메뉴 건너뛰기




Volumn 105, Issue 1, 2014, Pages 237-247

Seawater accelerated ageing of poly(3-hydroxybutyrate-co-3-hydroxyvalerate)

Author keywords

Accelerated ageing; Hydrothermal degradation; Poly(3 hydroxybutyrate co 3 hydroxyvalerate); Seawater

Indexed keywords

DEGRADATION; HYDROLYSIS;

EID: 84901323424     PISSN: 01413910     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.polymdegradstab.2014.04.026     Document Type: Article
Times cited : (74)

References (40)
  • 1
    • 77952955154 scopus 로고    scopus 로고
    • Polyhydroxyalkanoates: Bioplastics with a green agenda
    • T. Keshavarz, and I. Roy Polyhydroxyalkanoates: bioplastics with a green agenda Curr Opin Microbiol 13 2010 321 326
    • (2010) Curr Opin Microbiol , vol.13 , pp. 321-326
    • Keshavarz, T.1    Roy, I.2
  • 2
    • 84879410967 scopus 로고    scopus 로고
    • Expanding bioplastics production: Sustainable business innovation in the chemical industry
    • A. Iles, and A.N. Martin Expanding bioplastics production: sustainable business innovation in the chemical industry J Clean Prod 45 2013 38 49
    • (2013) J Clean Prod , vol.45 , pp. 38-49
    • Iles, A.1    Martin, A.N.2
  • 3
    • 0028972398 scopus 로고
    • Distribution and abundance of debris on the continental shelf of the north-western Mediterranean Sea
    • F. Galgani, S. Jaunet, A. Campillo, X. Guenegen, and E. His Distribution and abundance of debris on the continental shelf of the north-western Mediterranean Sea Mar Pollut Bull 30 1995 713 717 (Pubitemid 26463605)
    • (1995) Marine Pollution Bulletin , vol.30 , Issue.11 , pp. 713-717
    • Galgani, F.1    Jaunet, S.2    Campillo, A.3    Guenegen, X.4    His, E.5
  • 6
    • 78650228112 scopus 로고    scopus 로고
    • Plastic ingestion by planktivorous fishes in the North Pacific Central Gyre
    • C.M. Boerger, G.L. Lattin, S.L. Moore, and C.J. Moore Plastic ingestion by planktivorous fishes in the North Pacific Central Gyre Mar Pollut Bull 60 2010 2275 2278
    • (2010) Mar Pollut Bull , vol.60 , pp. 2275-2278
    • Boerger, C.M.1    Lattin, G.L.2    Moore, S.L.3    Moore, C.J.4
  • 7
    • 0034501647 scopus 로고    scopus 로고
    • Synthesis, structure and properties of polyhydroxyalkanoates: Biological polyesters
    • DOI 10.1016/S0079-6700(00)00035-6
    • K. Sudesh, H. Abe, and Y. Doi Synthesis, structure and properties of polyhydroxyalkanoates: biological polyesters Prog Polym Sci 25 2000 1503 1555 (Pubitemid 32029920)
    • (2000) Progress in Polymer Science (Oxford) , vol.25 , Issue.10 , pp. 1503-1555
    • Sudesh, K.1    Abe, H.2    Doi, Y.3
  • 9
    • 20344362177 scopus 로고    scopus 로고
    • Life cycle assessment study of biopolymers (Polyhydroxyalkanoates) derived from no-tilled corn
    • DOI 10.1065/lca2004.08.171
    • S. Kim, and B. Dale Life cycle assessment study of biopolymers (polyhydroxyalkanoates) - derived from no-tilled corn (11 pp) Int J Life Cycle Assess 10 2005 200 210 (Pubitemid 40791076)
    • (2005) International Journal of Life Cycle Assessment , vol.10 , Issue.3 , pp. 200-210
    • Kim, S.1    Dale, B.E.2
  • 10
    • 34247393752 scopus 로고    scopus 로고
    • Environmental analysis of plastic production processes: Comparing petroleum-based polypropylene and polyethylene with biologically-based poly-β-hydroxybutyric acid using life cycle analysis
    • DOI 10.1016/j.jbiotec.2007.02.012, PII S0168165607001514
