Volumn 43, Issue 1, 2012, Pages 198-207

Mode i interfacial toughening through discontinuous interleaves for damage suppression and control

Author keywords

B. Delamination; B. Fracture toughness; Crack arrest; D. Fractography

Indexed keywords

CRACK ARREST; CRACK PATHS; DAMAGE SUPPRESSION; DOUBLE CANTILEVER BEAM; E-GLASS; FIBRE-REINFORCED EPOXY; GLASS/EPOXY; HOST MATERIALS; INTERACTION POINTS; INTERLAMINAR CRACKS; PREPREGS; THERMOPLASTIC FILMS; THERMOSET ADHESIVES; UNDERLYING MECHANISM;

EID: 81855207353     PISSN: 1359835X     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.compositesa.2011.10.009     Document Type: Article
Times cited : (131)

References (58)
  • 2
    • 0040118317 scopus 로고
    • Crack arrest methodology and applications
    • T. Kobayashi, and J.W. Dally Crack arrest methodology and applications ASTM STP 711 1979 189 210
    • (1979) ASTM STP , vol.711 , pp. 189-210
    • Kobayashi, T.1    Dally, J.W.2
  • 4
    • 0037330624 scopus 로고    scopus 로고
    • The assessment of novel materials and processes for the impact tolerant design of stiffened composite aerospace structures
    • E. Greenhalgh, and M. Hiley The assessment of novel materials and processes for the impact tolerant design of stiffened composite aerospace structures Compos Part A 34 2003 151 161
    • (2003) Compos Part A , vol.34 , pp. 151-161
    • Greenhalgh, E.1    Hiley, M.2
  • 5
    • 3543133630 scopus 로고    scopus 로고
    • Integral manufacturing of composite skin-stringer assembly and their stability analyses
    • H. Mahfuz, P. Majumdar, M. Saha, F. Shamery, and S. Jeelani Integral manufacturing of composite skin-stringer assembly and their stability analyses Appl Compos Mater 11 2004 155 171
    • (2004) Appl Compos Mater , vol.11 , pp. 155-171
    • Mahfuz, H.1    Majumdar, P.2    Saha, M.3    Shamery, F.4    Jeelani, S.5
  • 6
    • 53849127137 scopus 로고    scopus 로고
    • Crack-growth arrest by redirecting crack growth by drilling stop holes and inserting pins into them
    • C. Makabe, A. Murdani, K. Kuniyoshi, Y. Irei, and A. Saimoto Crack-growth arrest by redirecting crack growth by drilling stop holes and inserting pins into them Eng Fail Anal 16 2009 475 483
    • (2009) Eng Fail Anal , vol.16 , pp. 475-483
    • Makabe, C.1    Murdani, A.2    Kuniyoshi, K.3    Irei, Y.4    Saimoto, A.5
  • 8
    • 40649112892 scopus 로고    scopus 로고
    • A status report on delamination resistance testing of polymer-matrix composites
    • DOI 10.1016/j.engfracmech.2007.03.012, PII S0013794407001208
    • A. Brunner, B. Blackman, and P. Davies A status report on delamination resistance testing of polymer-matrix composites Eng Fract Mech 75 June 2008 2779 2794 (Pubitemid 351372777)
    • (2008) Engineering Fracture Mechanics , vol.75 , Issue.9 , pp. 2779-2794
    • Brunner, A.J.1    Blackman, B.R.K.2    Davies, P.3
  • 13
    • 0026257580 scopus 로고
    • Analysis of interleaved end-notched flexure specimen for measuring mode II fracture toughness
    • L.A. Carlsson, and A. Aksoy Analysis of interleaved end-notched flexure specimen for measuring mode II fracture toughness Int J Fract 52 1991 67 77
    • (1991) Int J Fract , vol.52 , pp. 67-77
    • Carlsson, L.A.1    Aksoy, A.2
  • 14
    • 0029276773 scopus 로고
    • Effect of interleaving on the impact response of a unidirectional carbon/epoxy composite
