메뉴 건너뛰기




Volumn 27, Issue 9, 2011, Pages 948-953

The effect of porcelain thickness and surface liner application on the fracture behavior of a ceramic system

Author keywords

Ceramic; Flexural strength; Liner; Stress concentration; Thickness

Indexed keywords

3-POINT BENDING; CERAMIC; CERAMIC SYSTEMS; FRACTURE BEHAVIOR; FRACTURE INITIATION; LINER; MAXIMUM LOAD; ONE-WAY ANOVA; PORCELAIN VENEERS; THICKNESS; WEIBULL MODULUS; ZIRCONIA-BASED CERAMICS;

EID: 80051470857     PISSN: 01095641     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.dental.2011.05.009     Document Type: Article
Times cited : (50)

References (42)
  • 1
    • 38349192796 scopus 로고    scopus 로고
    • State of the art of zirconia for dental applications
    • I. Denry, and J.R. Kelly State of the art of zirconia for dental applications Dent Mater 24 3 2008 299 307
    • (2008) Dent Mater , vol.24 , Issue.3 , pp. 299-307
    • Denry, I.1    Kelly, J.R.2
  • 2
    • 38349162274 scopus 로고    scopus 로고
    • Stabilized zirconia as a structural ceramic: An overview
    • J.R. Kelly, and I. Denry Stabilized zirconia as a structural ceramic: an overview Dent Mater 24 3 2008 289 298
    • (2008) Dent Mater , vol.24 , Issue.3 , pp. 289-298
    • Kelly, J.R.1    Denry, I.2
  • 4
    • 1942468620 scopus 로고    scopus 로고
    • Strength, reliability and mode of fracture of bilayered porcelain/zirconia (Y-TZP) dental ceramics
    • DOI 10.1016/j.biomaterials.2004.02.036, PII S0142961204001747
    • M. Guazzato, K. Proos, L. Quach, and M.V. Swain Strength, reliability and mode of fracture of bilayered porcelain/zirconia (Y-TZP) dental ceramics Biomaterials 25 20 2004 5045 5052 (Pubitemid 38520834)
    • (2004) Biomaterials , vol.25 , Issue.20 , pp. 5045-5052
    • Guazzato, M.1    Proos, K.2    Quach, L.3    Swain, M.V.4
  • 5
    • 34250164925 scopus 로고    scopus 로고
    • The biaxial flexural strength and fatigue property of Lava™ Y-TZP dental ceramic
    • DOI 10.1016/j.dental.2006.09.003, PII S0109564106002454
    • P. Pittayachawan, A. McDonald, A. Petrie, and J.C. Knowles The biaxial flexural strength and fatigue property of Lava Y-TZP dental ceramic Dent Mater 23 8 2007 1018 1029 (Pubitemid 46907965)
    • (2007) Dental Materials , vol.23 , Issue.8 , pp. 1018-1029
    • Pittayachawan, P.1    McDonald, A.2    Petrie, A.3    Knowles, J.C.4
  • 6
    • 78651244912 scopus 로고    scopus 로고
    • Color related to ceramic and zirconia restorations: A review
    • A. Vichi, C. Louca, G. Corciolani, and M. Ferrari Color related to ceramic and zirconia restorations: a review Dent Mater 27 1 2011 97 108
    • (2011) Dent Mater , vol.27 , Issue.1 , pp. 97-108
    • Vichi, A.1    Louca, C.2    Corciolani, G.3    Ferrari, M.4
  • 8
    • 52449088061 scopus 로고    scopus 로고
    • The clinical success of all-ceramic restorations
    • Della Bona, and J.R. Kelly The clinical success of all-ceramic restorations JADA 139 2008 8S 13S
    • (2008) JADA , vol.139
    • Bona, D.1    Kelly, J.R.2
  • 9
    • 78650487512 scopus 로고    scopus 로고
    • A clinical comparison of zirconia, metal and alumina fixed-prosthesis frameworks veneered with layered or pressed ceramic: A three-year report
    • R.P. Christensen, and B.J. Ploeger A clinical comparison of zirconia, metal and alumina fixed-prosthesis frameworks veneered with layered or pressed ceramic: a three-year report J Am Dent Assoc 141 11 2010 1317 1329
