Selective infiltration-etching technique for a strong and durable bond of resin cements to zirconia-based materials

Author keywords

[No Author keywords available]

Indexed keywords

BIOMEDICAL AND DENTAL MATERIALS; RESIN CEMENT; ZIRCONIUM; ZIRCONIUM OXIDE;

EID: 36049040304     PISSN: 00223913     EISSN: None     Source Type: Journal    
DOI: 10.1016/S0022-3913(07)60123-1     Document Type: Article
Times cited : (271)

References (32)
  • 1
    • 33746623731 scopus 로고    scopus 로고
    • Microtensile bond strength of different components of core veneered all-ceramic restorations: Part II: Zirconia veneering ceramics
    • Aboushelib M., Kleverlaan C., and Feilzer A. Microtensile bond strength of different components of core veneered all-ceramic restorations: Part II: Zirconia veneering ceramics. Dent Mater 22 (2006) 857-863
    • (2006) Dent Mater , vol.22 , pp. 857-863
    • Aboushelib, M.1    Kleverlaan, C.2    Feilzer, A.3
  • 2
    • 0034157359 scopus 로고    scopus 로고
    • Bond strength of luting cements to zirconium oxide ceramics
    • Derand P., and Derand T. Bond strength of luting cements to zirconium oxide ceramics. Int J Prosthodont 13 (2000) 131-135
    • (2000) Int J Prosthodont , vol.13 , pp. 131-135
    • Derand, P.1    Derand, T.2
  • 3
    • 33644642412 scopus 로고    scopus 로고
    • A single-retainer zirconium dioxide ceramic resin-bonded fixed partial denture for single tooth replacement: a clinical report
    • Komine F., and Tomic M. A single-retainer zirconium dioxide ceramic resin-bonded fixed partial denture for single tooth replacement: a clinical report. J Oral Sci 47 (2005) 139-142
    • (2005) J Oral Sci , vol.47 , pp. 139-142
    • Komine, F.1    Tomic, M.2
  • 4
    • 0033111440 scopus 로고    scopus 로고
    • Long-term survival characteristics of 832 resin-retained bridges and splints provided in a post-graduate teaching hospital between 1978 and 1993
    • Djemal S., Setchell D., King P., and Wickens J. Long-term survival characteristics of 832 resin-retained bridges and splints provided in a post-graduate teaching hospital between 1978 and 1993. J Oral Rehabil 26 (1999) 302-320
    • (1999) J Oral Rehabil , vol.26 , pp. 302-320
    • Djemal, S.1    Setchell, D.2    King, P.3    Wickens, J.4
  • 5
    • 0038644503 scopus 로고    scopus 로고
    • Resin-ceramic bonding: A review of the literature
    • Blatz M., Sadan A., and Kern M. Resin-ceramic bonding: A review of the literature. J Prosthet Dent 89 (2003) 268-274
    • (2003) J Prosthet Dent , vol.89 , pp. 268-274
    • Blatz, M.1    Sadan, A.2    Kern, M.3
  • 6
    • 32044438490 scopus 로고    scopus 로고
    • Microtensile bond strength of a resin cement to glass infiltrated zirconia-reinforced ceramic: the effect of surface conditioning
    • Amaral R., Ozcan M., Bottino M., and Valandro L. Microtensile bond strength of a resin cement to glass infiltrated zirconia-reinforced ceramic: the effect of surface conditioning. Dent Mater 22 (2006) 283-290
    • (2006) Dent Mater , vol.22 , pp. 283-290
    • Amaral, R.1    Ozcan, M.2    Bottino, M.3    Valandro, L.4
  • 7
    • 13444310582 scopus 로고    scopus 로고
    • Effect of surface treatments on the resin bond to zirconium-based ceramic
    • Bottino M., Valandro L., Scotti R., and Buso L. Effect of surface treatments on the resin bond to zirconium-based ceramic. Int J Prosthodont 18 (2005) 60-65
    • (2005) Int J Prosthodont , vol.18 , pp. 60-65
    • Bottino, M.1    Valandro, L.2    Scotti, R.3    Buso, L.4
  • 8
    • 0042994086 scopus 로고    scopus 로고
    • A new adhesive technology for all-ceramics
    • Janda R., Roulet J., Wulf M., and Tiller H. A new adhesive technology for all-ceramics. Dent Mater 19 (2003) 567-573
    • (2003) Dent Mater , vol.19 , pp. 567-573
    • Janda, R.1    Roulet, J.2    Wulf, M.3    Tiller, H.4
  • 9
    • 31544457886 scopus 로고    scopus 로고
    • Microstructural and crystallographic surface changes after grinding zirconia-based dental ceramics
    • Denry I., and Holloway J. Microstructural and crystallographic surface changes after grinding zirconia-based dental ceramics. J Biomed Mater Res B Appl Biomater 76 (2006) 440-448
