메뉴 건너뛰기




Volumn 6, Issue , 2012, Pages 120-127

Measuring residual stress in ceramic zirconia-porcelain dental crowns by nanoindentation

Author keywords

Dental crowns; Nanoindentation; Porcelain; Residual stress; Zirconia

Indexed keywords

CERAMIC CROWNS; CERAMIC DENTAL CROWNS; COMPLEX SHAPES; CRITICAL LOCATION; DENTAL CROWNS; DISTRIBUTION OF RESIDUAL STRESS; FINITE ELEMENT MODELING; MEASURED RESULTS; NANOINDENTATION IMPRESSIONS; NANOINDENTATION TESTS; PILE-UPS; SCANNING PROBE MICROSCOPE;

EID: 82955207630     PISSN: 17516161     EISSN: 18780180     Source Type: Journal    
DOI: 10.1016/j.jmbbm.2011.11.006     Document Type: Article
Times cited : (56)

References (41)
  • 2
    • 79952381176 scopus 로고    scopus 로고
    • Measurement and analysis of residual stresses in zirconia dental composites using micro X-ray.
    • Dissertation, Oklahoma State University.
    • Bale, H.A., 2010. Measurement and analysis of residual stresses in zirconia dental composites using micro X-ray. Dissertation, Oklahoma State University.
    • (2010)
    • Bale, H.A.1
  • 3
    • 84856388115 scopus 로고    scopus 로고
    • Microbeam X-ray grain averaged residual stress in dental ceramics.
    • In: 35th International Conference on Advanced Ceramics & Composites, ICACC, FL, USA.
    • Bale, H.A., Allahkarami, M., Tamura, N., Hanan, J.C., 2011. Microbeam X-ray grain averaged residual stress in dental ceramics. In: 35th International Conference on Advanced Ceramics & Composites, ICACC, FL, USA.
    • (2011)
    • Bale, H.A.1    Allahkarami, M.2    Tamura, N.3    Hanan, J.C.4
  • 5
    • 0030105652 scopus 로고    scopus 로고
    • Influence of stress on the measurement of mechanical properties using nanoindentation: part II. Finite element simulations
    • Bolshakov A., Oliver W.C., Pharr G.M. Influence of stress on the measurement of mechanical properties using nanoindentation: part II. Finite element simulations. J. Mater. Res. 1996, 11(3):760-768.
    • (1996) J. Mater. Res. , vol.11 , Issue.3 , pp. 760-768
    • Bolshakov, A.1    Oliver, W.C.2    Pharr, G.M.3
  • 6
    • 0035902678 scopus 로고    scopus 로고
    • On the determination of residual stress and strain fields by sharp indentation testing part II: experimental investigation
    • Carlsson S., Larsson P.L. On the determination of residual stress and strain fields by sharp indentation testing part II: experimental investigation. Acta Mater. 2001, 49:2193-2203.
    • (2001) Acta Mater. , vol.49 , pp. 2193-2203
    • Carlsson, S.1    Larsson, P.L.2
  • 8
    • 11244316444 scopus 로고    scopus 로고
    • Analysis of sharp-tip-indentation load-depth curve for contact area determination taking account pile-up and sink-in effects
    • Choi Y., Lee H.S., Kwon D. Analysis of sharp-tip-indentation load-depth curve for contact area determination taking account pile-up and sink-in effects. J. Mater. Res. 2004, 19(11):3307-3315.
    • (2004) J. Mater. Res. , vol.19 , Issue.11 , pp. 3307-3315
    • Choi, Y.1    Lee, H.S.2    Kwon, D.3
  • 9
    • 0024546336 scopus 로고
    • Mechanical properties and short-term in-vivo evaluation of yttrium-oxide-partially-stablized zirconia
    • Christel P., Munier A., Heller M., Torre J.P., Peille C.N. Mechanical properties and short-term in-vivo evaluation of yttrium-oxide-partially-stablized zirconia. J. Biomed. Mater. Res. 1989, 23(1):45-61.
    • (1989) J. Biomed. Mater. Res. , vol.23 , Issue.1 , pp. 45-61
    • Christel, P.1    Munier, A.2    Heller, M.3    Torre, J.P.4    Peille, C.N.5
  • 12
    • 38349192796 scopus 로고    scopus 로고
    • State of the art of zircionia for dental application
    • Denry I., Kelly J.R. State of the art of zircionia for dental application. Dent. Mater. 2008, 24:299-307.