    • (2010) J Am Dent Assoc , vol.141 , Issue.11 , pp. 1317-1329
    • Christensen, R.P.1    Ploeger, B.J.2
  • 10
    • 67349113799 scopus 로고    scopus 로고
    • SEM observations of porcelain Y-TZP interface
    • M.J. Tholey, M.V. Swain, and N. Thiel SEM observations of porcelain Y-TZP interface Dent Mater 25 2009 857 862
    • (2009) Dent Mater , vol.25 , pp. 857-862
    • Tholey, M.J.1    Swain, M.V.2    Thiel, N.3
  • 11
    • 67349133480 scopus 로고    scopus 로고
    • Unstable cracking (chipping) of veneering porcelain on all-ceramic dental crowns and fixed partial dentures
    • M.V. Swain Unstable cracking (chipping) of veneering porcelain on all-ceramic dental crowns and fixed partial dentures Acta Biomater 5 5 2009 1668 1677
    • (2009) Acta Biomater , vol.5 , Issue.5 , pp. 1668-1677
    • Swain, M.V.1
  • 12
    • 77953684274 scopus 로고    scopus 로고
    • Evaluation of thermal compatibility between core and veneer dental ceramics using shear bond strength test and contact angle measurement
    • P. Benetti, J.R. Kelly, and A. Della Bona Evaluation of thermal compatibility between core and veneer dental ceramics using shear bond strength test and contact angle measurement Dent Mater 26 8 2010 743 750
    • (2010) Dent Mater , vol.26 , Issue.8 , pp. 743-750
    • Benetti, P.1    Kelly, J.R.2    Della Bona, A.3
  • 13
    • 3242741859 scopus 로고    scopus 로고
    • A comparison of fracture strength of yttrium-oxide-partially-stabilized zirconia ceramic crowns with varying core thickness, shapes and veneer ceramics
    • DOI 10.1111/j.1365-2842.2004.01284.x
    • A. Sundh, and G. Sjögren A comparison of fracture strength of yttrium-oxide-partially-stabilized zirconia ceramic crowns with varying core thickness, shapes and veneer ceramics J Oral Rehabil 31 7 2004 682 688 (Pubitemid 38953624)
    • (2004) Journal of Oral Rehabilitation , vol.31 , Issue.7 , pp. 682-688
    • Sundh, A.1    Sjogren, G.2
  • 14
    • 52049118769 scopus 로고    scopus 로고
    • Shear bond strengths between different zirconia cores and veneering ceramics and their susceptibility to thermocycling
    • P.C. Guess, A. Kulis, S. Witkowski, M. Wolkewitz, Y. Zhang, and J.R. Strub Shear bond strengths between different zirconia cores and veneering ceramics and their susceptibility to thermocycling Dent Mater 24 11 2008 1556 1567
    • (2008) Dent Mater , vol.24 , Issue.11 , pp. 1556-1567
    • Guess, P.C.1    Kulis, A.2    Witkowski, S.3    Wolkewitz, M.4    Zhang, Y.5    Strub, J.R.6
  • 15
    • 33746623731 scopus 로고    scopus 로고
    • Microtensile bond strength of different components of core veneered all-ceramic restorations. Part II: Zirconia veneering ceramics
    • DOI 10.1016/j.dental.2005.11.014, PII S010956410500299X
    • M.N. Aboushelib, C.J. Kleverlaan, and A.J. Feilzer Microtensile bond strength of different components of core veneered all-ceramic restorations. Part II: Zirconia veneering ceramics Dent Mater 22 9 2006 857 863 (Pubitemid 44148813)
    • (2006) Dental Materials , vol.22 , Issue.9 , pp. 857-863
    • Aboushelib, M.N.1    Kleverlaan, C.J.2    Feilzer, A.J.3
  • 16
    • 79952279197 scopus 로고    scopus 로고
