메뉴 건너뛰기




Volumn 21, Issue 1, 2012, Pages 22-27

Fatigue and Fracture Resistance of Zirconia Crowns Prepared with Different Finish Line Designs

Author keywords

Design; Fatigue; Finish line; Fracture resistance; Margin; SEM; Strength; Zirconia

Indexed keywords

ZIRCONIUM; ZIRCONIUM OXIDE;

EID: 84855965907     PISSN: 1059941X     EISSN: 1532849X     Source Type: Journal    
DOI: 10.1111/j.1532-849X.2011.00787.x     Document Type: Article
Times cited : (33)

References (28)
  • 1
    • 59149092803 scopus 로고    scopus 로고
    • Bridging the gap between clinical failure and laboratory fracture strength tests using a fractographic approach
    • Aboushelib MN, Feilzer AJ, Kleverlaan CJ: Bridging the gap between clinical failure and laboratory fracture strength tests using a fractographic approach. Dent Mater 2009;25:383-391
    • (2009) Dent Mater , vol.25 , pp. 383-391
    • Aboushelib, M.N.1    Feilzer, A.J.2    Kleverlaan, C.J.3
  • 2
    • 77957268841 scopus 로고    scopus 로고
    • Influence of framework color and layering technique on the final color of zirconia veneered restorations
    • Aboushelib MN, Dozic A, Liem JK: Influence of framework color and layering technique on the final color of zirconia veneered restorations. Quintessence Int 2010;41:84-89
    • (2010) Quintessence Int , vol.41 , pp. 84-89
    • Aboushelib, M.N.1    Dozic, A.2    Liem, J.K.3
  • 4
    • 25144511110 scopus 로고    scopus 로고
    • Microtensile bond strength of different components of core veneered all-ceramic restorations
    • Aboushelib MN, de Jager N, Kleverlaan CJ, et al: Microtensile bond strength of different components of core veneered all-ceramic restorations. Dent Mater 2005;21:984-991
    • (2005) Dent Mater , vol.21 , pp. 984-991
    • Aboushelib, M.N.1    de Jager, N.2    Kleverlaan, C.J.3
  • 5
    • 0021519062 scopus 로고
    • Effect of metal design on marginal distortion of metal-ceramic crowns
    • DeHoff PH, Anusavice KJ: Effect of metal design on marginal distortion of metal-ceramic crowns. J Dent Res 1984;63: 1327-1331
    • (1984) J Dent Res , vol.63 , pp. 1327-1331
    • DeHoff, P.H.1    Anusavice, K.J.2
  • 6
    • 43049144663 scopus 로고    scopus 로고
    • The effect of finish line preparation and layer thickness on the failure load and fractography of ZrO2 copings
    • Reich S, Petschelt A, Lohbauer U: The effect of finish line preparation and layer thickness on the failure load and fractography of ZrO2 copings. J Prosthet Dent 2008;99: 369-376
    • (2008) J Prosthet Dent , vol.99 , pp. 369-376
    • Reich, S.1    Petschelt, A.2    Lohbauer, U.3
  • 7
    • 34250185998 scopus 로고    scopus 로고
    • Effect of loading method on the fracture mechanics of two layered all-ceramic restorative systems
    • Aboushelib MN, de Jager N, Kleverlaan CJ, et al: Effect of loading method on the fracture mechanics of two layered all-ceramic restorative systems. Dent Mater 2007;23:952-959
    • (2007) Dent Mater , vol.23 , pp. 952-959
    • Aboushelib, M.N.1    de Jager, N.2    Kleverlaan, C.J.3
  • 8
    • 23144462161 scopus 로고    scopus 로고
    • Nanostructured ceramic oxides with a slow crack growth resistance close to covalent materials
    • Chevalier J, Deville S, Fantozzi G, et al: Nanostructured ceramic oxides with a slow crack growth resistance close to covalent materials. Nano Lett 2005;5:1297-1301
    • (2005) Nano Lett , vol.5 , pp. 1297-1301
    • Chevalier, J.1    Deville, S.2    Fantozzi, G.3
  • 9
    • 12444332060 scopus 로고    scopus 로고
    • fracture behavior of lithia disilicate- and leucite-based ceramics
    • Bona AD, Mecholsky JJ, Anusavice KJ: fracture behavior of lithia disilicate- and leucite-based ceramics. Dent Mater 2004; 20:956-962
    • (2004) Dent Mater , vol.20 , pp. 956-962
    • Bona, A.D.1    Mecholsky, J.J.2    Anusavice, K.J.3
  • 10
    • 0029318343 scopus 로고
