메뉴 건너뛰기




Volumn 26, Issue 6, 2010, Pages 524-532

TEM characterization of a silorane composite bonded to enamel/dentin

Author keywords

Adhesion; Low shrinking composite; Nano interaction; Self etch adhesive; Silorane

Indexed keywords

ADHESIVE INTERFACES; ADHESIVE LAYERS; ADHESIVE RESINS; GERMANY; HIGH PH; HYBRID LAYER; NANO-INTERACTION; OXIRANES; PROCESSING PROCEDURES; RESIN TAGS; SELF-ETCH ADHESIVES; SILORANES; TEM; TEM CHARACTERIZATION; ULTRA STRUCTURE;

EID: 77951294799     PISSN: 01095641     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.dental.2010.01.010     Document Type: Article
Times cited : (71)

References (29)
  • 1
    • 1342264220 scopus 로고    scopus 로고
    • Determination of polymerization shrinkage stress by means of a photoelastic investigation
    • Ernst C.P., Meyer G.R., Klöcker K., and Willershausen B. Determination of polymerization shrinkage stress by means of a photoelastic investigation. Dent Mater 20 (2004) 313-321
    • (2004) Dent Mater , vol.20 , pp. 313-321
    • Ernst, C.P.1    Meyer, G.R.2    Klöcker, K.3    Willershausen, B.4
  • 4
    • 33745669458 scopus 로고    scopus 로고
    • Stability of silorane dental monomers in aqueous systems
    • Eick J.D., Smith R.E., Pinzino C.S., and Kostoryz E.L. Stability of silorane dental monomers in aqueous systems. J Dent 34 (2006) 405-410
    • (2006) J Dent , vol.34 , pp. 405-410
    • Eick, J.D.1    Smith, R.E.2    Pinzino, C.S.3    Kostoryz, E.L.4
  • 5
    • 67349133097 scopus 로고    scopus 로고
    • Macro-, micro- and nano-mechanical investigations on silorane and methacrylate-based composites
    • Ilie N., and Hickel R. Macro-, micro- and nano-mechanical investigations on silorane and methacrylate-based composites. Dent Mater 25 (2009) 810-819
    • (2009) Dent Mater , vol.25 , pp. 810-819
    • Ilie, N.1    Hickel, R.2
  • 6
    • 43449131827 scopus 로고    scopus 로고
    • Buonocore Lecture. Placing dental composites-a stressful experience
    • Ferracane J.L. Buonocore Lecture. Placing dental composites-a stressful experience. Oper Dent 33 (2008) 247-257
    • (2008) Oper Dent , vol.33 , pp. 247-257
    • Ferracane, J.L.1
  • 8
    • 0036885702 scopus 로고    scopus 로고
    • Inter-crystallite nanoretention of self-etching adhesives at enamel imaged by transmission electron microscopy
    • Hanning M., Bock H., and Hoth-Hanning W. Inter-crystallite nanoretention of self-etching adhesives at enamel imaged by transmission electron microscopy. Eur J Oral Sci 110 (2002) 464-470
    • (2002) Eur J Oral Sci , vol.110 , pp. 464-470
    • Hanning, M.1    Bock, H.2    Hoth-Hanning, W.3
  • 9
    • 0035983862 scopus 로고    scopus 로고
    • Two modes of nanoleakage expression in single step adhesives
    • Tay F.R., Pashley D.H., and Yoshiyama M. Two modes of nanoleakage expression in single step adhesives. J Dent Res 81 (2002) 472-476
    • (2002) J Dent Res , vol.81 , pp. 472-476
    • Tay, F.R.1    Pashley, D.H.2    Yoshiyama, M.3
  • 10
    • 0141924427 scopus 로고    scopus 로고
    • Buonocore memorial lecture. Adhesion to enamel and dentin: current status and future challenges
    • Van Meerbeek B., De Munck J., Yoshida Y., Inoue S., Vargas M., Vijay P., et al. Buonocore memorial lecture. Adhesion to enamel and dentin: current status and future challenges. Oper Dent 28 (2003) 647-660
    • (2003) Oper Dent , vol.28 , pp. 647-660