    • Influence of thickness and cooling rate on development of spontaneous cracks in porcelain/zirconia structures
    • M. Guazzato, T.R. Walton, W. Franklin, G. Davis, C. Bohl, and I. Klineberg Influence of thickness and cooling rate on development of spontaneous cracks in porcelain/zirconia structures J. Aust Dent 55 3 2010 306 310
    • (2010) J. Aust Dent , vol.55 , Issue.3 , pp. 306-310
    • Guazzato, M.1    Walton, T.R.2    Franklin, W.3    Davis, G.4    Bohl, C.5    Klineberg, I.6
  • 17
    • 58749089146 scopus 로고    scopus 로고
    • The influence of veneering porcelain thickness of all-ceramic and metal ceramic crowns on failure resistance after cyclic loading
    • A. Shirakura, H. Lee, A. Geminiani, C. Ercoli, and C. Feng The influence of veneering porcelain thickness of all-ceramic and metal ceramic crowns on failure resistance after cyclic loading J Prosthet Dent 101 2 2009 119 127
    • (2009) J Prosthet Dent , vol.101 , Issue.2 , pp. 119-127
    • Shirakura, A.1    Lee, H.2    Geminiani, A.3    Ercoli, C.4    Feng, C.5
  • 18
    • 0006757528 scopus 로고    scopus 로고
    • International Organization For Standardization. Iso 6872 third ed International Organization for Standardization Geneva
    • International Organization for Standardization. ISO 6872 Dental ceramics third ed 2008 International Organization for Standardization Geneva
    • (2008) Dental Ceramics
  • 20
    • 0042128629 scopus 로고    scopus 로고
    • Weibull analysis and flexural strength of hot-pressed core and veneer ceramic structures
    • A. Della Bona, J.K. Anusavice, and P.H. DeHoff Weibull analysis and flexural strength of hot-pressed core and veneer ceramic structures Dent Mater 19 7 2003 662 669
    • (2003) Dent Mater , vol.19 , Issue.7 , pp. 662-669
    • Della Bona, A.1    Anusavice, J.K.2    Dehoff, P.H.3
  • 21
    • 37848999076 scopus 로고    scopus 로고
    • A systematic review of the survival and complication rates of resin-bonded bridges after an observation period of at least 5 years
    • B.E. Pjetursson, W.C. Tan, K. Tan, U. Brägger, M. Zwahlen, and N.P. Lang A systematic review of the survival and complication rates of resin-bonded bridges after an observation period of at least 5 years Clin Oral Implant Res 19 2 2008 131 141
    • (2008) Clin Oral Implant Res , vol.19 , Issue.2 , pp. 131-141
    • Pjetursson, B.E.1    Tan, W.C.2    Tan, K.3    Brägger, U.4    Zwahlen, M.5    Lang, N.P.6
  • 22
    • 0029318343 scopus 로고
    • Failure of all ceramic fixed partial denture in vitro and in vivo: Analysis and modeling
    • J.R. Kelly, J.A. Tesk, and J.A. Sorensen Failure of all ceramic fixed partial denture in vitro and in vivo: analysis and modeling J Dent Res 74 6 1995 1253 1258
    • (1995) J Dent Res , vol.74 , Issue.6 , pp. 1253-1258
    • Kelly, J.R.1    Tesk, J.A.2    Sorensen, J.A.3
  • 23
    • 22644448001 scopus 로고    scopus 로고
    • Flexural strength of a layered zirconia and porcelain dental all-ceramic system
    • DOI 10.1016/j.prosdent.2005.05.007, PII S002239130500257X
    • S.N. White, V.G. Miklus, E.A. McLaren, L.A. Lang, and A.A. Caputo Flexural strength of a layered zirconia and porcelain dental all-ceramic system J Prosthet Dent 94 2 2005 125 131 (Pubitemid 41024900)
    • (2005) Journal of Prosthetic Dentistry , vol.94 , Issue.2 , pp. 125-131
