메뉴 건너뛰기




Volumn 27, Issue 7, 2011, Pages 684-691

Subcritical crack growth behavior and life data analysis of two types of dental Y-TZP ceramics

Author keywords

Dynamic fatigue; Lifetime analysis; SPT diagram; Subcritical crack growth; Zirconia ceramic

Indexed keywords

DYNAMIC FATIGUE; LIFETIME ANALYSIS; SPT DIAGRAM; SUBCRITICAL CRACK GROWTH; ZIRCONIA CERAMIC;

EID: 79957744629     PISSN: 01095641     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.dental.2011.03.010     Document Type: Article
Times cited : (34)

References (42)
  • 1
    • 21244506130 scopus 로고    scopus 로고
    • A clinical report and overview of scientific studies and clinical procedures conducted on the 3M ESPE Lava™ all-ceramic system
    • DOI 10.1111/j.1532-849X.2005.00003.x
    • A. Piwowarczyk, P. Ottl, H.C. Lauer, and T. Kuretzky A clinical report and overview of scientific studies and clinical procedures conducted on the 3M ESPE lava all-ceramic system J Prosthodont 14 2005 39 45 (Pubitemid 41679756)
    • (2005) Journal of Prosthodontics , vol.14 , Issue.1 , pp. 39-45
    • Piwowarczyk, A.1    Ottl, P.2    Lauer, H.-C.3    Kuretzky, T.4
  • 2
    • 35148891671 scopus 로고    scopus 로고
    • An overview of zirconia ceramics: Basic properties and clinical applications
    • P.F. Manicone, P. Rossi Iommetti, and L. Raffaelli An overview of zirconia ceramics: basic properties and clinical applications J Dent 35 2007 819 826
    • (2007) J Dent , vol.35 , pp. 819-826
    • Manicone, P.F.1    Rossi Iommetti, P.2    Raffaelli, L.3
  • 3
    • 84980204606 scopus 로고
    • Mechanisms of toughening partially stabilized zirconia (PSZ)
    • D.L. Porter, and A.H. Heuer Mechanisms of toughening partially stabilized zirconia (PSZ) J Am Ceram Soc 60 1977 83 184
    • (1977) J Am Ceram Soc , vol.60 , pp. 83-184
    • Porter, D.L.1    Heuer, A.H.2
  • 4
    • 0024546336 scopus 로고
    • Mechanical properties and short-term in-vivo evaluation of yttrium-oxide-partially-stabilized zirconia
    • DOI 10.1002/jbm.820230105
    • P. Christel, A. Meunier, M. Heller, J.P. Torre, and C.N. Peille Mechanical properties and short-term in-vivo evaluation of yttrium-oxide- partially-stabilized zirconia J Biomed Mater Res 23 1989 45 61 (Pubitemid 19031252)
    • (1989) Journal of Biomedical Materials Research , vol.23 , Issue.1 , pp. 45-61
    • Christel, P.1    Meunier, A.2    Heller, M.3    Torre, J.P.4    Peille, C.N.5
  • 5
    • 26844583254 scopus 로고    scopus 로고
    • What future for zirconia as a biomaterial?
