Volumn 28, Issue 11, 2008, Pages 2247-2257

Synthesis and structural characterization of carbon-rich SiCxOy derived from a Ni-containing hybrid polymer

Author keywords

Carbides; Glass ceramics; Polymer pyrolysis; SiC

Indexed keywords

CARBON; CHARACTERIZATION; MOLECULAR STRUCTURE; NICKEL; NUCLEAR MAGNETIC RESONANCE; POLYMERS; PYROLYSIS; SILICON CARBIDE; STRUCTURAL PROPERTIES; SYNTHESIS (CHEMICAL); THERMAL EFFECTS; THERMODYNAMIC STABILITY;

EID: 43949090829     PISSN: 09552219     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.jeurceramsoc.2008.03.001     Document Type: Article
Times cited : (58)

References (50)
  • 2
    • 2542479641 scopus 로고
    • Silicon oxycarbide glasses. Part II. Structure and properties
    • Renlund G.M., Prochazka S., and Doremus R.H. Silicon oxycarbide glasses. Part II. Structure and properties. J. Mater. Res. 6 (1991) 2723-2734
    • (1991) J. Mater. Res. , vol.6 , pp. 2723-2734
    • Renlund, G.M.1    Prochazka, S.2    Doremus, R.H.3
  • 3
    • 0028542255 scopus 로고
    • Nanostructural characterization of silicon oxycarbide glasses and glass-ceramics
    • Breval E., Hammond M., and Pantano C.G. Nanostructural characterization of silicon oxycarbide glasses and glass-ceramics. J. Am. Ceram. Soc. 77 (1994) 3012-3018
    • (1994) J. Am. Ceram. Soc. , vol.77 , pp. 3012-3018
    • Breval, E.1    Hammond, M.2    Pantano, C.G.3
  • 6
    • 0036605224 scopus 로고    scopus 로고
    • Investigation on kinetics of thermal decomposition in polysiloxane networks used as precursors of silicon oxycarbide glasses
    • Schiavon M.A., Redondo S.U.A., Pina S.R.O., and Yoshida I.V.P. Investigation on kinetics of thermal decomposition in polysiloxane networks used as precursors of silicon oxycarbide glasses. J. Non-Cryst. Solids 304 (2002) 92-100
    • (2002) J. Non-Cryst. Solids , vol.304 , pp. 92-100
    • Schiavon, M.A.1    Redondo, S.U.A.2    Pina, S.R.O.3    Yoshida, I.V.P.4
  • 7
    • 3042533408 scopus 로고    scopus 로고
    • Systematic structural characterization of the high-temperature behavior of nearly stoichiometric silicon oxycarbide glasses
    • Bréquel H., Parmentier J., Walter S., Badheka R., Trimmel G., Masse S., et al. Systematic structural characterization of the high-temperature behavior of nearly stoichiometric silicon oxycarbide glasses. Chem. Mater. 16 (2004) 2585-2598
    • (2004) Chem. Mater. , vol.16 , pp. 2585-2598
    • Bréquel, H.1    Parmentier, J.2    Walter, S.3    Badheka, R.4    Trimmel, G.5    Masse, S.6
  • 8
    • 26444505955 scopus 로고    scopus 로고
    • Nanoprocesses in polymer-derived Si-O-C ceramics: electronmicroscopic observations and reaction kinetics
    • Berger A., Pippel E., Woltersdorf J., Scheffler M., Cromme P., and Greil P. Nanoprocesses in polymer-derived Si-O-C ceramics: electronmicroscopic observations and reaction kinetics. Phys. Status Solidi (A) 202 (2005) 2277-2286
    • (2005) Phys. Status Solidi (A) , vol.202 , pp. 2277-2286
    • Berger, A.1    Pippel, E.2    Woltersdorf, J.3    Scheffler, M.4    Cromme, P.5    Greil, P.6
  • 9
    • 33745585814 scopus 로고    scopus 로고
    • Evolution of C-rich SiOC ceramics. Part I. Characterization by integral spectroscopic techniques: solid-state NMR and Raman spectroscopy
    • Kleebe H.-J., Gregori G., Babonneau F., Blum Y.D., MacQueen D.B., and Masse S. Evolution of C-rich SiOC ceramics. Part I. Characterization by integral spectroscopic techniques: solid-state NMR and Raman spectroscopy. Int. J. Mater. Res. 97 (2006) 699-709
    • (2006) Int. J. Mater. Res. , vol.97 , pp. 699-709
