Volumn 92, Issue 6, 2004, Pages 551-556

Influence of cyclic loading and luting agents on the fracture load of two all-ceramic crown systems

Author keywords

[No Author keywords available]

Indexed keywords

BIOMEDICAL AND DENTAL MATERIALS; GLASS; LITHIUM DISILICATE; UNCLASSIFIED DRUG; WATER;

EID: 9944254157     PISSN: 00223913     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.prosdent.2004.09.002     Document Type: Article
Times cited : (108)

References (26)
  • 1
    • 0031112587 scopus 로고    scopus 로고
    • An update on fixed prosthodontics
    • R. Cronin, and D.R. Cagna An update on fixed prosthodontics J Am Dent Assoc 128 1997 425 436
    • (1997) J Am Dent Assoc , vol.128 , pp. 425-436
    • Cronin, R.1    Cagna, D.R.2
  • 2
    • 0036720154 scopus 로고    scopus 로고
    • An up to 5-year clinical evaluation of posterior In-ceram CAD/CAM core crowns
    • A. Bindl, and W.H. Mormann An up to 5-year clinical evaluation of posterior In-ceram CAD/CAM core crowns Int J Prosthodont 15 2002 451 456
    • (2002) Int J Prosthodont , vol.15 , pp. 451-456
    • Bindl, A.1    Mormann, W.H.2
  • 3
    • 1842527538 scopus 로고    scopus 로고
    • Fracture strength of all-ceramic crowns luted using two bonding methods
    • A. Attia, and M. Kern Fracture strength of all-ceramic crowns luted using two bonding methods J Prosthet Dent 91 2004 247 252
    • (2004) J Prosthet Dent , vol.91 , pp. 247-252
    • Attia, A.1    Kern, M.2
  • 4
    • 0033186809 scopus 로고    scopus 로고
    • Fracture resistance of teeth restored with dentin-bonded crowns constructed in a leucite-reinforced ceramic
    • F.J. Burke Fracture resistance of teeth restored with dentin-bonded crowns constructed in a leucite-reinforced ceramic Dent Mater 15 1999 359 362
    • (1999) Dent Mater , vol.15 , pp. 359-362
    • Burke, F.J.1
  • 5
    • 0033108186 scopus 로고    scopus 로고
    • Full-ceramic CAD/CIM anterior crowns and copings
    • A. Bindl, S. Windisch, and W.H. Mormann Full-ceramic CAD/CIM anterior crowns and copings Int J Comput Dent 2 1999 97 111
    • (1999) Int J Comput Dent , vol.2 , pp. 97-111
    • Bindl, A.1    Windisch, S.2    Mormann, W.H.3
  • 7
    • 0027585968 scopus 로고
    • Fracture strength of all-porcelain, resin-bonded bridges after testing in an artificial oral environment
    • M. Kern, W.H. Douglas, T. Fechtig, J.R. Strub, and R. DeLong Fracture strength of all-porcelain, resin-bonded bridges after testing in an artificial oral environment J Dent 21 1993 117 121
    • (1993) J Dent , vol.21 , pp. 117-121
    • Kern, M.1    Douglas, W.H.2    Fechtig, T.3    Strub, J.R.4    Delong, R.5
  • 8
    • 0035321760 scopus 로고    scopus 로고
    • Fracture strength of four different types of anterior 3-unit bridges after thermo-mechanical fatigue in the dual-axis chewing simulator
    • S. Kheradmandan, S.O. Koutayas, M. Bernhard, and J.R. Strub Fracture strength of four different types of anterior 3-unit bridges after thermo-mechanical fatigue in the dual-axis chewing simulator J Oral Rehabil 28 2001 361 369
    • (2001) J Oral Rehabil , vol.28 , pp. 361-369
    • Kheradmandan, S.1    Koutayas, S.O.2    Bernhard, M.3    Strub, J.R.4
  • 9
    • 0033755117 scopus 로고    scopus 로고
    • Cerec 3 as the first step in digitizing the dental office