    • White, S.N.1    Miklus, V.G.2    McLaren, E.A.3    Lang, L.A.4    Caputo, A.A.5
  • 25
    • 16344387546 scopus 로고    scopus 로고
    • Fracture resistance of yttrium oxide partially-stabilized zirconia all-ceramic bridges after veneering and mechanical fatigue testing
    • DOI 10.1016/j.dental.2004.07.013, PII S0109564104001526
    • A. Sundh, M. Molin, and G. Sjögren Fracture resistance of yttrium oxide partially-stabilized zirconia all-ceramic bridges after veneering and mechanical fatigue testing Dent Mater 21 5 2005 476 482 (Pubitemid 40467038)
    • (2005) Dental Materials , vol.21 , Issue.5 , pp. 476-482
    • Sundh, A.1    Molin, M.2    Sjogren, G.3
  • 28
    • 0034264517 scopus 로고    scopus 로고
    • Structural reliability of alumina-, feldspar-, leucite-, mica- and zirconia-based ceramics
    • J. Tinschert, D. Zwez, R. Marx, and K.J. Anusavice Structural reliability of alumina-, feldspar-, leucite-, mica- and zirconia-based ceramics J Dent 28 7 2000 529 535
    • (2000) J Dent , vol.28 , Issue.7 , pp. 529-535
    • Tinschert, J.1    Zwez, D.2    Marx, R.3    Anusavice, K.J.4
  • 29
    • 0035319974 scopus 로고    scopus 로고
    • Reliability and strength of all-ceramic dental restorations fabricated by direct ceramic machining (DCM)
    • F. Filser, P. Kocher, and F. Weibel Reliability and strength of all-ceramic dental restorations fabricated by direct ceramic machining (DCM) Int J Comput Dent 4 2 2001 89 106
    • (2001) Int J Comput Dent , vol.4 , Issue.2 , pp. 89-106
    • Filser, F.1    Kocher, P.2    Weibel, F.3
  • 30
    • 47249123700 scopus 로고    scopus 로고
    • The effects of viscoelastic parameters on residual stress development in a zirconia/glass bilayer dental ceramic
    • B. Taskonak, G.A. Borges, J.J. Mecholsky, K.J. Anusavice, B.K. Moore, and J. Yan The effects of viscoelastic parameters on residual stress development in a zirconia/glass bilayer dental ceramic Dent Mater 24 9 2008 1149 1155
    • (2008) Dent Mater , vol.24 , Issue.9 , pp. 1149-1155
    • Taskonak, B.1    Borges, G.A.2    Mecholsky, J.J.3    Anusavice, K.J.4    Moore, B.K.5    Yan, J.6
  • 31
    • 3843138283 scopus 로고    scopus 로고
    • Shear relaxation of dental ceramics determined from creep behavior
    • P.H. DeHoff, and J.K. Anusavice Shear relaxation of dental ceramics determined from creep behavior Dent Mater 20 8 2004 717 725
    • (2004) Dent Mater , vol.20 , Issue.8 , pp. 717-725
    • Dehoff, P.H.1    Anusavice, J.K.2
  • 32
    • 32044472550 scopus 로고    scopus 로고
    • The influence of different core material on the FEA-determined stress distribution in dental crowns
    • DOI 10.1016/j.dental.2005.04.034, PII S0109564105001624
    • De Jager, M. de Kler, and J.M. Van Der Zel The influence of different core materials on the FEA-determined stress distribution in dental crowns Dent Mater 22 3 2006 234 242 (Pubitemid 43199612)
    • (2006) Dental Materials , vol.22 , Issue.3 , pp. 234-242
    • De Jager, N.1    De Kler, M.2    Van Der Zel, J.M.3
  • 34
    • 18544379604 scopus 로고    scopus 로고
    • The influence of multiple firing on thermal contraction of ceramic materials used for the fabrication of layered all-ceramic dental restorations
    • DOI 10.1016/j.dental.2004.08.006, PII S0109564104001630