    • DOI 10.1016/j.biomaterials.2005.07.034, PII S0142961205007039
    • J. Chevalier What future for zirconia as a biomaterial? Biomaterials 27 2006 535 543 (Pubitemid 41464249)
    • (2006) Biomaterials , vol.27 , Issue.4 , pp. 535-543
    • Chevalier, J.1
  • 6
    • 0030250781 scopus 로고    scopus 로고
    • Sintering of partially-stabilized zirconia and partially-stabilized zirconia-hydroxyapatite composites by hot isostatic pressing and pressureless sintering
    • DOI 10.1016/0142-9612(95)00356-8
    • J. Li, H. Liao, and L. Hermansson Sintering of partially-stabilized zirconia and partially-stabilized zirconia-hydroxyapatite composites by hot isostatic pressing and pressureless sintering Biomaterials 17 18 1996 1787 1790 (Pubitemid 26355422)
    • (1996) Biomaterials , vol.17 , Issue.18 , pp. 1787-1790
    • Li, J.1    Liao, H.2    Hermansson, L.3
  • 9
    • 0242575980 scopus 로고    scopus 로고
    • Mechanical properties and low-temperature aging of tetragonal zirconia polycrystals processed by hot isostatic pressing
    • J. Munñoz-Saldaña, D. Jaramillo-Vigueras, T. Iga, and G.A. Schneider Mechanical properties and low-temperature aging of tetragonal zirconia polycrystals processed by hot isostatic pressing J Mater Res 18 2003 2364 2370
    • (2003) J Mater Res , vol.18 , pp. 2364-2370
    • Munñoz-Saldaña, J.1    Jaramillo-Vigueras, D.2    Iga, T.3    Schneider, G.A.4
  • 10
    • 0024733463 scopus 로고
    • Hot isostatic pressing of a presintered yttria-stabilized zirconia ceramic
    • A.P. Druschitz, and J.G. Schroth Hot isostatic pressing of a presintered yttria-stabilized zirconia ceramic J Am Ceram Soc 72 1989 1591 1597
    • (1989) J Am Ceram Soc , vol.72 , pp. 1591-1597
    • Druschitz, A.P.1    Schroth, J.G.2
  • 11
    • 0034951336 scopus 로고    scopus 로고
    • Effect of HIPping, stress and surface finish on the environmental degradation of Y-TZP ceramics
    • DOI 10.1023/A:1011284016483
    • K.L. Grant, R.D. Rawlings, and R. Sweeney Effect of HIPping, stress and surface finish on the environmental degradation of Y-TZP ceramics J Mater Sci Mater Med 12 2001 557 564 (Pubitemid 32612626)
    • (2001) Journal of Materials Science: Materials in Medicine , vol.12 , Issue.6 , pp. 557-564
    • Grant, K.L.1    Rawlings, R.D.2    Sweeney, R.3
  • 12
    • 5044248225 scopus 로고    scopus 로고
    • CAD/CAM-machining effects on Y-TZP zirconia
    • R.G. Luthard CAD/CAM-machining effects on Y-TZP zirconia Dent Mater 20 2004 655 662
    • (2004) Dent Mater , vol.20 , pp. 655-662
    • Luthard, R.G.1
  • 14
    • 84977695915 scopus 로고
    • Influence of water vapor on crack propagation in soda-lime-glass
    • S.M. Wiederhorn Influence of water vapor on crack propagation in soda-lime-glass J Am Ceram Soc 50 1967 407 414
    • (1967) J Am Ceram Soc , vol.50 , pp. 407-414
    • Wiederhorn, S.M.1
  • 16
    • 0001412634 scopus 로고
    • Determination of subcritical crack growth parameters by in situ observation of indentation cracks
    • P.J. Dwivedi, and D.J. Green Determination of subcritical crack growth parameters by in situ observation of indentation cracks J Am Ceram Soc 78 1995 2122 2128
    • (1995) J Am Ceram Soc , vol.78 , pp. 2122-2128
    • Dwivedi, P.J.1    Green, D.J.2
  • 17
    • 84950437463 scopus 로고
    • Constant stress of glass: I
    • R.J. Charles Constant stress of glass: I J Appl Phys 29 1959 1549 11549
    • (1959) J Appl Phys , vol.29 , pp. 1549-11549
    • Charles, R.J.1
