Thermal gradients and residual stresses in veneered Y-TZP frameworks

Author keywords

Chipping; Residual stress; Temperature gradients; Veneering porcelain; Y TZP frameworks; Zirconia

Indexed keywords

ALL-CERAMIC; CHIPPING; COOLING METHODS; COOLING PROCEDURE; COOLING RATES; DENTAL RESTORATIONS; LOWER STRESS; OUTER SURFACE; SLOW COOLING; TEMPERATURE DIFFERENCES; TEMPERATURE GRADIENT; Y-TZP FRAMEWORKS;

EID: 80053634985     PISSN: 01095641     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.dental.2011.08.001     Document Type: Article
Times cited : (130)

References (22)
  • 1
    • 34250612616 scopus 로고    scopus 로고
    • A systematic review of the survival complication rates of all-ceramic and metal-ceramic reconstructions after an observation period of at least 3 years
    • B. Pjertursson, I. Sailer, M. Zwahlen, and C. Haemmerle A systematic review of the survival complication rates of all-ceramic and metal-ceramic reconstructions after an observation period of at least 3 years Clin Oral Implants Res 18 3 2007 73 85
    • (2007) Clin Oral Implants Res , vol.18 , Issue.3 , pp. 73-85
    • Pjertursson, B.1    Sailer, I.2    Zwahlen, M.3    Haemmerle, C.4
  • 2
    • 67349199548 scopus 로고    scopus 로고
    • Haftverbundmechanismen in dentalen Schichtsystemen
    • M. Tholey, and M. Stephan Haftverbundmechanismen in dentalen Schichtsystemen Quintessenz Zahntech 33 2 2007 160 168
    • (2007) Quintessenz Zahntech , vol.33 , Issue.2 , pp. 160-168
    • Tholey, M.1    Stephan, M.2
  • 3
    • 67349091036 scopus 로고    scopus 로고
    • Thermal Stresses in Ceramometallic Crowns: Firing in Layers
    • J. Lenz, M. Thies, K. Schweizerhof, and Q. Rong Thermal stresses in ceramometallic crowns: firing in layers Chi J Dent Res 5 3 2002 5 24 (Pubitemid 36165685)
    • (2002) Chi J Dent Res , vol.5 , Issue.3 , pp. 5-24
    • Lenz, J.1    Thies, M.2    Schweizerhof, K.3    Rong, Q.4
  • 5
    • 79952640114 scopus 로고    scopus 로고
    • Imaging measurement of stress birefringence in optical materials and components
    • H. Katte Imaging measurement of stress birefringence in optical materials and components Photonik Int 1 2009 39
    • (2009) Photonik Int , vol.1 , pp. 39
    • Katte, H.1
  • 6
    • 33749537632 scopus 로고    scopus 로고
    • Optimal configurations for imaging polarimeters: Impact of image noise and systematic errors
    • DOI 10.1088/1464-4258/8/9/015, PII S1464425806196440, 015
    • J. Zallat, S. Ainouz, and M. Stoll Optimal configurations for imaging polarimeters: impact of image noise and systematic errors J Optics 8 2006 807 814 (Pubitemid 44523079)
    • (2006) Journal of Optics A: Pure and Applied Optics , vol.8 , Issue.9 , pp. 807-814
    • Zallat, J.1    Ainouz, S.2    Stoll, M.Ph.3
  • 7
    • 77953684274 scopus 로고    scopus 로고
    • Evaluation of thermal compatibility between core and veneer dental ceramics using shear bond strength test and contact angle measurement
    • P. Benetti, A. Della Bona, and J.R. Kelly Evaluation of thermal compatibility between core and veneer dental ceramics using shear bond strength test and contact angle measurement Dent Mater 26 8 2010 743 750
    • (2010) Dent Mater , vol.26 , Issue.8 , pp. 743-750
    • Benetti, P.1    Della Bona, A.2    Kelly, J.R.3
  • 9
    • 1842850520 scopus 로고    scopus 로고
    • Strength, reliability, and mode of fracture of bilayered porcelain/core ceramics
    • M. Guazzato, K. Proos, G. Sara, and M.V. Swain Strength, reliability, and mode of fracture of bilayered porcelain/core ceramics Int J Prosthodont 17 2 2004 142 149 (Pubitemid 38490974)
    • (2004) International Journal of Prosthodontics , vol.17 , Issue.2 , pp. 142-149
    • Guazzato, M.1    Proos, K.2    Sara, G.3    Swain, M.V.4
  • 10
    • 67349133480 scopus 로고    scopus 로고
    • Unstable cracking (chipping) of veneering porcelain on all-ceramic dental crowns and fixed partial dentures
    • M.V. Swain Unstable cracking (chipping) of veneering porcelain on all-ceramic dental crowns and fixed partial dentures Acta Biomat 5 5 2009 1668 1677
    • (2009) Acta Biomat , vol.5 , Issue.5 , pp. 1668-1677
    • Swain, M.V.1
  • 11
    • 38349192796 scopus 로고    scopus 로고
    • State of the art of zirconia for dental applications
    • I. Denry, and J. Kelly State of the art of zirconia for dental applications Dent Mater 24 3 2008 299 307
    • (2008) Dent Mater , vol.24 , Issue.3 , pp. 299-307
    • Denry, I.1    Kelly, J.2
  • 12
    • 80053648492 scopus 로고    scopus 로고
    • Long-term Behaviour of Zirconia-based Bridges: Three year results