    • K. Wiedhahn Cerec 3 as the first step in digitizing the dental office Int J Comput Dent 3 2000 67 71
    • (2000) Int J Comput Dent , vol.3 , pp. 67-71
    • Wiedhahn, K.1
  • 10
    • 0034330894 scopus 로고    scopus 로고
    • The Cerec 3 - A quantum leap for computer-aided restorations: Initial clinical results
    • W.H. Mormann, and A. Bindl The Cerec 3 - a quantum leap for computer-aided restorations: initial clinical results Quintessence Int 31 2000 699 712
    • (2000) Quintessence Int , vol.31 , pp. 699-712
    • Mormann, W.H.1    Bindl, A.2
  • 11
    • 0034332357 scopus 로고    scopus 로고
    • Strength and microstructure of IPS Empress 2 glass-ceramic after different treatments
    • S.C. Oh, J.K. Dong, H. Luthy, and P. Scharer Strength and microstructure of IPS Empress 2 glass-ceramic after different treatments Int J Prosthodont 13 2000 468 472
    • (2000) Int J Prosthodont , vol.13 , pp. 468-472
    • Oh, S.C.1    Dong, J.K.2    Luthy, H.3    Scharer, P.4
  • 12
    • 0033209858 scopus 로고    scopus 로고
    • Effects of surface finish and fatigue testing on the fracture strength of CAD-CAM and pressed-ceramic crowns
    • H.Y. Chen, R. Hickel, J.C. Setcos, and K.H. Kunzelmann Effects of surface finish and fatigue testing on the fracture strength of CAD-CAM and pressed-ceramic crowns J Prosthet Dent 82 1999 468 475
    • (1999) J Prosthet Dent , vol.82 , pp. 468-475
    • Chen, H.Y.1    Hickel, R.2    Setcos, J.C.3    Kunzelmann, K.H.4
  • 13
    • 0031614740 scopus 로고    scopus 로고
    • Effect of differing resin luting systems on fracture resistance of teeth restored with dentin-bonded crowns
    • F.J. Burke, and D.C. Watts Effect of differing resin luting systems on fracture resistance of teeth restored with dentin-bonded crowns Quintessence Int 29 1998 21 27
    • (1998) Quintessence Int , vol.29 , pp. 21-27
    • Burke, F.J.1    Watts, D.C.2
  • 14
    • 0033146116 scopus 로고    scopus 로고
    • Clinically relevant approach to failure testing of all-ceramic restorations
    • J.R. Kelly Clinically relevant approach to failure testing of all-ceramic restorations J Prosthet Dent 81 1999 652 661
    • (1999) J Prosthet Dent , vol.81 , pp. 652-661
    • Kelly, J.R.1
  • 15
    • 0035351260 scopus 로고    scopus 로고
    • Fracture resistance of lithium disilicate-, alumina-, and zirconia-based three-unit fixed partial dentures: A laboratory study
    • J. Tinschert, G. Natt, W. Mautsch, M. Augthun, and H. Spiekermann Fracture resistance of lithium disilicate-, alumina-, and zirconia-based three-unit fixed partial dentures: a laboratory study Int J Prosthodont 14 2001 231 238
    • (2001) Int J Prosthodont , vol.14 , pp. 231-238
    • Tinschert, J.1    Natt, G.2    Mautsch, W.3    Augthun, M.4    Spiekermann, H.5
  • 16
    • 0033070963 scopus 로고    scopus 로고
    • Current status of luting agents for fixed prosthodontics
    • A.M. Diaz -Arnold, M.A. Vargas, and D.R. Haselton Current status of luting agents for fixed prosthodontics J Prosthet Dent 81 1999 135 141
    • (1999) J Prosthet Dent , vol.81 , pp. 135-141
    • Diaz -Arnold, A.M.1    Vargas, M.A.2    Haselton, D.R.3
  • 17
    • 0026251060 scopus 로고
    • Fracture incidence on debonding of orthodontic brackets from porcelain veneer laminates
    • E.C. Kao, and W.M. Johnston Fracture incidence on debonding of orthodontic brackets from porcelain veneer laminates J Prosthet Dent 66 1991 631 637