    • F.S. Liao, W.H. Lu, A.C. Su, P.W. Kao, and T.J. Hsu Effect of interleaving on the impact response of a unidirectional carbon/epoxy composite Composites 26 1995 215 222
    • (1995) Composites , vol.26 , pp. 215-222
    • Liao, F.S.1    Lu, W.H.2    Su, A.C.3    Kao, P.W.4    Hsu, T.J.5
  • 15
    • 0024877008 scopus 로고
    • Improved impact and delamination resistance through interleafing
    • J.E. Masters Improved impact and delamination resistance through interleafing Key Eng Mater 37 1989 317 348
    • (1989) Key Eng Mater , vol.37 , pp. 317-348
    • Masters, J.E.1
  • 16
    • 0029412880 scopus 로고
    • Mixed-mode fracture in an interleaved carbon-fibre/epoxy composite
    • S. Singh, and I.K. Partridge Mixed-mode fracture in an interleaved carbon-fibre/epoxy composite Compos Sci Technol 55 1995 319 327
    • (1995) Compos Sci Technol , vol.55 , pp. 319-327
    • Singh, S.1    Partridge, I.K.2
  • 18
    • 81855181960 scopus 로고
    • Concepts for crack arrestment in composites
    • G. Sendeckyj Concepts for crack arrestment in composites ASTM Spec Tech Publ 593 1976 215
    • (1976) ASTM Spec Tech Publ , vol.593 , pp. 215
    • Sendeckyj, G.1
  • 19
    • 0022863704 scopus 로고
    • Delamination arrester-an adhesive inner layer in laminated composites
    • W.S. Chan Delamination arrester-an adhesive inner layer in laminated composites Compos Mater 1986 176
    • (1986) Compos Mater , pp. 176
    • Chan, W.S.1
  • 20
    • 0024734084 scopus 로고
    • Interlaminar fracture toughness and toughening of laminated composite materials: A review
    • N. Sela, and O. Ishai Interlaminar fracture toughness and toughening of laminated composite materials: a review Composites 20 September 1989 423 435
    • (1989) Composites , vol.20 , pp. 423-435
    • Sela, N.1    Ishai, O.2
  • 21
    • 33745964340 scopus 로고    scopus 로고
    • Modes I and II interlaminar fracture toughness and fatigue delamination of CF/epoxy laminates with self-same epoxy interleaf
    • DOI 10.1016/j.ijfatigue.2006.02.004, PII S0142112306000351
    • M. Hojo, T. Ando, M. Tanaka, T. Adachi, S. Ochiai, and Y. Endo Modes I and II interlaminar fracture toughness and fatigue delamination of CF/epoxy laminates with self-same epoxy interleaf Int J Fatigue 28 October 2006 1154 1165 (Pubitemid 44061956)
    • (2006) International Journal of Fatigue , vol.28 , Issue.SPEC. ISS. , pp. 1154-1165
    • Hojo, M.1    Ando, T.2    Tanaka, M.3    Adachi, T.4    Ochiai, S.5    Endo, Y.6
  • 22
    • 0024657358 scopus 로고
    • The effect of adhesive thickness on interlaminar fracture toughness of interleaved cfrp specimens
    • N. Sela, O. Ishai, and L. Bankssills The effect of adhesive thickness on interlaminar fracture toughness of interleaved cfrp specimens Composites 20 May 1989 257 264
    • (1989) Composites , vol.20 , pp. 257-264
    • Sela, N.1    Ishai, O.2    Bankssills, L.3
  • 23
    • 0035385656 scopus 로고    scopus 로고
    • Improvement of vibration damping capacity and fracture toughness in composite laminates by the use of polymeric interleaves
    • DOI 10.1115/1.1370385
    • R.F. Gibson, Y. Chen, and H. Zhao Improvement of vibration damping capacity and fracture toughness in composite laminates by the use of polymeric interleaves J Eng Mater Technol, Trans ASME 123 2001 309 314 (Pubitemid 32981859)