    • Kleebe, H.-J.1    Gregori, G.2    Babonneau, F.3    Blum, Y.D.4    MacQueen, D.B.5    Masse, S.6
  • 10
    • 0037061125 scopus 로고    scopus 로고
    • Microstructural characterization of monolithic ceramic matrix composites from polysiloxane and SiC powder
    • Schiavon M.A., Radovanovic E., and Yoshida I.V.P. Microstructural characterization of monolithic ceramic matrix composites from polysiloxane and SiC powder. Powder Technol. 123 (2002) 232-241
    • (2002) Powder Technol. , vol.123 , pp. 232-241
    • Schiavon, M.A.1    Radovanovic, E.2    Yoshida, I.V.P.3
  • 11
    • 0035354002 scopus 로고    scopus 로고
    • Phase-separation in an SiCO glass studied by transmission electron microscopy and electron energy-loss spectroscopy
    • Kleebe H.-J., Turquat C., and Sorarù G.D. Phase-separation in an SiCO glass studied by transmission electron microscopy and electron energy-loss spectroscopy. J. Am. Ceram. Soc. 84 (2001) 1073-1080
    • (2001) J. Am. Ceram. Soc. , vol.84 , pp. 1073-1080
    • Kleebe, H.-J.1    Turquat, C.2    Sorarù, G.D.3
  • 12
    • 33745623977 scopus 로고    scopus 로고
    • Evolution of C-rich SiOC ceramics. Part II. Characterization by high lateral resolution techniques: electron energy-loss spectroscopy, high-resolution TEM and energy-filtered TEM
    • Gregori G., Kleebe H.J., Blum Y.D., and Babonneau F. Evolution of C-rich SiOC ceramics. Part II. Characterization by high lateral resolution techniques: electron energy-loss spectroscopy, high-resolution TEM and energy-filtered TEM. Int. J. Mater. Res. 97 (2006) 710-720
    • (2006) Int. J. Mater. Res. , vol.97 , pp. 710-720
    • Gregori, G.1    Kleebe, H.J.2    Blum, Y.D.3    Babonneau, F.4
  • 13
    • 0035497588 scopus 로고    scopus 로고
    • Transmission electron microscopy and electron energy-loss spectroscopy study of nonstoichiometric silicon-carbon-oxygen glasses
    • Turquat C., Kleebe H.-J., Gregori G., Walter S., and Sorarù G.D. Transmission electron microscopy and electron energy-loss spectroscopy study of nonstoichiometric silicon-carbon-oxygen glasses. J. Am. Ceram. Soc. 84 (2001) 2189-2196
    • (2001) J. Am. Ceram. Soc. , vol.84 , pp. 2189-2196
    • Turquat, C.1    Kleebe, H.-J.2    Gregori, G.3    Walter, S.4    Sorarù, G.D.5
  • 14
    • 9544237149 scopus 로고    scopus 로고
    • Poly(borosilazanes) as precursors of Si-B-C-N glasses: synthesis and high temperature properties
    • Schiavon M.A., Sorarù G.D., and Yoshida I.V.P. Poly(borosilazanes) as precursors of Si-B-C-N glasses: synthesis and high temperature properties. J. Non-Cryst. Solids 348 (2004) 156-161
    • (2004) J. Non-Cryst. Solids , vol.348 , pp. 156-161
    • Schiavon, M.A.1    Sorarù, G.D.2    Yoshida, I.V.P.3
  • 15
    • 2942560859 scopus 로고    scopus 로고
    • Amorphous SiBCO ceramics derived from novel polymeric precursors
    • Liebau V., Hauser R., and Riedel R. Amorphous SiBCO ceramics derived from novel polymeric precursors. C.R. Chim. 7 (2004) 463-469
    • (2004) C.R. Chim. , vol.7 , pp. 463-469
    • Liebau, V.1    Hauser, R.2    Riedel, R.3
  • 16
    • 36349017235 scopus 로고    scopus 로고
    • New insights on the high-temperature nanostructure evolution of SiOC and B-doped SiBOC polymer-derived glasses
    • Alonso R.P., Mariotto G., Gervais C., Babonneau F., and Sorarù G.D. New insights on the high-temperature nanostructure evolution of SiOC and B-doped SiBOC polymer-derived glasses. Chem. Mater. 19 (2007) 5694-5702
    • (2007) Chem. Mater. , vol.19 , pp. 5694-5702
    • Alonso, R.P.1    Mariotto, G.2    Gervais, C.3    Babonneau, F.4    Sorarù, G.D.5