    • (2008) Dent. Mater. , vol.24 , pp. 299-307
    • Denry, I.1    Kelly, J.R.2
  • 13
    • 20444433625 scopus 로고    scopus 로고
    • Influence of annealing temperature on the strength of dental glass ceramic materials
    • Fischer H., Hemelik M., Telle R., Mark R. Influence of annealing temperature on the strength of dental glass ceramic materials. Dent. Mater. 2005, 21:671-677.
    • (2005) Dent. Mater. , vol.21 , pp. 671-677
    • Fischer, H.1    Hemelik, M.2    Telle, R.3    Mark, R.4
  • 14
    • 41849125937 scopus 로고    scopus 로고
    • Flexural strength of veneering ceramics for zirconia
    • Fischer J., Stawarczyk B., Hammerle C.H.F. Flexural strength of veneering ceramics for zirconia. J. Dent. 2008, 36:316-321.
    • (2008) J. Dent. , vol.36 , pp. 316-321
    • Fischer, J.1    Stawarczyk, B.2    Hammerle, C.H.F.3
  • 15
    • 63149192830 scopus 로고    scopus 로고
    • Nanoindentation of yttria dopped zirconia: effect of crystallographic structure on deformation mechanisms
    • Gaillard Y., Anglada M., Jimenez-Pique E. Nanoindentation of yttria dopped zirconia: effect of crystallographic structure on deformation mechanisms. J. Mater. Res. 2009, 24(3):719-727.
    • (2009) J. Mater. Res. , vol.24 , Issue.3 , pp. 719-727
    • Gaillard, Y.1    Anglada, M.2    Jimenez-Pique, E.3
  • 16
    • 0000081071 scopus 로고
    • Vickers and knoop indentation behavior of cubic and partially stabilized zirconia crystals
    • Gogotsi G.A., Dub S.N., Lomonova E.E., Ozersky B.I. Vickers and knoop indentation behavior of cubic and partially stabilized zirconia crystals. J. Eur. Ceram. Soc. 1995, 15:405-413.
    • (1995) J. Eur. Ceram. Soc. , vol.15 , pp. 405-413
    • Gogotsi, G.A.1    Dub, S.N.2    Lomonova, E.E.3    Ozersky, B.I.4
  • 17
    • 1642437931 scopus 로고    scopus 로고
    • Analysis of the nanoindentation data measured with a Berkovich indenter for brittle materials: effect of the residual contact stress
    • Gong J., Miao H., Peng Z. Analysis of the nanoindentation data measured with a Berkovich indenter for brittle materials: effect of the residual contact stress. Acta Mater. 2004, 52:785-793.
    • (2004) Acta Mater. , vol.52 , pp. 785-793
    • Gong, J.1    Miao, H.2    Peng, Z.3
  • 18
    • 67349093999 scopus 로고    scopus 로고
    • Effect of abrasive grinding on the strength of Y-TZP
    • Ho C.J., Liu H.C., Tuan W.H.M. Effect of abrasive grinding on the strength of Y-TZP. J. Eur. Ceram. Soc. 2009, 29:2665-2669.
    • (2009) J. Eur. Ceram. Soc. , vol.29 , pp. 2665-2669
    • Ho, C.J.1    Liu, H.C.2    Tuan, W.H.M.3
  • 19
    • 37049008682 scopus 로고    scopus 로고
    • Analysis of layer-thickness effects in bilayer dental ceramics subjected to thermal stresses and ring on ring tests
    • Hsueh C.H., Thompson G.A., Jadaan O.M., Wereszczak A.A., Becher P.F. Analysis of layer-thickness effects in bilayer dental ceramics subjected to thermal stresses and ring on ring tests. Dent. Mater. 2008, 24:9-19.
    • (2008) Dent. Mater. , vol.24 , pp. 9-19
    • Hsueh, C.H.1    Thompson, G.A.2    Jadaan, O.M.3    Wereszczak, A.A.4    Becher, P.F.5
  • 20
    • 85040956871 scopus 로고
    • Cambridge University Press, Cambridge
    • Johnson K.L. Contact Mechanics 1985, Cambridge University Press, Cambridge.
    • (1985) Contact Mechanics
    • Johnson, K.L.1
  • 21
    • 69249235701 scopus 로고    scopus 로고
    • Strength and grinding residual stresses of Y-TZP with duplex microstructures
    • Juy A., Anglada M. Strength and grinding residual stresses of Y-TZP with duplex microstructures. Eng. Fail. Anal. 2009, 16:2586-2597.
    • (2009) Eng. Fail. Anal. , vol.16 , pp. 2586-2597
    • Juy, A.1    Anglada, M.2