    • (2001) Journal of Engineering Materials and Technology, Transactions of the ASME , vol.123 , Issue.3 , pp. 309-314
    • Gibson, R.F.1    Chen, Y.2    Zhao, H.3
  • 24
    • 0026711933 scopus 로고
    • Mode i interlaminar fracture of interleaved graphite/epoxy
    • F. Ozdil, and L.A. Carlsson Mode I interlaminar fracture of interleaved graphite/epoxy J Compos Mater 26 1 1992 432 459
    • (1992) J Compos Mater , vol.26 , Issue.1 , pp. 432-459
    • Ozdil, F.1    Carlsson, L.A.2
  • 25
    • 0035516471 scopus 로고    scopus 로고
    • Loading rate dependence of mode II fracture behavior in interleaved carbon fibre/epoxy composite laminates
    • DOI 10.1023/A:1012658114593
    • W.E.I. Jiang, F.F.Y. Tsang, S.C. Tjong, and R.K.Y. Li Loading rate dependence of mode II fracture behavior in interleaved carbon fibre/epoxy composite laminates Appl Compos Mater 2006 361 369 (Pubitemid 34002777)
    • (2001) Applied Composite Materials , vol.8 , Issue.6 , pp. 361-369
    • Jiang, W.1    Tsang, F.F.Y.2    Tjong, S.C.3    Li, R.K.Y.4    Kim, J.K.5    Mai, Y.-W.6
  • 26
    • 0036378552 scopus 로고    scopus 로고
    • Effect of interleaved non-woven carbon tissue on interlaminar fracture toughness of laminated composites: Part I-mode II
    • S.H. Lee, H. Noguchi, Y.B. Kim, and S.K. Cheong Effect of interleaved non-woven carbon tissue on interlaminar fracture toughness of laminated composites: Part I-mode II J Compos Mater 36 2002 2153
    • (2002) J Compos Mater , vol.36 , pp. 2153
    • Lee, S.H.1    Noguchi, H.2    Kim, Y.B.3    Cheong, S.K.4
  • 27
    • 0036378543 scopus 로고    scopus 로고
    • Effect of interleaved non-woven carbon tissue on interlaminar fracture toughness of laminated composites: Part II-mode i
    • S.H. Lee, H. Noguchi, Y.B. Kim, and S.K. Cheong Effect of interleaved non-woven carbon tissue on interlaminar fracture toughness of laminated composites: Part II-mode I J Compos Mater 36 2002 2169
    • (2002) J Compos Mater , vol.36 , pp. 2169
    • Lee, S.H.1    Noguchi, H.2    Kim, Y.B.3    Cheong, S.K.4
  • 28
    • 50949095558 scopus 로고    scopus 로고
    • A toughening and strengthening technique of hybrid composites with non-woven tissue
    • S. Lee, J. Lee, S. Cheong, and H. Noguchi A toughening and strengthening technique of hybrid composites with non-woven tissue J Mater Process Technol 207 October 2008 21 29
    • (2008) J Mater Process Technol , vol.207 , pp. 21-29
    • Lee, S.1    Lee, J.2    Cheong, S.3    Noguchi, H.4
  • 30
    • 0001250009 scopus 로고
    • Comparative study of dynamic and static delamination behaviour of carbon fibre/epoxy composite laminates
    • M.S. Sohn, and X.Z. Hu Comparative study of dynamic and static delamination behaviour of carbon fibre/epoxy composite laminates Composites 26 1995 849
    • (1995) Composites , vol.26 , pp. 849
    • Sohn, M.S.1    Hu, X.Z.2
  • 31
    • 70450225053 scopus 로고    scopus 로고
    • Interlaminar and intralaminar reinforcement of composite laminates with aligned carbon nanotubes
    • S.S. Wicks, R.G. de Villoria, and B.L. Wardle Interlaminar and intralaminar reinforcement of composite laminates with aligned carbon nanotubes Compos Sci Technol 70 January 2010 20 28
    • (2010) Compos Sci Technol , vol.70 , pp. 20-28
    • Wicks, S.S.1    De Villoria, R.G.2    Wardle, B.L.3