  • 18
    • 0942266491 scopus 로고    scopus 로고
    • Nickel-catalysed in situ formation of carbon nanotubes and turbostratic carbon in polymer-derived ceramics
    • Scheffler M., Greil P., Berger A., Pippel E., and Woltersdorf J. Nickel-catalysed in situ formation of carbon nanotubes and turbostratic carbon in polymer-derived ceramics. Mater. Chem. Phys. 84 (2004) 131-139
    • (2004) Mater. Chem. Phys. , vol.84 , pp. 131-139
    • Scheffler, M.1    Greil, P.2    Berger, A.3    Pippel, E.4    Woltersdorf, J.5
  • 19
    • 18844402857 scopus 로고    scopus 로고
    • Carbon nanostructures on high-temperature ceramics-a novel composite material and its functionalization
    • Haberecht J., Krumeich F., Stalder M., and Nesper R. Carbon nanostructures on high-temperature ceramics-a novel composite material and its functionalization. Catal. Today 102/103 (2005) 40-44
    • (2005) Catal. Today , vol.102-103 , pp. 40-44
    • Haberecht, J.1    Krumeich, F.2    Stalder, M.3    Nesper, R.4
  • 20
    • 33749599741 scopus 로고    scopus 로고
    • Field emission study of SiC nanowires/nanorods directly grown on SiC ceramic substrate
    • Deng S.Z., Li Z.B., Wang W.L., Xu N.S., Zhou J., Zheng X.G., et al. Field emission study of SiC nanowires/nanorods directly grown on SiC ceramic substrate. Appl. Phys. Lett. 89 (2006) 023118-023118-3
    • (2006) Appl. Phys. Lett. , vol.89
    • Deng, S.Z.1    Li, Z.B.2    Wang, W.L.3    Xu, N.S.4    Zhou, J.5    Zheng, X.G.6
  • 21
    • 30144435147 scopus 로고    scopus 로고
    • Synthesis of nickel nanoparticles and carbon encapsulated nickel nanoparticles supported on carbon nanotubes
    • Cheng J., Zhang X., and Ye Y. Synthesis of nickel nanoparticles and carbon encapsulated nickel nanoparticles supported on carbon nanotubes. J. Solid State Chem. 179 (2006) 91-95
    • (2006) J. Solid State Chem. , vol.179 , pp. 91-95
    • Cheng, J.1    Zhang, X.2    Ye, Y.3
  • 25
    • 0008970950 scopus 로고
    • Determination of carbon content in carbides by an elemental analyzer
    • Borda P.P., and Legzdins P. Determination of carbon content in carbides by an elemental analyzer. Anal. Chem. 52 (1980) 1777-1778
    • (1980) Anal. Chem. , vol.52 , pp. 1777-1778
    • Borda, P.P.1    Legzdins, P.2
  • 27
    • 12444272525 scopus 로고
    • Adsorption of gases in multimolecular layers
    • Brunauer S., Emmett P.H., and Teller E. Adsorption of gases in multimolecular layers. J. Am. Chem. Soc. 60 (1938) 309-319
    • (1938) J. Am. Chem. Soc. , vol.60 , pp. 309-319
    • Brunauer, S.1    Emmett, P.H.2    Teller, E.3
  • 28
    • 0342445773 scopus 로고
    • The determination of pore volume and area distributions in porous substances. I. Computations from nitrogen isotherms
    • Barrett E.P., Joyner L.G., and Halenda P.P. The determination of pore volume and area distributions in porous substances. I. Computations from nitrogen isotherms. J. Am. Chem. Soc. 73 (1951) 373-380
    • (1951) J. Am. Chem. Soc. , vol.73 , pp. 373-380
    • Barrett, E.P.1    Joyner, L.G.2    Halenda, P.P.3
  • 29
    • 0035284053 scopus 로고    scopus 로고
    • Polydimethylsiloxane thermal degradation. Part I. Kinetic aspects
    • Camino G., Lomakin S.M., and Lazzari M. Polydimethylsiloxane thermal degradation. Part I. Kinetic aspects. Polymer 42 (2001) 2395-2402
    • (2001) Polymer , vol.42 , pp. 2395-2402
    • Camino, G.1    Lomakin, S.M.2    Lazzari, M.3
  • 30
    • 0037196302 scopus 로고    scopus 로고
    • Thermal polydimethylsiloxane degradation. Part 2. The degradation mechanisms
