메뉴 건너뛰기




Volumn 25, Issue 4, 2006, Pages 669-674

Effects of alumina-blasting and adhesive primers on bonding between resin luting agent and zirconia ceramics

Author keywords

Bond strength; Resin luting agent; Zirconia ceramic

Indexed keywords

4 MET ADHESION PROMOTING MONOMER; 4-MET ADHESION PROMOTING MONOMER; ALUMINUM OXIDE; GC METAL PRIMER; MDP ADHESION PROMOTING MONOMER; METHACRYLIC ACID DERIVATIVE; ORGANOPHOSPHORUS COMPOUND; RESIN CEMENT; TRICARBOXYLIC ACID; UNCLASSIFIED DRUG; YTTRIA STABILIZED TETRAGONAL ZIRCONIA POLYCRYSTALS CERAMIC; YTTRIA-STABILIZED TETRAGONAL ZIRCONIA POLYCRYSTALS CERAMIC; YTTRIUM;

EID: 33947507846     PISSN: 02874547     EISSN: None     Source Type: Journal    
DOI: 10.4012/dmj.25.669     Document Type: Article
Times cited : (107)

References (38)
  • 1
    • 0027548762 scopus 로고
    • Recent developments in restorative dental ceramics
    • Anusavice KJ. Recent developments in restorative dental ceramics. J Am Dent Assoc 1993; 124: 72-84.
    • (1993) J Am Dent Assoc , vol.124 , pp. 72-84
    • Anusavice, K.J.1
  • 2
    • 0029678682 scopus 로고    scopus 로고
    • Ceramics in dentistry: Historical roots and current perspectives
    • Kelly JR, Nishimura I, Compbell SD. Ceramics in dentistry: Historical roots and current perspectives. J Prosthet Dent 1996; 75: 18-32.
    • (1996) J Prosthet Dent , vol.75 , pp. 18-32
    • Kelly, J.R.1    Nishimura, I.2    Compbell, S.D.3
  • 3
    • 0032917811 scopus 로고    scopus 로고
    • Zirconia as a ceramic biomaterial
    • Piconi C, Maccauro G. Zirconia as a ceramic biomaterial. Biomaterials 1999; 20: 1-25.
    • (1999) Biomaterials , vol.20 , pp. 1-25
    • Piconi, C.1    Maccauro, G.2
  • 4
    • 0028434170 scopus 로고
    • Long-term in vivo and in vitro aging of a zirconia ceramic used in orthopaedy
    • Cales B, Stefani Y, Lilley E. Long-term in vivo and in vitro aging of a zirconia ceramic used in orthopaedy. J Biomed Mater Res 1994; 28: 619-624.
    • (1994) J Biomed Mater Res , vol.28 , pp. 619-624
    • Cales, B.1    Stefani, Y.2    Lilley, E.3
  • 5
    • 0024546336 scopus 로고
    • Mechanical properties and short-term in-vivo evaluation of yttrium-oxide-partially- stabilized zirconia
    • Christel P, Meunier A, Heller M, Torre JP, Peille CN. Mechanical properties and short-term in-vivo evaluation of yttrium-oxide-partially- stabilized zirconia. J Biomed Mater Res 1989; 23: 45-61.
    • (1989) J Biomed Mater Res , vol.23 , pp. 45-61
    • Christel, P.1    Meunier, A.2    Heller, M.3    Torre, J.P.4    Peille, C.N.5
  • 6
    • 85039199354 scopus 로고    scopus 로고
    • Description of the performance of the main inert bioceramics
    • Barbucci R ed, Kluwer Academic/Plenum, New York
    • Krajewski A, Ravaglioli A. Description of the performance of the main inert bioceramics. In: Integrated biomaterials science, Barbucci R (ed.), Kluwer Academic/Plenum, New York, 2002, pp.210-213.
    • (2002) Integrated biomaterials science , pp. 210-213
    • Krajewski, A.1    Ravaglioli, A.2
  • 7
    • 0029436750 scopus 로고
    • Zirconia posts: A new all-ceramic concept for nonvital abutment teeth
    • Meyenberg KH, Lüthy H, Schärer P. Zirconia posts: A new all-ceramic concept for nonvital abutment teeth. J Esthet Dent 1995; 7: 73-80.
    • (1995) J Esthet Dent , vol.7 , pp. 73-80
    • Meyenberg, K.H.1    Lüthy, H.2    Schärer, P.3
  • 8
    • 0035231506 scopus 로고    scopus 로고
    • Lopes GC, Baratieri LN, Caldeira de Andrada MA, Maia HP. All-ceramic post, core, and crown: Technique and case report. J Esthet Restor Dent 2001; 13: 285-295.9
    • Lopes GC, Baratieri LN, Caldeira de Andrada MA, Maia HP. All-ceramic post, core, and crown: Technique and case report. J Esthet Restor Dent 2001; 13: 285-295.9)
  • 9
