Volumn 87, Issue 1, 2008, Pages 139-145

Prestresses in bilayered all-ceramic restorations

Author keywords

Ceramic; Finite element analysis; Fractography; Zirconia

Indexed keywords

BIOCERAMICS; BOND STRENGTH (MATERIALS); BUILDING MATERIALS; CERAMIC MATERIALS; DELAMINATION; FINITE ELEMENT METHOD; FRACTOGRAPHY; FRACTURE MECHANICS; ICE; IMAGING TECHNIQUES; MATERIALS TESTING; METALS; MICROSCOPIC EXAMINATION; REPAIR; RESTORATION; SAFETY ENGINEERING; TECHNOLOGY; THERMAL EXPANSION; THERMAL SPRAYING; THERMAL STRESS; VENEERS;

EID: 52449101679     PISSN: 15524973     EISSN: 15524981     Source Type: Journal    
DOI: 10.1002/jbm.b.31083     Document Type: Article
Times cited : (68)

References (21)
  • 1
    • 0024760939 scopus 로고
    • Fracture-surface analysis of dental ceramics
    • Kelly J, Campbell S, Bowen H. Fracture-surface analysis of dental ceramics. J Prosthet Dent 1989;62:536-541.
    • (1989) J Prosthet Dent , vol.62 , pp. 536-541
    • Kelly, J.1    Campbell, S.2    Bowen, H.3
  • 2
    • 16344387546 scopus 로고    scopus 로고
    • Fracture resistance of yttrium oxide partially-stabilized zirconia all-ceramic bridges after veneering and mechanical fatigue testing
    • Sundh A, Molin M, Sjogren G. Fracture resistance of yttrium oxide partially-stabilized zirconia all-ceramic bridges after veneering and mechanical fatigue testing. Dent Mater 2005;21:476-482.
    • (2005) Dent Mater , vol.21 , pp. 476-482
    • Sundh, A.1    Molin, M.2    Sjogren, G.3
  • 3
    • 84985100223 scopus 로고    scopus 로고
    • Liu S-Y, Chen I-W. Fatigue of yttria-stabilized zirconia. I. Fatigue damage, fracture origins, and lifetime prediction. J Am Ceram Soc 19914:1197-1205.
    • Liu S-Y, Chen I-W. Fatigue of yttria-stabilized zirconia. I. Fatigue damage, fracture origins, and lifetime prediction. J Am Ceram Soc 19914:1197-1205.
  • 4
    • 36849094920 scopus 로고    scopus 로고
    • The all-ceramic CAM system by degussa dental
    • Volkl L. Cercon® - The all-ceramic CAM system by degussa dental. Quintessencia 2001;52:811-814.
    • (2001) Quintessencia , vol.52 , pp. 811-814
    • Cercon®, V.L.1
  • 5
    • 0242289420 scopus 로고    scopus 로고
    • The influence of the veneering porcelain and different surface treatments on the biaxial flexural strength of a heat-pressed ceramic
    • Isgro G, Pallav P, van der Zel JM, Feilzer AJ. The influence of the veneering porcelain and different surface treatments on the biaxial flexural strength of a heat-pressed ceramic. J Prosthet Dent 2003;90:465-473.
    • (2003) J Prosthet Dent , vol.90 , pp. 465-473
    • Isgro, G.1    Pallav, P.2    van der Zel, J.M.3    Feilzer, A.J.4
  • 6
    • 0025378845 scopus 로고
    • Transient and residual stress in a porcelain-metal strip
    • Asaoka K, Tesk JA. Transient and residual stress in a porcelain-metal strip. J Dent Res 1990;69:463-469.
    • (1990) J Dent Res , vol.69 , pp. 463-469
    • Asaoka, K.1    Tesk, J.A.2
  • 7
    • 17044429404 scopus 로고    scopus 로고
    • The in-vitro clinical failure of all-ceramic crowns and the connector area of fixed partial dentures: The influence of interfacial surface roughness
    • Fleming GJ, Nolan L, Harris JJ. The in-vitro clinical failure of all-ceramic crowns and the connector area of fixed partial dentures: The influence of interfacial surface roughness. J Dent 2005;33:405-412.
    • (2005) J Dent , vol.33 , pp. 405-412
    • Fleming, G.J.1    Nolan, L.2    Harris, J.J.3
  • 8
    • 33745865941 scopus 로고    scopus 로고
    • The in vitro failure of all-ceramic crowns and the connector area of fixed partial dentures using bilayered ceramic specimens: The influence of core to dentine thickness ratio
    • Fleming GJP, Dickens M, Thomas LJ, Harris JJ. The in vitro failure of all-ceramic crowns and the connector area of fixed partial dentures using bilayered ceramic specimens: The influence of core to dentine thickness ratio. Dent Mater 2006;22:1-7.
    • (2006) Dent Mater , vol.22 , pp. 1-7
    • Fleming, G.J.P.1    Dickens, M.2    Thomas, L.J.3    Harris, J.J.4
  • 9
    • 13444311681 scopus 로고    scopus 로고
    • The influence of design parameters on the FEA-determined stress distribution in CAD-CAM produced all-ceramic dental crowns
    • De Jager N, Pallav P, Feilzer AJ. The influence of design parameters on the FEA-determined stress distribution in CAD-CAM produced all-ceramic dental crowns. Dent Mater 2005;21:242-251.
