Volumn 58, Issue 8-9 SPEC. ISS., 2007, Pages 786-793

A comparative study of the SSC resistance of a novel welding process IEA with SAW and MIG

Author keywords

Hydrogen embrittlement; Indirect electric arc; Slow strain rate test; Stress sulphide cracking

Indexed keywords

ELECTRIC ARC WELDING; ELECTRIC ARCS; FERRITES; HYDROGEN EMBRITTLEMENT; PERMEATION; STRAIN RATE; STRESS CORROSION CRACKING; SULFIDE CORROSION CRACKING;

EID: 34250743157     PISSN: 10445803     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.matchar.2006.12.005     Document Type: Article
Times cited : (3)

References (28)
  • 1
    • 0037437398 scopus 로고    scopus 로고
    • Hydrogen permeation in a submerged arc weldment of TMCP steel
    • Wang S.H., Luu W.C., Ho K.F., and Wu J.K. Hydrogen permeation in a submerged arc weldment of TMCP steel. Mater Chem Phys 77 2 (2003) 447-454
    • (2003) Mater Chem Phys , vol.77 , Issue.2 , pp. 447-454
    • Wang, S.H.1    Luu, W.C.2    Ho, K.F.3    Wu, J.K.4
  • 2
    • 0036502938 scopus 로고    scopus 로고
    • Characteristics of near neutral pH stress corrosion cracks in a X-65 pipeline
    • Chen W., King F., and Vokes E. Characteristics of near neutral pH stress corrosion cracks in a X-65 pipeline. Corrosion 58 3 (2002) 267-275
    • (2002) Corrosion , vol.58 , Issue.3 , pp. 267-275
    • Chen, W.1    King, F.2    Vokes, E.3
  • 3
    • 0036532859 scopus 로고    scopus 로고
    • Use of the Devanathan-Stachurski cell to measure hydrogen permeation in aluminum alloys
    • Danielson M.J. Use of the Devanathan-Stachurski cell to measure hydrogen permeation in aluminum alloys. Corros Sci 44 4 (2002) 829-840
    • (2002) Corros Sci , vol.44 , Issue.4 , pp. 829-840
    • Danielson, M.J.1
  • 4
    • 0036591729 scopus 로고    scopus 로고
    • Effect of hydrogen environment on the notched tensile properties of T-250 maraging steel annealed by laser treatment
    • Tsay L.W., Lee W.C., Luu W.C., and Wu J.K. Effect of hydrogen environment on the notched tensile properties of T-250 maraging steel annealed by laser treatment. Corros Sci 44 6 (2002) 1311-1327
    • (2002) Corros Sci , vol.44 , Issue.6 , pp. 1311-1327
    • Tsay, L.W.1    Lee, W.C.2    Luu, W.C.3    Wu, J.K.4
  • 5
    • 0012861135 scopus 로고    scopus 로고
    • Characterization of hydrogen permeation through a corrosion-resistant zinc-nickel-phosphorous alloy
    • Durairajan A., Krishnayer A., Haran B.S., White R.E., and Popov B.N. Characterization of hydrogen permeation through a corrosion-resistant zinc-nickel-phosphorous alloy. Corrosion 56 3 (2000) 283-288
    • (2000) Corrosion , vol.56 , Issue.3 , pp. 283-288
    • Durairajan, A.1    Krishnayer, A.2    Haran, B.S.3    White, R.E.4    Popov, B.N.5
  • 7
    • 0037119889 scopus 로고    scopus 로고
    • J Alloys Compd 343 1-2 (2002) 234-237
    • (2002) J Alloys Compd , vol.343 , Issue.1-2 , pp. 234-237
  • 8
    • 0035331188 scopus 로고    scopus 로고
    • Effect of thiosulfate and sulfite on the permeation rate of hydrogen though iron
    • Abd Elhamid M.H., Ateya B.G., Weil K.G., and Pickering H.W. Effect of thiosulfate and sulfite on the permeation rate of hydrogen though iron. Corrosion 57 5 (2001) 428-432
    • (2001) Corrosion , vol.57 , Issue.5 , pp. 428-432