    • Camino G., Lomakin S.M., and Lageard M. Thermal polydimethylsiloxane degradation. Part 2. The degradation mechanisms. Polymer 43 (2002) 2011-2015
    • (2002) Polymer , vol.43 , pp. 2011-2015
    • Camino, G.1    Lomakin, S.M.2    Lageard, M.3
  • 31
    • 0000887007 scopus 로고
    • High-temperature stabilization of cross-linked siloxanes glasses
    • Michalczyk M.J., Farneth W.E., and Vega A.J. High-temperature stabilization of cross-linked siloxanes glasses. Chem. Mater. 5 (1993) 1687-1689
    • (1993) Chem. Mater. , vol.5 , pp. 1687-1689
    • Michalczyk, M.J.1    Farneth, W.E.2    Vega, A.J.3
  • 32
    • 7744241650 scopus 로고    scopus 로고
    • Synthesis and characterization of carbon-enriched silicon oxycarbides
    • Blum Y.D., MacQueen D.B., and Kleebe H.-J. Synthesis and characterization of carbon-enriched silicon oxycarbides. J. Eur. Ceram. Soc. 25 (2005) 143-149
    • (2005) J. Eur. Ceram. Soc. , vol.25 , pp. 143-149
    • Blum, Y.D.1    MacQueen, D.B.2    Kleebe, H.-J.3
  • 34
    • 33646349494 scopus 로고    scopus 로고
    • Growth of nanowires from annealing SiBONC nanopowders
    • Li F., Wen G., and Song L. Growth of nanowires from annealing SiBONC nanopowders. J. Cryst. Growth 290 (2006) 466-472
    • (2006) J. Cryst. Growth , vol.290 , pp. 466-472
    • Li, F.1    Wen, G.2    Song, L.3
  • 36
    • 0028565416 scopus 로고
    • NMR, XRD and IR study on microcrystalline opals
    • Graetsch H., Gies H., and Topalovié I. NMR, XRD and IR study on microcrystalline opals. Phys. Chem. Miner. 21 (1994) 166-175
    • (1994) Phys. Chem. Miner. , vol.21 , pp. 166-175
    • Graetsch, H.1    Gies, H.2    Topalovié, I.3
  • 37
  • 38
    • 0001367159 scopus 로고
    • Structural characterization of sol-gel derived oxycarbide glasses. 2. Study of the thermal stability of the silicon oxycarbide phase
    • Bois L., Maquet J., and Babonneau F. Structural characterization of sol-gel derived oxycarbide glasses. 2. Study of the thermal stability of the silicon oxycarbide phase. Chem. Mater. 7 (1995) 975-981
    • (1995) Chem. Mater. , vol.7 , pp. 975-981
    • Bois, L.1    Maquet, J.2    Babonneau, F.3
  • 39
    • 34447580242 scopus 로고    scopus 로고
    • Controllable growth of nanostructured carbon from coal tar pitch by chemical vapor deposition
    • Liu X., Yang Y., Ji W., Liu H., Zhang C., and Xu B. Controllable growth of nanostructured carbon from coal tar pitch by chemical vapor deposition. Mater. Chem. Phys. 104 (2007) 320-326
    • (2007) Mater. Chem. Phys. , vol.104 , pp. 320-326
    • Liu, X.1    Yang, Y.2    Ji, W.3    Liu, H.4    Zhang, C.5    Xu, B.6
  • 40
    • 31144432931 scopus 로고    scopus 로고
    • NiO films consisting of vertically aligned cone-shaped NiO rods
    • Zhang Z., Zhao Y., and Zhu M. NiO films consisting of vertically aligned cone-shaped NiO rods. Appl. Phys. Lett. 88 (2006) 033101-1-033101-3
    • (2006) Appl. Phys. Lett. , vol.88
    • Zhang, Z.1    Zhao, Y.2    Zhu, M.3
  • 41
    • 4444322708 scopus 로고    scopus 로고
    • Processing of closed-cell silicon oxycarbide foams from a preceramic polymer
    • Kim Y.-W., Kim S.-H., Kim H.-D., and Park C.B. Processing of closed-cell silicon oxycarbide foams from a preceramic polymer. J. Mater. Sci. 39 (2004) 5647-5652
    • (2004) J. Mater. Sci. , vol.39 , pp. 5647-5652
    • Kim, Y.-W.1    Kim, S.-H.2    Kim, H.-D.3    Park, C.B.4
  • 42
    • 0032668876 scopus 로고    scopus 로고
    • High temperature behavior of a gel-derived SiOC glass: elasticity and viscosity
    • Rouxel T., Massouras G., and Sorarù G.D. High temperature behavior of a gel-derived SiOC glass: elasticity and viscosity. J. Sol-Gel Sci. Technol. 14 (1999) 87-94