    • Failure of all-ceramic fixed partial denture in vitro and in vivo: analysis and modeling
    • Kelly J, Tesk JA: Failure of all-ceramic fixed partial denture in vitro and in vivo: analysis and modeling. J Dent Res 1995;74: 1253-1258
    • (1995) J Dent Res , vol.74 , pp. 1253-1258
    • Kelly, J.1    Tesk, J.A.2
  • 11
    • 0033225415 scopus 로고    scopus 로고
    • Subcritical crack propagation in 3Y-TZP ceramics: static and cyclic fatigue
    • Chevalier J, Olagnon C, Fantozzi G: Subcritical crack propagation in 3Y-TZP ceramics: static and cyclic fatigue. J Am Ceram Soc 1999;82:3129-3138
    • (1999) J Am Ceram Soc , vol.82 , pp. 3129-3138
    • Chevalier, J.1    Olagnon, C.2    Fantozzi, G.3
  • 12
    • 69549084939 scopus 로고    scopus 로고
    • Influence of CAM vs. CAD/CAM scanning methods and finish line of tooth preparation in the vertical misfit of zirconia bridge structures
    • Castillo de Oyague R, Sanchez-Jorge MI, Sanchez-Turrion A, et al: Influence of CAM vs. CAD/CAM scanning methods and finish line of tooth preparation in the vertical misfit of zirconia bridge structures. Am J Dent 2009;22:79-83
    • (2009) Am J Dent , vol.22 , pp. 79-83
    • Castillo de Oyague, R.1    Sanchez-Jorge, M.I.2    Sanchez-Turrion, A.3
  • 13
    • 0036634261 scopus 로고    scopus 로고
    • Finite element analysis studies of an all-ceramic crown on a first premolar
    • Proos KA, Swain MV, Ironside J, et al: Finite element analysis studies of an all-ceramic crown on a first premolar. Int J Prosthodont 2002;15:404-412
    • (2002) Int J Prosthodont , vol.15 , pp. 404-412
    • Proos, K.A.1    Swain, M.V.2    Ironside, J.3
  • 15
    • 0141516401 scopus 로고    scopus 로고
    • Influence of margin design and taper abutment angle on a restored crown of a first premolar using finite element analysis
    • Proos KA, Swain MV, Ironside J, et al: Influence of margin design and taper abutment angle on a restored crown of a first premolar using finite element analysis. Int J Prosthodont 2003;16:442-449
    • (2003) Int J Prosthodont , vol.16 , pp. 442-449
    • Proos, K.A.1    Swain, M.V.2    Ironside, J.3
  • 16
    • 0033227159 scopus 로고    scopus 로고
    • Effect of margin design, cement polymerization, and angle of loading on stress in porcelain veneers
    • Troedson M, Derand T: Effect of margin design, cement polymerization, and angle of loading on stress in porcelain veneers. J Prosthet Dent 1999;82:518-524
    • (1999) J Prosthet Dent , vol.82 , pp. 518-524
    • Troedson, M.1    Derand, T.2
  • 17
    • 1942468620 scopus 로고    scopus 로고
    • Strength, reliability and mode of fracture of bilayered porcelain/zirconia (Y-TZP) dental ceramics
    • Guazzato M, Proos K, Quach L, et al: Strength, reliability and mode of fracture of bilayered porcelain/zirconia (Y-TZP) dental ceramics. Biomaterials 2004;25:5045-5052
    • (2004) Biomaterials , vol.25 , pp. 5045-5052
    • Guazzato, M.1    Proos, K.2    Quach, L.3
  • 18
    • 0027604534 scopus 로고
    • The effect of finish line form and luting agent on the breaking strength of Dicor crowns
    • Bernal G, Jones RM, Brown DT, et al: The effect of finish line form and luting agent on the breaking strength of Dicor crowns. Int J Prosthodont 1993;6:286-290
    • (1993) Int J Prosthodont , vol.6 , pp. 286-290
    • Bernal, G.1    Jones, R.M.2    Brown, D.T.3
  • 19
    • 46249088169 scopus 로고    scopus 로고
    • Effect of preparation design on the fracture resistance of zirconia crown copings
    • Beuer F, Aggstaller H, Edelhoff D, et al: Effect of preparation design on the fracture resistance of zirconia crown copings. Dent Mater J 2008;27:362-367
    • (2008) Dent Mater J , vol.27 , pp. 362-367
    • Beuer, F.1    Aggstaller, H.2    Edelhoff, D.3
  • 20
    • 25144475575 scopus 로고    scopus 로고
    • Fractographic analyses of three ceramic whole crown restoration failures