  • 22
    • 0034806288 scopus 로고    scopus 로고
    • Mechanical properties of glass-only porcelains prepared by the use of two feldspathic frits with different thermal properties
    • Kon M., O'Brian W.J., Rasmussen S.T., Asaoka K. Mechanical properties of glass-only porcelains prepared by the use of two feldspathic frits with different thermal properties. J. Dent. Res. 2001, 80(8):1758-1763.
    • (2001) J. Dent. Res. , vol.80 , Issue.8 , pp. 1758-1763
    • Kon, M.1    O'Brian, W.J.2    Rasmussen, S.T.3    Asaoka, K.4
  • 24
    • 33745810915 scopus 로고    scopus 로고
    • All-ceramic two and five-unit implant-supported reconstructions, a randomized, prospective clinical trial
    • Larsson C., Von S.P., Sunzel B., Nilner K. All-ceramic two and five-unit implant-supported reconstructions, a randomized, prospective clinical trial. Swed. Dent. J. 2006, 30:45-53.
    • (2006) Swed. Dent. J. , vol.30 , pp. 45-53
    • Larsson, C.1    Von, S.P.2    Sunzel, B.3    Nilner, K.4
  • 25
    • 79953247025 scopus 로고    scopus 로고
    • Residual stress measurement in veneering ceramic by hole-drilling
    • Mainjot A.K., Schajer G.S., Vanheusden A.J., Sadoun M.J. Residual stress measurement in veneering ceramic by hole-drilling. Dent. Mater. 2011, 27:439-444.
    • (2011) Dent. Mater. , vol.27 , pp. 439-444
    • Mainjot, A.K.1    Schajer, G.S.2    Vanheusden, A.J.3    Sadoun, M.J.4
  • 26
    • 0026875935 scopus 로고
    • An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments
    • Oliver W.C., Pharr G.M. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments. J. Mater. Res. 1992, 7:1564-1583.
    • (1992) J. Mater. Res. , vol.7 , pp. 1564-1583
    • Oliver, W.C.1    Pharr, G.M.2
  • 27
    • 34250612616 scopus 로고    scopus 로고
    • A systematic review of the survival and complication rates of all-ceramic and metal-ceramic reconstructions after an observation period of at least 3 years. Part I: single crowns
    • Clin. Oral Impl. Res. 19, 326-328 (erratum)
    • Pjetursson B.E., Sailer I., Zwahlen M., Hammerle C.H. A systematic review of the survival and complication rates of all-ceramic and metal-ceramic reconstructions after an observation period of at least 3 years. Part I: single crowns. Clin. Oral Implan. Res. 2008, 18(Suppl. 3):S73-S85. Clin. Oral Impl. Res. 19, 326-328 (erratum).
    • (2008) Clin. Oral Implan. Res. , vol.18 , Issue.SUPPL. 3
    • Pjetursson, B.E.1    Sailer, I.2    Zwahlen, M.3    Hammerle, C.H.4
  • 28
    • 9944229063 scopus 로고    scopus 로고
    • Contemporary materials and technologies for all-ceramic fixed partial dentures: a review of the literature
    • Raigrodski A.J. Contemporary materials and technologies for all-ceramic fixed partial dentures: a review of the literature. J. Prosthet. Dent. 2004, 92(6):557-562.
    • (2004) J. Prosthet. Dent. , vol.92 , Issue.6 , pp. 557-562
    • Raigrodski, A.J.1
  • 29
    • 33749677224 scopus 로고    scopus 로고
    • The efficacy of posterior three-unit zirconium-oxide-based ceramic fixed partial denture prostheses: a prospective clinical pilot study
    • Raigrodski A.J., Chiche G.J., Potiket N., Hochstedler J.L., Mohamed S.E., Billot S. The efficacy of posterior three-unit zirconium-oxide-based ceramic fixed partial denture prostheses: a prospective clinical pilot study. J. Prosthet. Dent. 2006, 96:237-244.
    • (2006) J. Prosthet. Dent. , vol.96 , pp. 237-244
    • Raigrodski, A.J.1    Chiche, G.J.2    Potiket, N.3    Hochstedler, J.L.4    Mohamed, S.E.5    Billot, S.6
  • 30
    • 0032500440 scopus 로고    scopus 로고
    • A new method estimating residual stress by instrumented sharp indentation