    • K.G. Harding, J.S. Dennis, H. von Blottnitz, and S.T.L. Harrison Environmental analysis of plastic production processes: comparing petroleum-based polypropylene and polyethylene with biologically-based poly-β-hydroxybutyric acid using life cycle analysis J Biotechnol 130 2007 57 66 (Pubitemid 46634644)
    • (2007) Journal of Biotechnology , vol.130 , Issue.1 , pp. 57-66
    • Harding, K.G.1    Dennis, J.S.2    Von Blottnitz, H.3    Harrison, S.T.L.4
  • 11
    • 0001815198 scopus 로고
    • Biologically produced (R)-3-hydroxy-alkanoate polymers and copolymers
    • D.C. Bassett, Springer Netherlands
    • P.A. Holmes Biologically produced (R)-3-hydroxy-alkanoate polymers and copolymers D.C. Bassett, Dev. Cryst. Polym 1988 Springer Netherlands 1 65
    • (1988) Dev. Cryst. Polym , pp. 1-65
    • Holmes, P.A.1
  • 12
    • 0032740674 scopus 로고    scopus 로고
    • Biodegradation of poly(3-hydroxyalkanoic acids) fibers and isolation of poly(3-hydroxybutyric acid)-degrading microorganisms under aquatic environments
    • T. Ohura, Y. Aoyagi, K. Takagi, Y. Yoshida, K. Kasuya, and Y. Doi Biodegradation of poly(3-hydroxyalkanoic acids) fibers and isolation of poly(3-hydroxybutyric acid)-degrading microorganisms under aquatic environments Polym Degrad Stab 63 1999 23 29
    • (1999) Polym Degrad Stab , vol.63 , pp. 23-29
    • Ohura, T.1    Aoyagi, Y.2    Takagi, K.3    Yoshida, Y.4    Kasuya, K.5    Doi, Y.6
  • 13
    • 34250806489 scopus 로고    scopus 로고
    • Thermal degradation and (nano)mechanical behavior of layered silicate reinforced poly(3-hydroxybutyrate-co-3-hydroxyvalerate) nanocomposites
    • DOI 10.1016/j.polymertesting.2007.04.001, PII S0142941807000578
    • S. Bruzaud, and A. Bourmaud Thermal degradation and (nano)mechanical behavior of layered silicate reinforced poly(3-hydroxybutyrate-co-3- hydroxyvalerate) nanocomposites Polym Test 26 2007 652 659 (Pubitemid 46978380)
    • (2007) Polymer Testing , vol.26 , Issue.5 , pp. 652-659
    • Bruzaud, S.1    Bourmaud, A.2
  • 15
    • 0034583011 scopus 로고    scopus 로고
    • Biodegradation of poly(3-hydroxybutyrate-co-3-hydroxyvalerate) by a tropical marine bacterium, Pseudoalteromonas sp. NRRL B-30083
    • DOI 10.1023/A:1014873731961
    • T.D. Leathers, N.S. Govind, and R.V. Greene Biodegradation of Poly(3-hydroxybutyrate-co-3-hydroxyvalerate) by a Tropical Marine Bacterium, Pseudoalteromonas sp. NRRL B-30083 J Polym Environ 8 2000 119 124 (Pubitemid 34589640)
    • (2000) Journal of Polymers and the Environment , vol.8 , Issue.3 , pp. 119-124
    • Leathers, T.D.1    Govind, N.S.2    Greene, R.V.3
  • 16
    • 33845427850 scopus 로고    scopus 로고
    • Degradation of commercially important polyhydroxyalkanoates in tropical mangrove ecosystem
    • DOI 10.1016/j.polymdegradstab.2006.08.027, PII S0141391006002680
    • N. Sridewi, K. Bhubalan, and K. Sudesh Degradation of commercially important polyhydroxyalkanoates in tropical mangrove ecosystem Polym Degrad Stab 91 2006 2931 2940 (Pubitemid 44894308)
    • (2006) Polymer Degradation and Stability , vol.91 , Issue.12 , pp. 2931-2940
    • Sridewi, N.1    Bhubalan, K.2    Sudesh, K.3
  • 17
    • 78649413039 scopus 로고    scopus 로고
    • Biodegradation of polyhydroxyalkanoates (PHAs) in tropical coastal waters and identification of PHA-degrading bacteria
