Volumn 26, Issue 7, 2006, Pages 1267-1272

Grain boundary crystallization during furnace cooling of α-SiC sintered with Y2O3-Al2O3-CaO

Author keywords

Crystallization; Grain boundary; Liquid phase sintering; SiC

Indexed keywords

COMPOSITION; CRYSTALLIZATION; ENERGY DISPERSIVE SPECTROSCOPY; EPITAXIAL GROWTH; GRAIN BOUNDARIES; SEGREGATION (METALLOGRAPHY); SINTERED CARBIDES; SPECIMEN PREPARATION;

EID: 31744440440     PISSN: 09552219     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.jeurceramsoc.2005.01.050     Document Type: Article
Times cited : (35)

References (30)
  • 2
    • 0028529919 scopus 로고
    • Toughness properties of a silicon carbide with an in situ induced heterogeneous grain structure
    • N.P. Padture B.R. Lawn Toughness properties of a silicon carbide with an in situ induced heterogeneous grain structure J. Am. Ceram. Soc. 77 1994 2518-2522
    • (1994) J. Am. Ceram. Soc. , vol.77 , pp. 2518-2522
    • Padture, N.P.1    Lawn, B.R.2
  • 3
    • 0033351893 scopus 로고    scopus 로고
    • Role of the powder bed in the densification of silicon carbide sintered with yttria and alumina additives
    • E.J. Winn W.J. Clegg Role of the powder bed in the densification of silicon carbide sintered with yttria and alumina additives J. Am. Ceram. Soc. 82 1999 3466-3470
    • (1999) J. Am. Ceram. Soc. , vol.82 , pp. 3466-3470
    • Winn, E.J.1    Clegg, W.J.2
  • 4
    • 0028382729 scopus 로고
    • In situ-toughened silicon carbide
    • N.P. Padture In situ-toughened silicon carbide J. Am. Ceram. Soc. 77 1994 519-523
    • (1994) J. Am. Ceram. Soc. , vol.77 , pp. 519-523
    • Padture, N.P.1
  • 5
    • 0032297867 scopus 로고    scopus 로고
    • Effect of initial α-phase content on microstructure and mechanical properties of sintered silicon carbide
    • Y.-W. Kim M. Mitomo H. Emoto J.G. Lee Effect of initial α-phase content on microstructure and mechanical properties of sintered silicon carbide J. Am. Ceram. Soc. 81 1998 3136-3140
    • (1998) J. Am. Ceram. Soc. , vol.81 , pp. 3136-3140
    • Kim, Y.-W.1    Mitomo, M.2    Emoto, H.3    Lee, J.G.4
  • 7
    • 0030190934 scopus 로고    scopus 로고
    • Fabrication of silicon carbide nano-ceramics
    • M. Mitomo Y.-W. Kim H. Hirotsuru Fabrication of silicon carbide nano-ceramics J. Mater. Res. 11 1996 1601-1604
    • (1996) J. Mater. Res. , vol.11 , pp. 1601-1604
    • Mitomo, M.1    Kim, Y.-W.2    Hirotsuru, H.3
  • 8
    • 0030822378 scopus 로고    scopus 로고
    • Microstructural development of silicon carbide containing large seed grains
    • Y.-W. Kim M. Mitomo H. Hirotsuru Microstructural development of silicon carbide containing large seed grains J. Am. Ceram. Soc. 80 1997 99-105
    • (1997) J. Am. Ceram. Soc. , vol.80 , pp. 99-105
    • Kim, Y.-W.1    Mitomo, M.2    Hirotsuru, H.3
  • 9
    • 0033078320 scopus 로고    scopus 로고
    • Microstructure and mechanical properties of α-silicon carbide sintered with yttrium-aluminum garnet and silica
    • J.Y. Kim Y.-W. Kim M. Mitomo G.-D. Zhan J.G. Lee Microstructure and mechanical properties of α-silicon carbide sintered with yttrium-aluminum garnet and silica J. Am. Ceram. Soc. 82 1999 441-444
    • (1999) J. Am. Ceram. Soc. , vol.82 , pp. 441-444
    • Kim, J.Y.1    Kim, Y.-W.2    Mitomo, M.3    Zhan, G.-D.4    Lee, J.G.5
  • 10
    • 0034508789 scopus 로고    scopus 로고
    • Role of the grain-boundary phase on the elevated-temperature strength, toughness, fatigue and creep resistance of silicon carbide sintered with Al, B and C
    • D. Chen M.E. Sixta X.F. Zhang L.C. De Jonghe R.O. Ritchie Role of the grain-boundary phase on the elevated-temperature strength, toughness, fatigue and creep resistance of silicon carbide sintered with Al, B and C Acta Mater. 48 2000 4599-4608
    • (2000) Acta Mater. , vol.48 , pp. 4599-4608
    • Chen, D.1    Sixta, M.E.2    Zhang, X.F.3    De Jonghe, L.C.4    Ritchie, R.O.5
  • 11
    • 0034251462 scopus 로고    scopus 로고
    • Effect of grain-boundary structure on the strength, toughness, and cyclic-fatigue properties of a monolithic silicon carbide
    • D. Chen X.F. Zhang R.O. Ritchie Effect of grain-boundary structure on the strength, toughness, and cyclic-fatigue properties of a monolithic silicon carbide J. Am. Ceram. Soc. 83 2000 2079-2081
    • (2000) J. Am. Ceram. Soc. , vol.83 , pp. 2079-2081
    • Chen, D.1    Zhang, X.F.2    Ritchie, R.O.3
  • 12
    • 0032036295 scopus 로고    scopus 로고
    • Controlling interface chemical and structure to process and toughen silicon carbide