    • Abd Elhamid, M.H.1    Ateya, B.G.2    Weil, K.G.3    Pickering, H.W.4
  • 9
    • 0011119562 scopus 로고    scopus 로고
    • Localized corrosion of carbon steel weldments
    • Sephton M., and Pistorius P.C. Localized corrosion of carbon steel weldments. Corrosion 56 12 (2000) 1272-1279
    • (2000) Corrosion , vol.56 , Issue.12 , pp. 1272-1279
    • Sephton, M.1    Pistorius, P.C.2
  • 10
    • 0032046239 scopus 로고    scopus 로고
    • Influence of residual stresses and loading frequencies on corrosion fatigue crack growth behavior of weldments
    • Kitsunai Y., Tanaka M., and Yoshihisa E. Influence of residual stresses and loading frequencies on corrosion fatigue crack growth behavior of weldments. Metall Mater Trans A 29 4 (1998) 1289-1298
    • (1998) Metall Mater Trans A , vol.29 , Issue.4 , pp. 1289-1298
    • Kitsunai, Y.1    Tanaka, M.2    Yoshihisa, E.3
  • 11
    • 0037997609 scopus 로고    scopus 로고
    • Performance of welded high-strength low-alloy steels in sour environments
    • Omweg G.M., Frankel G.S., Bruce W.A., Ramirez J.E., and Koch G. Performance of welded high-strength low-alloy steels in sour environments. Corrosion 59 7 (2003) 640-653
    • (2003) Corrosion , vol.59 , Issue.7 , pp. 640-653
    • Omweg, G.M.1    Frankel, G.S.2    Bruce, W.A.3    Ramirez, J.E.4    Koch, G.5
  • 12
    • 0038354792 scopus 로고    scopus 로고
    • Large-scale wet hydrogen sulfide cracking performance: evaluation of metallurgical, mechanical, and welding variables
    • Cayard M.S., and Kane R.D. Large-scale wet hydrogen sulfide cracking performance: evaluation of metallurgical, mechanical, and welding variables. Corrosion 53 (1997) 227-230
    • (1997) Corrosion , vol.53 , pp. 227-230
    • Cayard, M.S.1    Kane, R.D.2
  • 13
    • 0037116303 scopus 로고    scopus 로고
    • MIG welding process with indirect electric arc
    • Garcia R., Lopez V.H., and Bedolla E. MIG welding process with indirect electric arc. J Mater Sci Lett 21 (2002) 1965-1967
    • (2002) J Mater Sci Lett , vol.21 , pp. 1965-1967
    • Garcia, R.1    Lopez, V.H.2    Bedolla, E.3
  • 14
    • 0037116303 scopus 로고    scopus 로고
    • J Mater Sci Lett 21 24 (2002) 1965-1967
    • (2002) J Mater Sci Lett , vol.21 , Issue.24 , pp. 1965-1967
  • 15
    • 0036989902 scopus 로고    scopus 로고
    • Comparative welding study of metal matrix composites with the MIG welding process, using direct and indirect electric arc
    • Garcia R., Manzano A., Lopez V.H., and Bedolla E. Comparative welding study of metal matrix composites with the MIG welding process, using direct and indirect electric arc. Metall Mater Trans B 33 6 (2002) 932-937
    • (2002) Metall Mater Trans B , vol.33 , Issue.6 , pp. 932-937
    • Garcia, R.1    Manzano, A.2    Lopez, V.H.3    Bedolla, E.4
  • 16
    • 0041341983 scopus 로고    scopus 로고
    • A comparative study of the MIG welding of Al/TiC composites using direct and indirect electric arc processes
    • Garcia R., Lopez V.H., Bedolla E., and Manzano A. A comparative study of the MIG welding of Al/TiC composites using direct and indirect electric arc processes. J Mater Sci 38 12 (2003) 2771-2779
    • (2003) J Mater Sci , vol.38 , Issue.12 , pp. 2771-2779
    • Garcia, R.1    Lopez, V.H.2    Bedolla, E.3    Manzano, A.4