  • 32
    • 44149116674 scopus 로고    scopus 로고
    • Joining prepreg composite interfaces with aligned carbon nanotubes
    • E.J. Garcia, B.L. Wardle, and A. John Hart Joining prepreg composite interfaces with aligned carbon nanotubes Compos Part A 39 2008 1065 1070
    • (2008) Compos Part A , vol.39 , pp. 1065-1070
    • Garcia, E.J.1    Wardle, B.L.2    John Hart, A.3
  • 33
    • 38649108553 scopus 로고    scopus 로고
    • Improvement of damage resistance in laminated composites with electrospun nano-interlayers
    • DOI 10.1016/j.compscitech.2007.09.015, PII S0266353807003624
    • S. Sihn, R.Y. Kim, W. Huh, K.-H. Lee, and A.K. Roy Improvement of damage resistance in laminated composites with electrospun nano-interlayers Compos Sci Technol 68 2008 673 683 (Pubitemid 351168377)
    • (2008) Composites Science and Technology , vol.68 , Issue.3-4 , pp. 673-683
    • Sihn, S.1    Kim, R.Y.2    Huh, W.3    Lee, K.-H.4    Roy, A.K.5
  • 34
    • 37349028020 scopus 로고    scopus 로고
    • Mode I and mode II interlaminar fracture toughness of CFRP laminates toughened by carbon nanofiber interlayer
    • DOI 10.1016/j.compscitech.2007.06.007, PII S0266353807002497
    • M. Arai, Y. Noro, K.-Ichi Sugimoto, and M. Endo Mode I and mode II interlaminar fracture toughness of CFRP laminates toughened by carbon nanofiber interlayer Compos Sci Technol 68 2008 516 525 (Pubitemid 350286649)
    • (2008) Composites Science and Technology , vol.68 , Issue.2 , pp. 516-525
    • Arai, M.1    Noro, Y.2    Sugimoto, K.-i.3    Endo, M.4
  • 35
    • 64249120738 scopus 로고    scopus 로고
    • B-staged epoxy/single-walled carbon nanotube nanocomposite thin films for composite reinforcement
    • G.L. Warren, L. Sun, V.G. Hadjiev, D. Davis, D. Lagoudas, and H.J. Sue B-staged epoxy/single-walled carbon nanotube nanocomposite thin films for composite reinforcement J Appl Polym Sci 112 2009 290 298
    • (2009) J Appl Polym Sci , vol.112 , pp. 290-298
    • Warren, G.L.1    Sun, L.2    Hadjiev, V.G.3    Davis, D.4    Lagoudas, D.5    Sue, H.J.6
  • 36
    • 77955333345 scopus 로고    scopus 로고
    • Electrospun nanofibre toughened carbon/epoxy composites: Effects of polyetherketone cardo (PEK-C) nanofibre diameter and interlayer thickness
    • J. Zhang, T. Lin, and X. Wang Electrospun nanofibre toughened carbon/epoxy composites: effects of polyetherketone cardo (PEK-C) nanofibre diameter and interlayer thickness Compos Sci Technol 70 October 2010 1660 1666
    • (2010) Compos Sci Technol , vol.70 , pp. 1660-1666
    • Zhang, J.1    Lin, T.2    Wang, X.3
  • 37
    • 75449093785 scopus 로고    scopus 로고
    • Effect of nylon-66 nano-fiber interleaving on impact damage resistance of epoxy/carbon fiber composite laminates
    • P. Akangah, S. Lingaiah, and K. Shivakumar Effect of nylon-66 nano-fiber interleaving on impact damage resistance of epoxy/carbon fiber composite laminates Compos Struct 92 2010 1432 1439
    • (2010) Compos Struct , vol.92 , pp. 1432-1439
    • Akangah, P.1    Lingaiah, S.2    Shivakumar, K.3
  • 39
    • 36448981378 scopus 로고    scopus 로고
    • Novel carbon fiber/epoxy composite toughened by electrospun polysulfone nanofibers
    • DOI 10.1016/j.matlet.2007.05.080, PII S0167577X07005885
    • G. Li, P. Li, Y. Yu, X. Jia, S. Zhang, and X. Yang Novel carbon fiber/epoxy composite toughened by electrospun polysulfone nanofibers Mater Lett 62 2008 511 514 (Pubitemid 350166626)