    • (2006) J Biomed Mater Res B Appl Biomater , vol.76 , pp. 440-448
    • Denry, I.1    Holloway, J.2
  • 10
    • 0036561939 scopus 로고    scopus 로고
    • Effect of different artificial aging conditions on ceramic-composite bond strength
    • Wegner S., Gerdes W., and Kern M. Effect of different artificial aging conditions on ceramic-composite bond strength. Int J Prosthodont 15 (2002) 267-272
    • (2002) Int J Prosthodont , vol.15 , pp. 267-272
    • Wegner, S.1    Gerdes, W.2    Kern, M.3
  • 11
    • 30344433724 scopus 로고    scopus 로고
    • Effect of thermocycling on bond strength of luting cements to zirconia ceramic
    • Luthy H., Loeffel O., and Hammerle C. Effect of thermocycling on bond strength of luting cements to zirconia ceramic. Dent Mater 22 (2006) 95-200
    • (2006) Dent Mater , vol.22 , pp. 95-200
    • Luthy, H.1    Loeffel, O.2    Hammerle, C.3
  • 12
    • 0034208413 scopus 로고    scopus 로고
    • Long-term resin bond strength to zirconia ceramic
    • Wegner S., and Kern M. Long-term resin bond strength to zirconia ceramic. J Adhes Dent 2 (2000) 139-147
    • (2000) J Adhes Dent , vol.2 , pp. 139-147
    • Wegner, S.1    Kern, M.2
  • 13
    • 5344253044 scopus 로고    scopus 로고
    • In vitro fracture resistance of posterior metal-ceramic and all-ceramic inlay-retained resin-bonded fixed partial dentures
    • Kilicarslan M., Kedici P., Kucukesmen H., and Uludag B. In vitro fracture resistance of posterior metal-ceramic and all-ceramic inlay-retained resin-bonded fixed partial dentures. J Prosthet Dent 92 (2004) 365-370
    • (2004) J Prosthet Dent , vol.92 , pp. 365-370
    • Kilicarslan, M.1    Kedici, P.2    Kucukesmen, H.3    Uludag, B.4
  • 14
    • 19744367539 scopus 로고    scopus 로고
    • The shear bond strength between luting cements and zirconia ceramics after two pre-treatments
    • Piwowarczyk A., Lauer H., and Sorensen J. The shear bond strength between luting cements and zirconia ceramics after two pre-treatments. Oper Dent 30 (2005) 382-388
    • (2005) Oper Dent , vol.30 , pp. 382-388
    • Piwowarczyk, A.1    Lauer, H.2    Sorensen, J.3
  • 15
    • 0029266741 scopus 로고
    • Bonding to glass infiltrated alumina ceramic: adhesive methods and their durability
    • Kern M., and Thompson V. Bonding to glass infiltrated alumina ceramic: adhesive methods and their durability. J Prosthet Dent 73 (1995) 240-249
    • (1995) J Prosthet Dent , vol.73 , pp. 240-249
    • Kern, M.1    Thompson, V.2
  • 16
    • 0031598657 scopus 로고    scopus 로고
    • Bonding to zirconia ceramic: adhesion methods and their durability
    • Kern M., and Wegner S. Bonding to zirconia ceramic: adhesion methods and their durability. Dent Mater 14 (1998) 64-71
    • (1998) Dent Mater , vol.14 , pp. 64-71
    • Kern, M.1    Wegner, S.2
  • 17
    • 0029363971 scopus 로고
    • Tensile bond strength of resin luting cement to glass infiltrated porous aluminum oxide cores (In-Ceram)
    • Isidor F., Stokholm R., and Ravnholt G. Tensile bond strength of resin luting cement to glass infiltrated porous aluminum oxide cores (In-Ceram). Eur J Prosthodont Restor Dent 3 (1995) 199-202
    • (1995) Eur J Prosthodont Restor Dent , vol.3 , pp. 199-202
    • Isidor, F.1    Stokholm, R.2    Ravnholt, G.3
  • 18
    • 33744789998 scopus 로고    scopus 로고
    • Effect of zirconium-oxide ceramic surface treatments on the bond strength to adhesive resin
    • Atsu S., Kilicarslan M., Kucukesmen H., and Aka P. Effect of zirconium-oxide ceramic surface treatments on the bond strength to adhesive resin. J Prosthet Dent 95 (2006) 430-436
    • (2006) J Prosthet Dent , vol.95 , pp. 430-436
    • Atsu, S.1    Kilicarslan, M.2    Kucukesmen, H.3    Aka, P.4
  • 19
    • 0032917811 scopus 로고    scopus 로고
    • Zirconia as a ceramic biomaterial
    • Piconi C., and Maccauro G. Zirconia as a ceramic biomaterial. Biomaterials 20 (1999) 1-25
    • (1999) Biomaterials , vol.20 , pp. 1-25
    • Piconi, C.1    Maccauro, G.2
  • 20
    • 2342500842 scopus 로고    scopus 로고