  • 17
    • 23044432773 scopus 로고    scopus 로고
    • Stress corrosion testing of welded supermartensitic stainless gas steels for oil and gas pipelines
    • Turnbull A., and Nimmo B. Stress corrosion testing of welded supermartensitic stainless gas steels for oil and gas pipelines. Corros Eng Sci Technol 40 2 (2005) 103-109
    • (2005) Corros Eng Sci Technol , vol.40 , Issue.2 , pp. 103-109
    • Turnbull, A.1    Nimmo, B.2
  • 18
    • 0037997609 scopus 로고    scopus 로고
    • Performance of welded high-strength low-alloy steels in sour environments
    • Omweg G.M., Frankel G.S., Bruce W.A., Ramirez J.E., and Koch G. Performance of welded high-strength low-alloy steels in sour environments. Corrosion 59 7 (2003) 640-653
    • (2003) Corrosion , vol.59 , Issue.7 , pp. 640-653
    • Omweg, G.M.1    Frankel, G.S.2    Bruce, W.A.3    Ramirez, J.E.4    Koch, G.5
  • 19
    • 33750882524 scopus 로고    scopus 로고
    • Relationship between yield strength and near-neutral pH stress corrosion cracking resistance of pipeline steels-an effect of microstructure
    • Lu B.T., and Luo J.L. Relationship between yield strength and near-neutral pH stress corrosion cracking resistance of pipeline steels-an effect of microstructure. Corrosion 62 2 (2006) 129-140
    • (2006) Corrosion , vol.62 , Issue.2 , pp. 129-140
    • Lu, B.T.1    Luo, J.L.2
  • 20
    • 34250691680 scopus 로고    scopus 로고
    • Natividad C., Salazar M., Garcia R., Gonzalez-Rodriguez J.G., Perez R. Sulphide stress cracking behaviour of weldments produced by indirect electric arc welding. Corros Eng Sci Technol, in press.
  • 21
    • 34250775646 scopus 로고    scopus 로고
    • ASTM A 370-2002. Standard test methods and definitions for mechanical testing of steel products.
  • 22
    • 34250699643 scopus 로고    scopus 로고
    • NACE TM 0198-2004. Slow strain rate test method for screening corrosion-resistant alloys (CRAs) for stress corrosion cracking in sour oilfield service.
  • 23
    • 34250722293 scopus 로고    scopus 로고
    • ASTM G 129-2000. Standard practice for slow strain rate testing to evaluate the susceptibility of metallic materials to environmentally assisted cracking.
  • 24
    • 34250725056 scopus 로고    scopus 로고
    • 2S environments-Errata sheet.
  • 25
    • 0002490486 scopus 로고
    • The adsorption and diffusion of electrolytic hydrogen in palladium
    • Philadelphia
    • Devanathan M.A.V., and Stachurski Z. The adsorption and diffusion of electrolytic hydrogen in palladium. Proc R Soc Lond Ser A, Math Phys Sci 270 1340 (1962) 90-102 Philadelphia
    • (1962) Proc R Soc Lond Ser A, Math Phys Sci , vol.270 , Issue.1340 , pp. 90-102
    • Devanathan, M.A.V.1    Stachurski, Z.2
  • 26
    • 34250718263 scopus 로고    scopus 로고
    • CRC Press LLC, NW Boca Raton, FL
    • Weman K. Welding processes handbook (2000), CRC Press LLC, NW Boca Raton, FL 41-80
    • (2000) Welding processes handbook , pp. 41-80
    • Weman, K.1
  • 28
    • 34250709724 scopus 로고    scopus 로고
    • 2S-Containing Environments in Oil and Gas Production, Part 1: General Principles for Selection of Cracking-Resistant Materials, NACE International/ISO 2001.


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.