  • 18
    • 0025751739 scopus 로고
    • New test methods for engineering ceramics-in-situ: Microscopy investigation
    • H. Frei, and G. Grathwohl New test methods for engineering ceramics-in-situ: microscopy investigation Ceram Forum Int 68 1991 27 35
    • (1991) Ceram Forum Int , vol.68 , pp. 27-35
    • Frei, H.1    Grathwohl, G.2
  • 19
    • 84987266075 scopus 로고
    • A statistical distribution function of wide applicability
    • W. Weibull A statistical distribution function of wide applicability J Appl Mech. 18 1951 293 297
    • (1951) J Appl Mech. , vol.18 , pp. 293-297
    • Weibull, W.1
  • 20
    • 0015725371 scopus 로고
    • Strength-probability-time (SPT) relationships in ceramics
    • R.W. Davidge, J.R. McLaren, and G. Tappin Strength-probability-time (SPT) relationships in ceramics J Membr Sci 8 1973 1699 1705
    • (1973) J Membr Sci , vol.8 , pp. 1699-1705
    • Davidge, R.W.1    McLaren, J.R.2    Tappin, G.3
  • 21
    • 84987335986 scopus 로고
    • A critical evaluation of indentation techniques for measuring fracture toughness. Pt I. Direct crack measurements
    • G.R. Anstis, P. Chantikul, B.R. Lawn, and D.B. Marshall A critical evaluation of indentation techniques for measuring fracture toughness. Pt I. Direct crack measurements J Am Ceram Soc 64 1981 533 538
    • (1981) J Am Ceram Soc , vol.64 , pp. 533-538
    • Anstis, G.R.1    Chantikul, P.2    Lawn, B.R.3    Marshall, D.B.4
  • 22
    • 84979434138 scopus 로고
    • Hardness, toughness, and brittleness - An indentation analysis
    • B.R. Lawn, and D.B. Marshall Hardness, toughness, and brittleness - an indentation analysis J Am Ceram Soc 62 1979 347 350
    • (1979) J Am Ceram Soc , vol.62 , pp. 347-350
    • Lawn, B.R.1    Marshall, D.B.2
  • 24
    • 0018440956 scopus 로고
    • Static and dynamic fatigue of polycrystalline alumina
    • J.E. Ritter, and J.N. Humenik Static and dynamic fatigue of polycrystalline alumina J Membr Sci 14 1979 1573 4803
    • (1979) J Membr Sci , vol.14 , pp. 1573-4803
    • Ritter, J.E.1    Humenik, J.N.2
  • 25
    • 33846988966 scopus 로고    scopus 로고
    • Lifetime of alumina- and zirconia ceramics used for crown and bridge restorations
    • J. Tinschert Lifetime of alumina- and zirconia ceramics used for crown and bridge restorations J Biomed Mater Res B: Appl Biomater 80B 2007 317 321
    • (2007) J Biomed Mater Res B: Appl Biomater , vol.80 , pp. 317-321
    • Tinschert, J.1
  • 26
    • 33845290307 scopus 로고    scopus 로고
    • Durability of the resin bond strength to zirconia ceramic after using different surface conditioning methods
    • DOI 10.1016/j.dental.2005.11.040, PII S0109564105003568
    • M. Wolfart, F. Lehmann, S. Wolfart, and M. Kern Durability of the resin bond strength to zirconia ceramic after using different surface conditioning methods Dent Mater 23 2007 45 50 (Pubitemid 44880064)
    • (2007) Dental Materials , vol.23 , Issue.1 , pp. 45-50
    • Wolfart, M.1    Lehmann, F.2    Wolfart, S.3    Kern, M.4
  • 27
    • 40749115551 scopus 로고    scopus 로고
    • Strength influencing variables on CAD/CAM zirconia frameworks
    • DOI 10.1016/j.dental.2007.06.030, PII S0109564107001765
    • H. Wang, M.N. Aboushelib, and A.J. Feilzer Strength influencing variables on CAD/CAM zirconia frameworks Dent Mater 24 2008 633 638 (Pubitemid 351389493)
    • (2008) Dental Materials , vol.24 , Issue.5 , pp. 633-638
    • Wang, H.1    Aboushelib, M.N.2    Feilzer, A.J.3