    • T.G. Volova, A.N. Boyandin, A.D. Vasiliev, V.A. Karpov, S.V. Prudnikova, and O.V. Mishukova et al. Biodegradation of polyhydroxyalkanoates (PHAs) in tropical coastal waters and identification of PHA-degrading bacteria Polym Degrad Stab 95 2010 2350 2359
    • (2010) Polym Degrad Stab , vol.95 , pp. 2350-2359
    • Volova, T.G.1    Boyandin, A.N.2    Vasiliev, A.D.3    Karpov, V.A.4    Prudnikova, S.V.5    Mishukova, O.V.6
  • 19
    • 0036151323 scopus 로고    scopus 로고
    • Environmental degradation of biodegradable polyesters 1. Poly(ε-caprolactone), poly[(R)-3-hydroxybutyrate], and poly(L-lactide) films in controlled static seawater
    • DOI 10.1016/S0141-3910(01)00240-3, PII S0141391001002403
    • H. Tsuji, and K. Suzuyoshi Environmental degradation of biodegradable polyesters 1. Poly(ε-caprolactone), poly[(R)-3-hydroxybutyrate], and poly(L-lactide) films in controlled static seawater Polym Degrad Stab 75 2002 347 355 (Pubitemid 34086306)
    • (2002) Polymer Degradation and Stability , vol.75 , Issue.2 , pp. 347-355
    • Tsuji, H.1    Suzuyoshi, K.2
  • 20
    • 0036151351 scopus 로고    scopus 로고
    • Environmental degradation of biodegradable polyesters 2. Poly(ε-caprolactone), poly[(R)-3-hydroxybutyrate], and poly(L-lactide) films in natural dynamic seawater
    • DOI 10.1016/S0141-3910(01)00239-7, PII S0141391001002397
    • H. Tsuji, and K. Suzuyoshi Environmental degradation of biodegradable polyesters 2. Poly(ε-caprolactone), poly[(R)-3-hydroxybutyrate], and poly(L-lactide) films in natural dynamic seawater Polym Degrad Stab 75 2002 357 365 (Pubitemid 34086307)
    • (2002) Polymer Degradation and Stability , vol.75 , Issue.2 , pp. 357-365
    • Tsuji, H.1    Suzuyoshi, K.2
  • 21
    • 58049193743 scopus 로고    scopus 로고
    • Environmental degradation of blends of atactic poly[(R,S)-3- hydroxybutyrate] with natural PHBV in Baltic sea water and compost with activated sludge
    • M. Rutkowska, K. Krasowska, A. Heimowska, G. Adamus, M. Sobota, and M. Musioł et al. Environmental degradation of blends of atactic poly[(R,S)-3-hydroxybutyrate] with natural PHBV in Baltic sea water and compost with activated sludge J Polym Environ 16 2008 183 191
    • (2008) J Polym Environ , vol.16 , pp. 183-191
    • Rutkowska, M.1    Krasowska, K.2    Heimowska, A.3    Adamus, G.4    Sobota, M.5    Musioł, M.6
  • 22
    • 55449092751 scopus 로고    scopus 로고
    • Comparing the degradation of Poly-B-(hydroxybutyrate), poly-B-(hydroxbutyrate-co-valerate)(PHBV) and PHBV/cellulose tricate blend
    • I.I. Muhamad, K.J. Lee, and M.A. Mohd Noor Comparing the degradation of Poly-B-(hydroxybutyrate), poly-B-(hydroxbutyrate-co-valerate)(PHBV) and PHBV/cellulose tricate blend Malays Polym J 1 2006 39 46
    • (2006) Malays Polym J , vol.1 , pp. 39-46
    • Muhamad, I.I.1    Lee, K.J.2    Mohd Noor, M.A.3
  • 23
    • 0028262871 scopus 로고
    • Efficient hydrolysis of polyhydroxyalkanoates by Pseudomonas stutzeri YM1414 isolated from lake water
    • K. Mukai, K. Yamada, and Y. Doi Efficient hydrolysis of polyhydroxyalkanoates by Pseudomonas stutzeri YM1414 isolated from lake water Polym Degrad Stab 43 1994 319 327
    • (1994) Polym Degrad Stab , vol.43 , pp. 319-327
    • Mukai, K.1    Yamada, K.2    Doi, Y.3
  • 24
    • 77955305767 scopus 로고    scopus 로고
    • Biodegradation behavior of PHBV films in a pilot-scale composting condition