    • 85039188416 scopus 로고    scopus 로고
    • Luthardt R, Herold V, Sandkuhl O, Reitz B, Knaak JP, Lenz E. Kronen aus Hochleistungskeramik, Zirkonoxid-Keramik, ein neuer Werkstoff in der Kronenprothetik. Dtsch Zahnärztl Z 1998; 53: 280-285.
    • Luthardt R, Herold V, Sandkuhl O, Reitz B, Knaak JP, Lenz E. Kronen aus Hochleistungskeramik, Zirkonoxid-Keramik, ein neuer Werkstoff in der Kronenprothetik. Dtsch Zahnärztl Z 1998; 53: 280-285.
  • 10
    • 0032018397 scopus 로고    scopus 로고
    • All-ceramic alternatives to conventional metal-ceramic restorations
    • McLaren EA. All-ceramic alternatives to conventional metal-ceramic restorations. Compend Contin Educ Dent 1998; 19: 307-312.
    • (1998) Compend Contin Educ Dent , vol.19 , pp. 307-312
    • McLaren, E.A.1
  • 11
    • 0036593234 scopus 로고    scopus 로고
    • Long-term clinical success of all-ceramic posterior restorations
    • Blatz MB. Long-term clinical success of all-ceramic posterior restorations. Quintessence Int 2002; 33: 415-426.
    • (2002) Quintessence Int , vol.33 , pp. 415-426
    • Blatz, M.B.1
  • 12
    • 0022732872 scopus 로고
    • The adhesion mechanism of dental adhesive resin to the alloy: Relationship between Co-Cr alloy surface structure analyzed by ESCA and bonding strength of adhesive resin
    • Ohno H, Araki Y, Sagara M. The adhesion mechanism of dental adhesive resin to the alloy: Relationship between Co-Cr alloy surface structure analyzed by ESCA and bonding strength of adhesive resin. Dent Mater J 1986; 5: 46-65.
    • (1986) Dent Mater J , vol.5 , pp. 46-65
    • Ohno, H.1    Araki, Y.2    Sagara, M.3
  • 13
    • 0013553958 scopus 로고    scopus 로고
    • Study on adhesive primer to dental metal used for composite type resin cement
    • Kojima K, Kadoma Y, Yamauchi J. Study on adhesive primer to dental metal used for composite type resin cement. J J Dent Mater 1997; 16: 316-321.
    • (1997) J J Dent Mater , vol.16 , pp. 316-321
    • Kojima, K.1    Kadoma, Y.2    Yamauchi, J.3
  • 14
    • 0001725930 scopus 로고
    • Funktionelle Gruppen an Festkörper-Oberflächen
    • HP Boehm. Funktionelle Gruppen an Festkörper-Oberflächen. Angew Chem 1966; 78: 617-628.
    • (1966) Angew Chem , vol.78 , pp. 617-628
    • Boehm, H.P.1
  • 15
    • 0021903030 scopus 로고
    • Etched porcelain veneers: The current state of the art
    • Calamia JR. Etched porcelain veneers: the current state of the art. Quintessence Int 1985; 1: 5-12.
    • (1985) Quintessence Int , vol.1 , pp. 5-12
    • Calamia, J.R.1
  • 16
    • 0023413139 scopus 로고
    • Shear strength of the composite bond to etched porcelain
    • Stangel I, Nathanson D, Hsu CS. Shear strength of the composite bond to etched porcelain. J Dent Res 1987; 66: 1460-1465.
    • (1987) J Dent Res , vol.66 , pp. 1460-1465
    • Stangel, I.1    Nathanson, D.2    Hsu, C.S.3
  • 17
    • 0028489343 scopus 로고
    • Comparison of acidulated phosphate fluoride gel and hydrofluoric acid etchants for porcelain-composite repair
    • Tylka DF, Stewart G. Comparison of acidulated phosphate fluoride gel and hydrofluoric acid etchants for porcelain-composite repair. J Prosthet Dent 1994; 72: 121-127.
    • (1994) J Prosthet Dent , vol.72 , pp. 121-127
    • Tylka, D.F.1    Stewart, G.2
  • 18
    • 0028523833 scopus 로고
    • Effect of porcelain surface treatments on bond strengths of composite resin bonded to porcelain
    • Thurmond JW, Barkmeier WW, Wilwerding TM. Effect of porcelain surface treatments on bond strengths of composite resin bonded to porcelain. J Prosthet Dent 1994; 72: 355-359.
    • (1994) J Prosthet Dent , vol.72 , pp. 355-359
    • Thurmond, J.W.1    Barkmeier, W.W.2    Wilwerding, T.M.3
  • 19
    • 0029299001 scopus 로고
    • Adhesion of composite to porcelain with various surface conditions