    • [Abstract 230]
    • P. Pospiech, and F.P. Nothdurft Long-term Behaviour of Zirconia-based Bridges: three year results J Dent Res 83 2003 [Abstract 230]
    • (2003) J Dent Res , vol.83
    • Pospiech, P.1    Nothdurft, F.P.2
  • 13
    • 52449088061 scopus 로고    scopus 로고
    • The clinical success of all-ceramic restorations
    • A. Della Bona, and J.R. Kelly The clinical success of all-ceramic restorations J Am Dent Assoc 139 2008 8 13
    • (2008) J Am Dent Assoc , vol.139 , pp. 8-13
    • Della Bona, A.1    Kelly, J.R.2
  • 14
    • 78049302564 scopus 로고    scopus 로고
    • Effect of firing protocols on cohesive failure of all-ceramic crowns
    • S. Rues, E. Kröger, D. Müller, and M. Schmitter Effect of firing protocols on cohesive failure of all-ceramic crowns Am J Dent 38 12 2010 987 994
    • (2010) Am J Dent , vol.38 , Issue.12 , pp. 987-994
    • Rues, S.1    Kröger, E.2    Müller, D.3    Schmitter, M.4
  • 15
    • 27744593950 scopus 로고    scopus 로고
    • Viscoelastic finite element analysis of an all-ceramic fixed partial denture
    • DOI 10.1016/j.jbiomech.2004.11.007, PII S0021929004005457
    • P. DeHoff, K. Anusavice, and N. Götzen Viscoelastic finite element analysis of an all-ceramic fixed partial denture J Biomech 39 2006 40 48 (Pubitemid 41585007)
    • (2006) Journal of Biomechanics , vol.39 , Issue.1 , pp. 40-48
    • DeHoff, P.H.1    Anusavice, K.J.2    Gotzen, N.3
  • 16
    • 47249123700 scopus 로고    scopus 로고
    • The effects of viscoelastic parameters on residual stress development in a zirconia/glass bilayer dental ceramic
    • B. Taskonak, G. Borges, J. Mecholsky, K. Anusavice, B. Moore, and J. Yan The effects of viscoelastic parameters on residual stress development in a zirconia/glass bilayer dental ceramic Dent Mater 24 2008 1149 1155
    • (2008) Dent Mater , vol.24 , pp. 1149-1155
    • Taskonak, B.1    Borges, G.2    Mecholsky, J.3    Anusavice, K.4    Moore, B.5    Yan, J.6
  • 17
    • 0017454086 scopus 로고
    • Contact fracture resistance of physically and chemically tempered glass Plates - Theoretical model
    • B.R. Lawn, and D.B. Marshall Contact fracture resistance of physically and chemically tempered glass Plates - theoretical model Phys Chem Glasses 18 1 1977 7 18
    • (1977) Phys Chem Glasses , vol.18 , Issue.1 , pp. 7-18
    • Lawn, B.R.1    Marshall, D.B.2
  • 18
    • 77951662356 scopus 로고    scopus 로고
    • Thermal/mechanical simulation and laboratory fatigue testing of an alternative yttria tetragonal zirconia polycrystal core-veneer all-ceramic layered crown design
    • E.A. Bonfante, B. Rafferty, R.A. Zavanelli, N.R.F.A. Silva, E.D. Rekow, V.P. Thompson, and P.G. Coelho Thermal/mechanical simulation and laboratory fatigue testing of an alternative yttria tetragonal zirconia polycrystal core-veneer all-ceramic layered crown design Eur J Oral Sci 118 2010 202 209
    • (2010) Eur J Oral Sci , vol.118 , pp. 202-209
    • Bonfante, E.A.1    Rafferty, B.2    Zavanelli, R.A.3    Silva, N.R.F.A.4    Rekow, E.D.5    Thompson, V.P.6    Coelho, P.G.7
  • 19
    • 0017703485 scopus 로고
    • Framework design in ceramo-metal restorations
    • L.L. Miller Framework design in ceramo-metal restorations Dent Clin North Am 21 1977 699 716 (Pubitemid 8250087)
    • (1977) Dental Clinics of North America , vol.21 , Issue.4 , pp. 699-716
    • Miller, L.L.1
  • 20
    • 33746913496 scopus 로고    scopus 로고
    • Metal-ceramic failure in noble metal crowns: 7-Year results of a prospective clinical trial in private practices
    • B. Reitemeier, K. Hansel, C. Kastner, and M.H. Walter Metal-ceramic failure in noble metal crowns: 7-year results of a prospective clinical trial in private practices Int J Prosthodont 19 2006 397 399 (Pubitemid 44197796)
    • (2006) International Journal of Prosthodontics , vol.19 , Issue.4 , pp. 397-399
    • Reitemeier, B.1    Hansel, K.2    Kastner, C.3    Walter, M.H.4
  • 22
    • 79952279197 scopus 로고    scopus 로고
    • Influence of thickness and cooling rate on development of spontaneous cracks in porcelain/zirconia structures
    • M. Guazzato, T.R. Walton, W. Franklin, G. Davis, C. Bohl, and I. Klineberg Influence of thickness and cooling rate on development of spontaneous cracks in porcelain/zirconia structures Aust Dent J 55 3 2010 306 310
    • (2010) Aust Dent J , vol.55 , Issue.3 , pp. 306-310
    • Guazzato, M.1    Walton, T.R.2    Franklin, W.3    Davis, G.4    Bohl, C.5    Klineberg, I.6


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.