • 84979455274 scopus 로고
    • Phase analysis in zirconia systems
    • Garvie RC, Nicholson PS. Phase analysis in zirconia systems. J Am Ceram Soc. 1972 ; 55: 303-305
    • (1972) J Am Ceram Soc , vol.55 , pp. 303-305
    • Garvie, R.C.1    Nicholson, P.S.2
  • 8
    • 6344240437 scopus 로고    scopus 로고
    • Property degradation of tetragonal zirconia induced by low-temperature defect reaction with water molecules
    • Guo X. Property degradation of tetragonal zirconia induced by low-temperature defect reaction with water molecules. Chem Mater. 2004 ; 16: 3988-3994
    • (2004) Chem Mater , vol.16 , pp. 3988-3994
    • Guo, X.1
  • 9
    • 0027001643 scopus 로고
    • Inhibition of low temperature degradation of tetragonal zirconia ceramics. A review
    • Hirano M. Inhibition of low temperature degradation of tetragonal zirconia ceramics: a review. Br Ceram Trans J. 1992 ; 91: 139-147 (Pubitemid 23620436)
    • (1992) British Ceramic Transactions , vol.91 , Issue.5 , pp. 139-147
    • Hirano Masanori1
  • 10
    • 77953556773 scopus 로고    scopus 로고
    • ISO 6872 Geneva, Switzerland: ISO Central Secretariat
    • ISO 6872 (2008). Dentistry-ceramic materials. Geneva, Switzerland: ISO Central Secretariat. http://www.iso.org/iso/iso-catalogue/catalogue-tc/ catalogue-detail.htm?csnumber=41385
    • (2008) Dentistry-ceramic Materials
  • 12
    • 71649097261 scopus 로고    scopus 로고
    • Influence of surface treatments on surface roughness, phase transformation, and biaxial flexure strength of Y-TZP ceramics
    • Karakoca S, Yilmaz H. Influence of surface treatments on surface roughness, phase transformation, and biaxial flexure strength of Y-TZP ceramics. J Biomed Mater Res B Appl Biomater. 2009 ; 91: 930-937
    • (2009) J Biomed Mater Res B Appl Biomater , vol.91 , pp. 930-937
    • Karakoca, S.1    Yilmaz, H.2
  • 13
    • 76949095895 scopus 로고    scopus 로고
    • Osseointegration of one-piece zirconia implants compared with a titanium implant of identical design: A histomorphometric study in the dog
    • Koch FP, Weng D, Kramer S, Biesterfeld S, Jahn-Eimermacher A, Wagner W. Osseointegration of one-piece zirconia implants compared with a titanium implant of identical design: a histomorphometric study in the dog. Clin Oral Implants Res. 2010 ; 21: 350-356
    • (2010) Clin Oral Implants Res , vol.21 , pp. 350-356
    • Koch, F.P.1    Weng, D.2    Kramer, S.3    Biesterfeld, S.4    Jahn-Eimermacher, A.5    Wagner, W.6
  • 16
    • 0032917811 scopus 로고    scopus 로고
    • Zirconia as a ceramic biomaterial
    • DOI 10.1016/S0142-9612(98)00010-6, PII S0142961298000106
    • Piconi C, Maccauro G. Zirconia as a ceramic biomaterial. Biomaterials. 1999 ; 20: 1-25 (Pubitemid 29002541)
    • (1999) Biomaterials , vol.20 , Issue.1 , pp. 1-25
    • Piconi, C.1    Maccauro, G.2
  • 17
    • 34250164925 scopus 로고    scopus 로고
    • The biaxial flexural strength and fatigue property of Lava™ Y-TZP dental ceramic
    • DOI 10.1016/j.dental.2006.09.003, PII S0109564106002454
    • Pittayachawan P, McDonald A, Petrie A, Knowles JC. The biaxial flexure strength and fatigue property of Lava Y-TZP dental ceramic. Dent Mater. 2007 ; 23: 1018-1029 (Pubitemid 46907965)
    • (2007) Dental Materials , vol.23 , Issue.8 , pp. 1018-1029
    • Pittayachawan, P.1    McDonald, A.2    Petrie, A.3    Knowles, J.C.4