    • Critical effect of cubic phase on aging in 3mol% yttria-stabilized zirconia ceramics for hip replacement prosthesis
    • Chevalier J., Deville S., Munch E., Jullian R., and Lair F. Critical effect of cubic phase on aging in 3mol% yttria-stabilized zirconia ceramics for hip replacement prosthesis. Biomaterials 25 (2004) 5539-5545
    • (2004) Biomaterials , vol.25 , pp. 5539-5545
    • Chevalier, J.1    Deville, S.2    Munch, E.3    Jullian, R.4    Lair, F.5
  • 21
    • 25144511110 scopus 로고    scopus 로고
    • Microtensile bond strength of different components of core veneered all-ceramic restorations
    • Aboushelib M., de Jager N., Kleverlaan C., and Feilzer A. Microtensile bond strength of different components of core veneered all-ceramic restorations. Dent Mater 21 (2005) 984-991
    • (2005) Dent Mater , vol.21 , pp. 984-991
    • Aboushelib, M.1    de Jager, N.2    Kleverlaan, C.3    Feilzer, A.4
  • 22
    • 0024107289 scopus 로고
    • Deformation mechanisms in yttria-stabilized zirconia
    • Lankford J., Page R., and Rabenberg L. Deformation mechanisms in yttria-stabilized zirconia. J Mater Sci 23 (1988) 4144-4156
    • (1988) J Mater Sci , vol.23 , pp. 4144-4156
    • Lankford, J.1    Page, R.2    Rabenberg, L.3
  • 23
    • 27644579439 scopus 로고    scopus 로고
    • Atomic force microscopy study and qualitative analysis of martensite relief in zirconia
    • Deville S., Chevalier J., and El Attaoui H. Atomic force microscopy study and qualitative analysis of martensite relief in zirconia. J Am Ceram Soc 88 (2005) 1261-1267
    • (2005) J Am Ceram Soc , vol.88 , pp. 1261-1267
    • Deville, S.1    Chevalier, J.2    El Attaoui, H.3
  • 26
    • 0035790828 scopus 로고    scopus 로고
    • Strain hardening in superplastic codoped yttria-stabilized tetragonal-zirconia polycrystals
    • Sasaki K., Nakano M., Mimurada J., Ikuhara Y., and Sakuma T. Strain hardening in superplastic codoped yttria-stabilized tetragonal-zirconia polycrystals. J Am Ceram Soc 84 (2001) 2981-2986
    • (2001) J Am Ceram Soc , vol.84 , pp. 2981-2986
    • Sasaki, K.1    Nakano, M.2    Mimurada, J.3    Ikuhara, Y.4    Sakuma, T.5
  • 27
    • 27644497277 scopus 로고    scopus 로고
    • Direct evidence of dopant-enhanced grain-boundary sliding in yttria-stabilized zirconia bicrystals
    • Nakamora A., Shibata N., Morishige N., Mastsunaga K., Ikuhara Y., and Yamamoto T. Direct evidence of dopant-enhanced grain-boundary sliding in yttria-stabilized zirconia bicrystals. J Am Ceram Soc 88 (2005) 938-942
    • (2005) J Am Ceram Soc , vol.88 , pp. 938-942
    • Nakamora, A.1    Shibata, N.2    Morishige, N.3    Mastsunaga, K.4    Ikuhara, Y.5    Yamamoto, T.6
  • 28
    • 0030191024 scopus 로고    scopus 로고
    • 3: Defect mechanism and dopant effects
    • 3: Defect mechanism and dopant effects. J Am Ceram Soc 79 (1996) 1801-1809
    • (1996) J Am Ceram Soc , vol.79 , pp. 1801-1809
    • Chen, P.1    Chen, I.2
  • 30
    • 36048937881 scopus 로고    scopus 로고
    • Aboushelib M, Feilzer A: New surface treatment for zirconia based materials. European patent application No 050773969;2006.
  • 31
    • 0029298930 scopus 로고
    • Flexural strength of an infused ceramic, glass ceramic, and feldspathic porcelain
    • Giordano II R., Pelletier L., Campbell S., and Pober R. Flexural strength of an infused ceramic, glass ceramic, and feldspathic porcelain. J Prosthet Dent 73 (1995) 411-418
    • (1995) J Prosthet Dent , vol.73 , pp. 411-418
    • Giordano II, R.1    Pelletier, L.2    Campbell, S.3    Pober, R.4
  • 32
    • 0043130574 scopus 로고    scopus 로고
    • Microtensile bond strength testing of luting cements to prefabricated CAD/CAM ceramic and composite blocks
    • El Zohairy A., De Gee A., Mohsen M., and Feilzer A. Microtensile bond strength testing of luting cements to prefabricated CAD/CAM ceramic and composite blocks. Dent Mater 19 (2003) 575-583
    • (2003) Dent Mater , vol.19 , pp. 575-583
    • El Zohairy, A.1    De Gee, A.2    Mohsen, M.3    Feilzer, A.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.