    • (2008) Materials Letters , vol.62 , Issue.3 , pp. 511-514
    • Li, G.1    Li, P.2    Yu, Y.3    Jia, X.4    Zhang, S.5    Yang, X.6    Ryu, S.7
  • 40
    • 0036567075 scopus 로고    scopus 로고
    • Improvement of the interlaminar fracture toughness of composite laminates by whisker reinforced interlamination
    • DOI 10.1016/S0266-3538(02)00052-0, PII S0266353802000520
    • W.X. Wang, Y. Takao, T. Matsubara, and H.S. Kim Improvement of the interlaminar fracture toughness of composite laminates by whisker reinforced interlamination Compos Sci Technol 62 2002 767 774 (Pubitemid 34527730)
    • (2002) Composites Science and Technology , vol.62 , Issue.6 , pp. 767-774
    • Wang, W.X.1    Takao, Y.2    Matsubara, T.3    Kim, H.S.4
  • 41
    • 33845530963 scopus 로고    scopus 로고
    • Mode II delamination and damage resistance of carbon/epoxy composite laminates interleaved with thermoplastic particles
    • DOI 10.1177/0021998306063356
    • F. Gao, G. Jiao, Z. Lu, and R. Ning Mode II delamination and damage resistance of carbon/epoxy composite laminates interleaved with thermoplastic particles J Compos Mater 41 March 2006 111 123 (Pubitemid 44927122)
    • (2007) Journal of Composite Materials , vol.41 , Issue.1 , pp. 111-123
    • Gao, F.1    Jiao, G.2    Lu, Z.3    Ning, R.4
  • 43
    • 45849119018 scopus 로고    scopus 로고
    • The effect of surface treatment on delamination for a nylon interleaving material
    • G. Heness, M. Stevens, and B. Dossett The effect of surface treatment on delamination for a nylon interleaving material Mater Forum 2007 90 95
    • (2007) Mater Forum , pp. 90-95
    • Heness, G.1    Stevens, M.2    Dossett, B.3
  • 44
    • 0037349957 scopus 로고    scopus 로고
    • Interlayer toughened unidirectional carbon prepreg systems: Effect of preformed particle morphology
    • E. Gilbert, B. Hayes, and J. Seferis Interlayer toughened unidirectional carbon prepreg systems: effect of preformed particle morphology Compos Part A 34 March 2003 245 252
    • (2003) Compos Part A , vol.34 , pp. 245-252
    • Gilbert, E.1    Hayes, B.2    Seferis, J.3
  • 45
    • 0025747678 scopus 로고
    • Fracture behaviour of interleaved fiber-resin composites
    • DOI 10.1016/0266-3538(91)90054-S
    • S. Chen, and B. Jang Fracture behaviour of interleaved fiber-resin composites Compos Sci Technol 41 1991 77 97 (Pubitemid 21651306)
    • (1991) Composites Science and Technology , vol.41 , Issue.1 , pp. 77-97
    • Chen, S.F.1    Jang, B.Z.2
  • 46
    • 0030192575 scopus 로고    scopus 로고
    • The influence of thermoplastic film interleaving on the interlaminar shear strength and mode i fracture of laminated composites
    • L. Li, P. Lee-Sullivan, and K. Liew The influence of thermoplastic film interleaving on the interlaminar shear strength and mode I fracture of laminated composites J Eng Mater Technol 118 1996 302
    • (1996) J Eng Mater Technol , vol.118 , pp. 302
    • Li, L.1    Lee-Sullivan, P.2    Liew, K.3
  • 47
    • 0035062967 scopus 로고    scopus 로고
    • Interlaminar fracture properties of carbon fibre/epoxy matrix composites interleaved with polyethylene terephthalate (PET) films