  • 18
    • 60849115260 scopus 로고    scopus 로고
    • Flexure strength, fatigue life, and stress-induced phase transformation study of Y-TZP dental ceramic
    • Pittayachawan P, McDonald A, Young A, Knowles JC. Flexure strength, fatigue life, and stress-induced phase transformation study of Y-TZP dental ceramic. J Biomed Mater Res B Appl Biomater. 2009 ; 88: 366-377
    • (2009) J Biomed Mater Res B Appl Biomater , vol.88 , pp. 366-377
    • Pittayachawan, P.1    McDonald, A.2    Young, A.3    Knowles, J.C.4
  • 19
    • 46249121351 scopus 로고    scopus 로고
    • Mechanical properties of dental zirconia ceramics changed with sandblasting and heat treatment
    • Sato H, Yamada K, Pezzotti G, Nawa M, Ban S. Mechanical properties of dental zirconia ceramics changed with sandblasting and heat treatment. Dent Mater J. 2008 ; 27: 408-414
    • (2008) Dent Mater J , vol.27 , pp. 408-414
    • Sato, H.1    Yamada, K.2    Pezzotti, G.3    Nawa, M.4    Ban, S.5
  • 20
    • 0022077265 scopus 로고
    • Transformation of yttria-doped tetragonal ZrO2 polycrystals by annealing in water
    • Sato T, Shimada M. Transformation of yttria-doped tetragonal ZrO2 polycrystals by annealing in water. J Am Ceram Soc. 1985 ; 68: 356
    • (1985) J Am Ceram Soc , vol.68 , pp. 356
    • Sato, T.1    Shimada, M.2
  • 21
    • 0037809315 scopus 로고    scopus 로고
    • Bone response to zirconia ceramic implants: An experimental study in rabbits
    • Scarano A, Di Carlo F, Quaranta M, Piattelli A. Bone response to zirconia ceramic implants: an experimental study in rabbits. J Oral Implantol. 2003 ; 29: 8-12
    • (2003) J Oral Implantol , vol.29 , pp. 8-12
    • Scarano, A.1    Di Carlo, F.2    Quaranta, M.3    Piattelli, A.4
  • 22
    • 33947116243 scopus 로고    scopus 로고
    • In vitro lifetime of dental ceramics under cyclic loading in water
    • DOI 10.1016/j.biomaterials.2006.12.033, PII S0142961207000208
    • Studart AR, Filser F, Kocher P, Gauckler LJ. In vitro lifetime of dental ceramics under cyclic loading in water. Biomaterials. 2007 ; 28: 2695-2705 (Pubitemid 46413342)
    • (2007) Biomaterials , vol.28 , Issue.17 , pp. 2695-2705
    • Studart, A.R.1    Filser, F.2    Kocher, P.3    Gauckler, L.J.4
  • 23
    • 0012644095 scopus 로고
    • Grinding-induced tempering of ceramics containing metastable tetragonal zirconia
    • Swain MV. Grinding-induced tempering of ceramics containing metastable tetragonal zirconia. J Mater Sci Lett. 1980 ; 15: 1577-1579
    • (1980) J Mater Sci Lett , vol.15 , pp. 1577-1579
    • Swain, M.V.1
  • 26
    • 0029364035 scopus 로고
    • Cyclic mechanical fatigue of a feldspathic dental porcelain
    • White SN, Zhao XY, Zhaokun Y, Li ZC. Cyclic mechanical fatigue of a feldspathic dental porcelain. Int J Prosthodont. 1995 ; 8: 413-420
    • (1995) Int J Prosthodont , vol.8 , pp. 413-420
    • White, S.N.1    Zhao, X.Y.2    Zhaokun, Y.3    Li, Z.C.4
  • 27
    • 0029421177 scopus 로고
    • Tensile fatigue strength of light cure composite resins for posterior teeth
    • Yamamoto M, Takahashi H. Tensile fatigue strength of light cure composite resins for posterior teeth. Dent Mater J. 1995 ; 14: 175-184
    • (1995) Dent Mater J , vol.14 , pp. 175-184
    • Yamamoto, M.1    Takahashi, H.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.