    • (2005) Dent Mater , vol.21 , pp. 242-251
    • De Jager, N.1    Pallav, P.2    Feilzer, A.J.3
  • 10
    • 18544386835 scopus 로고    scopus 로고
    • Twiggs SW, Mackert JJR, Oxford AL, Ergle JW, Lockwood PE. Isothermal phase transformations of a dental porcelain. Dent Mater 2005;21:580-584.
    • Twiggs SW, Mackert JJR, Oxford AL, Ergle JW, Lockwood PE. Isothermal phase transformations of a dental porcelain. Dent Mater 2005;21:580-584.
  • 12
    • 0028709614 scopus 로고
    • Fracture surface characterization of clinically failed all-ceramic crowns
    • Thompson JY, Anusavice KJ, Naman A, Morris HF. Fracture surface characterization of clinically failed all-ceramic crowns. J Dent Res 1994;73:1824-1832.
    • (1994) J Dent Res , vol.73 , pp. 1824-1832
    • Thompson, J.Y.1    Anusavice, K.J.2    Naman, A.3    Morris, H.F.4
  • 13
    • 27644503075 scopus 로고    scopus 로고
    • Stress distributions in thin bilayer discs subjected to ball-on-ring tests
    • Hsueh C, Lance M, Ferber M. Stress distributions in thin bilayer discs subjected to ball-on-ring tests. J Am Ceram Soc 2005;88:1687-1689.
    • (2005) J Am Ceram Soc , vol.88 , pp. 1687-1689
    • Hsueh, C.1    Lance, M.2    Ferber, M.3
  • 14
    • 0032531287 scopus 로고    scopus 로고
    • Thermal incompatibility analysis of metal-ceramic systems based on flexural displacement data
    • DeHoff PH, Anusavice KJ, Hojjatie B. Thermal incompatibility analysis of metal-ceramic systems based on flexural displacement data. J Biomed Mater Res 1998;41:614-623.
    • (1998) J Biomed Mater Res , vol.41 , pp. 614-623
    • DeHoff, P.H.1    Anusavice, K.J.2    Hojjatie, B.3
  • 15
    • 25144475575 scopus 로고    scopus 로고
    • Fractographic analyses of three ceramic whole crown restoration failures
    • Quinn JB, Quinn GD, Kelly JR, Scherrer SS. Fractographic analyses of three ceramic whole crown restoration failures. Dent Mater 2005;21:920-929.
    • (2005) Dent Mater , vol.21 , pp. 920-929
    • Quinn, J.B.1    Quinn, G.D.2    Kelly, J.R.3    Scherrer, S.S.4
  • 16
    • 25144511110 scopus 로고    scopus 로고
    • Microtensile bond strength of different components of core veneered all-ceramic restorations
    • Aboushelib MN, de Jager N, Kleverlaan CJ, Feilzer AJ. Microtensile bond strength of different components of core veneered all-ceramic restorations. Dent Mater 2005;21:984-991.
    • (2005) Dent Mater , vol.21 , pp. 984-991
    • Aboushelib, M.N.1    de Jager, N.2    Kleverlaan, C.J.3    Feilzer, A.J.4
  • 18
    • 33746623731 scopus 로고    scopus 로고
    • Microtensile bond strength of different components of core veneered all-ceramic restorations. Part II: Zirconia veneering Ceramics
    • Aboushelib MN, Kleverlaan CJ, Feilzer AJ. Microtensile bond strength of different components of core veneered all-ceramic restorations. Part II: Zirconia veneering Ceramics. Dent Mater 2005;22:857-863.
    • (2005) Dent Mater , vol.22 , pp. 857-863
    • Aboushelib, M.N.1    Kleverlaan, C.J.2    Feilzer, A.J.3
  • 19
    • 1842850520 scopus 로고    scopus 로고
    • Strength, reliability, and mode of fracture of bilayered porcelain/core ceramics
    • Guazzato M, Proos K, Sara G, Swain MV. Strength, reliability, and mode of fracture of bilayered porcelain/core ceramics. Int J Prosthodont 2004;17:142-149.
    • (2004) Int J Prosthodont , vol.17 , pp. 142-149
    • Guazzato, M.1    Proos, K.2    Sara, G.3    Swain, M.V.4
  • 20
    • 3242741859 scopus 로고    scopus 로고
    • A comparison of fracture strength of yttrium-oxide-partially-stabilized zirconia ceramic crowns with varying core thickness, shapes, and veneer ceramics
    • Sundh A, Sjogren G. A comparison of fracture strength of yttrium-oxide-partially-stabilized zirconia ceramic crowns with varying core thickness, shapes, and veneer ceramics. J Oral Rehabil 2004;31:682-688.
    • (2004) J Oral Rehabil , vol.31 , pp. 682-688
    • Sundh, A.1    Sjogren, G.2
  • 21
    • 22644448001 scopus 로고    scopus 로고
    • Flexural strength of a layered zirconia and porcelain dental all-ceramic system
    • White SN, Miklus VG, McLaren EA, Lang LA, Caputo AA. Flexural strength of a layered zirconia and porcelain dental all-ceramic system. J Prosthet Dent 2005;94:125-131.
    • (2005) J Prosthet Dent , vol.94 , pp. 125-131
    • White, S.N.1    Miklus, V.G.2    McLaren, E.A.3    Lang, L.A.4    Caputo, A.A.5


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.