    • W.J. MoberlyChan L.C. De Jonghe Controlling interface chemical and structure to process and toughen silicon carbide Acta Mater. 46 1998 2471-2477
    • (1998) Acta Mater. , vol.46 , pp. 2471-2477
    • MoberlyChan, W.J.1    De Jonghe, L.C.2
  • 14
    • 0010132041 scopus 로고
    • SiC-based ceramics with improved strength
    • J.D. Cawley C.E. Semler The American Ceramic Society Westerville, OH
    • T.B. Jackson A.C. Hurford S.L. Bruner R.A. Cutler SiC-based ceramics with improved strength J.D. Cawley C.E. Semler Silicon Carbide '87 1989 The American Ceramic Society Westerville, OH 227-240
    • (1989) Silicon Carbide '87 , pp. 227-240
    • Jackson, T.B.1    Hurford, A.C.2    Bruner, S.L.3    Cutler, R.A.4
  • 15
    • 0029338688 scopus 로고
    • Homogeneous distribution of sintering additives in liquid-phase sintered silicon carbide
    • E. Liden E. Carlstrom L. Eklund B. Nyberg R. Carlsson Homogeneous distribution of sintering additives in liquid-phase sintered silicon carbide J. Am. Ceram. Soc. 78 1995 1761-1768
    • (1995) J. Am. Ceram. Soc. , vol.78 , pp. 1761-1768
    • Liden, E.1    Carlstrom, E.2    Eklund, L.3    Nyberg, B.4    Carlsson, R.5
  • 17
    • 0033878959 scopus 로고    scopus 로고
    • High temperature cyclic fatigue-crack growth behavior in an in situ toughened silicon carbide
    • D. Chen C.J. Gilbert X.F. Zhang R.O. Ritchie High temperature cyclic fatigue-crack growth behavior in an in situ toughened silicon carbide Acta Mater. 48 2000 659-674
    • (2000) Acta Mater. , vol.48 , pp. 659-674
    • Chen, D.1    Gilbert, C.J.2    Zhang, X.F.3    Ritchie, R.O.4
  • 18
    • 0035470729 scopus 로고    scopus 로고
    • Flexural creep of an in situ-toughened silicon carbide
    • M.E. Sixta X.F. Zhang L.C. De Jonghe Flexural creep of an in situ-toughened silicon carbide J. Am. Ceram. Soc. 84 2001 2002-2028
    • (2001) J. Am. Ceram. Soc. , vol.84 , pp. 2002-2028
    • Sixta, M.E.1    Zhang, X.F.2    De Jonghe, L.C.3
  • 20
    • 0004873491 scopus 로고
    • Nucleation in glass-forming materials
    • A.C. Zettlemoyer Nucleation Marcel Dekker New York
    • J.J. Hammel Nucleation in glass-forming materials A.C. Zettlemoyer Nucleation 1969 Marcel Dekker New York 489-525
    • (1969) Nucleation , pp. 489-525
    • Hammel, J.J.1
  • 22
    • 0028597288 scopus 로고
    • Grain boundary phase analysis of silcon nitride by a newly developed 300kV field-emission electron microscope
    • Y. Bando H. Suematsu M. Mitomo Grain boundary phase analysis of silcon nitride by a newly developed 300 kV field-emission electron microscope Mater. Res. Soc. Symp. Proc. 346 1994 733-738
    • (1994) Mater. Res. Soc. Symp. Proc. , vol.346 , pp. 733-738
    • Bando, Y.1    Suematsu, H.2    Mitomo, M.3
  • 25
    • 0027552344 scopus 로고
    • Core/rim structure of liquid-phase-sintered silicon carbide
    • L.S. Sigl H.J. Kleebe Core/rim structure of liquid-phase-sintered silicon carbide J. Am. Ceram. Soc. 76 1993 773-776
    • (1993) J. Am. Ceram. Soc. , vol.76 , pp. 773-776
    • Sigl, L.S.1    Kleebe, H.J.2
  • 26
    • 0035470704 scopus 로고    scopus 로고
    • Heat-resistant silicon carbide with aluminum nitride and erbium oxide
    • Y.-W. Kim M. Mitomo T. Nishimura Heat-resistant silicon carbide with aluminum nitride and erbium oxide J. Am. Ceram. Soc. 84 2001 2060-2064
    • (2001) J. Am. Ceram. Soc. , vol.84 , pp. 2060-2064
    • Kim, Y.-W.1    Mitomo, M.2    Nishimura, T.3
  • 27
    • 31744436456 scopus 로고
    • ed. E. A. Porai-Koshits. Consultants Bureau, New York
    • Rabinovich, E. M., Structure of Glass (Vol 3), ed. E. A. Porai-Koshits. Consultants Bureau, New York, 1964, pp. 21-26.
    • (1964) Structure of Glass , vol.3 , pp. 21-26
    • Rabinovich, E.M.1
  • 28
    • 0001417742 scopus 로고
    • Nucleation in liquids and solutions
    • A.C. Zettlemoyer Marcel Dekker New York
    • A.G. Walton Nucleation in liquids and solutions A.C. Zettlemoyer Nucleation 1969 Marcel Dekker New York 225-307
    • (1969) Nucleation , pp. 225-307
    • Walton, A.G.1
  • 29
    • 31744449384 scopus 로고    scopus 로고
    • The Formation of Glass-Ceramics from OCF E-glass
    • Final Report to the Center for Environmental and Energy Research at Alfred University, 31 September
    • Hedlund, A., The Formation of Glass-Ceramics from OCF E-glass. Final Report to the Center for Environmental and Energy Research at Alfred University, 31 September 2003.
    • (2003)
    • Hedlund, A.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.