    • (1991) J Prosthet Dent , vol.66 , pp. 631-637
    • Kao, E.C.1    Johnston, W.M.2
  • 18
    • 0028476223 scopus 로고
    • Fracture strength of all-ceramic crowns
    • M. Yoshinari, and T. Derand Fracture strength of all-ceramic crowns Int J Prosthodont 7 1994 329 338
    • (1994) Int J Prosthodont , vol.7 , pp. 329-338
    • Yoshinari, M.1    Derand, T.2
  • 20
    • 0030276099 scopus 로고    scopus 로고
    • Fracture resistance of human enamel and three all-ceramic crown systems on extracted teeth
    • S.S. Scherrer, W.G. De Rijk, and U.C. Belser Fracture resistance of human enamel and three all-ceramic crown systems on extracted teeth Int J Prosthodont 9 1996 580 585
    • (1996) Int J Prosthodont , vol.9 , pp. 580-585
    • Scherrer, S.S.1    De Rijk, W.G.2    Belser, U.C.3
  • 21
    • 0032195997 scopus 로고    scopus 로고
    • Fracture strength of 5 different all-ceramic crown systems
    • J.R. Strub, and S.M. Beschnidt Fracture strength of 5 different all-ceramic crown systems Int J Prosthodont 11 1998 602 609
    • (1998) Int J Prosthodont , vol.11 , pp. 602-609
    • Strub, J.R.1    Beschnidt, S.M.2
  • 22
    • 0026922592 scopus 로고
    • Compressive strength of two modern all-ceramic crowns
    • L. Probster Compressive strength of two modern all-ceramic crowns Int J Prosthodont 5 1992 409 414
    • (1992) Int J Prosthodont , vol.5 , pp. 409-414
    • Probster, L.1
  • 23
    • 0036514134 scopus 로고    scopus 로고
    • Fracture strength of all-ceramic lithium disilicate and porcelain-fused-to-metal bridges for molar replacement after dynamic loading
    • S. Chitmongkolsuk, G. Heydecke, C. Stappert, and J.R. Strub Fracture strength of all-ceramic lithium disilicate and porcelain-fused-to-metal bridges for molar replacement after dynamic loading Eur J Prosthodont Restor Dent 10 2002 15 22
    • (2002) Eur J Prosthodont Restor Dent , vol.10 , pp. 15-22
    • Chitmongkolsuk, S.1    Heydecke, G.2    Stappert, C.3    Strub, J.R.4
  • 24
    • 0032610772 scopus 로고    scopus 로고
    • Effects of cyclic loading on the strength of all-ceramic materials
    • T. Ohyama, M. Yoshinari, and Y. Oda Effects of cyclic loading on the strength of all-ceramic materials Int J Prosthodont 12 1999 28 37
    • (1999) Int J Prosthodont , vol.12 , pp. 28-37
    • Ohyama, T.1    Yoshinari, M.2    Oda, Y.3
  • 25
    • 0032062509 scopus 로고    scopus 로고
    • Investigation of the dry and wet fatigue properties of three all-ceramic crown systems
    • L.C. Sobrinho, M.J. Cattell, R.H. Glover, and J.C. Knowles Investigation of the dry and wet fatigue properties of three all-ceramic crown systems Int J Prosthodont 11 1998 255 262
    • (1998) Int J Prosthodont , vol.11 , pp. 255-262
    • Sobrinho, L.C.1    Cattell, M.J.2    Glover, R.H.3    Knowles, J.C.4
  • 26
    • 0038488606 scopus 로고    scopus 로고
    • Marginal discrepancies and leakage of all-ceramic crowns: Influence of luting agents and aging conditions
    • X.H. Gu, and M. Kern Marginal discrepancies and leakage of all-ceramic crowns: influence of luting agents and aging conditions Int J Prosthodont 16 2003 109 116
    • (2003) Int J Prosthodont , vol.16 , pp. 109-116
    • Gu, X.H.1    Kern, M.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.