    • G. Isgr, C.J. Kleverlaan, H. Wang, and A.J. Feilzer The influence of multiple firing on thermal contraction of ceramic materials used for the fabrication of layered all-ceramic dental restorations Dent Mater 21 6 2005 557 564 (Pubitemid 40655130)
    • (2005) Dental Materials , vol.21 , Issue.6 , pp. 557-564
    • Isgro, G.1    Kleverlaan, C.J.2    Wang, H.3    Feilzer, A.J.4
  • 35
    • 27744593950 scopus 로고    scopus 로고
    • Viscoelastic finite element analysis of an all-ceramic fixed partial denture
    • DOI 10.1016/j.jbiomech.2004.11.007, PII S0021929004005457
    • P.H. DeHoff, K.J. Anusavice, and N. Gotzen Viscoelastic finite element analysis of an all-ceramic fixed partial denture J Biomech 39 1 2006 40 48 (Pubitemid 41585007)
    • (2006) Journal of Biomechanics , vol.39 , Issue.1 , pp. 40-48
    • DeHoff, P.H.1    Anusavice, K.J.2    Gotzen, N.3
  • 36
    • 43049090522 scopus 로고    scopus 로고
    • Thermal compatibility of dental ceramic systems using cylindrical and spherical geometries
    • DOI 10.1016/j.dental.2007.08.008, PII S0109564107002096
    • P.H. DeHoff, A.A. Barrett, R.B. Lee, and K.J. Anusavice Thermal compatibility of dental ceramic systems using cylindrical and spherical geometries Dent Mater 24 6 2008 744 752 (Pubitemid 351626156)
    • (2008) Dental Materials , vol.24 , Issue.6 , pp. 744-752
    • DeHoff, P.H.1    Barrett, A.A.2    Lee, R.B.3    Anusavice, K.J.4
  • 37
    • 65549131011 scopus 로고    scopus 로고
    • Viscoelastic finite element stress analysis of the thermal compatibility of dental bilayer ceramic systems
    • P.H. DeHoff, and K.J. Anusavice Viscoelastic finite element stress analysis of the thermal compatibility of dental bilayer ceramic systems Int J Prosthet 22 1 2009 56 61
    • (2009) Int J Prosthet , vol.22 , Issue.1 , pp. 56-61
    • Dehoff, P.H.1    Anusavice, K.J.2
  • 38
    • 80051473738 scopus 로고    scopus 로고
    • Temperaturgradienten in Kronen mit Gerüsten aus Zirkoniumdioxid (Y-TZP)
    • M. Tholey, N. Thiel, S. Schindler, S. Rues, and J. Lenz Temperaturgradienten in Kronen mit Gerüsten aus Zirkoniumdioxid (Y-TZP) Quintess Zahntech 36 9 2010 1184 1198
    • (2010) Quintess Zahntech , vol.36 , Issue.9 , pp. 1184-1198
    • Tholey, M.1    Thiel, N.2    Schindler, S.3    Rues, S.4    Lenz, J.5
  • 41
    • 77949462538 scopus 로고    scopus 로고
    • Mechanical strength and subcritical crack growth under wet cyclic loading of glass-infiltrated dental ceramics
    • S.M. Salazar Marocho, A.R. Studart, M.A. Bottino, and A. Della Bona Mechanical strength and subcritical crack growth under wet cyclic loading of glass-infiltrated dental ceramics Dent Mater 26 5 2010 483 490
    • (2010) Dent Mater , vol.26 , Issue.5 , pp. 483-490
    • Salazar Marocho, S.M.1    Studart, A.R.2    Bottino, M.A.3    Della Bona, A.4
  • 42
    • 80051473946 scopus 로고    scopus 로고
    • ASTM C 1239-07: Standard practice for reporting uniaxial strength data and estimating Weibull distribution parameters for advanced ceramics
    • American Society For Testing Materials
    • American Society for Testing Materials ASTM C 1239-07: Standard practice for reporting uniaxial strength data and estimating Weibull distribution parameters for advanced ceramics ASTM Int 15 01 2007 1 19
    • (2007) ASTM Int , vol.15 , Issue.1 , pp. 1-19


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.