  • 28
    • 0033222358 scopus 로고    scopus 로고
    • The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic
    • PII S0109564199000706
    • T. Kosmac, C. Oblak, P. Jevnikar, N. Funduk, and L. Marion The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic Dent Mater 15 1999 426 433 (Pubitemid 129586772)
    • (1999) Dental Materials , vol.15 , Issue.6 , pp. 426-433
    • Kosmac, T.1    Oblak, C.2    Jevnikar, P.3    Funduk, N.4    Marion, L.5
  • 29
    • 16344363996 scopus 로고    scopus 로고
    • Influence of surface and heat treatments on the flexural strength of a glass-infiltrated alumina/zirconia-reinforced dental ceramic
    • DOI 10.1016/j.dental.2004.07.010, PII S0109564104001307
    • M. Guazzato, M. Albakry, L. Quach, and M.V. Swain Influence of surface and heat treatments on the flexural strength of a glass-infiltrated alumina/zirconia-reinforced dental ceramic Dent Mater 21 2005 454 463 (Pubitemid 40467035)
    • (2005) Dental Materials , vol.21 , Issue.5 , pp. 454-463
    • Guazzato, M.1    Albakry, M.2    Quach, L.3    Swain, M.V.4
  • 31
    • 77955608581 scopus 로고    scopus 로고
    • Effect of surface treatment on flexural strength of circonia bars
    • August 2
    • M.N. Aboushelib, and H. Wang Effect of surface treatment on flexural strength of circonia bars J Prosthet Dent 104 August (2) 2010 98 104
    • (2010) J Prosthet Dent , vol.104 , pp. 98-104
    • Aboushelib, M.N.1    Wang, H.2
  • 32
    • 0036134528 scopus 로고    scopus 로고
    • Fracture toughness of dental ceramics: Comparison of bending and indentation method
    • DOI 10.1016/S0109-5641(01)00005-7, PII S0109564101000057
    • F. Fischer, and R. Marx Fracture toughness of dental ceramics: comparison of bending and indentation method Dent Mater 18 January (1) 2002 12 19 (Pubitemid 40072297)
    • (2002) Dental Materials , vol.18 , Issue.1 , pp. 12-19
    • Fischer, H.1    Marx, R.2
  • 33
    • 33847754280 scopus 로고    scopus 로고
    • On the vickers indentation fracture toughness Test
    • DOI 10.1111/j.1551-2916.2006.01482.x
    • G.D. Quinn, and R.C. Bradt On the Vickers indentation fracture toughness test J Am Ceram Soc 90 3 2007 673 680 (Pubitemid 46384771)
    • (2007) Journal of the American Ceramic Society , vol.90 , Issue.3 , pp. 673-680
    • Quinn, G.D.1    Bradt, R.C.2
  • 34
    • 37349076574 scopus 로고    scopus 로고
    • Investigations of subcritical crack propagation of the Empress 2 all-ceramic system
    • DOI 10.1016/j.dental.2007.05.010, PII S0109564107001108
    • G. Mitov, U. Lohbauer, M.A. Rabbo, A. Petschelt, and P. Pospiech Investigations of subcritical crack propagation of the Empress 2 all-ceramic system Dent Mater 24 February (2) 2008 267 273 (Pubitemid 350299073)
    • (2008) Dental Materials , vol.24 , Issue.2 , pp. 267-273
    • Mitov, G.1    Lohbauer, U.2    Rabbo, M.A.3    Petschelt, A.4    Pospiech, P.5
  • 35
    • 0032656376 scopus 로고    scopus 로고
    • Contribution of residual stress to the strength of abrasive ground alumina
    • W.H. Tuan, and J.C. JC Kuo Contribution of residual stress to the strength of abrasive ground alumina J Eur Ceram Soc 19 1999 1593 1597
    • (1999) J Eur Ceram Soc , vol.19 , pp. 1593-1597
    • Tuan, W.H.1    Kuo, J.C.J.C.2
  • 36
    • 0024755144 scopus 로고
    • Effect of residual surface stress on the strength distribution of brittle materials
    • M.M. Tojek, and D.J. Green Effect of residual surface stress on the strength distribution of brittle materials J Am Ceram Soc 72 10 1989 1885 1890
