2
-
-
0003195882
-
Interlaminar Response of Composite Materials
-
Elsevier, Amsterdam
-
Pagano, N. J., Interlaminar Response of Composite Materials, Composite Materials Series, Vol. 5, Elsevier, Amsterdam, 1989.
-
(1989)
Composite Materials Series
, vol.5
-
-
Pagano, N.J.1
-
3
-
-
0029776094
-
Analysis of Local Delaminations Caused by Angle Ply Matrix Cracks
-
Salpekar, S. A., O'Brien, T. K., and Shivakumar, K. N., "Analysis of Local Delaminations Caused by Angle Ply Matrix Cracks," Journal of Composite Materials, Vol. 30, No. 4, 1996, pp. 418-440.
-
(1996)
Journal of Composite Materials
, vol.30
, Issue.4
, pp. 418-440
-
-
Salpekar, S.A.1
O'Brien, T.K.2
Shivakumar, K.N.3
-
4
-
-
0026171172
-
Design Approaches for Edge Delamination Resistance in Laminated Composites
-
Chan, W. C., "Design Approaches for Edge Delamination Resistance in Laminated Composites," Journal of Composites Technology and Research, Vol. 13, No. 2, 1991, pp. 91-96.
-
(1991)
Journal of Composites Technology and Research
, vol.13
, Issue.2
, pp. 91-96
-
-
Chan, W.C.1
-
5
-
-
0023829483
-
Delamination Durability of Composite Materials for Rotorcraft, NASA/Army Rotorcraft Technology
-
O'Brien, T. K., "Delamination Durability of Composite Materials for Rotorcraft," NASA/Army Rotorcraft Technology, NASA CP 2495, 1988, pp. 573-605.
-
(1988)
NASA CP
, vol.2495
, pp. 573-605
-
-
O'Brien, T.K.1
-
6
-
-
0022906917
-
Delamination Resistant Composite Concepts
-
edited by J. M. Whitney, American Society for Testing and Materials Special Technical Publication No. 893
-
Browning, C. E., and Schwartz, H. S., "Delamination Resistant Composite Concepts," Composite Materials: Testing and Design, edited by J. M. Whitney, American Society for Testing and Materials Special Technical Publication No. 893, 1986, pp. 256-265.
-
(1986)
Composite Materials: Testing and Design
, pp. 256-265
-
-
Browning, C.E.1
Schwartz, H.S.2
-
7
-
-
0001583520
-
Toughness Improved High Performance Torayca Prepreg T800H/3900 Series
-
Society for the Advancement of Material and Process Engineering, Covina, CA
-
Odagiri, N., Muraki, T., and Tobukuro, K., "Toughness Improved High Performance Torayca Prepreg T800H/3900 Series," Proc. 33rd Int. SAMPE Symp., Society for the Advancement of Material and Process Engineering, Covina, CA, 1988, pp. 272-283.
-
(1988)
Proc. 33rd Int. SAMPE Symp
, pp. 272-283
-
-
Odagiri, N.1
Muraki, T.2
Tobukuro, K.3
-
8
-
-
0014974517
-
The Influence of Stacking Sequence on Laminate Strength
-
doi:10.1177/002199837100500105
-
Pagano, N. J., and Pipes, R. B., "The Influence of Stacking Sequence on Laminate Strength," Journal of Composite Materials, Vol. 5, No. 1, 1971, pp. 50-57. doi:10.1177/002199837100500105
-
(1971)
Journal of Composite Materials
, vol.5
, Issue.1
, pp. 50-57
-
-
Pagano, N.J.1
Pipes, R.B.2
-
9
-
-
0022201794
-
-
American Society for Testing and Materials Special Technical Publication No. 876
-
Mignery, L. A., Tan, T. M., and Sun, C. T., The Use of Stitching to Suppress Delamination in Laminated Composites, American Society for Testing and Materials Special Technical Publication No. 876, 1985, pp. 371-385.
-
(1985)
The Use of Stitching to Suppress Delamination in Laminated Composites
, pp. 371-385
-
-
Mignery, L.A.1
Tan, T.M.2
Sun, C.T.3
-
10
-
-
0004035089
-
-
NASA TP-97-206234, Nov
-
Dow, M. B., and Dexter, H. B., "Development of Stitched, Braided and Woven Composite Structures in the ACT Program and Langley Research Center," NASA TP-97-206234, Nov. 1997.
