Enhanced CuO nanowire formation by thermal oxidation of roughened copper

Author keywords

[No Author keywords available]

Indexed keywords

COPPER SURFACE; CU ATOMS; DIFFUSIONAL TRANSPORT; FINER GRAINS; GRAIN SIZE; LAYERED OXIDES; METAL SUBSTRATE; NANOWIRE FORMATION; NANOWIRE GROWTH; NUCLEATION AND GROWTH; OXIDE LAYER; THERMAL OXIDATION;

EID: 84857389218     PISSN: 00134651     EISSN: None     Source Type: Journal    
DOI: 10.1149/2.102204jes     Document Type: Article
Times cited : (59)

References (37)
  • 1
    • 33744789387 scopus 로고    scopus 로고
    • Quasi-one-dimensional metal oxide materials-Synthesis, properties and applications
    • DOI 10.1016/j.mser.2006.04.002, PII S0927796X06000283
    • J. G. Lu, P. Chang, and Z. Fan, Materials Science and Engineering: R: Reports, 52, 49 (2006). 10.1016/j.mser.2006.04.002 (Pubitemid 43831607)
    • (2006) Materials Science and Engineering R: Reports , vol.52 , Issue.1-3 , pp. 49-91
    • Lu, J.G.1    Chang, P.2    Fan, Z.3
  • 9
    • 0005357948 scopus 로고
    • 10.1143/JPSJ.12.1212
    • R. Takagi, J. Phys. Soc. Japan, 12, 1212 (1957). 10.1143/JPSJ.12.1212
    • (1957) J. Phys. Soc. Japan , vol.12 , pp. 1212
    • Takagi, R.1
  • 26
    • 8344278007 scopus 로고    scopus 로고
    • A study of the initial oxidation of copper in 0.1 MPa oxygen and the effect of purity by metallographic methods
    • DOI 10.1016/j.corsci.2004.02.002, PII S0010938X04000472
    • Y. Zhu, K. Mimura, and M. Isshiki, Corrosion Science, 46, 2445 (2004). 10.1016/j.corsci.2004.02.002 (Pubitemid 39483753)
    • (2004) Corrosion Science , vol.46 , Issue.10 , pp. 2445-2454
    • Zhu, Y.1    Mimura, K.2    Isshiki, M.3
  • 27
    • 25644436284 scopus 로고    scopus 로고
    • Influence of small amounts of impurities on initial oxidation of copper at 400 and 800°C in 0.1 MPa oxygen atmosphere
    • DOI 10.1149/1.1943667
    • Y. Zhu, K. Mimura, S.-H. Hong, and M. Isshiki, Journal of The Electrochemical Society, 152, B296 (2005). 10.1149/1.1943667 (Pubitemid 41381125)
    • (2005) Journal of the Electrochemical Society , vol.152 , Issue.8
    • Zhu, Y.1    Mimura, K.2    Hong, S.-H.3    Isshiki, M.4
  • 28
    • 10044270884 scopus 로고    scopus 로고
    • Influence of oxide grain morphology on formation of the CuO scale during oxidation of copper at 600-1000°C
    • DOI 10.1016/j.corsci.2004.06.020, PII S0010938X04002094
    • Y. Zhu, K. Mimura, and M. Isshiki, Corrosion Science, 47, 537 (2005). 10.1016/j.corsci.2004.06.020 (Pubitemid 39605945)
    • (2005) Corrosion Science , vol.47 , Issue.2 , pp. 537-544
    • Zhu, Y.1    Mimura, K.2    Isshiki, M.3
  • 36
    • 0038412482 scopus 로고    scopus 로고
    • 10.1016/S0039-6028(03)00539-9
    • G. W. Zhou and J. C. Yang, Surface Science, 531, 359 (2003). 10.1016/S0039-6028(03)00539-9
    • (2003) Surface Science , vol.531 , pp. 359
    • Zhou, G.W.1    Yang, J.C.2
  • 37
    • 2942536764 scopus 로고    scopus 로고
    • 10.1016/j.susc.2004.04.046
    • G. W. Zhou and J. C. Yang, Surface Science, 559, 100 (2004). 10.1016/j.susc.2004.04.046
    • (2004) Surface Science , vol.559 , pp. 100
    • Zhou, G.W.1    Yang, J.C.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.