    • (1989) J Am Ceram Soc , vol.72 , Issue.10 , pp. 1885-1890
    • Tojek, M.M.1    Green, D.J.2
  • 37
    • 84979438879 scopus 로고
    • Strengthening by surface damage in metastable tetragonal zirconia
    • T.K. Gupta Strengthening by surface damage in metastable tetragonal zirconia J Am Ceram Soc 63 1980 117 121
    • (1980) J Am Ceram Soc , vol.63 , pp. 117-121
    • Gupta, T.K.1
  • 38
    • 37049008055 scopus 로고    scopus 로고
    • Correlation of in vitro fatigue data and in vivo clinical performance of a glassceramic material
    • DOI 10.1016/j.dental.2007.01.011, PII S0109564107000450
    • U. Lohbauer, N. Krämer, A. Petschelt, and R. Frankenberger Correlation of in vitro fatigue data and in vivo clinical performance of a glassceramic material Dent Mater 24 January (1) 2008 39 44 (Pubitemid 350250806)
    • (2008) Dental Materials , vol.24 , Issue.1 , pp. 39-44
    • Lohbauer, U.1    Kramer, N.2    Petschelt, A.3    Frankenberger, R.4
  • 39
    • 0036568199 scopus 로고    scopus 로고
    • 0
    • DOI 10.1016/S0142-1123(01)00175-X, PII S014211230100175X
    • G.J. Zhihao, W. Hongjie, and J. Zhihao Comparison between fatigue behavior of some ceramics: a new concept of intrinsic stress-corrosion exponent n Int J Fatigue 24 2002 499 508 (Pubitemid 34201004)
    • (2002) International Journal of Fatigue , vol.24 , Issue.5 , pp. 499-508
    • Qiao, G.J.1    Hongjie, W.2    Zhihao, J.3
  • 40
    • 14844364021 scopus 로고    scopus 로고
    • All-ceramic fixed partial dentures designed according to the DC-Zirkon® technique. A 2-year clinical study
    • DOI 10.1111/j.1365-2842.2004.01437.x
    • V. von Steyern, F.P. Carlson, and K. Nilner All-ceramic fixed partial dentures designed according to the DC-Zirkon technique. A 2-year clinical study J Oral Rehabil 32 2005 180 187 (Pubitemid 40353824)
    • (2005) Journal of Oral Rehabilitation , vol.32 , Issue.3 , pp. 180-187
    • Vult Von Steyern, P.1    Carlson, P.2    Nilner, K.3
  • 41
    • 33749677224 scopus 로고    scopus 로고
    • The efficacy of posterior three-unit zirconium-oxide-based ceramic fixed partial dental prostheses: A prospective clinical pilot study
    • DOI 10.1016/j.prosdent.2006.08.010, PII S0022391306004033
    • A.J. Raigrodski, G.J. Chiche, N. Potiket, J.L. Hochstedler, S.E. Mohamed, S. Billiot, and D.E. Mercante The efficacy of posterior three-unit zirconium-oxide-based ceramic fixed partial dental prostheses: a prospective clinical pilot study J Prosthet Dent 96 2006 237 244 (Pubitemid 44556711)
    • (2006) Journal of Prosthetic Dentistry , vol.96 , Issue.4 , pp. 237-244
    • Raigrodski, A.J.1    Chiche, G.J.2    Potiket, N.3    Hochstedler, J.L.4    Mohamed, S.E.5    Billiot, S.6    Mercante, D.E.7
  • 42
    • 0036886280 scopus 로고    scopus 로고
    • Transformation-toughened zirconia for dental inlays, crowns and bridges: Chemical stability and effect of low-temperature aging on flexural strength and surface structure
    • DOI 10.1016/S0109-5641(01)00095-1, PII S0109564101000951
    • B.I. Ardlin Transformation-toughened zirconia for dental inlays, crowns and bridges: chemical stability and effect of low-temperature aging on flexural strength and surface structure Dent Mater 18 2002 590 595 (Pubitemid 40072229)
    • (2002) Dental Materials , vol.18 , Issue.8 , pp. 590-595
    • Ardlin, B.I.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.