    • W. Jiang, S. Tjong, P. Chu, and R. Li Interlaminar fracture properties of carbon fibre/epoxy matrix composites interleaved with polyethylene terephthalate (PET) films Polym Polym Compos 9 2001 141 146
    • (2001) Polym Polym Compos , vol.9 , pp. 141-146
    • Jiang, W.1    Tjong, S.2    Chu, P.3    Li, R.4
  • 48
    • 52949104043 scopus 로고    scopus 로고
    • Experimental optimization of the impact energy absorption of epoxy-carbon laminates through controlled delamination
    • A. Pegoretti, I. Cristelli, and C. Migliaresi Experimental optimization of the impact energy absorption of epoxy-carbon laminates through controlled delamination Compos Sci Technol 68 10 2008 2653 2662
    • (2008) Compos Sci Technol , vol.68 , Issue.10 , pp. 2653-2662
    • Pegoretti, A.1    Cristelli, I.2    Migliaresi, C.3
  • 51
    • 0034745718 scopus 로고    scopus 로고
    • The effects of strain-rate and temperature on the interlaminar fracture toughness of interleaved PEEK/CF composites
    • R. Fracasso, M. Rink, A. Pavan, and R. Frassine The effects of strain-rate and temperature on the interlaminar fracture toughness of interleaved PEEK/CF composites Compos Sci Technol 61 1 2001 57 63
    • (2001) Compos Sci Technol , vol.61 , Issue.1 , pp. 57-63
    • Fracasso, R.1    Rink, M.2    Pavan, A.3    Frassine, R.4
  • 54
    • 33744947517 scopus 로고    scopus 로고
    • Tailoring mechanical properties of highly porous polymer foams: Silica particle reinforced polymer foams via emulsion templating
    • DOI 10.1016/j.polymer.2006.03.114, PII S0032386106005635
    • K. Haibach, A. Menner, R. Powell, and A. Bismarck Tailoring mechanical properties of highly porous polymer foams: silica particle reinforced polymer foams via emulsion templating Polymer 47 June 2006 4513 4519 (Pubitemid 43851039)
    • (2006) Polymer , vol.47 , Issue.13 , pp. 4513-4519
    • Haibach, K.1    Menner, A.2    Powell, R.3    Bismarck, A.4
  • 55
    • 0024645613 scopus 로고
    • Interlaminar fracture behavior and fiber bridging of glass-epoxy composite under mode i static and cyclic loadings
    • W. Hwang, and K.S. Han Interlaminar fracture behavior and fiber bridging of glass-epoxy composite under mode I static and cyclic loadings J Compos Mater 23 1989 396 430
    • (1989) J Compos Mater , vol.23 , pp. 396-430
    • Hwang, W.1    Han, K.S.2
  • 56
    • 0033222057 scopus 로고    scopus 로고
    • Influence of fibre volume fraction on the mode I interlaminar fracture toughness of a glass-fibre/vinyl ester composite
    • DOI 10.1023/A:1008973211347
    • P. Compston, and P.Y.B. Jar The influence of fibre volume fraction on the mode I interlaminar fracture toughness of a glass-fibre/vinyl ester composite Appl Compos Mater 6 1999 353 368 (Pubitemid 32081562)
    • (1999) Applied Composite Materials , vol.6 , Issue.6 , pp. 353-368
    • Compston, P.1    Jar, P.-Y.B.2
  • 58
    • 81855218069 scopus 로고    scopus 로고
    • Mode II interfacial toughening through discontinuous interleaves for damage suppression and control
    • M. Yasaee, I.P. Bond, R.S. Trask, and E.S. Greenhalgh Mode II interfacial toughening through discontinuous interleaves for damage suppression and control Compos-Part A: Appl Sci Manuf 43 2012 121 128
    • (2012) Compos-Part A: Appl Sci Manuf , vol.43 , pp. 121-128
    • Yasaee, M.1    Bond, I.P.2    Trask, R.S.3    Greenhalgh, E.S.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.