    • Quinn JB, Quinn GD, Kelly JR, et al: Fractographic analyses of three ceramic whole crown restoration failures. Dent Mater 2005;21:920-929
    • (2005) Dent Mater , vol.21 , pp. 920-929
    • Quinn, J.B.1    Quinn, G.D.2    Kelly, J.R.3
  • 21
    • 45049087586 scopus 로고    scopus 로고
    • Fractographic failure analysis of a Procera AllCeram crown using stereo and scanning electron microscopy
    • Scherrer SS, Quinn GD, Quinn JB: Fractographic failure analysis of a Procera AllCeram crown using stereo and scanning electron microscopy. Dent Mater 2008;24:1107-1113
    • (2008) Dent Mater , vol.24 , pp. 1107-1113
    • Scherrer, S.S.1    Quinn, G.D.2    Quinn, J.B.3
  • 22
    • 45049088335 scopus 로고    scopus 로고
    • Fractographic analyses of zirconia-based fixed partial dentures
    • Taskonak B, Yan J, Mecholsky JJ, Jr., et al: Fractographic analyses of zirconia-based fixed partial dentures. Dent Mater 2008;24:1077-1082
    • (2008) Dent Mater , vol.24 , pp. 1077-1082
    • Taskonak, B.1    Yan, J.2    Mecholsky Jr, J.J.3
  • 23
    • 0036561773 scopus 로고    scopus 로고
    • Tooth structure removal associated with various preparation designs for anterior teeth
    • Edelhoff D, Sorensen JA: Tooth structure removal associated with various preparation designs for anterior teeth. J Prosthet Dent 2002;87:503-509
    • (2002) J Prosthet Dent , vol.87 , pp. 503-509
    • Edelhoff, D.1    Sorensen, J.A.2
  • 24
    • 33646228872 scopus 로고    scopus 로고
    • Marginal adaptation of Cerec 3 CAD/CAM composite crowns using two different finish line preparation designs
    • Akbar JH, Petrie CS, Walker MP, et al: Marginal adaptation of Cerec 3 CAD/CAM composite crowns using two different finish line preparation designs. J Prosthodont 2006;15:155-163
    • (2006) J Prosthodont , vol.15 , pp. 155-163
    • Akbar, J.H.1    Petrie, C.S.2    Walker, M.P.3
  • 25
    • 4444369817 scopus 로고    scopus 로고
    • Vertical marginal discrepancy of ceramic copings with different ceramic materials, finish lines, and luting agents: an in vitro evaluation
    • Quintas AF, Oliveira F, Bottino MA: Vertical marginal discrepancy of ceramic copings with different ceramic materials, finish lines, and luting agents: an in vitro evaluation. J Prosthet Dent 2004;92:250-257
    • (2004) J Prosthet Dent , vol.92 , pp. 250-257
    • Quintas, A.F.1    Oliveira, F.2    Bottino, M.A.3
  • 26
    • 33746623731 scopus 로고    scopus 로고
    • Microtensile bond strength of different components of core veneered all-ceramic restorations: Part II: zirconia veneering ceramics
    • Aboushelib MN, Kleverlaan CJ, Feilzer AJ: Microtensile bond strength of different components of core veneered all-ceramic restorations: Part II: zirconia veneering ceramics. Dent Mater 2006;22:857-863
    • (2006) Dent Mater , vol.22 , pp. 857-863
    • Aboushelib, M.N.1    Kleverlaan, C.J.2    Feilzer, A.J.3
  • 27
    • 40749115551 scopus 로고    scopus 로고
    • Strength influencing variables on CAD/CAM zirconia frameworks
    • Wang H, Aboushelib MN, Feilzer AJ: Strength influencing variables on CAD/CAM zirconia frameworks. Dent Mater 2008;24:633-638
    • (2008) Dent Mater , vol.24 , pp. 633-638
    • Wang, H.1    Aboushelib, M.N.2    Feilzer, A.J.3
  • 28
    • 48749100438 scopus 로고    scopus 로고
    • The effect of all-ceramic and porcelain-fused-to-metal restorations on marginal peri-implant soft tissue color: a randomized controlled clinical trial
    • Jung RE, Holderegger C, Sailer I, et al: The effect of all-ceramic and porcelain-fused-to-metal restorations on marginal peri-implant soft tissue color: a randomized controlled clinical trial. Int J Periodontics Restorative Dent 2008;28:357-365
    • (2008) Int J Periodontics Restorative Dent , vol.28 , pp. 357-365
    • Jung, R.E.1    Holderegger, C.2    Sailer, I.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.