-
(1997)
Development of Stitched, Braided and Woven Composite Structures in the ACT Program and Langley Research Center
-
-
Dow, M.B.1
Dexter, H.B.2
-
11
-
-
68149111850
-
-
AIAA Paper No. 86-0972
-
Howard, W. E., Gossard, T., Jr., and Jones, R. M., "Reinforcement of Composite Laminate Free-Edges with U-Shaped Caps," AIAA Paper No. 86-0972, 1986.
-
(1986)
Reinforcement of Composite Laminate Free-Edges with U-Shaped Caps
-
-
Howard, W.E.1
Gossard Jr., T.2
Jones, R.M.3
-
12
-
-
0024901976
-
Edge Delamination Resistance by a Critical Ply Termination
-
doi:10.4028/www.scientific.net/KEM.37.285
-
Chan, W. S., and Ochoa, O. O., "Edge Delamination Resistance by a Critical Ply Termination," Key Engineering Materials, Vol. 37, 1989, pp. 285-304. doi:10.4028/www.scientific.net/KEM.37.285
-
(1989)
Key Engineering Materials
, vol.37
, pp. 285-304
-
-
Chan, W.S.1
Ochoa, O.O.2
-
13
-
-
0024877008
-
Improved Impact and Delamination Resistance Through Interleafing
-
doi:10.4028/www.scientific.net/KEM.37.317
-
Masters, J. E., "Improved Impact and Delamination Resistance Through Interleafing," Key Engineering Materials, Vol. 37, 1989, pp. 317-348. doi:10.4028/www.scientific.net/KEM.37.317
-
(1989)
Key Engineering Materials
, vol.37
, pp. 317-348
-
-
Masters, J.E.1
-
14
-
-
30344485711
-
Mode I Delamination Fatigue Properties of Interlayer-Toughened CF/Epoxy Laminates
-
doi:10.1016/j.compscitech.2005.07.038
-
Hojo, M. Matsude, S., Tanaka, M., Ochiai, S., and Murakami, A., "Mode I Delamination Fatigue Properties of Interlayer-Toughened CF/Epoxy Laminates," Composites Science and Technology, Vol. 66, No. 5, 2006, pp. 665-675. doi:10.1016/j.compscitech.2005.07.038
-
(2006)
Composites Science and Technology
, vol.66
, Issue.5
, pp. 665-675
-
-
Hojo, M.1
Matsude, S.2
Tanaka, M.3
Ochiai, S.4
Murakami, A.5
-
15
-
-
33745734504
-
Method and Apparatus for Spinning,
-
U.S. Patent No. 2160962
-
Formhals, A., "Method and Apparatus for Spinning," U.S. Patent No. 2160962, 1939.
-
(1939)
-
-
Formhals, A.1
-
16
-
-
84870976424
-
Nanofiber Technology: Bridging the Gap Between Nano and Macro World
-
Kluwer Academic, Norwell, MA
-
Ko, F. K., "Nanofiber Technology: Bridging the Gap Between Nano and Macro World," NATO ASI on Nanoengineered Nanofibrous Materials, Kluwer Academic, Norwell, MA, 2004.
-
(2004)
NATO ASI on Nanoengineered Nanofibrous Materials
-
-
Ko, F.K.1
-
17
-
-
85076868815
-
Ultra Lightweight Materials for Bio-Inspired Microsystems
-
Japan Society of Composite Materials, Tokyo, July
-
Shivakumar, K., and Lingaiah, S., "Ultra Lightweight Materials for Bio-Inspired Microsystems," Proceedings of 16th International Conference on Composite Materials (ICCM-16), Japan Society of Composite Materials, Tokyo, July 2007.
-
(2007)
Proceedings of 16th International Conference on Composite Materials (ICCM-16)
-
-
Shivakumar, K.1
Lingaiah, S.2
-
18
-
-
68149098091
-
Electrospinning of Nylon-66 Polymer Nanofabrics
-
April
-
Lingaiah, S., Shivakumar, K. N., and Sadler, R. L., "Electrospinning of Nylon-66 Polymer Nanofabrics," AIAA 2008-1787, April 2008.