    • Y.-X. Weng, Y. Wang, X.-L. Wang, and Y.-Z. Wang Biodegradation behavior of PHBV films in a pilot-scale composting condition Polym Test 29 2010 579 587
    • (2010) Polym Test , vol.29 , pp. 579-587
    • Weng, Y.-X.1    Wang, Y.2    Wang, X.-L.3    Wang, Y.-Z.4
  • 25
    • 84856338003 scopus 로고    scopus 로고
    • Morphology and functional properties of commercial polyhydroxyalkanoates: A comprehensive and comparative study
    • Y.-M. Corre, S. Bruzaud, J.-L. Audic, and Y. Grohens Morphology and functional properties of commercial polyhydroxyalkanoates: a comprehensive and comparative study Polym Test 31 2012 226 235
    • (2012) Polym Test , vol.31 , pp. 226-235
    • Corre, Y.-M.1    Bruzaud, S.2    Audic, J.-L.3    Grohens, Y.4
  • 26
    • 18844422758 scopus 로고    scopus 로고
    • Mechanical properties of short flax fibre bundle/polypropylene composites: Influence of matrix/fibre modification, fibre content, water uptake and recycling
    • DOI 10.1016/j.compscitech.2005.01.008, PII S0266353805000370
    • A. Arbelaiz, B. Fernández, J.A. Ramos, A. Retegi, R. Llano-Ponte, and I. Mondragon Mechanical properties of short flax fibre bundle/polypropylene composites: Influence of matrix/fibre modification, fibre content, water uptake and recycling Compos Sci Technol 65 2005 1582 1592 (Pubitemid 40697051)
    • (2005) Composites Science and Technology , vol.65 , Issue.10 , pp. 1582-1592
    • Arbelaiz, A.1    Fernandez, B.2    Ramos, J.A.3    Retegi, A.4    Llano-Ponte, R.5    Mondragon, I.6
  • 27
    • 0021494341 scopus 로고
    • Crystallization and morphology of a bacterial thermoplastic: Poly-3-hydroxybutyrate
    • P.J. Barham, A. Keller, E.L. Otun, and P.A. Holmes Crystallization and morphology of a bacterial thermoplastic: poly-3-hydroxybutyrate J Mater Sci 19 1984 2781 2794 (Pubitemid 14668617)
    • (1984) Journal of Materials Science , vol.19 , Issue.9 , pp. 2781-2794
    • Barham, P.J.1    Keller, A.2    Otun, E.L.3    Holmes, P.A.4
  • 28
    • 0033909174 scopus 로고    scopus 로고
    • Poly(3-hydroxybutyrate-co-3-hydroxyvalerate) and wheat straw fibre composites: Thermal, mechanical properties and biodegradation behaviour
    • DOI 10.1023/A:1004773603516
    • M. Avella, G.L. Rota, E. Martuscelli, M. Raimo, P. Sadocco, and G. Elegir et al. Poly(3-hydroxybutyrate-co-3-hydroxyvalerate) and wheat straw fibre composites: thermal, mechanical properties and biodegradation behaviour J Mater Sci 35 2000 829 836 (Pubitemid 30553616)
    • (2000) Journal of Materials Science , vol.35 , Issue.4 , pp. 829-836
    • Avella, M.1    La Rota, G.2    Martuscelli, E.3    Raimo, M.4    Sadocco, P.5    Elegir, G.6    Riva, R.7
  • 30
    • 67349160778 scopus 로고    scopus 로고
    • Seawater ageing of flax/poly(lactic acid) biocomposites
    • A. Le Duigou, P. Davies, and C. Baley Seawater ageing of flax/poly(lactic acid) biocomposites Polym Degrad Stab 94 2009 1151 1162
    • (2009) Polym Degrad Stab , vol.94 , pp. 1151-1162
    • Le Duigou, A.1    Davies, P.2    Baley, C.3
  • 32
    • 0036320242 scopus 로고    scopus 로고
    • Why degradable polymers undergo surface erosion or bulk erosion
    • DOI 10.1016/S0142-9612(02)00170-9, PII S0142961202001709
    • F. von Burkersroda, L. Schedl, and A. Göpferich Why degradable polymers undergo surface erosion or bulk erosion Biomaterials 23 2002 4221 4231 (Pubitemid 34814991)