    • (1999) J. Sol-Gel Sci. Technol. , vol.14 , pp. 87-94
    • Rouxel, T.1    Massouras, G.2    Sorarù, G.D.3
  • 43
    • 0001447577 scopus 로고    scopus 로고
    • Structural evolution of a poly(methylsilane)/tetra-allylsilane mixture into silicon carbide
    • Gozzi M.F., and Yoshida I.V.P. Structural evolution of a poly(methylsilane)/tetra-allylsilane mixture into silicon carbide. Eur. Polym. J. 33 (1997) 1301-1306
    • (1997) Eur. Polym. J. , vol.33 , pp. 1301-1306
    • Gozzi, M.F.1    Yoshida, I.V.P.2
  • 44
    • 1342283771 scopus 로고    scopus 로고
    • Structural evaluation of polysilane-derived products: from amorphous to thermodynamically stable phases
    • Li X., and Edirisinghe M.J. Structural evaluation of polysilane-derived products: from amorphous to thermodynamically stable phases. Philos. Mag. 84 (2004) 647-671
    • (2004) Philos. Mag. , vol.84 , pp. 647-671
    • Li, X.1    Edirisinghe, M.J.2
  • 45
    • 0014829099 scopus 로고
    • Raman spectrum of graphite
    • Tuinstra F., and Koenig J.L. Raman spectrum of graphite. J. Chem. Phys. 53 (1970) 1126-1130
    • (1970) J. Chem. Phys. , vol.53 , pp. 1126-1130
    • Tuinstra, F.1    Koenig, J.L.2
  • 46
    • 0242603790 scopus 로고    scopus 로고
    • Interpretation of Raman spectra of disordered and amorphous carbon
    • Ferrari A.C., and Robertson J. Interpretation of Raman spectra of disordered and amorphous carbon. Phys. Rev. B 61 (2000) 14095-14107
    • (2000) Phys. Rev. B , vol.61 , pp. 14095-14107
    • Ferrari, A.C.1    Robertson, J.2
  • 47
    • 0032640819 scopus 로고    scopus 로고
    • Structural investigation of the first stages of pyrolysis of Si-C-O preceramic polymers containing Si-H bonds
    • Gualandris V., Bahloul D.H., and Babonneau F. Structural investigation of the first stages of pyrolysis of Si-C-O preceramic polymers containing Si-H bonds. J. Sol-Gel Sci. Technol. 14 (1999) 39-48
    • (1999) J. Sol-Gel Sci. Technol. , vol.14 , pp. 39-48
    • Gualandris, V.1    Bahloul, D.H.2    Babonneau, F.3
  • 48
    • 2542437011 scopus 로고    scopus 로고
    • Structural characterization and thermal oxidation resistance of silicon oxycarbides produced by polysiloxane pyrolysis
    • Kolar F., Machovic V., Svítilová J., and Brecká L. Structural characterization and thermal oxidation resistance of silicon oxycarbides produced by polysiloxane pyrolysis. Mater. Chem. Phys. 86 (2004) 88-98
    • (2004) Mater. Chem. Phys. , vol.86 , pp. 88-98
    • Kolar, F.1    Machovic, V.2    Svítilová, J.3    Brecká, L.4
  • 49
    • 18944363199 scopus 로고    scopus 로고
    • Microstructure evolution of precursors-derived SiCN ceramics upon thermal treatment between 1000 and 1400 °C
    • Gregori G., Kleebe H.-J., Brequel H., Enzo S., and Ziegler G. Microstructure evolution of precursors-derived SiCN ceramics upon thermal treatment between 1000 and 1400 °C. J. Non-Cryst. Solids 351 (2005) 1393-1402
    • (2005) J. Non-Cryst. Solids , vol.351 , pp. 1393-1402
    • Gregori, G.1    Kleebe, H.-J.2    Brequel, H.3    Enzo, S.4    Ziegler, G.5
  • 50
    • 0035500669 scopus 로고    scopus 로고
    • Characterization of the free-carbon phase in precursor-derived SiCN ceramics
    • Trassl S., Motz G., Rössler E., and Ziegler G. Characterization of the free-carbon phase in precursor-derived SiCN ceramics. J. Non-Cryst. Solids 293-295 (2001) 261-267
    • (2001) J. Non-Cryst. Solids , vol.293-295 , pp. 261-267
    • Trassl, S.1    Motz, G.2    Rössler, E.3    Ziegler, G.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.