-
(2008)
AIAA
, vol.2008 -1787
-
-
Lingaiah, S.1
Shivakumar, K.N.2
Sadler, R.L.3
-
19
-
-
0032309782
-
Micromechanical Characterization of Local Deformation in Interlaminar-Toughened CFRP Laminates
-
doi:10.1016/S1359-835X(98)00067-0
-
Takeda, N., and Ogihara, S., "Micromechanical Characterization of Local Deformation in Interlaminar-Toughened CFRP Laminates," Composites, Part A: Applied Science and Manufacturing, Vol. 29A, No. 12, 1998, pp. 1545-1552. doi:10.1016/S1359-835X(98)00067-0
-
(1998)
Composites, Part A: Applied Science and Manufacturing
, vol.29 A
, Issue.12
, pp. 1545-1552
-
-
Takeda, N.1
Ogihara, S.2
-
20
-
-
64249103382
-
A Re-Examination of DMA Testing of Polymer Matrix Composites
-
doi:10.1177/ 0731684407087740
-
Swaminathan, G., and Shivakumar, K., "A Re-Examination of DMA Testing of Polymer Matrix Composites," Journal of Reinforced Plastics and Composites, Vol. 28, No. 8, 2008, pp. 979-994. doi:10.1177/ 0731684407087740
-
(2008)
Journal of Reinforced Plastics and Composites
, vol.28
, Issue.8
, pp. 979-994
-
-
Swaminathan, G.1
Shivakumar, K.2
-
21
-
-
0020829247
-
Low Velocity Transverse Impact Behavior of 8-Ply, Graphite-Epoxy Laminates
-
doi:10.1177/073168448300200401
-
Lal, K. M., "Low Velocity Transverse Impact Behavior of 8-Ply, Graphite-Epoxy Laminates," Journal of Reinforced Plastics and Composites, Vol. 2, No. 4, 1983, pp. 216-225. doi:10.1177/073168448300200401
-
(1983)
Journal of Reinforced Plastics and Composites
, vol.2
, Issue.4
, pp. 216-225
-
-
Lal, K.M.1
-
23
-
-
12344284295
-
Standard Test Method for Mode I Interlaminar Fracture Toughness of Unidirectional Fiber-Reinforced Polymer Matrix Composites
-
ASTM Standard D5528-94a, American Society for Testing and Materials, Philadelphia
-
ASTM Standard D5528-94a, "Standard Test Method for Mode I Interlaminar Fracture Toughness of Unidirectional Fiber-Reinforced Polymer Matrix Composites," Annual Book of ASTM Standards, Vol. 15.03, American Society for Testing and Materials, Philadelphia, 1999, pp. 283-292
-
(1999)
Annual Book of ASTM Standards
, vol.15 .03
, pp. 283-292
-
-
-
24
-
-
33845257283
-
Corrections Needed in Double Cantilever Beam Tests for Assessing the Interlaminar Failure of Fiber Composites
-
doi:10.1007/BF00730701
-
Hashemi, S., Kinloch, A. J., and Williams, J. G., "Corrections Needed in Double Cantilever Beam Tests for Assessing the Interlaminar Failure of Fiber Composites," Journal of Materials Science Letters, Vol. 8, No. 2, 1989, pp. 125-129. doi:10.1007/BF00730701
-
(1989)
Journal of Materials Science Letters
, vol.8
, Issue.2
, pp. 125-129
-
-
Hashemi, S.1
Kinloch, A.J.2
Williams, J.G.3
-
25
-
-
27444433506
-
Standard Test Method for Mode I Fatigue Delamination Growth Onset of Unidirectional Fiber-Reinforced Polymer Matrix Composites
-
ASTM Standard D6115-97, American Society for Testing and Materials, Philadelphia
-
ASTM Standard D6115-97, "Standard Test Method for Mode I Fatigue Delamination Growth Onset of Unidirectional Fiber-Reinforced Polymer Matrix Composites," Annual Book of ASTM Standards, Vol. 15.03, American Society for Testing and Materials, Philadelphia, 1999, pp. 327-332.
-
(1999)
Annual Book of ASTM Standards
, vol.15 .03
, pp. 327-332
-
-
-
26
-
-
68149096310
-
Standard Test Method for Assignment of the Glass Transition Temperature by Dynamic Mechanical Analysis
-
ASTM Standard E1640-04, American Society for Testing and Materials International, West Conshohocken, PA
-
ASTM Standard E1640-04, "Standard Test Method for Assignment of the Glass Transition Temperature by Dynamic Mechanical Analysis," Annual Book of ASTM Standards, Vol. 14.02, American Society for Testing and Materials International, West Conshohocken, PA, 2004, pp. 562-566.
-
(2004)
Annual Book of ASTM Standards
, vol.14 .02
, pp. 562-566
-
-
|