    • (2002) Biomaterials , vol.23 , Issue.21 , pp. 4221-4231
    • Burkersroda, F.V.1    Schedl, L.2    Gopferich, A.3
  • 33
    • 84893163469 scopus 로고    scopus 로고
    • Accelerated ageing of polylactide in aqueous environments: Comparative study between distilled water and seawater
    • 10.1016/j.polymdegradstab.2014.01.020
    • M. Deroiné, A. Le Duigou, Y.-M. Corre, P.-Y. Le Gac, P. Davies, and S. Bruzaud Accelerated ageing of polylactide in aqueous environments: comparative study between distilled water and seawater Polym Degrad Stab 2014 10.1016/j.polymdegradstab.2014.01.020
    • (2014) Polym Degrad Stab
    • Deroiné, M.1    Le Duigou, A.2    Corre, Y.-M.3    Le Gac, P.-Y.4    Davies, P.5    Bruzaud, S.6
  • 34
    • 84884186895 scopus 로고    scopus 로고
    • 9.09-Poly(hydroxyalkanoate)s
    • K. Matyjaszewski, M. Möller, Elsevier Amsterdam
    • S. Taguchi, T. Iwata, H. Abe, and Y. Doi 9.09-Poly(hydroxyalkanoate)s K. Matyjaszewski, M. Möller, Polym. Sci. Compr. Ref 2012 Elsevier Amsterdam 157 182
    • (2012) Polym. Sci. Compr. Ref , pp. 157-182
    • Taguchi, S.1    Iwata, T.2    Abe, H.3    Doi, Y.4
  • 35
    • 44949109053 scopus 로고    scopus 로고
    • Enzymatic processes for biodegradation of poly(hydroxyalkanoate)s crystals
    • K. Numata, H. Abe, and Y. Doi Enzymatic processes for biodegradation of poly(hydroxyalkanoate)s crystals Can J Chem 86 2008 471 483
    • (2008) Can J Chem , vol.86 , pp. 471-483
    • Numata, K.1    Abe, H.2    Doi, Y.3
  • 36
    • 0027227008 scopus 로고
    • Enzymatic degradation of poly(hydroxyalkanoates) by a marine bacterium
    • K. Mukai, K. Yamada, and Y. Doi Enzymatic degradation of poly(hydroxyalkanoates) by a marine bacterium Polym Degrad Stab 41 1993 85 91
    • (1993) Polym Degrad Stab , vol.41 , pp. 85-91
    • Mukai, K.1    Yamada, K.2    Doi, Y.3
  • 38
    • 43249110043 scopus 로고    scopus 로고
    • Surface composition and morphology of poly(3-hydroxybutyrate) exposed to biodegradation
    • M.C.S. Corrêa, M.L. Rezende, D.S. Rosa, J.A.M. Agnelli, and P.A.P. Nascente Surface composition and morphology of poly(3-hydroxybutyrate) exposed to biodegradation Polym Test 27 2008 447 452
    • (2008) Polym Test , vol.27 , pp. 447-452
    • Corrêa, M.C.S.1    Rezende, M.L.2    Rosa, D.S.3    Agnelli, J.A.M.4    Nascente, P.A.P.5
  • 39
    • 0027329331 scopus 로고
    • Microbial degradation of poly(3-hydroxybutyrate) and poly(3- hydroxybutyrate-co-3-hydroxyvalerate) in soils
    • J. Mergaert, A. Webb, C. Anderson, A. Wouters, and J. Swings Microbial degradation of poly(3-hydroxybutyrate) and poly(3-hydroxybutyrate-co-3- hydroxyvalerate) in soils Appl Environ Microbiol 59 1993 3233 3238 (Pubitemid 23296437)
    • (1993) Applied and Environmental Microbiology , vol.59 , Issue.10 , pp. 3233-3238
    • Mergaert, J.1    Webb, A.2    Anderson, C.3    Wouters, A.4    Swings, J.5
  • 40
    • 0032917816 scopus 로고    scopus 로고
    • Further investigations on the hydrolytic degradation of poly (DL-lactide)
    • DOI 10.1016/S0142-9612(97)00226-3, PII S0142961297002263
    • S. Li, and S. McCarthy Further investigations on the hydrolytic degradation of poly (DL-lactide) Biomaterials 20 1999 35 44 (Pubitemid 29002543)
    • (1999) Biomaterials , vol.20 , Issue.1 , pp. 35-44
    • Li, S.1    McCarthy, S.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.