    • Aida M, Hayakawa T, Mizukawa K. Adhesion of composite to porcelain with various surface conditions. J Prosthet Dent 1995; 73: 464-470.
    • (1995) J Prosthet Dent , vol.73 , pp. 464-470
    • Aida, M.1    Hayakawa, T.2    Mizukawa, K.3
  • 20
    • 0024103132 scopus 로고    scopus 로고
    • Tensile bond to resin cements to porcelain veneers
    • Nicholls JI. Tensile bond to resin cements to porcelain veneers. J Prosthet Dent 1998; 60: 443-447.
    • (1998) J Prosthet Dent , vol.60 , pp. 443-447
    • Nicholls, J.I.1
  • 21
    • 0141727597 scopus 로고    scopus 로고
    • Effect of surface conditioning methods on the bond strength of luting cement to ceramics
    • Özcan M, Vallittu PK. Effect of surface conditioning methods on the bond strength of luting cement to ceramics. Dent Mater 2003; 19: 725-731.
    • (2003) Dent Mater , vol.19 , pp. 725-731
    • Özcan, M.1    Vallittu, P.K.2
  • 22
    • 0026815439 scopus 로고
    • An investigation of the composite resin/porcelain interface
    • Lu R, Harcourt JK, Tyas MJ, Alexander B. An investigation of the composite resin/porcelain interface. Aust Dent J 1992; 37: 12-19.
    • (1992) Aust Dent J , vol.37 , pp. 12-19
    • Lu, R.1    Harcourt, J.K.2    Tyas, M.J.3    Alexander, B.4
  • 23
    • 0029372422 scopus 로고
    • Shear vs. tensile bond strength of resin composite bonded to ceramic
    • Della Bona A, van Noort R. Shear vs. tensile bond strength of resin composite bonded to ceramic. J Dent Res 1995; 74: 1591-1596.
    • (1995) J Dent Res , vol.74 , pp. 1591-1596
    • Della Bona, A.1    van Noort, R.2
  • 24
    • 0042994079 scopus 로고    scopus 로고
    • Debnath S, Wunder SL, McCool JI, Baran GR. Silane treatment effects on glass/resin interfacial shear strengths. Dent Mater 2003; 19: 441-448.25
    • Debnath S, Wunder SL, McCool JI, Baran GR. Silane treatment effects on glass/resin interfacial shear strengths. Dent Mater 2003; 19: 441-448.25)
  • 25
    • 13444310582 scopus 로고    scopus 로고
    • Effect of surface treatments on the resin bond to zirconium-based ceramic
    • Bottino MA, Valandro LF, Scotti R, Buso L. Effect of surface treatments on the resin bond to zirconium-based ceramic. Int J Prosthodont 2005; 18: 60-65.
    • (2005) Int J Prosthodont , vol.18 , pp. 60-65
    • Bottino, M.A.1    Valandro, L.F.2    Scotti, R.3    Buso, L.4
  • 26
    • 0041919708 scopus 로고    scopus 로고
    • Effect of etching and airborne particle abrasion on the microstructure of different dental ceramics
    • Borges GA, Sophr AM, de Goes MF, Sobrinho LC, Chan DCN. Effect of etching and airborne particle abrasion on the microstructure of different dental ceramics. J Prosthet Dent 2003; 89: 479-488.
    • (2003) J Prosthet Dent , vol.89 , pp. 479-488
    • Borges, G.A.1    Sophr, A.M.2    de Goes, M.F.3    Sobrinho, L.C.4    Chan, D.C.N.5
  • 27
    • 0031598657 scopus 로고    scopus 로고
    • Bonding to zirconia ceramic: Adhesion methods and their durability
    • Kern M, Wegner SM. Bonding to zirconia ceramic: adhesion methods and their durability. Dent Mater 1998; 14: 64-71.
    • (1998) Dent Mater , vol.14 , pp. 64-71
    • Kern, M.1    Wegner, S.M.2
  • 28
    • 0034208413 scopus 로고    scopus 로고
    • Long-term resin bond strength to zirconia ceramic
    • Wegner SM, Kern M. Long-term resin bond strength to zirconia ceramic. J Adhes Dent 2000; 2: 139-147.
    • (2000) J Adhes Dent , vol.2 , pp. 139-147
    • Wegner, S.M.1    Kern, M.2
  • 29
    • 1942456928 scopus 로고    scopus 로고
    • In vitro evaluation of shear bond strengths of resin to densely-sintered high-purity zirconium-oxide ceramic after long-term storage and thermal cycling