    • Suresh S., Giannakopoulos A.E. A new method estimating residual stress by instrumented sharp indentation. Acta Mater. 1998, 46(16):5755-5767.
    • (1998) Acta Mater. , vol.46 , Issue.16 , pp. 5755-5767
    • Suresh, S.1    Giannakopoulos, A.E.2
  • 31
    • 0035410827 scopus 로고    scopus 로고
    • Measurement of residual stress by load and depth sensing indentation with spherical indenters
    • Swadner J.G., Taljat B., Pharr G.M. Measurement of residual stress by load and depth sensing indentation with spherical indenters. J. Mater. Res. 2001, 16(17):2091-2102.
    • (2001) J. Mater. Res. , vol.16 , Issue.17 , pp. 2091-2102
    • Swadner, J.G.1    Taljat, B.2    Pharr, G.M.3
  • 32
    • 67349133480 scopus 로고    scopus 로고
    • Unstable cracking (chipping) of veneering porcelain on all-ceramic dental crowns and fixed partial dentures
    • Swain M.V. Unstable cracking (chipping) of veneering porcelain on all-ceramic dental crowns and fixed partial dentures. Acta Biomater. 2009, 5:1668-1677.
    • (2009) Acta Biomater. , vol.5 , pp. 1668-1677
    • Swain, M.V.1
  • 33
    • 0004247573 scopus 로고
    • Cambridge University Press, Cambridge
    • Tabor D. Hardness of Metals 1951, Cambridge University Press, Cambridge.
    • (1951) Hardness of Metals
    • Tabor, D.1
  • 34
    • 0032625262 scopus 로고    scopus 로고
    • Acontinuum dislocation model of vickers indentation on zirconia
    • Tanaka K., Kanari M., Matsui N. Acontinuum dislocation model of vickers indentation on zirconia. Acta Mater. 1999, 47:2243-2257.
    • (1999) Acta Mater. , vol.47 , pp. 2243-2257
    • Tanaka, K.1    Kanari, M.2    Matsui, N.3
  • 35
    • 40749093600 scopus 로고    scopus 로고
    • Analysis of subcritical growth in dental ceramics using fracture mechanics and fractography
    • Taskonak B., Griggs J.A., Mecholsky J.J., Yan J. Analysis of subcritical growth in dental ceramics using fracture mechanics and fractography. Dent. Mater. 2008, 24:700-707.
    • (2008) Dent. Mater. , vol.24 , pp. 700-707
    • Taskonak, B.1    Griggs, J.A.2    Mecholsky, J.J.3    Yan, J.4
  • 36
    • 80053634985 scopus 로고    scopus 로고
    • Thermal gradients and residual stresses in veneered Y-TZP frameworks
    • Tholey M.J., Swain M.V., Thiel N. Thermal gradients and residual stresses in veneered Y-TZP frameworks. Dent. Mater. 2011, 10.1016/j.dental.2011.08.001.
    • (2011) Dent. Mater.
    • Tholey, M.J.1    Swain, M.V.2    Thiel, N.3
  • 37
  • 38
    • 0030109920 scopus 로고    scopus 로고
    • Influence of stress on the measurement of mechanical properties using nanoindentation: part I. Experimental studies in an aluminum alloy
    • Tsui T.Y., Oliver W.C., Pharr G.M. Influence of stress on the measurement of mechanical properties using nanoindentation: part I. Experimental studies in an aluminum alloy. J. Mater. Res. 1996, 11(3):752-759.
    • (1996) J. Mater. Res. , vol.11 , Issue.3 , pp. 752-759
    • Tsui, T.Y.1    Oliver, W.C.2    Pharr, G.M.3
  • 39
    • 21444455550 scopus 로고    scopus 로고
    • All-ceramic fixed partial dentures, studies on aluminum oxide- and zirconium dioxide based ceramic systems
    • Von S.P. All-ceramic fixed partial dentures, studies on aluminum oxide- and zirconium dioxide based ceramic systems. Swed. Dent. J. Suppl. 2005, 173:1-69.
    • (2005) Swed. Dent. J. Suppl. , vol.173 , pp. 1-69
    • Von, S.P.1
  • 41
    • 84856388116 scopus 로고    scopus 로고
    • Residual stress in ceramic zirconia-porcelain crowns by nanoindentation.
    • In: ICACC, Daytona, FL.
    • Zhang, Y., Hanan, J.C., 2011. Residual stress in ceramic zirconia-porcelain crowns by nanoindentation. In: ICACC, Daytona, FL.
    • (2011)
    • Zhang, Y.1    Hanan, J.C.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.