    • Van Meerbeek, B.1    De Munck, J.2    Yoshida, Y.3    Inoue, S.4    Vargas, M.5    Vijay, P.6
  • 11
    • 68149174592 scopus 로고    scopus 로고
    • The current status of bonding to dentin anno 2007
    • De Munck J., and Van Meerbeek B. The current status of bonding to dentin anno 2007. Int J Oral Med Sci 6 (2007) 45-60
    • (2007) Int J Oral Med Sci , vol.6 , pp. 45-60
    • De Munck, J.1    Van Meerbeek, B.2
  • 14
    • 38349178714 scopus 로고    scopus 로고
    • Marginal integrity of class V restorations: SEM versus dye penetration
    • Ernst C.P., Galler P., Willershausen B., and Haller B. Marginal integrity of class V restorations: SEM versus dye penetration. Dent Mater 24 (2008) 319-327
    • (2008) Dent Mater , vol.24 , pp. 319-327
    • Ernst, C.P.1    Galler, P.2    Willershausen, B.3    Haller, B.4
  • 16
    • 2342613606 scopus 로고    scopus 로고
    • Osmotic blistering in enamel bonded with one-step self-etch adhesives
    • Tay F.R., Lai C.N., Chersoni S., Pashley D.H., Mak Y.F., Suppa P., et al. Osmotic blistering in enamel bonded with one-step self-etch adhesives. J Dent Res 83 (2004) 290-295
    • (2004) J Dent Res , vol.83 , pp. 290-295
    • Tay, F.R.1    Lai, C.N.2    Chersoni, S.3    Pashley, D.H.4    Mak, Y.F.5    Suppa, P.6
  • 18
    • 41949094632 scopus 로고    scopus 로고
    • Can the durability of one-step self-etch adhesives be improved by double application or by an extra layer of hydrophobic resin?
    • Reis A., Albuquerque M., Pegoraro M., Mattei G., Bauer J.R., Grande R.H., et al. Can the durability of one-step self-etch adhesives be improved by double application or by an extra layer of hydrophobic resin?. J Dent 36 (2008) 309-315
    • (2008) J Dent , vol.36 , pp. 309-315
    • Reis, A.1    Albuquerque, M.2    Pegoraro, M.3    Mattei, G.4    Bauer, J.R.5    Grande, R.H.6
  • 19
    • 0037640986 scopus 로고    scopus 로고
    • How can nanoleakage occur in self-etching adhesive systems that demineralize and infiltrate simultaneously?
    • Tay F.R., King N.M., Chan K.M., and Pashley D.H. How can nanoleakage occur in self-etching adhesive systems that demineralize and infiltrate simultaneously?. J Adhes Dent 4 (2002) 255-269
    • (2002) J Adhes Dent , vol.4 , pp. 255-269
    • Tay, F.R.1    King, N.M.2    Chan, K.M.3    Pashley, D.H.4
  • 21
    • 75449104289 scopus 로고    scopus 로고
    • Does a low-shrinking composite induce less stress at the adhesive interface?
    • Van Ende A., De Munck J., Mine A., Lambrechts P., and Van Meerbeek B. Does a low-shrinking composite induce less stress at the adhesive interface?. Dent Mater 26 (2010) 215-222
    • (2010) Dent Mater , vol.26 , pp. 215-222
    • Van Ende, A.1    De Munck, J.2    Mine, A.3    Lambrechts, P.4    Van Meerbeek, B.5
  • 23
  • 28
    • 0042522352 scopus 로고    scopus 로고
    • Water treeing-a potential mechanism for degradation of dentin adhesives
    • Tay F.R., and Pashley D.H. Water treeing-a potential mechanism for degradation of dentin adhesives. Am J Dent 16 (2003) 6-12
    • (2003) Am J Dent , vol.16 , pp. 6-12
    • Tay, F.R.1    Pashley, D.H.2
  • 29
    • 37549057992 scopus 로고    scopus 로고
    • The "Myth" of nanoleakage
    • Van Meerbeek B. The "Myth" of nanoleakage. J Adhes Dent 9 (2007) 491-492
    • (2007) J Adhes Dent , vol.9 , pp. 491-492
    • Van Meerbeek, B.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.