    • Blatz MB, Sadan A, Martin J, Lang B. In vitro evaluation of shear bond strengths of resin to densely-sintered high-purity zirconium-oxide ceramic after long-term storage and thermal cycling. J Prosthet Dent 2004; 91: 356-362.
    • (2004) J Prosthet Dent , vol.91 , pp. 356-362
    • Blatz, M.B.1    Sadan, A.2    Martin, J.3    Lang, B.4
  • 30
    • 0027605367 scopus 로고
    • Bond strength of composite to etched and sandblasted porcelain
    • Wolf DM, Powers JM, O'Keefe KL. Bond strength of composite to etched and sandblasted porcelain. Am J Dent 1993; 6: 155-158.
    • (1993) Am J Dent , vol.6 , pp. 155-158
    • Wolf, D.M.1    Powers, J.M.2    O'Keefe, K.L.3
  • 31
    • 0029349125 scopus 로고
    • Relationship between sandblasting and composite resin-alloy bond strength by a silica coating
    • Mukai M, Fukui H, Hasegawa J. Relationship between sandblasting and composite resin-alloy bond strength by a silica coating. J Prosthet Dent 1995; 74: 151-155.
    • (1995) J Prosthet Dent , vol.74 , pp. 151-155
    • Mukai, M.1    Fukui, H.2    Hasegawa, J.3
  • 32
    • 0033210779 scopus 로고    scopus 로고
    • Effect of sandblasting and silicoating on bond strength of polymer-glass composite to cast titanium
    • Watanabe I, Kurtz KS, Kabcenell JL, Okabe T. Effect of sandblasting and silicoating on bond strength of polymer-glass composite to cast titanium. J Prosthet Dent 1999; 82: 462-467.
    • (1999) J Prosthet Dent , vol.82 , pp. 462-467
    • Watanabe, I.1    Kurtz, K.S.2    Kabcenell, J.L.3    Okabe, T.4
  • 33
    • 0842290826 scopus 로고    scopus 로고
    • Bonding indirect resin composites to metal: Part 2. Effect of alloy surface treatment on elemental composition of alloy and bond strength
    • Petridis H, Garefis P, Hirayama H, Kafantaris NM, Koidis PT. Bonding indirect resin composites to metal: Part 2. Effect of alloy surface treatment on elemental composition of alloy and bond strength. Int J Prosthodont 2004; 17: 77-82.
    • (2004) Int J Prosthodont , vol.17 , pp. 77-82
    • Petridis, H.1    Garefis, P.2    Hirayama, H.3    Kafantaris, N.M.4    Koidis, P.T.5
  • 34
    • 34247392255 scopus 로고    scopus 로고
    • The characteristic of metal primer 'GC METAL PRIMER II'
    • Abstract No.2385
    • Ueno T, Kumagai T, Hirota K. The characteristic of metal primer 'GC METAL PRIMER II'. J Dent Res 1997; 76 (Special Issue 312): Abstract No.2385.
    • (1997) J Dent Res , vol.76 , Issue.SPEC. ISSUE 312
    • Ueno, T.1    Kumagai, T.2    Hirota, K.3
  • 35
    • 0020781261 scopus 로고
    • Strong composites of dimethylacrylates with 4-methacryloxyethyl trimellitic anhydride
    • Atsuta M, Nagata K, Turner DT. Strong composites of dimethylacrylates with 4-methacryloxyethyl trimellitic anhydride. J Biomed Mater Res 1983; 17: 679-690.
    • (1983) J Biomed Mater Res , vol.17 , pp. 679-690
    • Atsuta, M.1    Nagata, K.2    Turner, D.T.3
  • 36
    • 33645419309 scopus 로고    scopus 로고
    • Bonding of dual-cured resin cement to zirconia ceramic using phosphate acid ester monomer and zirconate coupler
    • Yoshida K, Tsuo Y, Atsuta M. Bonding of dual-cured resin cement to zirconia ceramic using phosphate acid ester monomer and zirconate coupler. J Biomed Mater Res 2006; 77B: 28-33.
    • (2006) J Biomed Mater Res , vol.77 B , pp. 28-33
    • Yoshida, K.1    Tsuo, Y.2    Atsuta, M.3
  • 38
    • 33744789998 scopus 로고    scopus 로고
    • Effect of zirconium-oxide ceramic surface treatments on the bond strength to adhesive resin
    • Atsu SS, Kilicarslan MA, Kucukesmen HC, Aka PS. Effect of zirconium-oxide ceramic surface treatments on the bond strength to adhesive resin. J Prosthet Dent 2006; 95: 430-436.
    • (2006) J Prosthet Dent , vol.95 , pp. 430-436
    • Atsu, S.S.1    Kilicarslan, M.A.2    Kucukesmen, H.C.3    Aka, P.S.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.